JPH1044175A - Mold structure used for manufacturing multilayer molded product - Google Patents
Mold structure used for manufacturing multilayer molded productInfo
- Publication number
- JPH1044175A JPH1044175A JP21693896A JP21693896A JPH1044175A JP H1044175 A JPH1044175 A JP H1044175A JP 21693896 A JP21693896 A JP 21693896A JP 21693896 A JP21693896 A JP 21693896A JP H1044175 A JPH1044175 A JP H1044175A
- Authority
- JP
- Japan
- Prior art keywords
- skin material
- mold
- resin
- molded product
- peripheral wall
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
【発明の属する技術分野】本発明は、熱可塑性樹脂単味
表面の所定部分のみに表皮材を被覆した表皮材と熱可塑
性樹脂単味とよりなる多層成形品を製造するための金型
構造に関する。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a mold structure for producing a multilayer molded product comprising a skin material in which only a predetermined portion of a surface of a thermoplastic resin is coated with a skin material and a thermoplastic resin alone. .
【0002】[0002]
【従来の技術】上記のような表面の所定部分のみを表皮
材で被覆した表皮材と熱可塑性樹脂単味との多層成形品
は、自動車のドアトリム、リヤトリム等の内装部品に用
いられている。このような多層成形品の製造は、熱可塑
性樹脂を射出成形等で予め成形しておき、該成形品に接
着剤等を用いて所定形状の表皮材を貼着するか、予め表
皮材をハードボード等に貼着させた部品を製作しておい
て、この部品をビス等を用いて該成形品に取り付ける方
法等があるが、このような方法では、後工程を要し手間
がかかると共にコストアップの要因となっていた。2. Description of the Related Art A multilayer molded product of a skin material in which only a predetermined portion of the surface is covered with a skin material and a plain thermoplastic resin is used for interior parts such as door trims and rear trims of automobiles. To manufacture such a multilayer molded product, a thermoplastic resin is preliminarily molded by injection molding or the like, and a skin material having a predetermined shape is adhered to the molded product using an adhesive or the like, or the skin material is hardened in advance. There is a method of manufacturing a part attached to a board or the like, and attaching this part to the molded product using a screw or the like. However, such a method requires a post-process, is time-consuming, and is costly. It was a factor of up.
【0003】そこで、このような多層成形品の製造につ
いて、改良すべく、例えば特開昭64−26414号公
報に記載されたものが提案されている。In order to improve the production of such a multilayer molded product, there has been proposed, for example, one described in Japanese Patent Application Laid-Open No. 64-26414.
【0004】これによると、未閉鎖のモールド成形用上
・下金型間に表皮材および溶融樹脂を供給し、上下金型
を閉じ、表皮材と熱可塑性樹脂単味からなる多層成形品
を製造するに際し、所定形状に裁断した表皮材を上また
は下金型上の所定位置に載置し、表皮材の裏面側のほぼ
中央部に溶着樹脂を供給することにより、所定部分のみ
を表皮材で被覆した表皮材と熱可塑性樹脂単味との多層
成形品を得るというものである。According to this, a skin material and a molten resin are supplied between an unclosed upper and lower mold for molding, and upper and lower molds are closed to produce a multilayer molded product composed of the skin material and a thermoplastic resin. In doing so, the skin material cut into a predetermined shape is placed at a predetermined position on the upper or lower mold, and the welding resin is supplied to a substantially central portion on the back side of the skin material, so that only the predetermined portion is made of the skin material. The purpose is to obtain a multilayer molded product of the coated skin material and the thermoplastic resin alone.
【0005】[0005]
【発明が解決しようとする課題】上記のような多層成形
品の製造に当たって、表皮材が熱可塑性樹脂単味の所定
位置を被覆するため、予め所定形状に裁断された表皮材
を下金型上の所定位置に位置決めした後、溶融樹脂を供
給し、型成形している必要があり、このために、上記の
多層成形品の製造に用いる金型構造は、図7乃至図9に
示すように、上下両金型1、2を有し、上金型1のキャ
ビティ面には、表皮材3が熱可塑性樹脂単味4を覆う見
切り線に相当する位置に小凸壁5が形成されており、小
凸壁5に対応する下金型2のキャビティ面には、木目込
み溝(凹条溝)6を有する駒7が設けられ、更には、下
金型2には、ピン8が2本設けられ、これらピン8及び
駒7は、下金型2の上下方向に摺動可能になっている。
また、下金型2には、不図示の樹脂通路と供給口が設け
られている。In the production of a multilayer molded article as described above, the skin material is cut into a predetermined shape in advance so that the skin material covers a predetermined position of the thermoplastic resin. It is necessary to supply the molten resin and perform the molding after the positioning at the predetermined position. For this reason, the mold structure used in the production of the above-mentioned multilayer molded product is as shown in FIGS. 7 to 9. A small convex wall 5 is formed on the cavity surface of the upper mold 1 at a position corresponding to a parting line where the skin material 3 covers the plain thermoplastic resin 4. On the cavity surface of the lower mold 2 corresponding to the small convex wall 5, a piece 7 having a wood groove (recessed groove) 6 is provided, and further, the lower mold 2 is provided with two pins 8. The pins 8 and the pieces 7 are slidable in the vertical direction of the lower mold 2.
