JPH08257491A - Two-tone color coating method - Google Patents

Two-tone color coating method

Info

Publication number
JPH08257491A
JPH08257491A JP6584795A JP6584795A JPH08257491A JP H08257491 A JPH08257491 A JP H08257491A JP 6584795 A JP6584795 A JP 6584795A JP 6584795 A JP6584795 A JP 6584795A JP H08257491 A JPH08257491 A JP H08257491A
Authority
JP
Japan
Prior art keywords
coating
color
tone color
stripe
printed
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP6584795A
Other languages
Japanese (ja)
Other versions
JP2900231B2 (en
Inventor
Ryuichi Akita
龍一 秋田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Honda Motor Co Ltd
Original Assignee
Honda Motor Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Honda Motor Co Ltd filed Critical Honda Motor Co Ltd
Priority to JP7065847A priority Critical patent/JP2900231B2/en
Publication of JPH08257491A publication Critical patent/JPH08257491A/en
Application granted granted Critical
Publication of JP2900231B2 publication Critical patent/JP2900231B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

PURPOSE: To remarkably reduce the total coating time by sticking a solid sticking stripe printed with the unicolor paint of a two-tone color on a substrate and then coating the substrate with a body color as another color paint of the two-tone color. CONSTITUTION: A solid sticking stripe 2 printed with a two-tone color printed part 5 and with a masking application tape 7 stuck to the upper face is stuck to the surface of a pretreated synthetic-resin substrate 1, a primer 8 is applied on the substrate 1 surface, and a body color 9 as another part of the two-tone color is applied on the primer 8. The tape 7 on the stripe 2 is released, a clear overcoat is applied on the stripe 2 and the entire surface of the body color 9 while the applied body color 9 is still wet, and the coated surface is finished, cured and dried. Consequently, the coating of the two-tone color part and the application of the clear overcoat are respectively omitted, and only one finish- drying is needed.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【産業上の利用分野】本発明は、自動二輪車用部品等
の、合成樹脂製基材に施される、オーバコートクリヤー
仕様によるツートン・カラー塗装方法に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a two-tone color coating method applied to a synthetic resin base material such as a motorcycle part by overcoat clear specification.

【0002】[0002]

【従来の技術】一般に自動二輪車のサイドカバー、燃料
タンク等の構成部品の外表面には、アクセントとして、
あるいは意匠効果を高めるためにツートン・カラー塗装
が施され、さらに品質を高め、高級感を彷彿させ、外観
上の体裁を高めるために、ツートン・カラー塗装上にオ
ーバコートクリヤー塗装を施すようにした、オーバコー
トクリヤー仕様によるツートン・カラー塗装が採用され
ている。
2. Description of the Related Art Generally, as an accent on outer surfaces of components such as motorcycle side covers and fuel tanks,
Or, two-tone color coating is applied to enhance the design effect, and in order to further improve quality, reminding a high-class feeling, and to enhance the appearance, an overcoat clear coating is applied on the two-tone color coating. , Two-tone color coating with overcoat clear specifications is used.

【0003】ところで従来のオーバコートクリヤー仕様
によるツートン・カラー塗装方法は、概ね次の工程より
なっているのが一般的であり、この工程を図9〜13を
参照して説明する。
By the way, the conventional two-tone color coating method according to the overcoat clear specification generally includes the following steps, which will be described with reference to FIGS.

【0004】図9は従来方法の工程を示すブロック図、
図9〜13はその工程順を示す、塗装部の断面図であ
る。
FIG. 9 is a block diagram showing the steps of a conventional method,
9 to 13 are cross-sectional views of the coating section showing the order of the steps.

【0005】.前処理ラインで、前処理を行い、水切
り乾燥した合成樹脂製基材01を、塗装ラインへと移送
し、そこで清掃処理した後、前記基材01の表面にプラ
イマー(下塗り塗料)08を塗装(第1回塗装)して、
そのプライマー08の全面にツートン・カラー部分05
を塗装し、さらにその上面にクリヤー012を塗装(第
2,3回塗装)した後、硬化乾燥(第1回乾燥)を行な
う(図10参照)。
.. The pretreatment line is pretreated in the pretreatment line, the drained and dried synthetic resin base material 01 is transferred to a coating line, where it is cleaned, and then a primer (undercoat paint) 08 is applied to the surface of the base material 01 ( After the first painting)
Two-tone color part 05 on the entire surface of the primer 08
Is coated, and clear 012 is further coated on the upper surface thereof (second and third coatings), followed by curing and drying (first drying) (see FIG. 10).

