JPH11169942A - Build-up line for stainless steel strip - Google Patents
Build-up line for stainless steel stripInfo
- Publication number
- JPH11169942A JPH11169942A JP33290797A JP33290797A JPH11169942A JP H11169942 A JPH11169942 A JP H11169942A JP 33290797 A JP33290797 A JP 33290797A JP 33290797 A JP33290797 A JP 33290797A JP H11169942 A JPH11169942 A JP H11169942A
- Authority
- JP
- Japan
- Prior art keywords
- steel strip
- stainless steel
- dust
- build
- line
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
Description
【0001】[0001]
【発明の属する技術分野】本発明は、冷間圧延前のステ
ンレス鋼帯にダミー材の接続や耳切り等の事前処理を施
すステンレス鋼帯のビルドアップラインに係わり、特
に、ステンレス鋼帯表面に付着した粉塵を除去して清浄
にすることのできるステンレス鋼帯のビルドアップライ
ンに関する。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a stainless steel strip build-up line in which a stainless steel strip before cold rolling is subjected to a pre-treatment such as connection of a dummy material and trimming of the stainless steel strip. The present invention relates to a stainless steel strip build-up line capable of removing adhered dust and cleaning the stainless steel strip.
【0002】[0002]
【従来の技術】一般に、熱延後のステンレス鋼帯は、焼
鈍及び酸洗が施された後(鋼種・用途によっては焼鈍が
省略されることもある)、センジミアミル等のリバース
圧延機で冷間圧延される。このリバース圧延では、コイ
ル状のステンレス鋼帯(以下、コイル)を巻き戻し、巻
き取りながらステンレス鋼帯を往復させて所定厚みにな
るまで冷間圧延を行う。従って、巻取機・巻戻機に巻き
ついているステンレス鋼帯の先後端部分は圧延ができ
ず、その分だけ歩留りが低下する。2. Description of the Related Art Generally, a stainless steel strip after hot rolling is subjected to annealing and pickling (the annealing may be omitted depending on the type of steel and application), and then cold-rolled by a reverse rolling mill such as a Sendzimir mill. Rolled. In this reverse rolling, a coiled stainless steel strip (hereinafter referred to as a coil) is rewound, and the stainless steel strip is reciprocated while being wound up to perform cold rolling until a predetermined thickness is obtained. Therefore, the front and rear end portions of the stainless steel strip wound around the winding machine / rewinding machine cannot be rolled, and the yield is reduced accordingly.
【0003】そこで、上記冷間圧延に先立ち、ビルドア
ップラインにおいて、ステンレス鋼帯の先後端にダミー
材を溶接したり、あるいはコイルを数巻分溶接してコイ
ルを大型化することにより、被圧延部分の長尺化が行わ
れる。しかしながら、鋼帯とダミー材、あるいは鋼帯同
士の厚みは必ずしも合致したものばかりでなく、溶接に
よる接続部に段差(以下、段付部)の生じている場合が
多い。段付部を有する状態で巻き取ると、該段付部で鋼
帯に折れが生じ、製品品質を損なうことになる。そのた
め、溶接後にこの段付け部を砥石で研削して段差をなく
すようにしている。Therefore, prior to the cold rolling, a dummy material is welded to the front and rear ends of the stainless steel strip in the build-up line, or the coil is welded by several turns to increase the size of the coil to be rolled. Part lengthening is performed. However, the thickness of the steel strip and the dummy material or the thickness of the steel strips do not always match each other, and there are many cases where a step (hereinafter referred to as a “stepped portion”) occurs in a connection portion by welding. If the steel strip is wound with the stepped portion, the steel strip is broken at the stepped portion, and the product quality is impaired. Therefore, after welding, the stepped portion is ground with a grindstone to eliminate the step.
