JPS5228421A - Low alloy steel accompanying no stress relieving annealing crack at we lded parts - Google Patents
Low alloy steel accompanying no stress relieving annealing crack at we lded partsInfo
- Publication number
- JPS5228421A JPS5228421A JP10414175A JP10414175A JPS5228421A JP S5228421 A JPS5228421 A JP S5228421A JP 10414175 A JP10414175 A JP 10414175A JP 10414175 A JP10414175 A JP 10414175A JP S5228421 A JPS5228421 A JP S5228421A
- Authority
- JP
- Japan
- Prior art keywords
- alloy steel
- low alloy
- lded
- parts
- stress relieving
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To prevent reheating crack of low alloy steel by adjusting Mn, Cr, etc., formed during stress relieving annealing to eliminate residual stress which generates when subjected to welding heat cycle.
COPYRIGHT: (C)1977,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10414175A JPS5228421A (en) | 1975-08-29 | 1975-08-29 | Low alloy steel accompanying no stress relieving annealing crack at we lded parts |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10414175A JPS5228421A (en) | 1975-08-29 | 1975-08-29 | Low alloy steel accompanying no stress relieving annealing crack at we lded parts |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5228421A true JPS5228421A (en) | 1977-03-03 |
Family
ID=14372809
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10414175A Pending JPS5228421A (en) | 1975-08-29 | 1975-08-29 | Low alloy steel accompanying no stress relieving annealing crack at we lded parts |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5228421A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55107763A (en) * | 1979-02-14 | 1980-08-19 | Kawasaki Steel Corp | High tensile structural steel having superior strain relief treating embrittlement resistance |
JPS59170243A (en) * | 1983-03-14 | 1984-09-26 | Nippon Steel Corp | High-strength and high-toughness low alloy heat- resisting steel having improved characteristics resistant to creep embrittleness |
JPS61247402A (en) * | 1984-09-28 | 1986-11-04 | 韓國ジツパ−株式会社 | Apparatus for continuously assembling slider for fastener |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS4991012A (en) * | 1972-12-30 | 1974-08-30 |
-
1975
- 1975-08-29 JP JP10414175A patent/JPS5228421A/en active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS4991012A (en) * | 1972-12-30 | 1974-08-30 |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55107763A (en) * | 1979-02-14 | 1980-08-19 | Kawasaki Steel Corp | High tensile structural steel having superior strain relief treating embrittlement resistance |
JPS625986B2 (en) * | 1979-02-14 | 1987-02-07 | Kawasaki Steel Co | |
JPS59170243A (en) * | 1983-03-14 | 1984-09-26 | Nippon Steel Corp | High-strength and high-toughness low alloy heat- resisting steel having improved characteristics resistant to creep embrittleness |
JPS6116419B2 (en) * | 1983-03-14 | 1986-04-30 | Nippon Steel Corp | |
JPS61247402A (en) * | 1984-09-28 | 1986-11-04 | 韓國ジツパ−株式会社 | Apparatus for continuously assembling slider for fastener |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5228421A (en) | Low alloy steel accompanying no stress relieving annealing crack at we lded parts | |
JPS5224908A (en) | High strength aluminium alloy for casting | |
JPS56163244A (en) | Heat resistant austenite steel with superior hot workability and oxidation resistance | |
JPS51148611A (en) | Heat-treatment process of steel | |
JPS51140817A (en) | Martensite tool steel for hot forming | |
JPS529620A (en) | Low alloy steel having excellent stress relieving temper brittleness a t parts affected by welding heat | |
JPS51126917A (en) | Process for heat treatment of 12%cr steel axle material | |
JPS529619A (en) | Low alloy steel having excellent stress relieving temper brittleness a t parts affected by welding heat | |
JPS51137610A (en) | Precipitation hardening tool steel with high toughness suitable for hot forming | |
JPS54134017A (en) | Steel plate for enamelling | |
JPS5538957A (en) | Austenitic stainless cast steel | |
JPS51134307A (en) | Martensitic tool steel for hot working | |
JPS53125216A (en) | Low alloy steel of excellent cold forgeability for high strength bolt | |
JPS5222506A (en) | Process for removal of impurities of metals or alloys | |
JPS5397964A (en) | Preparation of electric welded steel tube | |
SU605844A1 (en) | Method of manufacturing sheets from high-alloy precipitation-hardening steels | |
JPS51145420A (en) | Weldable, high tensile cast steel for centrifugal casting | |
JPS5445612A (en) | Low-alloy steel free of post-stress-removing-anneal embrittlement in heat affected zone | |
JPS52120911A (en) | Prevention of crack at grain boundary at high temperature | |
JPS51145419A (en) | Weldable, high tensile cast steel for centrifugal casting | |
JPS51149817A (en) | Sprocket for vehicles | |
JPS5386620A (en) | Manufacture of ni-containing steel for low temperature use | |
JPS5573480A (en) | Sheet iron shell crack propagation preventive method | |
JPS51140818A (en) | Martensite tool steel for hot forming | |
JPS5395142A (en) | Welding method of low alloy steel |