【0006】.次いで前記ツートン・カラー部分05
上には、ピンストライプ02を貼着して見切りをつけ
る。このピンストライプ02は、フイルム03の上面に
ピンストライプ印刷部分06の印刷がなされ、その下面
に接着剤04を塗布して構成されており、該接着剤04
によりツートン・カラー部分05上にクリヤー012を
介して貼着される。またピンストライプ02の上面に
は、ピンストライプ02の幅よりも若干幅広のマスキン
グアプリケーションテープ07が貼着され、さらにその
上に、ツートン・カラー部分05を覆うマスキング紙0
13が貼着される。(図11参照)。
[0006] Then the two-tone color part 05
A pin stripe 02 is attached to the upper part to form a parting line. The pin stripe 02 is formed by printing the pin stripe print portion 06 on the upper surface of the film 03 and applying the adhesive 04 on the lower surface thereof.
Is attached to the two-tone color portion 05 via the clear 012. A masking application tape 07, which is slightly wider than the width of the pin stripe 02, is attached to the upper surface of the pin stripe 02, and the masking paper 0 covering the two-tone color portion 05 is further applied thereon.
13 is attached. (See Figure 11).

【0007】.次いでその塗装面を清掃した後、ツー
トン・カラー部分05上にクリヤー012を介してツー
トン・カラーの他部分となる、ボデーカラー09を吹き
付け塗装(第4回塗装)し、前記マスキングアプリケー
ションテープ07およびマスキング紙013をを剥が
す。その後必要に応じて硬化乾燥を行なう(図12参
照)。
[0007]. Then, after cleaning the coated surface, a body color 09, which is another portion of the two-tone color, is spray-coated (fourth coating) on the two-tone color portion 05 via the clear 012, and the masking application tape 07 and Peel off the masking paper 013. Thereafter, if necessary, curing and drying are performed (see FIG. 12).

【0008】.最後に全面にオーバコートクリヤー0
10を塗装(第5回塗装)した後、仕上げ硬化乾燥(第
3回乾燥)を行い(図13参照)、塗装ラインより払出
す。
[0008] Finally overcoat clear 0 on the entire surface
After 10 is coated (fifth coating), finish curing drying (third drying) is performed (see FIG. 13) and the product is discharged from the coating line.

【0009】以上.〜.によりオーバコートクリヤ
ー仕様によるツートン・カラー塗装の全工程が終了す
る。
Above. ~. Will complete the whole process of two-tone color coating with overcoat clear specifications.

【0010】[0010]

【発明が解決しようとする課題】ところで前記従来の塗
装方法によれば、5回の塗装と少なくとも2回の乾燥処
理を必要として全体の塗装時間が長くなり、その結果生
産コストの大幅な上昇を招き、さらにツートン・カラー
を2色共塗装するので、VOC(揮発性有機溶剤)の使
用量が多くなり、環境衛生上も好ましくないという課題
がある。
By the way, according to the above-mentioned conventional coating method, five coatings and at least two drying treatments are required, and the entire coating time becomes long, resulting in a large increase in production cost. In addition, since two two-tone colors are coated together, there is a problem in that the amount of VOC (volatile organic solvent) used increases and environmental hygiene is not preferable.

【0011】本発明はかかる実情に鑑みてなされたもの
で、前記課題を解決できるようにした、新規なツートン
・カラー塗装方法を提供することを目的とする。
The present invention has been made in view of the above circumstances, and an object thereof is to provide a novel two-tone color coating method capable of solving the above-mentioned problems.

【0012】[0012]

