JPS53125925A - Austenite stainless steel excellent in resistibility to stress, corrosion, and crack and weldability when used in high temperature pure water - Google Patents
Austenite stainless steel excellent in resistibility to stress, corrosion, and crack and weldability when used in high temperature pure waterInfo
- Publication number
- JPS53125925A JPS53125925A JP4164477A JP4164477A JPS53125925A JP S53125925 A JPS53125925 A JP S53125925A JP 4164477 A JP4164477 A JP 4164477A JP 4164477 A JP4164477 A JP 4164477A JP S53125925 A JPS53125925 A JP S53125925A
- Authority
- JP
- Japan
- Prior art keywords
- resistibility
- weldability
- crack
- corrosion
- stress
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To provide an austenite stainless which is improved in the resistibility to stress, corrosion, crack and weldability in a high temperature pure water containing almost no chloride with simultaneous addition of Cr, Ni and Mo in a given quantity.
COPYRIGHT: (C)1978,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4164477A JPS53125925A (en) | 1977-04-11 | 1977-04-11 | Austenite stainless steel excellent in resistibility to stress, corrosion, and crack and weldability when used in high temperature pure water |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4164477A JPS53125925A (en) | 1977-04-11 | 1977-04-11 | Austenite stainless steel excellent in resistibility to stress, corrosion, and crack and weldability when used in high temperature pure water |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS53125925A true JPS53125925A (en) | 1978-11-02 |
Family
ID=12614036
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP4164477A Pending JPS53125925A (en) | 1977-04-11 | 1977-04-11 | Austenite stainless steel excellent in resistibility to stress, corrosion, and crack and weldability when used in high temperature pure water |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS53125925A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS57158359A (en) * | 1981-03-24 | 1982-09-30 | Nippon Stainless Steel Co Ltd | Corrosion resistant austenite stainless steel |
-
1977
- 1977-04-11 JP JP4164477A patent/JPS53125925A/en active Pending
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS57158359A (en) * | 1981-03-24 | 1982-09-30 | Nippon Stainless Steel Co Ltd | Corrosion resistant austenite stainless steel |
JPS5940901B2 (en) * | 1981-03-24 | 1984-10-03 | 日本ステンレス株式会社 | Corrosion-resistant austenitic stainless steel |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS52117224A (en) | Austenite stainless steel with excellent stress corrosion cracking res istance in water of high temperature and pressure | |
JPS54141310A (en) | Austentic stainless steel with superior corrosion resistance and hot workability | |
JPS5241113A (en) | Ferritic stainless steel having high toughness and high corrosion resi stance | |
JPS5260217A (en) | Watch case | |
JPS53125925A (en) | Austenite stainless steel excellent in resistibility to stress, corrosion, and crack and weldability when used in high temperature pure water | |
JPS5333916A (en) | Austenitic stainless steel with excellent intra- and intergranular stress corrosion cracking resistance | |
JPS5236512A (en) | Two phases (ferritic and austenitic) stainless steel of high hardness | |
JPS5346421A (en) | Seawater resistant stainless steel | |
JPS52119411A (en) | High carbon chromium-nickel steel | |
JPS5224914A (en) | Nickel-saving austenitic stainless steel | |
JPS51112719A (en) | Extra low carbon stainless steel with excellent corrosion resistance | |
JPS5360706A (en) | High performance turbo impeller | |
JPS52138420A (en) | Two-phased stainless steel | |
JPS52716A (en) | High chromium, low nickel, corrosion resistant twophase stainless stee l | |
JPS53144454A (en) | Deep drawn product of clad steel | |
JPS5439316A (en) | Mariensite stainless heat-resisting steel in which corrosion resistance is improved | |
JPS5433239A (en) | Corrosion resisting stainless steel having high temperature strength and its preparation | |
JPS52141414A (en) | Sea water corrosion resistant two phases stainless steel of high c# and low n# group | |
JPS52123917A (en) | 13cr stainless steel with excellent corrosion resistance | |
JPS52119414A (en) | Nickel saving type stainless steel having high stretchability | |
JPS5335617A (en) | Superhard stainless steel | |
JPS5361515A (en) | Production of watchcase | |
JPS5524960A (en) | Watch armor products | |
JPS52108314A (en) | Highly tough ferritic stainless steel having improved hydrogen-induced crack resistance | |
JPS5335613A (en) | Sheathing for watch |