The lower mold 2 is provided with a resin passage and a supply port (not shown).
【0006】[0006]
【0007】そして、多層成形品を製造する場合、次の
工程を経て行われる。[0007] When a multilayer molded article is manufactured, the following steps are performed.
【0008】所定寸法に裁断した表皮材3を、その表
面側を上にして、下金型2の凹溝6に沿って載置する
(図7示状態)。The skin material 3 cut to a predetermined size is placed along the concave groove 6 of the lower mold 2 with its surface side facing up (the state shown in FIG. 7).
【0009】次いで型締め装置の昇降機構(不図示)
を作動させて、上金型1を下降させて、下金型2との間
にキャビティを形成すべく、下金型2との間に一定の型
クリアランスを以て一旦停止する。該停止位置で、2本
のピン8を上方向に移動させ表皮材3を持ち上げて(図
8示状態)、上型キャビティ面の所定位置に軽く接触さ
せる。Next, an elevating mechanism (not shown) of the mold clamping device.
Is operated to lower the upper mold 1 and temporarily stop with a certain mold clearance between the upper mold 1 and the lower mold 2 in order to form a cavity with the lower mold 2. At the stop position, the two pins 8 are moved upward to lift the skin material 3 (the state shown in FIG. 8), and lightly contact a predetermined position on the upper mold cavity surface.
【0010】この状態で、溶融樹脂4aを押出し機等
溶融樹脂供給装置(不図示)により、下金型内に設けら
れた樹脂通路を通じて表皮材3の裏面側に供給を開始す
る。開始後一定時間内にピン8及び駒7を下金型2内に
引っ込める。In this state, the supply of the molten resin 4a to the back side of the skin material 3 is started by a molten resin supply device (not shown) such as an extruder through a resin passage provided in the lower mold. The pin 8 and the piece 7 are retracted into the lower mold 2 within a predetermined time after the start.
【0011】その後、上金型1を更に下降させること
により、表皮材3を押しながら溶融樹脂4aはキャビテ
ィ内に広げ、表皮材3と熱可塑性樹脂単味4とが一体と
なって賦形が完了する(図9示状態)。Thereafter, the upper mold 1 is further lowered to spread the molten resin 4a into the cavity while pressing the skin material 3, so that the skin material 3 and the thermoplastic resin plain 4 are integrally formed to form. This is completed (the state shown in FIG. 9).
【0012】次いで、冷却後、上金型1を上昇させ
て、上下両金型1,2を開き、成形された多層成形品1
0を取り出す。Next, after cooling, the upper mold 1 is raised, the upper and lower molds 1 and 2 are opened, and the formed multilayer molded article 1 is formed.
Take out 0.
【0013】しかしながら、多層成形品10は、熱可塑
性樹脂単味4の表面の一部に、表皮材2が被覆されて構
成されることとなり、この表皮材2は、熱可塑性樹脂単
味4の表面を装飾するために張設されるものであるか
ら、所定の位置に張設される必要があるが、成形に当た
って、表皮材3を下金型2のブランク形部2aに載置す
る場合、木目込み溝6を基準として、駒7上に単に載せ
るだけで、表皮材3の位置決めを行っていたために、所
定位置に載置するには、高度の熟練度を有する作業者で
も、非常に難しく、往々にしてずれてしまう場合があ
り、また成形時に、上金型1や溶融樹脂4aの移動によ
ってもずれてしまう場合があった。However, the multilayer molded article 10 has a structure in which a part of the surface of the thermoplastic resin 4 is covered with the skin material 2, and the skin material 2 is made of the thermoplastic resin 4. Since it is stretched to decorate the surface, it needs to be stretched at a predetermined position. However, when the skin material 3 is placed on the blank-shaped portion 2a of the lower mold 2 during molding, Since the skin material 3 has been positioned simply by being placed on the piece 7 with the wood grain groove 6 as a reference, it is very difficult for a worker having a high degree of skill to place the skin material 3 at a predetermined position. In some cases, the displacement may occur, and during molding, the displacement may also occur due to the movement of the upper mold 1 or the molten resin 4a.