【0004】また、ステンレス鋼帯の幅方向両端部(以
下、耳部)に微小な割れが存在すると、次工程の冷間圧
延でこの割れに起因して板の破断が生じるので、該ビル
ドアップラインでは、鋼帯の耳部を切断除去(サイドト
リミング、耳切り)したり、幅方向両端面を砥石で研削
することも行われている。このように、ビルドアップラ
インでは、溶接やサイドトリミング等の事前処理が冷間
圧延前に行われるが、この事前処理は、焼鈍・酸洗処理
の前に行われることもあり、あるいは後に行われること
もある。[0004] Further, if minute cracks are present at both ends (hereinafter referred to as "ears") in the width direction of the stainless steel strip, the sheet is broken in the next step of cold rolling due to the cracks. In the line, the edge of the steel strip is cut and removed (side trimming, edge cutting), and both end faces in the width direction are ground with a grindstone. Thus, in the build-up line, pre-processing such as welding and side trimming is performed before cold rolling, but this pre-processing may be performed before annealing or pickling or may be performed later. Sometimes.
【0005】[0005]
【発明が解決しようとする課題】上述したように、ステ
ンレス鋼帯のビルドアップラインでは、溶接による段差
(以下、溶接段差)除去のための研削や耳部を除去する
ためのサイドトリミングないし端面研削が行われる。ま
た、ビルドアップラインの入側では、溶接に先立って鋼
帯先後端部を切りそろえるためにシャーによる切断作業
も行われている。As described above, in the build-up line of a stainless steel strip, grinding for removing a step due to welding (hereinafter referred to as a welding step) and side trimming or edge grinding for removing a lug. Is performed. Also, on the entry side of the build-up line, a shearing operation is performed by a shear to trim the rear end of the steel strip prior to welding.
【0006】従って、上記研削作業や切断作業により切
断粉や研削粉が発生し、また、砥石からは砥粒が脱落す
る(以下、これらを総称して粉塵とする)。これらの粉
塵が鋼帯表面に付着したまま巻き取られると、鋼帯表面
には凹疵やすり疵が発生する。さらに、次工程の冷間圧
延においては、鋼帯表面に付着した前記粉塵が圧延ロー
ルに付着して圧延ロールを汚したり、圧延ロールに凹疵
を発生させたりする。このロール汚れは、圧延製品の表
面光沢を悪化させ、ロールの凹疵は、圧延製品に凸疵を
発生させることになる。[0006] Therefore, cutting powder and grinding powder are generated by the above-mentioned grinding and cutting operations, and abrasive grains fall off from the grindstone (hereinafter, these are collectively referred to as dust). If these dusts are wound up while adhering to the surface of the steel strip, dents and flaws are generated on the surface of the steel strip. Further, in the cold rolling in the next step, the dust adhering to the surface of the steel strip adheres to the rolling rolls, and contaminates the rolling rolls, or generates dents in the rolling rolls. The roll contamination deteriorates the surface gloss of the rolled product, and the roll dent causes the rolled product to have a convexity.
【0007】加えて、焼鈍・酸洗前のステンレス鋼帯を
ビルドアップラインで処理する場合には、鋼帯表面に酸
化スケールが存在していることから、研削や切断時の振
動、衝撃等により、鋼帯表面の微細な酸化スケール粉が
剥離・浮遊し、ビルドアップラインの各種ロールや装置
に付着して鋼帯表面に凹疵やすり疵を発生させたり、周
辺に酸化スケール粉が飛散して作業環境を悪化させると
いう問題もある。[0007] In addition, when a stainless steel strip before annealing and pickling is treated by a build-up line, because of the presence of oxide scale on the surface of the steel strip, vibrations and impacts during grinding and cutting may cause the steel strip. The fine oxide scale powder on the steel strip surface peels and floats and adheres to various rolls and equipment on the build-up line, causing dents and flaws on the steel strip surface, and the oxide scale powder scattered around. There is also a problem that the working environment is deteriorated.