【課題を解決するための手段】上記目的を達成するため
本請求項1記載の発明の特徴とするところは、合成樹脂
製基材上にオーバコートクリヤー仕様のツートン・カラ
ー塗装を施すにあたり、前処理後の合成樹脂製基材の表
面に、ツートン・カラーの印刷部分を印刷した、上面に
マスキングアプリケーションテープが貼着されているベ
タ貼り用ストライプを貼着する工程と、前記基材の表面
にプライマーを塗装する工程と、前記プライマー上にツ
ートン・カラーの他部分となる、ボデーカラーを塗装す
る工程と、前記塗装後のボデーカラーがウエット状態に
あるうちに、前記ベタ貼り用ストライプ上のマスキング
アプリケーションテープを剥がす工程と、前記ベタ貼り
用ストライプおよびボデーカラーの、全面にオーバコー
トクリヤーを塗装する工程と、塗装面を仕上乾燥する工
程とを備えることにある。
To achieve the above object, the present invention is characterized in that the two-tone color coating of the overcoat clear specification is applied on a synthetic resin substrate. On the surface of the synthetic resin base material after the treatment, the step of sticking the solid stripe with the masking application tape stuck on the upper surface, where the two-tone color printing part is printed, and the surface of the base material A step of applying a primer, a step of applying a body color which is the other part of the two-tone color on the primer, and a step of masking the solid applying stripe while the body color after the application is in a wet state. Overcoat clear is applied to the entire surface of the application tape peeling process and the solid stripe and body color. And that step is to include a step of drying finish the painted surface.

【0013】上記目的達成のため本請求項2記載の発明
の特徴とするところは、ベタ貼り用ストライプは、フイ
ルムの下面に、接着力を前記基材用に設定した接着剤が
塗布され、またその上面に、ツートン・カラーの印刷部
分が印刷されると共にその外縁に沿って見切り線となる
ピンストライプ印刷部分が印刷され、それらの印刷面上
にマスキングアプリケーションテープが貼着されること
にある。
In order to achieve the above-mentioned object, the invention according to claim 2 is characterized in that the solid-adhesive stripe has a lower surface of the film coated with an adhesive having an adhesive force set for the base material. A two-tone color printed portion is printed on the upper surface thereof, and a pin stripe printed portion serving as a parting line is printed along the outer edge of the printed portion, and a masking application tape is attached on the printed surface.

【0014】[0014]

【作用】合成樹脂製基材上に、ツートン・カラーの印刷
部分を有するベタ貼り用ストライプを貼着し、次いでそ
の基材上にツートン・カラーの他部分となるボデーカラ
ーを塗装した後、前記ストライプ上のマスキングアプリ
ケーションテープを剥がしてオーバコートクリヤーを塗
装し、仕上げ硬化乾燥を行なう。
[Function] A solid sticking stripe having a two-tone color printed portion is adhered on a synthetic resin base material, and then a body color to be the other part of the two-tone color is applied on the base material. Peel off the masking application tape on the stripe, paint the overcoat clear, and finish cure and dry.

【0015】[0015]

【実施例】以下、図1〜5を参照して本発明の好適な実
施例について説明する。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENT A preferred embodiment of the present invention will be described below with reference to FIGS.

【0016】図1は、本発明方法によりツートン・カラ
ー塗装の施された、自動二輪車用サイドカバーの斜視
図、図2は、本発明の方法による工程を示すブロック
図、図3〜6は、本発明の塗装工程の順序を示す、塗装
部の断面図である。
FIG. 1 is a perspective view of a motorcycle side cover which has been subjected to two-tone color painting by the method of the present invention, FIG. 2 is a block diagram showing steps by the method of the present invention, and FIGS. It is sectional drawing of a coating part which shows the order of the coating process of this invention.

【0017】この実施例では、本発明方法を自動二輪車
用のサイドカバーSに実施した場合で、図1に示すよう
に、合成樹脂製の部品であるサイドカバーSには、オー
バコートクリヤー仕様によるツートン・カラー塗装が施
される。
In this embodiment, when the method of the present invention is applied to the side cover S for a motorcycle, as shown in FIG. 1, the side cover S, which is a synthetic resin part, has an overcoat clear specification. Two-tone color painting is applied.

【0018】次にこの塗装方法を図2〜6を参照して詳
細に説明する。
Next, this coating method will be described in detail with reference to FIGS.

【0019】前記サイドカバーSを構成する硬質合成樹
脂製基材1の外表面には、オーバコートクリヤー仕様に
よるツートン・カラー塗装が施される。
The outer surface of the hard synthetic resin substrate 1 constituting the side cover S is subjected to two-tone color coating according to the overcoat clear specification.

【0020】(1).まず前処理ラインにおいて、合成樹脂
製基材1に通常の前処理を施し、水切り乾燥した後、基
材1を前処理ラインから塗装ラインへと移送する。
(1) First, in the pretreatment line, the synthetic resin substrate 1 is subjected to ordinary pretreatment, drained and dried, and then the substrate 1 is transferred from the pretreatment line to the coating line.