【0014】このような場合を防止するために、表皮材
3の先端外周端部壁3aをセットラインとして、この先
端外周端部壁3aを下金型2の木目込み溝6の外側周壁
6aに当接して、位置決めするということが考えられる
が、この場合、上金型1及び下金型2によって形成する
キャビティが、表皮材3の先端外周部壁で仕切られてし
まい、溶融樹脂4aがキャビティ内を一様に供給され得
なくなるという新たな問題が起こってくる。In order to prevent such a case, the outer peripheral end wall 3a of the skin material 3 is set as a set line, and the outer peripheral end wall 3a is brought into contact with the outer peripheral wall 6a of the groove 6 in the lower mold 2. In this case, it is conceivable that the cavity is formed by the upper mold 1 and the lower mold 2, and is separated by the outer peripheral wall of the front end of the skin material 3. A new problem arises in that it cannot be supplied uniformly.
【0015】そこで、この発明は、このような事情に鑑
み、表皮材が金型内に確実に位置決めをされ、且つ溶融
樹脂のキャビティ内への供給が一様になされるようにし
た多層成形品を製造するための金型構造を提供すること
を目的としている。In view of such circumstances, the present invention is directed to a multilayer molded product in which a skin material is reliably positioned in a mold and a molten resin is uniformly supplied into a cavity. The purpose of the present invention is to provide a mold structure for manufacturing the same.
【0016】[0016]
【課題を解決するための手段】上記の目的を達成するた
め、請求項1記載の本発明金型構造は、上・下金型から
なる金型のうち、下金型上の所定位置に、所定形状に裁
断した1個又は複数個の表皮材を載置して、該表皮材の
裏面側より溶融樹脂を供給することにより、前記溶融樹
脂が形成する樹脂単味表面の一部を表皮材により被覆
し、その他の部分は樹脂単味をそのまま表出させてなる
多層成形品製造に用いる金型構造において、前記下金型
に、前記樹脂単味における表皮材の木目込み部に相当す
る位置に凹条溝を形成し、この凹条溝の外側周壁側に複
数個の突起を間欠的に形成し、これら突起の少なくとも
一部の先端に前記表皮材のセットライン側壁を当接させ
て、表皮材の位置決めを行うように構成したことを特徴
とする。In order to achieve the above object, a mold structure of the present invention according to claim 1 is provided in a predetermined position on a lower mold in a mold composed of an upper mold and a lower mold. One or a plurality of skin materials cut into a predetermined shape are placed, and a molten resin is supplied from the back surface side of the skin material, so that a part of the resin plain surface formed by the molten resin is covered with the skin material. In the mold structure used for the production of a multilayer molded product in which the plain resin is exposed as it is, the other portion is located at a position corresponding to the grained portion of the skin material in the plain resin in the lower mold. A plurality of projections are intermittently formed on the outer peripheral wall side of the concave groove, and a set line side wall of the skin material is brought into contact with at least a part of the protrusion to form a skin. It is characterized in that the material is positioned.
【0017】また、請求項2記載の本発明金型構造は、
上・下金型からなる金型のうち、下金型上の所定位置
に、所定形状に裁断した1個又は複数個の表皮材を載置
して、該表皮材の裏面側より溶融樹脂を供給することに
より、前記溶融樹脂が形成する樹脂単味表面の一部を表
皮材により被覆し、その他の部分は樹脂単味をそのまま
表出させてなる多層成形品製造に用いる金型構造におい
て、前記下金型に、前記樹脂単味における表皮材の木目
込み部に相当する位置に凹条溝を形成し、この凹条溝に
囲まれた中接ぎブランク形部を、前記下金型のキャビテ
ィ形成面よりも段差を設けて、前記凹条溝の外側周壁を
内側周壁より前記上金型側に突出させて突出部を形成し
たことを特徴とする。The mold structure of the present invention according to claim 2 is
Of the upper and lower molds, one or a plurality of skin materials cut into a predetermined shape are placed at predetermined positions on the lower mold, and molten resin is applied from the back surface side of the skin material. By supplying, a part of the resin plain surface formed by the molten resin is covered with a skin material, and the other part is a mold structure used for manufacturing a multilayer molded product in which the resin plain is exposed as it is. In the lower mold, a concave groove is formed at a position corresponding to a grained portion of the skin material in the resin plain, and a blank-shaped blank portion surrounded by the concave groove is formed into a cavity of the lower mold. The outer peripheral wall of the concave groove is protruded from the inner peripheral wall toward the upper mold side so as to form a projection.