【0008】なお、溶接段差を除去する研削装置には、
発生する粉塵を吸引除去するための集塵装置が設置され
ているが、発生する粉塵を完全に除去することは難し
く、また、上記した切断による粉塵や酸化スケール粉ま
でを除去するものではない。本発明は、かかる事情に鑑
みてなされたものであり、冷間圧延前のステンレス鋼帯
から研削粉や切断粉、あるいは酸化スケール粉等の粉塵
を除去し、表面を清浄にすることのできるステンレス鋼
帯のビルドアップラインを提供することを目的とする。[0008] The grinding device for removing the welding step includes:
Although a dust collecting device for sucking and removing the generated dust is installed, it is difficult to completely remove the generated dust, and it does not remove the dust and oxide scale powder by the above-mentioned cutting. The present invention has been made in view of such circumstances, and it is possible to remove dust such as grinding powder, cutting powder, or oxide scale powder from a stainless steel strip before cold rolling, and to clean the surface of the stainless steel strip. The purpose is to provide a build-up line for steel strip.
【0009】[0009]
【課題を解決するための手段】上記課題を解決するため
に、本発明はコイル状のステンレス鋼帯を巻き戻す巻戻
機と、該巻戻機により巻き戻されたステンレス鋼帯の先
後端を切断するシャーと、このシャーにより先後端を切
断されたステンレス鋼帯同士あるいはステンレス鋼帯と
ダミー材とを溶接する溶接機と、該溶接機による溶接で
生成する溶接部を研削する研削装置と、前記溶接機で溶
接されたステンレス鋼帯の耳部を切断するサイドトリマ
と、前記ステンレス鋼帯を巻き取る巻取機と、を備え、
前記研削装置には研削により発生する粉塵を吸引除去す
る集塵装置を設けてなるステンレス鋼帯のビルドアップ
ラインにおいて、前記巻取機の入側に、ステンレス鋼帯
の表面に付着する粉塵を除去する粉塵除去手段を設けた
ことを特徴とするものである。SUMMARY OF THE INVENTION In order to solve the above problems, the present invention provides a rewinding machine for rewinding a coiled stainless steel strip, and a front and rear end of the stainless steel strip rewinded by the rewinding machine. A shear to be cut, a welding machine for welding the stainless steel strips or the stainless steel strip and the dummy material whose front and rear ends have been cut by the shear, and a grinding device for grinding a weld generated by welding with the welder, A side trimmer for cutting the ears of the stainless steel strip welded by the welding machine, and a winding machine for winding the stainless steel strip,
In the stainless steel strip build-up line, which is provided with a dust collecting device that suctions and removes dust generated by grinding in the grinding device, dust adhering to the surface of the stainless steel strip is removed on the entrance side of the winder. And a dust removing means.
【0010】本発明では、巻取機の入側に粉塵除去手段
を設けるようにしたので、ステンレス鋼帯を巻き取る前
に、表面に付着した粉塵を確実に除去でき、従って巻取
時に凹疵やすり疵を発生させることはない。さらに、次
工程の冷間圧延まで前記粉塵が持ち越されることはな
く、従って冷間圧延工程でのロール疵や光沢不良等の発
生を防止することができる。In the present invention, the dust removing means is provided on the entrance side of the winding machine, so that the dust adhering to the surface can be surely removed before the stainless steel strip is wound, and therefore, the concave flaws are formed at the time of winding. No flaws are generated. Furthermore, the dust is not carried over until the next step of cold rolling, so that it is possible to prevent the occurrence of roll flaws, poor gloss and the like in the cold rolling step.