【0021】(2).塗装ラインにおいて、基材1の表面適
所にベタ貼り用ストライプ2を貼着する。このベタ貼り
用ストライプ2は、フイルム3の下面に、基材用接着剤
4が塗布され、またその上面の中央部分にツートン・カ
ラーの印刷部分5が印刷されると共にその周囲に見切り
用のピンストライプ印刷部分6が印刷されている。また
このベタ貼り用ストライプ2の上面には透明なマスキン
グアプリケーションテープ7が貼着されている。そして
このマスキングアプリケーションテープ7を残したまま
このベタ貼り用のストライプ2は基材1上に接着剤4に
より接着される(図3参照)。
(2). In the coating line, the solid sticking stripes 2 are stuck on the surface of the base material 1 at appropriate places. This solid-adhesive stripe 2 has a base material adhesive 4 applied to the lower surface of a film 3, a two-tone color printed portion 5 is printed in the central portion of the upper surface thereof, and a peripheral parting pin. The striped print portion 6 is printed. Further, a transparent masking application tape 7 is attached to the upper surface of the solid attachment stripe 2. Then, with the masking application tape 7 left, the solid-adhesion stripe 2 is adhered to the base material 1 by the adhesive 4 (see FIG. 3).

【0022】而してこのマスキングアプリケーションテ
ープ7は後述するように、ウエット状態で塗布されるボ
デーカラー9を傷付けることなく、前記ベタ貼り用スト
ライプ2から容易に剥がせるように、図7,8に示すよ
うに、その外縁の一部にタブ片71 が一体に延長されて
おり、このタブ片71 の基部にはマスキングアプリケー
ションテープ7の輪郭線に沿うようにミシン目72 が入
れてあり、このタブ片71 を内側に折るときにこれがそ
のミシン目72 のところでシャープに直線状に折れるよ
うにしている。そしてこのタブ片71 は図7に示すよう
に内側に折り込んだ状態でベタ貼り用ストライプ2上に
重ねられる。
As will be described later, the masking application tape 7 is shown in FIGS. 7 and 8 so that it can be easily peeled from the solid stripe 2 without damaging the body collar 9 applied in a wet state. As shown, a tab piece 7 1 is integrally extended to a part of the outer edge thereof, and a perforation 7 2 is provided at the base of the tab piece 7 1 so as to follow the contour line of the masking application tape 7. When the tab piece 7 1 is folded inward, it is sharply folded linearly at the perforation 7 2 . Then, the tab piece 7 1 is overlapped on the solid bonding stripe 2 while being folded inward as shown in FIG.

【0023】(3).ベタ貼り用ストライプ2を貼着した
後、塗装面を清掃して、基材1の表面にはプライマー
(下塗り)8を吹き付け塗装し、さらにそのプライマー
8上にツートン・カラーの他部分となるボデーカラー9
を吹き付け塗装する(図4参照)。
(3). After sticking the solid striping stripe 2, the coated surface is cleaned, a primer (undercoat) 8 is spray-painted on the surface of the base material 1, and a two-tone coating is applied on the primer 8. Body color, which is the other part of the color 9
Spray coating (see FIG. 4).

【0024】(4).次にそのボデーカラー9が未だ乾燥し
ないウエット状態で、マスキングアプリケーションテー
プ7を剥がす(図5参照)。
(4) Next, the masking application tape 7 is peeled off in a wet state in which the body collar 9 is not yet dried (see FIG. 5).

【0025】ところでこのマスキングアプリケーション
テープ7を剥がすときは、ミシン目72 に沿って予め内
側に折り畳まれている前記タブ片71 を摘んで起立させ
てから該テープ7を剥がすことにより、ピンストライプ
印刷部分6の見切り線をシャープにして、しかもウエッ
ト状態のボデーカラー9を傷付ける心配がない。
By the way, when the masking application tape 7 is peeled off, the tab strip 7 1 previously folded inward along the perforations 7 2 is picked up to stand up, and then the tape 7 is peeled off to remove the pin stripe. The parting line of the printed portion 6 is made sharp and there is no fear of damaging the body color 9 in a wet state.

