JPS5230877A - Method of coating protective film on inside of metal pipe - Google Patents
Method of coating protective film on inside of metal pipeInfo
- Publication number
- JPS5230877A JPS5230877A JP10738875A JP10738875A JPS5230877A JP S5230877 A JPS5230877 A JP S5230877A JP 10738875 A JP10738875 A JP 10738875A JP 10738875 A JP10738875 A JP 10738875A JP S5230877 A JPS5230877 A JP S5230877A
- Authority
- JP
- Japan
- Prior art keywords
- protective film
- metal pipe
- coating protective
- coating
- pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Moulding By Coating Moulds (AREA)
- Lining Or Joining Of Plastics Or The Like (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
Priority Applications (10)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10738875A JPS5230877A (en) | 1975-09-03 | 1975-09-03 | Method of coating protective film on inside of metal pipe |
SE7607204A SE7607204L (en) | 1975-07-04 | 1976-06-23 | KIT AND APPLIANCE FOR FITTING METAL PIPES WITH INTERNAL PROTECTIVE COVER |
FR7619636A FR2316526A1 (en) | 1975-07-04 | 1976-06-28 | METHOD AND APPARATUS FOR COVERING THE INTERIOR SURFACES OF METAL PIPES WITH A PROTECTIVE COATING |
AU15403/76A AU1540376A (en) | 1975-07-04 | 1976-06-29 | Lining the inside surfaces of metal tubes with protective coats |
DE19762629876 DE2629876A1 (en) | 1975-07-04 | 1976-07-02 | METHOD AND DEVICE FOR LINING THE INTERIOR SURFACES OF METAL PIPES |
IT5025476A IT1062597B (en) | 1975-07-04 | 1976-07-02 | DEVICE AND PROCEDURE FOR COATING THE INTERIOR OF METAL TUBES WITH A PROTECTION LAYER |
NL7607330A NL7607330A (en) | 1975-07-04 | 1976-07-02 | METHOD AND DEVICE FOR COVERING THE INTERIOR SURFACES OF METAL PIPES WITH PROTECTIVE LAYERS. |
NO762309A NO762309L (en) | 1975-07-04 | 1976-07-02 | |
GB2782576A GB1549063A (en) | 1975-07-04 | 1976-07-05 | Method and apparatus for lining the inside surfaces of metal tubes with protective coats |
US05/703,150 US4071641A (en) | 1975-07-04 | 1976-07-07 | Method for protective coating the inside of surfaces of metal tubes by vapor deposition |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10738875A JPS5230877A (en) | 1975-09-03 | 1975-09-03 | Method of coating protective film on inside of metal pipe |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5230877A true JPS5230877A (en) | 1977-03-08 |
Family
ID=14457854
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10738875A Pending JPS5230877A (en) | 1975-07-04 | 1975-09-03 | Method of coating protective film on inside of metal pipe |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5230877A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55132217A (en) * | 1979-04-02 | 1980-10-14 | Usui Internatl Ind Co Ltd | Method of coating resin film on inside surface of metal pipe of small diameter |
JPS59189976A (en) * | 1983-04-13 | 1984-10-27 | Daido Steel Co Ltd | Lining method for hollow pipe |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5082914A (en) * | 1973-11-21 | 1975-07-04 |
-
1975
- 1975-09-03 JP JP10738875A patent/JPS5230877A/en active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5082914A (en) * | 1973-11-21 | 1975-07-04 |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55132217A (en) * | 1979-04-02 | 1980-10-14 | Usui Internatl Ind Co Ltd | Method of coating resin film on inside surface of metal pipe of small diameter |
JPS59189976A (en) * | 1983-04-13 | 1984-10-27 | Daido Steel Co Ltd | Lining method for hollow pipe |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS51115517A (en) | Method of forming protective film | |
JPS51134334A (en) | Hot dip coating method for tinnlead alloy | |
JPS5250376A (en) | Method of forming metallic film | |
JPS51147542A (en) | Method of coating metal surface | |
JPS526776A (en) | Method of coating protective film on inside of metal pipe | |
EG12367A (en) | Protection of pipes by coating | |
JPS5394518A (en) | Method of preventing metal corrosion | |
JPS5230877A (en) | Method of coating protective film on inside of metal pipe | |
JPS51147541A (en) | Method of coating metal surface | |
JPS5226352A (en) | Method of bending of metal pipe | |
JPS51139873A (en) | Method of coating inside of pipe with tubular film | |
JPS51140839A (en) | Method of forming coatings of different metals | |
JPS51124166A (en) | Method of coating metal pipe | |
JPS5296961A (en) | Method of forming flange around metal pipe | |
ZA761028B (en) | Method of coating metal tubes | |
JPS523537A (en) | Method of preventing corrosion of metals | |
JPS51145438A (en) | Method of coating with metal | |
JPS5273137A (en) | Process for forming protective coating on zinc or its alloy | |
JPS51112442A (en) | Method of coating plastics with metal film coating | |
JPS51130441A (en) | Method of providing coating on metal surface | |
JPS5228574A (en) | Method of repairing damaged coating section on coated pipe | |
AU1704576A (en) | Coated metal pipes | |
JPS524573A (en) | Method of coating | |
JPS5273965A (en) | Method of hardening protective coating | |
JPS5257238A (en) | Method of coating metal |