【0011】次に第2の本発明は、第1の発明に加え
て、前記シャーの出側に、ステンレス鋼帯の表面に付着
する粉塵を除去する粉塵除去手段を設けたことを特徴と
するものである。本発明では、上記作用に加えて、シャ
ー出側にも粉塵除去手段を設けるようにしたので、シャ
ー切断時に発生する粉塵や切断時の振動・衝撃により飛
散・浮遊する酸化スケール粉を除去できるので、確実に
巻取時や冷間圧延時の凹疵、すり疵、凸疵、光沢不良等
の発生を防止できると共に、作業環境を悪化させること
はない。Next, a second invention is characterized in that, in addition to the first invention, a dust removing means for removing dust adhering to the surface of the stainless steel strip is provided on the exit side of the shear. Things. In the present invention, in addition to the above operation, a dust removing means is also provided on the shed exit side, so that dust generated at the time of shear cutting and oxidized scale powder scattered / floating due to vibration / shock at the time of cutting can be removed. In addition, it is possible to reliably prevent the occurrence of dents, abrasions, projections, poor gloss, and the like during winding and cold rolling, and does not deteriorate the working environment.
【0012】次に、第3の本発明は、上記2つの発明の
粉塵除去手段を、ステンレス鋼帯表面をブラッシングす
る少なくとも上下一対のブラシロールと、該ブラシロー
ルによりステンレス鋼帯表面から剥離した粉塵を吸引す
る吸引装置とで形成させることを特徴とするものであ
る。本発明では、第1及び第2の発明の上記作用に加え
て、少なくとも上下一対のブラシロールで鋼帯を挟んで
表面をブラッシングするようにしたので、表面に付着し
た粉塵を確実に表面から剥離させることができ、さらに
吸引装置で吸引するようにしたので、剥離した粉塵及び
振動・衝撃により飛散・浮遊している粉塵を吸引除去で
きるようになる。Next, a third aspect of the present invention provides a dust removing means according to the above two aspects, comprising at least a pair of upper and lower brush rolls for brushing the surface of a stainless steel strip, and dust separated from the stainless steel strip surface by the brush rolls. And a suction device for sucking the air. In the present invention, in addition to the above-described functions of the first and second inventions, since the surface is brushed by sandwiching the steel strip with at least a pair of upper and lower brush rolls, dust adhering to the surface is reliably separated from the surface. In addition, since the suction is performed by the suction device, the separated dust and the dust scattered or floating due to vibration or impact can be suctioned and removed.
【0013】[0013]
【発明の実施の形態】以下、本発明の実施の形態を図面
を参照しつつ説明する。図1に本実施形態を示すステン
レス鋼帯のビルドアップラインを示す。2はステンレス
鋼帯1のコイルを巻き戻す巻戻機、3は巻き戻された鋼
帯1を搬送するとともに搬送方向を変えるためのデフレ
クトピンチロール、4は鋼帯1の先端部の形状を矯正す
るラフレベラー、5は鋼帯1の先後端部を切断するシャ
ー、6は例えば真空吸引方式によりライン外に用意され
ているダミー材をビルドアップラインに供給するダミー
材供給装置、7は鋼帯同士もしくは鋼帯とダミー材を接
続する溶接機である。8は、溶接機7による溶接で生じ
る溶接段差を砥石で研削して除去する研削装置であり、
研削時に発生する粉塵を吸引するための集塵装置9が設
けられている。すなわち、この集塵装置9は、研削装置
8を取り囲むように設けられた集塵フード9a、配管9
bを介してフード9aから大気と共に粉塵を吸引する吸
引ファン9d、フード9aとファン9dの途中に設けら
れたフィルター等の除塵機9c等から構成され、除塵後
の排気は大気中に放散される。Embodiments of the present invention will be described below with reference to the drawings. FIG. 1 shows a build-up line of a stainless steel strip according to the present embodiment. 2 is a rewinding machine for rewinding the coil of the stainless steel strip 1, 3 is a deflector pinch roll for transporting the unwound steel strip 1 and changing the transport direction, and 4 is the shape of the tip of the steel strip 1. Rough leveler for straightening, 5 is a shear for cutting the front and rear ends of the steel strip 1, 6 is a dummy material supply device for supplying a dummy material prepared outside the line to a build-up line by, for example, a vacuum suction method, and 7 is a steel strip. It is a welding machine that connects the steel strip and the dummy material to each other. 8 is a grinding device for grinding and removing a welding step generated by welding by the welding machine 7 with a grindstone,
A dust collecting device 9 for sucking dust generated during grinding is provided. That is, the dust collecting device 9 includes a dust collecting hood 9 a provided to surround the grinding device 8 and a pipe 9.
