- Publication number
- JPS4999546A JPS4999546A JP991673A JP991673A JPS4999546A JP S4999546 A JPS4999546 A JP S4999546A JP 991673 A JP991673 A JP 991673A JP 991673 A JP991673 A JP 991673A JP S4999546 A JPS4999546 A JP S4999546A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Compositions Of Macromolecular Compounds (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP991673A JPS5439856B2 (ja) | 1973-01-25 | 1973-01-25 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP991673A JPS5439856B2 (ja) | 1973-01-25 | 1973-01-25 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS4999546A true JPS4999546A (ja) | 1974-09-20 |
JPS5439856B2 JPS5439856B2 (ja) | 1979-11-30 |
Family
ID=11733408
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP991673A Expired JPS5439856B2 (ja) | 1973-01-25 | 1973-01-25 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5439856B2 (ja) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5162849A (ja) * | 1974-11-22 | 1976-05-31 | Mitsui Petrochemical Ind | Jushisoseibutsu |
JPS5262554A (en) * | 1975-11-15 | 1977-05-24 | Hinomoto Denki Kk | Barbers and beauty parlors appliance |
JPS5447752A (en) * | 1977-09-19 | 1979-04-14 | Phillips Petroleum Co | Method of improving processability of arylenesulfide polymer composition |
JPS5496558A (en) * | 1977-12-30 | 1979-07-31 | Gen Electric | Flameeretarded * reinforced thermoplastic composition of flexibility resistance |
JP2004331689A (ja) * | 2003-04-30 | 2004-11-25 | Kurabe Ind Co Ltd | 難燃性組成物 |
-
1973
- 1973-01-25 JP JP991673A patent/JPS5439856B2/ja not_active Expired
Cited By (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5162849A (ja) * | 1974-11-22 | 1976-05-31 | Mitsui Petrochemical Ind | Jushisoseibutsu |
JPS5313469B2 (ja) * | 1974-11-22 | 1978-05-10 | ||
JPS5262554A (en) * | 1975-11-15 | 1977-05-24 | Hinomoto Denki Kk | Barbers and beauty parlors appliance |
JPS557246B2 (ja) * | 1975-11-15 | 1980-02-23 | ||
JPS5447752A (en) * | 1977-09-19 | 1979-04-14 | Phillips Petroleum Co | Method of improving processability of arylenesulfide polymer composition |
JPS5496558A (en) * | 1977-12-30 | 1979-07-31 | Gen Electric | Flameeretarded * reinforced thermoplastic composition of flexibility resistance |
JPS6343425B2 (ja) * | 1977-12-30 | 1988-08-30 | Gen Electric | |
JP2004331689A (ja) * | 2003-04-30 | 2004-11-25 | Kurabe Ind Co Ltd | 難燃性組成物 |
Also Published As
Publication number | Publication date |
---|---|
JPS5439856B2 (ja) | 1979-11-30 |