JPH07290133A - Equipment for refining rolling stock - Google Patents

Equipment for refining rolling stock

Info

Publication number
JPH07290133A
JPH07290133A JP8708594A JP8708594A JPH07290133A JP H07290133 A JPH07290133 A JP H07290133A JP 8708594 A JP8708594 A JP 8708594A JP 8708594 A JP8708594 A JP 8708594A JP H07290133 A JPH07290133 A JP H07290133A
Authority
JP
Japan
Prior art keywords
equipment
reel
shear
rolls
deflector roll
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP8708594A
Other languages
Japanese (ja)
Other versions
JP3392937B2 (en
Inventor
Harutoshi Yamashita
陽俊 山下
Tadaaki Yasumi
忠明 八角
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP08708594A priority Critical patent/JP3392937B2/en
Publication of JPH07290133A publication Critical patent/JPH07290133A/en
Application granted granted Critical
Publication of JP3392937B2 publication Critical patent/JP3392937B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

PURPOSE:To enable stable supply of rolling stocks with satisfactory quality by providing plural deflector rolls that are replaceable into a transporting pass line in accordance with the surface condition of a rolling stock. CONSTITUTION:The equipment is so constructed that an oil coater 2, at least a set of pinch rolls, shear S and deflector roll 5 are successively arranged towards a reel 6 for coiling a rolled stock 1. Since the outer diameter of a coil changes every minute during the coiling of a rolled stock, the deflector roll 5 is arranged before the take-up reel in order to constantly stabilize the level of a transporting pass line. After the rolled stock 1 is cut off by the shear S, the rolling stock is not present between the shear and the take-up reel, consequently facilitating the exchange of the deflector roll 5. In the case where sticking of a coating oil is to be desirously avoided, the replacement of the deflector roll 5 has only to be performed, which not only dispenses with addition of extra processes but eliminates lowering of quality and also improves productivity.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【産業上の利用分野】この発明は、冷延板あるいは熱延
板などの圧延材の精整設備に関し、とくに、該圧延材の
表面性状に応じた適切な処置を行い、品質の安定化、生
産効率の改善を図ろうとするものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to equipment for adjusting rolled material such as cold-rolled sheet or hot-rolled sheet. It aims to improve production efficiency.

【0002】[0002]

【従来の技術】近年、冷延鋼板の製造コストを下げると
ともに、リードタイムを短縮する目的で、異なるプロセ
ス同士を接続して連続化する動きが見られるようになっ
てきた。
2. Description of the Related Art In recent years, there has been a tendency to connect different processes to make them continuous for the purpose of reducing the manufacturing cost of cold-rolled steel sheets and shortening the lead time.

【0003】このようなコンセプトに立ったものとして
は、調質圧延設備と精整設備を接続したプロセスライ
ン、あるいは調質圧延設備の上工程にさらに連続焼鈍炉
や各種表面処理設備を接続したプロセスラインが知られ
ており、日本国内でもすでに多数のラインが稼働してい
る状況にある。
Based on such a concept, a process line in which a temper rolling equipment and a conditioning equipment are connected, or a process in which a continuous annealing furnace and various surface treatment equipment are further connected to the upper process of the temper rolling equipment The line is known, and many lines are already in operation in Japan.

【0004】ここに、例えば調質圧延設備と精整設備を
接続したプロセスラインの構成としては、調質圧延用の
圧延機(スキンパスミル)、防錆油を塗布する塗油装
置、巻き取りリールが順次配列したものがあり、これに
よって従来は少なくとも2つのラインを通して処理して
いたものを単一のラインで処理できるようになり、上記
の目的を有利に達成することができるようになった。
[0004] Here, for example, as a process line configuration in which the temper rolling equipment and the conditioning equipment are connected, a rolling mill (skin pass mill) for temper rolling, an oil coating device for applying rust preventive oil, and a take-up reel There is a method in which the above-mentioned objects are arranged one after another, which makes it possible to process what was conventionally processed through at least two lines in a single line, and it is possible to achieve the above-mentioned object advantageously.