b, a suction fan 9d for sucking dust together with the atmosphere from the hood 9a, a dust remover 9c such as a filter provided in the middle of the hood 9a and the fan 9d, etc., and the exhaust gas after dust removal is radiated into the atmosphere. .
【0014】また、10は鋼帯1のセンタリングを行う
サイドガイド、11は鋼帯1の両耳部を切断するサイド
トリマ、12は鋼帯1を搬送するとともに搬送方向を変
えるデフレクトピンチロール、そして、13は鋼帯1を
コイル状に巻き取る巻取機である。以上のようにして構
成されるビルドアップラインにおいて、本発明の実施形
態では、シャー5の出側及びデフレクトピンチロール1
2の入側に粉塵除去手段14、15を設けている。この
粉塵除去手段は、鋼帯1の表面に付着した粉塵を剥離さ
せる少なくとも上下一対のブラシロール14a、15a
と、このブラシロール14a、15aで剥離した粉塵を
吸引する吸引装置14b、15bとから構成されてい
る。これらの吸引装置は前述した溶接段差を研削して除
去する際に発生する粉塵を除去する集塵装置9と同様の
構成でよいが、この実施形態では、集塵装置9のファン
9d、除塵機9c、及び配管9bの一部を共用とし、集
塵フードと一部の配管を新たに設けるようにした。Further, 10 is a side guide for centering the steel strip 1, 11 is a side trimmer for cutting both ears of the steel strip 1, 12 is a deflector pinch roll for transporting the steel strip 1 and changing the transport direction, Reference numeral 13 denotes a winder for winding the steel strip 1 into a coil. In the build-up line configured as described above, in the embodiment of the present invention, the output side of the shear 5 and the deflector pinch roll 1
Dust removing means 14 and 15 are provided on the input side of the second. This dust removing means includes at least a pair of upper and lower brush rolls 14a, 15a for removing dust adhering to the surface of the steel strip 1.
And suction devices 14b and 15b for sucking dust separated by the brush rolls 14a and 15a. These suction devices may have the same configuration as the dust collector 9 that removes dust generated when grinding and removing the welding step described above, but in this embodiment, the fan 9 d of the dust collector 9, 9c and a part of the pipe 9b are shared, and a dust collecting hood and a part of the pipe are newly provided.
【0015】次に本実施形態の作用について述べる。熱
間圧延されたステンレス鋼帯のコイルは、焼鈍・酸洗を
施された後、もしくは施される前に、ビルドアップライ
ンに搬送されてくる。巻戻機2で巻き戻されたステンレ
ス鋼帯1は、まず、先端部の巻きぐせをラフレベラー4
で矯正された後、先端部をシャー5により切断されて、
ダミー材供給装置6により供給されるダミー材(図示せ
ず)、もしくは先行ステンレス鋼帯の尾端(この尾端も
シャー5により切断されている)と溶接機7により溶接
される。シャー5による切断の際、切断屑が発生して鋼
帯1に付着したり飛散したりするが、粉塵除去手段14
によって除去される。また、酸洗されていない鋼帯であ
れば、ラフレベラー4による形状矯正及びシャー5によ
る切断の際、振動・衝撃により酸化スケールが飛散・浮
遊し、また、鋼帯1の表面に付着するが、これについて
も粉塵除去手段14で除去される。Next, the operation of the present embodiment will be described. The coil of the hot-rolled stainless steel strip is conveyed to the build-up line after or before being subjected to annealing and pickling. First, the stainless steel strip 1 unwound by the rewinding machine 2 is rolled up at a tip end by a rough leveler 4.