【0026】(5).最後にツートン・カラーの印刷部分5
およびピンストライプ印刷部分6の印刷された、ベタ貼
り用ストライプ2と、ツートン・カラーの他部分となる
ボデーカラー9との両面全面にわたりオーバコートクリ
ヤー10を吹き付け塗装した後、仕上硬化乾燥を行い、
塗装ラインより払い出す。
(5). Finally, the two-tone color printed portion 5
And, the overcoat clear 10 is spray-painted on both surfaces of the solid stripe 2 printed with the pin stripe printing part 6 and the body color 9 which is the other part of the two-tone color, and then finish curing and drying are performed,
Pay out from the painting line.

【0027】以上のように(1).〜(5).の工程によれば、
3回の塗装と、1回の硬化乾燥により、すなわち前記従
来方法のツートン・カラー部分塗装とクリヤ塗装とを省
略することができると共に途中での乾燥工程を省略する
ことができ、その結果オーバコートクリヤー仕様のツー
トン・カラー塗装工程を大幅に簡略化することができ、
また前記塗装工程の省略により有害なVOCの発生量を
低減することができる。
As described above, according to the steps (1) to (5),
By coating three times and curing and drying once, that is, the conventional two-tone color partial coating and clear coating can be omitted, and the drying step in the middle can be omitted, resulting in overcoating. The clear two-tone color painting process can be greatly simplified.
Further, by omitting the coating process, the amount of harmful VOCs generated can be reduced.

【0028】以上、本発明の一実施例について説明した
が、本発明はその実施例に限定されることなく、本発明
の範囲内で種々の実施例が可能である。たとえば前記実
施例では、本発明方法を自動二輪車用合成樹脂製サイド
カバーに実施した場合を説明したが、これを合成樹脂製
燃料タンク等の他の合成樹脂基材にも実施できることは
勿論である。
Although one embodiment of the present invention has been described above, the present invention is not limited to that embodiment, and various embodiments are possible within the scope of the present invention. For example, in the above-mentioned embodiment, the case where the method of the present invention is applied to the synthetic resin side cover for a motorcycle has been described, but it is needless to say that this can be applied to other synthetic resin base materials such as a synthetic resin fuel tank. .

【0029】[0029]

【発明の効果】以上のように本請求項各項記載の発明に
よれば、従来ツートン・カラー塗装方法における、ツー
トン・カラー部分の塗装工程と、クリヤ塗装工程とを省
略することができるとともに1回の仕上げ乾燥により、
オーバコートクリヤー仕様によるツートン・カラー塗装
をすることができるので、全体の塗装時間が著しく短縮
され、その結果塗装コストの大幅な低減化を図ることが
できる。
As described above, according to the invention described in each claim of the present invention, it is possible to omit the two-tone color coating process and the clear coating process in the conventional two-tone color coating method. By finishing drying once,
Since two-tone color coating with overcoat clear specifications can be performed, the overall coating time is significantly shortened, and as a result, the coating cost can be significantly reduced.

【0030】また前記塗装工程の省略により揮発性有機
溶剤の使用量を削減することができる。
Further, by omitting the coating step, the amount of volatile organic solvent used can be reduced.

【図面の簡単な説明】[Brief description of drawings]

【図1】本発明方法によりオーバコートクリヤー仕様に
よるツートン・カラー塗装の施された、自動二輪車用サ
イドカバーの斜視図
FIG. 1 is a perspective view of a side cover for a motorcycle, which is subjected to a two-tone color coating with an overcoat clear specification by the method of the present invention.

【図2】本発明方法による塗装工程を示すブロック図FIG. 2 is a block diagram showing a coating process according to the method of the present invention.

【図3】本発明による塗装工程の順序を示す、塗装部の
断面図
FIG. 3 is a sectional view of a coating section showing the sequence of coating steps according to the present invention.

【図4】本発明による塗装工程の順序を示す、塗装部の
断面図
FIG. 4 is a sectional view of a coating section showing the sequence of the coating process according to the present invention.

【図5】本発明による塗装工程の順序を示す、塗装部の
断面図
FIG. 5 is a sectional view of a coating section showing the sequence of coating steps according to the present invention.

【図6】本発明による塗装工程の順序を示す、塗装部の
断面図
FIG. 6 is a sectional view of a coating section showing the sequence of coating steps according to the present invention.

【図7】図3の7矢視拡大部分平面図FIG. 7 is an enlarged partial plan view taken along arrow 7 of FIG.

【図8】マスキングアプリケーションテープの部分斜視
FIG. 8 is a partial perspective view of a masking application tape.

【図9】従来方法による塗装工程を示すブロック図FIG. 9 is a block diagram showing a coating process by a conventional method.