【0018】従って、凹条溝の外側周壁に形成した複数
個の突起或いは突出部が、表皮材のセットライン側壁に
当接して、確実に金型上に位置決めされ、且つ、前記突
起は、凹条溝の外側周壁に間欠に形成されているため
に、表皮材のセットライン側壁と凹条溝の外側周壁との
間に間隔が形成されて、溶融樹脂のキャビティ内におけ
る流れが妨げられること無く、溶融樹脂がキャビティ内
全体に一様に供給されることとなる。Therefore, a plurality of protrusions or protrusions formed on the outer peripheral wall of the concave groove contact the set line side wall of the skin material, and are reliably positioned on the mold. Since the outer peripheral wall of the groove is formed intermittently, a space is formed between the set line side wall of the skin material and the outer peripheral wall of the concave groove, so that the flow of the molten resin in the cavity is not hindered. Thus, the molten resin is uniformly supplied to the entire inside of the cavity.
【0019】そして、本発明の金型構造によって成形さ
れた多層成形品において、前記樹脂単味の木目込み溝の
溝壁に複数個の薄肉部が間欠的に形成されることとな
り、この結果、樹脂単味の木目込み溝の溝壁における薄
肉部が、衝撃に対する応力集中の起点部として働くこと
となる。In the multilayer molded article formed by the mold structure of the present invention, a plurality of thin portions are intermittently formed on the groove wall of the wood grain groove of the resin alone. The thin portion of the groove wall of the simple grained groove serves as a starting point of stress concentration against impact.
【0020】そして、前記樹脂単味部は、ポリエチレ
ン、ポリスチレン、ポリ塩化ビニル、ポリアミド、ポリ
プロピレン等で構成されることが考えられる。It is conceivable that the plain resin portion is made of polyethylene, polystyrene, polyvinyl chloride, polyamide, polypropylene or the like.
【0021】表皮材は、クロス、PVCシート、発泡P
VCシート、ポリエチレンフォームシート、不織布等を
用い、また、ソフト感を向上するために、クロス+圧縮
ウレタン、クロス+ポリエチレンフォーム、ポリエチレ
ンフォーム+PVCシート等からなる2層構成のもの
や、クロス+ウレタン+不織布(裏面処理)或いはクロ
ス+ウレタン+TPOシート(裏面処理)等からなる3
層構成のものが使用されることも考えられる。The skin material is cloth, PVC sheet, foamed P
In order to use a VC sheet, a polyethylene foam sheet, a non-woven fabric, etc., and to improve the soft feeling, a two-layer structure composed of cloth + compressed urethane, cloth + polyethylene foam, polyethylene foam + PVC sheet, or cloth + urethane + 3 consisting of nonwoven fabric (backside treatment) or cloth + urethane + TPO sheet (backside treatment)
It is also conceivable that a layer configuration is used.
【0022】表皮材の裏面側より溶融樹脂を供給して、
上下金型により、互いに表皮材と樹脂単味が一体に形成
された多層成形品を成形する場合、前記下金型に対し
て、上金型を下降させ、上下金型の型クリアランスが所
定幅になると、上金型を一旦停止して、表皮材の裏面側
に溶融樹脂を投入し、一定量の投入が完了すると、上金
型を、型クリアランス=0の所まで再下降して、多層成
形品に成形するのである。そして、前記上金型が一旦停
止する上下金型の型クリアランスは、通常15mm〜2mm
が最適であり、上金型の一旦停止後の再下降時の下降ス
ピードは、毎秒4〜12mmの範囲で、最適値は、毎秒4
mmである。The molten resin is supplied from the back side of the skin material,
When molding a multilayer molded product in which the skin material and the resin material are integrally formed by the upper and lower molds, the upper mold is lowered with respect to the lower mold, and the mold clearance of the upper and lower molds becomes a predetermined width. , The upper mold is stopped once, molten resin is injected into the back side of the skin material, and after the fixed amount of injection is completed, the upper mold is lowered again to the mold clearance = 0, and the multilayer It is molded into a molded product. And the mold clearance of the upper and lower molds at which the upper mold temporarily stops is usually 15 mm to 2 mm.
Is optimal, and the lowering speed when lowering the upper mold once after stopping is in the range of 4 to 12 mm / sec, and the optimal value is 4 / sec.
mm.
【0023】成形地の表皮材のダメージ対策として、溶
融樹脂の温度は、通常、摂氏190度前後が良く、ま
た、予熱される金型温度は、摂氏30〜70度の範囲が
最適である。As a countermeasure against damage to the skin material of the molding ground, the temperature of the molten resin is usually good at around 190 degrees Celsius, and the temperature of the preheated mold is optimally in the range of 30 to 70 degrees Celsius.
【0024】[0024]
【発明の実施の形態】次に、本発明の実施の形態につい
て、図面を参照しながら説明する。Next, embodiments of the present invention will be described with reference to the drawings.
【0025】図1は、本発明の金型構造により製作しよ
うとしている多層成形品である自動車のドアトリム11
の斜視図である。このドアトリム11は、アームレスト
部12、ポケット部13或いはスピーカグリル取付部1
4等が配置されて、熱可塑性樹脂単味である基材15
と、この基材15の一部を装飾等の目的から中接表皮材
として覆うように張設された表皮材16とを有して構成
されている。FIG. 1 shows an automobile door trim 11 which is a multilayer molded product to be manufactured by the mold structure of the present invention.