After the straightening, the tip is cut by the shear 5
The dummy material (not shown) supplied by the dummy material supply device 6 or the tail end of the preceding stainless steel strip (this tail end is also cut by the shear 5) is welded by the welding machine 7. At the time of cutting by the shear 5, cutting debris is generated and adheres or scatters to the steel strip 1.
Removed by Further, in the case of a steel strip that has not been pickled, at the time of shape correction by the rough leveler 4 and cutting by the shear 5, the oxide scale is scattered and floated by vibration and impact, and adheres to the surface of the steel strip 1, This is also removed by the dust removing means 14.
【0016】次に、溶接段差は研削装置8で除去される
と共に、この時発生する研削粉は集塵装置9で吸引除去
され、その後、鋼帯1はサイドトリマ12で耳切りされ
る。耳切り時にも切断粉や酸化スケールが発生するが、
これは粉塵除去手段15で除去される。さらに粉塵除去
手段14及び集塵装置9で取りきれなかった粉塵もここ
で除去される。次いで、ステンレス鋼帯1は、巻取機1
3でコイルに巻き取られるが、表面が清浄になっている
ので、巻き取り時に凹疵やすり疵が発生することはな
い。Next, the welding step is removed by the grinding device 8, and the grinding powder generated at this time is removed by suction by the dust collecting device 9, and then the steel strip 1 is trimmed by the side trimmer 12. Cutting powder and oxidized scale are also generated at the time of trimming,
This is removed by the dust removing means 15. Further, dust that cannot be removed by the dust removing means 14 and the dust collecting device 9 is also removed here. Next, the stainless steel strip 1 is
In step 3, the coil is wound around the coil, but since the surface is clean, no dents or scratches occur during winding.
【0017】ビルドアップラインを出たコイルを冷間圧
延する場合には、表面が清浄であるから、冷間圧延工程
においても疵が発生することはない。なお、粉塵除去手
段15をデフレクトピンチロール12の入側に設けた
が、これは鋼帯1の表面に粉塵が付着した状態でデフレ
クトピンチロール12に通すと、鋼帯1の表面に疵が発
生するから、これを防止するためである。When the coil that has exited the build-up line is cold-rolled, the surface is clean, so that no flaw occurs even in the cold rolling step. The dust removing means 15 is provided on the entry side of the deflector pinch roll 12. However, when the dust removal means 15 is passed through the deflector pinch roll 12 with dust adhered to the surface of the steel strip 1, the surface of the steel strip 1 is damaged. This is to prevent this from occurring.
【0018】本実施形態では、粉塵除去手段を、巻取機
の入側とシャーの出側に2ケ所に設置したが、巻取機の
入側のみに設けるようにしてもよい。要は、ステンレス
鋼帯を巻き取る前に表面の粉塵を除去しておけばよいの
である。なお、上記粉塵除去装置14、15は、集塵装
置9の吸引ファン9d、除塵機9cおよび配管9bの一
部を共用としたが、別々に設けてもよい。In this embodiment, the dust removing means is provided at two locations on the inlet side of the winder and on the outlet side of the shear. However, the dust removing means may be provided only on the inlet side of the winder. In short, it is only necessary to remove dust on the surface before winding the stainless steel strip. The dust removing devices 14 and 15 share a part of the suction fan 9d, the dust remover 9c and the pipe 9b of the dust collecting device 9, but may be provided separately.
【0019】また、上記ブラシロール14a、15a
は、これに限らず、例えばエアーブローによってもよ
い。The brush rolls 14a, 15a
However, the present invention is not limited to this. For example, air blowing may be used.
