JPS5311813A - Soft magnetic material - Google Patents
Soft magnetic materialInfo
- Publication number
- JPS5311813A JPS5311813A JP8561876A JP8561876A JPS5311813A JP S5311813 A JPS5311813 A JP S5311813A JP 8561876 A JP8561876 A JP 8561876A JP 8561876 A JP8561876 A JP 8561876A JP S5311813 A JPS5311813 A JP S5311813A
- Authority
- JP
- Japan
- Prior art keywords
- magnetic material
- soft magnetic
- permalloy
- substituting
- decreasing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To develop the soft magnetic material, having a superior magnetic flux density and magnetic permeability, decreasing the content of expensive Ni, by substituting a part of Fe in low Ni-Fe group Permalloy for Cu.
COPYRIGHT: (C)1978,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP51085618A JPS597780B2 (en) | 1976-07-20 | 1976-07-20 | soft magnetic material |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP51085618A JPS597780B2 (en) | 1976-07-20 | 1976-07-20 | soft magnetic material |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5311813A true JPS5311813A (en) | 1978-02-02 |
JPS597780B2 JPS597780B2 (en) | 1984-02-21 |
Family
ID=13863824
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP51085618A Expired JPS597780B2 (en) | 1976-07-20 | 1976-07-20 | soft magnetic material |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS597780B2 (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6274607U (en) * | 1985-10-30 | 1987-05-13 | ||
JPS62155093U (en) * | 1986-03-25 | 1987-10-01 | ||
JPH0383703A (en) * | 1989-08-26 | 1991-04-09 | Yoshida Kogyo Kk <Ykk> | Slider replenishing device |
-
1976
- 1976-07-20 JP JP51085618A patent/JPS597780B2/en not_active Expired
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6274607U (en) * | 1985-10-30 | 1987-05-13 | ||
JPS62155093U (en) * | 1986-03-25 | 1987-10-01 | ||
JPH0450233Y2 (en) * | 1986-03-25 | 1992-11-26 | ||
JPH0383703A (en) * | 1989-08-26 | 1991-04-09 | Yoshida Kogyo Kk <Ykk> | Slider replenishing device |
Also Published As
Publication number | Publication date |
---|---|
JPS597780B2 (en) | 1984-02-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5415126A (en) | Dc to dc converter | |
JPS5311813A (en) | Soft magnetic material | |
JPS53131222A (en) | Permanent magnet material | |
JPS5335618A (en) | High permeability amorphous alloy with high magnetic flux density and large rectangular form ratio | |
JPS5360303A (en) | Amorphous alloy of high magnetic permeability | |
JPS5423022A (en) | Amorphous alloy | |
JPS5375497A (en) | Fabrication of magnetic material | |
JPS53113216A (en) | High magnetic permeable amorphous alloy excellent in corrosion resistance | |
JPS5411823A (en) | Magnetic alloy | |
JPS5288796A (en) | Magnetic material block | |
JPS5343616A (en) | Corrosion resistant magnetic alloy | |
JPS53147617A (en) | Soft magnetic material | |
JPS5323608A (en) | Magnet ic recording medium | |
JPS5576041A (en) | Amorphous alloy | |
JPS543294A (en) | Soft magnetic material | |
JPS55107760A (en) | Fe-co type magnetic material | |
JPS52106500A (en) | Magnetic recording medium | |
JPS51112320A (en) | A magnetic head | |
JPS55107758A (en) | Fe-co type magnetic material | |
JPS5212498A (en) | Magnetic alloy | |
JPS5268998A (en) | Magnetic head | |
JPS5359160A (en) | Rotary yoke material for magnetic bearing | |
JPS5319720A (en) | Wireless type pen for data input | |
JPS5330800A (en) | Peparing magnetic thin film | |
JPS5295097A (en) | Magnetic recording material |