It is a perspective view of. The door trim 11 includes an armrest portion 12, a pocket portion 13, or a speaker grill attachment portion 1.
4 and the like, and a base material 15 which is a thermoplastic resin alone.
And a skin material 16 stretched so as to cover a part of the base material 15 as an insulated skin material for the purpose of decoration or the like.
【0026】基材15は、ポリエチレン、ポリスチレ
ン、ポリ塩化ビニル、ポリアミド、ポリプロピレン等で
構成されている。The substrate 15 is made of polyethylene, polystyrene, polyvinyl chloride, polyamide, polypropylene or the like.
【0027】表皮材16は、クロス、PVCシート、発
泡PVCシート、ポリエチレンフォームシート、不織布
等を用い、また、ソフト感を向上するために、クロス+
圧縮ウレタン、クロス+ポリエチレンフォーム、ポリエ
チレンフォーム+PVCシート等からなる2層構成のも
のや、クロス+ウレタン+不織布(裏面処理)或いクロ
ス+ウレタン+TPOシート(裏面処理)等からなる3
層構成のものが使用されることがある。As the skin material 16, a cloth, a PVC sheet, a foamed PVC sheet, a polyethylene foam sheet, a non-woven fabric, or the like is used.
3 layers composed of compressed urethane, cloth + polyethylene foam, polyethylene foam + PVC sheet, etc., or cloth + urethane + non-woven fabric (backside treatment) or cloth + urethane + TPO sheet (backside treatment)
A layered structure may be used.
【0028】そして、この表皮材16は、略四辺形を呈
しており、外周縁部全周が基材15の木目込み溝17内
に木目込まれている。The skin material 16 has a substantially quadrilateral shape, and the entire periphery of the outer peripheral edge is cut into the wood cut groove 17 of the base material 15.
【0029】このように構成するドアトリム11は、本
実施の形態では、図2に示される金型構造により製作さ
れる。In the present embodiment, the door trim 11 configured as described above is manufactured by a mold structure shown in FIG.
【0030】すなわち、この金型構造は、図2に示すよ
うに、上金型21及び下金型22とから構成されてい
て、上金型21のキャビティ構成面21a側には、ドア
トリム11の外形を形成すべく、大凹部23が形成さ
れ、この大凹部23の略中央部位に、環状に形成された
小凸起24が下金型22側に突出するように形成されて
いる。下金型22のキャビティ構成面22aには、同様
に前記大凹部23と共にドアトリム11の外形を形成す
べく、大凸部25が形成されており、この大凸部25に
は、前記小凸起24に対応して、凹条溝26が環状に形
成されている。That is, as shown in FIG. 2, the mold structure is composed of an upper mold 21 and a lower mold 22, and the cavity trimming surface 21a of the upper mold 21 is In order to form the outer shape, a large concave portion 23 is formed, and an annular small protrusion 24 is formed at a substantially central portion of the large concave portion 23 so as to protrude toward the lower mold 22. Similarly, a large convex portion 25 is formed on the cavity forming surface 22a of the lower mold 22 so as to form the outer shape of the door trim 11 together with the large concave portion 23. The large convex portion 25 has the small convex portion. 24, the concave groove 26 is formed in an annular shape.
【0031】凹条溝26は、図3に示すように、その外
側周壁27側に、内側周壁28側に一定幅離間して突出
する複数個の突起29が間欠的に形成されている。As shown in FIG. 3, the recessed groove 26 has a plurality of projections 29 intermittently formed on the outer peripheral wall 27 side thereof at a predetermined distance from the inner peripheral wall 28 side.
【0032】そして、この突起29は、前記内側周壁2
8に囲まれた中接ぎブランク形部30に中接ぎ表皮材と
しての表皮材16を載置した際、該表皮材16の位置決
め部材となるものである。The projection 29 is provided on the inner peripheral wall 2.
When the skin material 16 is placed as a mid-skin material on the mid-strip blank shape portion 30 surrounded by the inner surface 8, the positioning member serves as a positioning member for the skin material 16.
【0033】すなわち、表皮材16は、例えば、略矩形
状を呈し、その4つの辺の側壁31〜34をすべての突
起29に当接して、表皮材16の位置決めをする場合も
考えられるが、表皮材16の裁断寸法の誤差等を吸収す
るために、例えば、互いに交わる2辺の側壁31,32
を、表皮材16のセットライン側壁として、これに対向
する突起29に当接させて、表皮材16の位置決めを行
うように構成されている(図4参照)。That is, the skin material 16 has, for example, a substantially rectangular shape, and the side walls 31 to 34 of the four sides abut on all the projections 29 to position the skin material 16. In order to absorb an error or the like in the cut size of the skin material 16, for example, two side walls 31 and 32 intersecting each other are used.