【図10】従来方法による塗装工程の順序を示す、塗装
部の断面図
FIG. 10 is a sectional view of a coating section showing the sequence of coating steps according to the conventional method.

【図11】従来方法による塗装工程の順序を示す、塗装
部の断面図
FIG. 11 is a cross-sectional view of a coating section showing the sequence of coating steps according to the conventional method.

【図12】従来方法による塗装工程の順序を示す、塗装
部の断面図
FIG. 12 is a cross-sectional view of a coating section showing the sequence of coating steps according to the conventional method.

【図13】従来方法による塗装工程の順序を示す、塗装
部の断面図
FIG. 13 is a cross-sectional view of a coating section showing the sequence of coating steps according to the conventional method.

【符号の説明】[Explanation of symbols]

1・・・・・・・基材 2・・・・・・・ベタ貼り用ストライプ 3・・・・・・・フィルム 4・・・・・・・接着剤 5・・・・・・・ツートン・カラーの印刷部分 6・・・・・・・ピンストライプ印刷部分 7・・・・・・・マスキングアプリケーションテープ 8・・・・・・・プライマー 9・・・・・・・ボデーカラー 10・・・・・・オーバコートクリヤー 1 ... Base material 2 ... Solid stripe 3 ... Film 4 ... Adhesive 5 ... Two-tone・ Color printed area 6 ・ ・ ・ ・ Pin stripe printed area 7 ・ ・ ・ ・ Masking application tape 8 ・ ・ ・ ・ ・ ・ Primer 9 ・ ・ ・ ・ ・ ・ ・ Body color 10 ・ ・.... Overcoat clear

Claims (2)

【特許請求の範囲】[Claims] 【請求項1】 合成樹脂製基材(1)上にオーバコート
クリヤー仕様のツートン・カラー塗装を施すにあたり、 前処理後の合成樹脂製基材(1)の表面に、ツートン・
カラーの印刷部分(5)を印刷した、上面にマスキング
アプリケーションテープ(7)が貼着されているベタ貼
り用ストライプ(2)を貼着する工程と、 前記基材(1)の表面にプライマー(8)を塗装する工
程と、 前記プライマー(8)上にツートン・カラーの他部分と
なる、ボデーカラー(9)を塗装する工程と、 前記塗装後のボデーカラー(9)がウエット状態にある
うちに、前記ベタ貼り用ストライプ(2)上のマスキン
グアプリケーションテープ(7)を剥がす工程と、 前記ベタ貼り用ストライプ(2)およびボデーカラー
(9)の、全面にオーバコートクリヤー(10)を塗装
する工程と、 塗装面を仕上乾燥する工程と、を少なくとも備える、ツ
ートン・カラー塗装方法。
1. When applying a two-tone color coating of an overcoat clear specification on a synthetic resin substrate (1), a two-tone coating is applied to the surface of the synthetic resin substrate (1) after pretreatment.
A step of sticking a solid stripe (2) on which a masking application tape (7) is stuck on the upper surface, on which a color printing part (5) is printed, and a primer ( 8), a step of applying a body color (9) which is the other part of the two-tone color on the primer (8), and a step of applying the body color (9) after the application in a wet state. Then, a step of peeling off the masking application tape (7) on the solid stripe (2), and coating the overcoat clear (10) on the entire surface of the solid stripe (2) and the body color (9). A two-tone color coating method comprising at least a step and a step of finishing and drying the coated surface.
【請求項2】 ベタ貼り用ストライプ(2)は、フイル
ム(3)の下面に、接着力を前記基材(1)用に設定し
た接着剤(4)が塗布され、またその上面に、ツートン
・カラーの印刷部分(5)が印刷されると共にその外縁
に沿って見切り線となるピンストライプ印刷部分(6)
が印刷され、それらの印刷面上にマスキングアプリケー
ションテープ(7)が貼着される、前記請求項1記載の
ツートン・カラー塗装方法。
2. The solid sticking stripe (2) has a lower surface of a film (3) coated with an adhesive agent (4) having an adhesive force set for the base material (1), and an upper surface thereof having a two-tone structure. A pin-striped printed part (6) which is a parting line along the outer edge of the printed part (5) of color
The two-tone color coating method according to claim 1, wherein the masking application tapes (7) are applied to the printed surfaces of the printed products.
JP7065847A 1995-03-24 1995-03-24 Two-tone painting method Expired - Fee Related JP2900231B2 (en)