【0020】[0020]
【発明の効果】以上述べたように、本発明によるステン
レス鋼帯のビルドアップラインを採用すれば、切断や研
削により発生する粉塵がステンレス鋼帯の表面に付着し
ても、これを確実に除去することができ、従って、巻き
取り時、あるいは次工程の冷間圧延時に、凹疵、すり
疵、凸疵、光沢不良等を発生させることはない。As described above, if the stainless steel strip build-up line according to the present invention is adopted, even if dust generated by cutting or grinding adheres to the surface of the stainless steel strip, it is reliably removed. Therefore, no dents, scratches, protrusions, poor gloss, etc. are generated during winding or cold rolling in the next step.
【図1】本発明に係るステンレス鋼帯のビルドアップラ
インの一例を示す模式図である。FIG. 1 is a schematic view showing an example of a build-up line of a stainless steel strip according to the present invention.
1 ステンレス鋼帯 2 巻戻機 3 デフレクトピンチロール 4 ラフレベラー 5 シャー 6 ダミー材供給装置 7 溶接機 8 研削装置 9 集塵装置 10 サイドガイド 11 サイドトイマ 12 デフレクトピンチロール 13 巻取機 14、15 粉塵除去手段 DESCRIPTION OF SYMBOLS 1 Stainless steel strip 2 Rewinding machine 3 Deflection pinch roll 4 Rough leveler 5 Shear 6 Dummy material supply device 7 Welding machine 8 Grinding device 9 Dust collection device 10 Side guide 11 Side tomer 12 Deflection pinch roll 13 Winding machine 14, 15 Dust Removal means
Claims (3)
戻機と、該巻戻機により巻き戻されたステンレス鋼帯の
先後端を切断するシャーと、このシャーにより先後端を
切断されたステンレス鋼帯同士あるいはステンレス鋼帯
とダミー材とを溶接する溶接機と、該溶接機による溶接
で生成する溶接部を研削する研削装置と、前記溶接機で
溶接されたステンレス鋼帯の耳部を切断するサイドトリ
マと、前記ステンレス鋼帯を巻き取る巻取機と、を備
え、前記研削装置には研削により発生する粉塵を吸引除
去する集塵装置を設けてなるステンレス鋼帯のビルドア
ップラインにおいて、 前記巻取機の入側に、ステンレス鋼帯の表面に付着する
粉塵を除去する粉塵除去手段を設けたことを特徴とする
ステンレス鋼帯のビルドアップライン。1. A rewinding machine for rewinding a coiled stainless steel strip, a shear for cutting the front and rear ends of the stainless steel strip unwound by the rewinding machine, and a stainless steel for which the front and rear ends are cut by the shear. A welding machine for welding steel strips or a stainless steel strip to a dummy material, a grinding device for grinding a weld formed by welding by the welding machine, and cutting a lug of the stainless steel strip welded by the welding machine A side trimmer, and a winder for winding the stainless steel strip, and in the build-up line of the stainless steel strip provided with a dust collector for sucking and removing dust generated by grinding in the grinding device, A dust-up device for removing dust adhering to a surface of a stainless steel strip on an entrance side of the winder, wherein a build-up line for the stainless steel strip is provided.
表面に付着する粉塵を除去する粉塵除去手段を設けたこ
とを特徴とする請求項1記載のステンレス鋼帯のビルド
アップライン。2. The stainless steel strip build-up line according to claim 1, further comprising dust removal means for removing dust adhering to the surface of the stainless steel strip on the outlet side of the shear.
面をブラッシングする少なくとも上下一対のブラシロー
ルと、該ブラシロールによりステンレス鋼帯表面から剥
離した粉塵を吸引する吸引装置とを有することを特徴と
する請求項1又は2記載のステンレス鋼帯のビルドアッ
プライン。3. The dust removing means has at least a pair of upper and lower brush rolls for brushing the surface of the stainless steel strip, and a suction device for sucking dust separated from the surface of the stainless steel strip by the brush rolls. The build-up line of the stainless steel strip according to claim 1.