Are set as the set line side walls of the skin material 16 and are brought into contact with the projections 29 facing the set line side walls to position the skin material 16 (see FIG. 4).
【0034】また、前記中接ぎブランク形部30は、図
5に示すように、下金型22の一般キャビティ形成面3
5より、A分だけ段差を設けて、凹条溝26の外側周壁
27を、内側周壁28より上金型22側に突出36させ
てある。この結果、中接ぎブランク形部30は、突出部
36に囲まれることとなり、表皮材16のセット性を向
上させている。Further, as shown in FIG. 5, the intermediate joint blank-shaped portion 30 is formed on the general cavity forming surface 3 of the lower mold 22.
5, the outer peripheral wall 27 of the concave groove 26 protrudes 36 from the inner peripheral wall 28 toward the upper mold 22 with a step A provided. As a result, the inscribed blank-shaped part 30 is surrounded by the protruding part 36, and the setting property of the skin material 16 is improved.
【0035】このように構成する金型構造によって、ド
アトリム11を製作する場合、まず、図2に示すよう
に、下金型22に対して、上金型21が型開き(未閉鎖
状態)した状態で、クロス原反等を所定寸法に裁断して
形成された表皮材16を、下金型22の中接ぎブランク
形30上に載置する。この時、外側周壁27の突出部3
6が、表皮材16を確実に中接ぎブランク形部30に案
内する。そして、表皮材16のセットライン側壁31,
32を突起29の先端に当接させて、表皮材16を中接
ぎブランク形部の所定位置にセット載置する。When the door trim 11 is manufactured by using the thus-configured mold structure, the upper mold 21 is first opened (not closed) with respect to the lower mold 22 as shown in FIG. In this state, the skin material 16 formed by cutting the cloth cloth or the like into a predetermined size is placed on the intermediate blank 30 of the lower mold 22. At this time, the protrusion 3 of the outer peripheral wall 27
6 ensures that the skin material 16 is guided to the intermediate blank shape part 30. Then, the set line side wall 31, of the skin material 16,
32 is brought into contact with the tip of the projection 29, and the skin material 16 is set and placed at a predetermined position of the blank-shaped portion with the middle contact.
【0036】次に、この状態より、上金型21を下金型
22方向に下降させて、型クリアランスが所定幅になる
と、上金型21を一旦停止して、ゲート40から溶融樹
脂を投入する。この上金型21の一旦停止時の型クリア
ランスCは、15mm〜2mmが最適である。また、溶融樹
脂温度は、通常、摂氏190度前後にして、樹脂温度に
よる表皮材16のダメージ対策をしており、溶融樹脂の
MI値は、80〜120の範囲を選ぶこととなる。更
に、上下金型21,22は、適度に予熱されていること
が望ましく、通常、予熱される金型温度は、摂氏30〜
70度の範囲が最適である。Next, from this state, the upper mold 21 is lowered in the direction of the lower mold 22, and when the mold clearance reaches a predetermined width, the upper mold 21 is stopped once and molten resin is injected from the gate 40. I do. The optimal mold clearance C when the upper mold 21 is temporarily stopped is 15 mm to 2 mm. In addition, the temperature of the molten resin is usually set at around 190 degrees Celsius to prevent the skin material 16 from being damaged by the resin temperature, and the MI value of the molten resin is selected in the range of 80 to 120. Further, it is desirable that the upper and lower molds 21 and 22 are appropriately preheated. Usually, the temperature of the preheated mold is 30 to 100 degrees Celsius.
A range of 70 degrees is optimal.
【0037】溶融樹脂が一定量投入されると、その投入
は完了し、上金型21は、型クリアランス=0のところ
まで再下降させて型閉めを行ない、溶融樹脂をキャビテ
ィ内に充満させて、ドアトリム11を形作る。この時、
表皮材16のセットライン側壁31、32が他の辺3
3,34と共に、上金型21の小凸起24によって、凹
状溝26内に押し込まれて、凹状溝26が形成するドア
トリム11の基材15側の木目込み溝17内に木目込み
処理されて(図6参照)、見栄えを向上させることとな
る。When a fixed amount of the molten resin is charged, the charging is completed, and the upper mold 21 is lowered again to the mold clearance = 0 to close the mold, thereby filling the cavity with the molten resin. , Forming the door trim 11. At this time,
The set line side walls 31 and 32 of the skin material 16 are the other sides 3
3 and 34 are pressed into the concave groove 26 by the small protrusion 24 of the upper mold 21, and are subjected to the wood graining process into the wood grained groove 17 on the base material 15 side of the door trim 11 formed by the concave groove 26 (FIG. 6), and the appearance is improved.
【0038】そして、突起29は、凹条溝26の外側周
壁27に間欠に複数個形成されているために、表皮材1
6のセットライン側壁31,32と凹条溝26の外側周
壁27との間に間隔が形成されて、溶融樹脂のキャビテ
ィ内における流れを妨げること無く、溶融樹脂がキャビ
ティ内全体に一様に供給されることとなる。Since the plurality of projections 29 are intermittently formed on the outer peripheral wall 27 of the concave groove 26, the surface material 1
6 is formed between the set line side walls 31 and 32 and the outer peripheral wall 27 of the concave groove 26 so that the molten resin is uniformly supplied to the entire cavity without obstructing the flow of the molten resin in the cavity. Will be done.
【0039】そして、上下金型21,22は、型閉め後
そのまま一定時間の冷却工程を経て、再び、上金型21
を上昇させて、凝固したドアトリム11をキャビティ内
から取り出して、成形工程を終了する。After the molds are closed, the upper and lower molds 21 and 22 undergo a cooling process for a certain period of time as they are, and then again the upper mold 21.
And the solidified door trim 11 is taken out of the cavity, and the molding step is completed.
【0040】このように成形されたドアトリム11は、
図6に示すように、その基材15の木目込み溝17の外
側(基材15の裏側表出部)には、下金型22の突起2
9によって、凹部38が形成され、木目込み溝壁17a
に薄肉部39が存在することとなる。The door trim 11 thus formed is
As shown in FIG. 6, the protrusions 2 of the lower mold 22 are provided outside the wood groove 17 of the base material 15 (the exposed portion on the back side of the base material 15).
9, a recess 38 is formed, and the wood grain groove wall 17a is formed.
The thin portion 39 exists.
【0041】この薄肉部39は、応力集中の起点となっ
て、自動車の側突等による衝撃吸収の効果を発揮する。The thin portion 39 serves as a starting point of stress concentration and exhibits an effect of absorbing a shock due to a side collision of an automobile.
【0042】[0042]
【発明の効果】以上、説明したように、本発明において
は、木目込み溝を形成する凹条溝の外側周壁に形成した
複数個の突起或いは突出部が、表皮材のセットライン側
壁に当接して、表皮材を確実に金型上に位置決めするこ
ととなり、表皮材のセット性を向上させることができ、
しかもこのセット性向上に特別な装置を使用することが
ないので、金型コストの軽減を図ることができる。As described above, according to the present invention, a plurality of projections or protrusions formed on the outer peripheral wall of the groove forming the wood grain groove contact the set line side wall of the skin material. , The skin material is reliably positioned on the mold, and the setability of the skin material can be improved,
In addition, since no special device is used for improving the setability, the cost of the mold can be reduced.
【0043】また、前記突起は、凹条溝の外側周壁に間
欠に形成されているために、溶融樹脂のキャビティ内に
おける流れを妨げること無く、溶融樹脂がキャビティ内
全体に一様に供給されることとなる。この結果、成形さ
れた多層成形品は、樹脂単味部も所定の厚さのものが得
られ、歩留まり率を向上させて、この面からも、コスト
低減に寄与することとなる。Further, since the projection is formed intermittently on the outer peripheral wall of the concave groove, the molten resin is uniformly supplied to the entire cavity without obstructing the flow of the molten resin in the cavity. It will be. As a result, the molded multi-layered product has a single resin portion having a predetermined thickness, thereby improving the yield rate and contributing to the cost reduction from this aspect as well.
【0044】更に、本発明の金型構造によって成形され
た多層成形品において、前記樹脂単味の木目込み溝の溝
壁に複数個の薄肉部を間欠的に形成されることとなり、
この結果、樹脂単味の木目込み溝の溝壁における薄肉部
が、衝撃に対する応力集中の起点部として働くこととな
る。Further, in the multilayer molded article molded by the mold structure of the present invention, a plurality of thin portions are intermittently formed on the groove wall of the resin-like wood grain groove,
As a result, the thin portion of the groove wall of the wood grain groove of the resin alone functions as a starting point of stress concentration with respect to impact.
【図1】本発明の金型構造により成形される自動車用ド
アトリムの正面斜視図である。FIG. 1 is a front perspective view of an automobile door trim formed by a mold structure of the present invention.
【図2】本発明の実施の形態による多層成形品の金型構
造を示す断面図である。FIG. 2 is a sectional view showing a mold structure of a multilayer molded product according to the embodiment of the present invention.
【図3】図1に示す下金型の中接ぎブランク形部付近を
拡大して示す平面図である。FIG. 3 is an enlarged plan view showing the vicinity of an intermediate blank-shaped portion of the lower mold shown in FIG. 1;
【図4】図3の円内を拡大して示す斜視図である。FIG. 4 is an enlarged perspective view showing the inside of a circle of FIG. 3;
【図5】図2の中接ぎブランク形部付近を拡大して示す
断面図である。FIG. 5 is an enlarged cross-sectional view showing the vicinity of a middle blank portion of FIG. 2;
【図6】図1のI−I線に沿って切断して示す断面斜視
図である。FIG. 6 is a cross-sectional perspective view taken along line II of FIG. 1;
【図7】従来の多層成形品の金型構造を示す断面図で、
表皮材を下金型に載置した場合の型開き状態を示してい
る。FIG. 7 is a cross-sectional view showing a mold structure of a conventional multilayer molded product,
The mold opening state when the skin material is placed on the lower mold is shown.
【図8】同じく、表皮材裏面に溶融樹脂を投入すべく、
表皮材を所定位置上金型側に持ち上げた場合の型開き状
態を示している。FIG. 8 Similarly, in order to put molten resin on the back surface of the skin material,
The mold opening state when the skin material is lifted to the mold side above a predetermined position is shown.
【図9】同じく、型閉め状態を示している。FIG. 9 also shows a mold closed state.
11 ドアトリム(多層成形品) 15 基材(樹脂単味部) 16 表皮材 17 木目込み溝 21 上金型 22 下金型 26 凹条溝 27 外側周壁 28 内側周壁 29 突起 30 中接ぎブランク形部 31、32 セットライン側壁 DESCRIPTION OF SYMBOLS 11 Door trim (multilayer molded product) 15 Substrate (plain resin part) 16 Skin material 17 Wood grain groove 21 Upper die 22 Lower die 26 Concave groove 27 Outer peripheral wall 28 Inner peripheral wall 29 Projection 30 Middle joint blank part 31, 32 set line side wall
Claims (2)
上の所定位置に、所定形状に裁断した1個又は複数個の
表皮材を載置して、該表皮材の裏面側より溶融樹脂を供
給することにより、前記溶融樹脂が形成する樹脂単味表
面の一部を表皮材により被覆し、その他の部分は樹脂単
味をそのまま表出させてなる多層成形品製造に用いる金
型構造において、前記下金型に、前記樹脂単味における
表皮材の木目込み部に相当する位置に凹条溝を形成し、
この凹条溝の外側周壁側に複数個の突起を間欠的に形成
し、これら突起の少なくとも一部の先端に前記表皮材の
セットライン側壁を当接させて、表皮材の位置決めを行
うように構成したことを特徴とする多層成形品製造に用
いる金型構造。1. One or a plurality of skin materials cut into a predetermined shape are placed at predetermined positions on a lower die among upper and lower dies, and a back surface of the skin material is provided. By supplying the molten resin from the side, a part of the resin plain surface formed by the molten resin is covered with a skin material, and the other part is used for the production of a multilayer molded product in which the resin plain is exposed as it is. In the mold structure, in the lower mold, a concave groove is formed at a position corresponding to a grained portion of the skin material in the resin alone,
A plurality of protrusions are formed intermittently on the outer peripheral wall side of the concave groove, and the set line side wall of the skin material is brought into contact with at least a part of the protrusion to position the skin material. A mold structure used for manufacturing a multilayer molded product, characterized in that it is constituted.
上の所定位置に、所定形状に裁断した1個又は複数個の
表皮材を載置して、該表皮材の裏面側より溶融樹脂を供
給することにより、前記溶融樹脂が形成する樹脂単味表
面の一部を表皮材により被覆し、その他の部分は樹脂単
味をそのまま表出させてなる多層成形品製造に用いる金
型構造において、前記下金型に、前記樹脂単味における
表皮材の木目込み部に相当する位置に凹条溝を形成し、
この凹条溝に囲まれた中接ぎブランク形部を、前記下金
型のキャビティ形成面よりも段差を設けて、前記凹条溝
の外側周壁を内側周壁より前記上金型側に突出させて突
出部を形成したことを特徴とする多層成形品製造に用い
る金型構造。 【0001】2. One or a plurality of skin materials cut into a predetermined shape are placed at predetermined positions on a lower die among upper and lower dies, and a back surface of the skin material is provided. By supplying the molten resin from the side, a part of the resin plain surface formed by the molten resin is covered with a skin material, and the other part is used for the production of a multilayer molded product in which the resin plain is exposed as it is. In the mold structure, in the lower mold, a concave groove is formed at a position corresponding to a grained portion of the skin material in the resin alone,
By providing a step between the cavity forming surface of the lower mold and the outer peripheral wall of the concave groove so that the outer peripheral wall of the concave groove protrudes toward the upper mold side from the inner peripheral wall, by forming the middle joint blank portion surrounded by the concave groove. A mold structure used for manufacturing a multilayer molded product, wherein a protrusion is formed. [0001]