【0005】ところで、かかるプロセスライン(調質圧
延設備+精整設備)においては以下に述べるような問題
があった。
By the way, the above-mentioned process line (temper rolling equipment + refining equipment) has the following problems.

【0006】すなわち、操業中に定期的にワークロール
の組み替えを行う場合やワークロールに疵が入り突発的
にロールの組み替えを行う必要が生じた場合には、スキ
ンパスミルを開放(調質圧延を行わない)し、その圧延
材(調質圧延を行わないものを以下、「ノースキンパス
材」と略記する)はそのまま通過させて巻き取り工程に
入ることになる。ここで問題となるのが、先に処理した
圧延材に塗布した際の油が塗油装置〜巻き取りリールの
間に設置される数個の通板ロールに付着し、この油が、
防錆油の塗布を必要としないノースキンパス材にまで付
着することである。(同様な問題は、無塗油製品と塗油
製品を同一のラインで作り分ける場合にも生ずる。)そ
して、このノースキンパス材を改めて調質圧延する際
に、かかる板材の表面に防錆油が付着していると、通常
の板とはその表面状態が著しく異なるため、伸び率に差
異が生じる不利があるほか、表面に汚れが付着しやす
く、品質低下を招く不利があった。この傾向はドライス
キンパス材においてとくに顕著であった。
That is, when the work rolls are regularly recombined during the operation, or when the work rolls are damaged and the rolls need to be reconfigured suddenly, the skin pass mill is opened (temper rolling is performed). Then, the rolled material (a material not subjected to temper rolling is abbreviated as “North Kinpas material” hereinafter) is passed as it is to enter the winding step. The problem here is that the oil when applied to the previously processed rolled material adheres to several threading rolls installed between the oil coating device and the take-up reel, and this oil,
It is to adhere even to North Kinpasu material that does not require the application of rust preventive oil. (A similar problem occurs when oil-free products and oil-coated products are produced separately on the same line.) When this North Kinpas material is temper-rolled again, rust preventive oil is applied to the surface of the plate material. Since the surface condition of the adhered sheet is significantly different from that of an ordinary plate, there is a disadvantage that the elongation rate is different and stains are likely to adhere to the surface, which causes a deterioration in quality. This tendency was particularly remarkable in the dry skin pass material.

【0007】こうした品質低下を防止するために、従来
一般的にとられていた方法として、調質圧延を行うに先
立って、他のラインで電解洗浄を行い防錆油を除去する
ことが採用されていたが、この方法は生産性を著しく阻
害していた。
In order to prevent such deterioration in quality, a method generally used in the past has been adopted in which electrolytic corrosion is performed in another line to remove rust-preventing oil prior to temper rolling. However, this method significantly hindered productivity.

【0008】また、品質低下防止のための別の方法とし
て、塗油装置以降に配置されたロールにつき、十分な手
入れを行うことによって電解洗浄ラインの省略を図る試
みもあるが、このような手入れの付加は連続ラインの稼
働能率ひいては生産性の向上に対して極めて不利であっ
た。
[0008] As another method for preventing quality deterioration, there is an attempt to omit the electrolytic cleaning line by performing sufficient care for the rolls arranged after the oiling device. The addition of was extremely disadvantageous for improving the operating efficiency of the continuous line and thus the productivity.

【0009】さらにまた、防錆油の付着を避ける技術と
しては、カットシャーで鋼板を切断した後にピンチロー
ルで鋼板をオイラーロールに押しつけるようにした特開
平5−269525号公報に開示のような方法が知られ
ている。この方法によれば、塗油後、通板ロールを介在
させずに直ちに板を巻き取るので、塗油装置を停止させ
さえすれば鋼板表面への防錆油の付着を完全に防止する
ことができる。
Furthermore, as a technique for avoiding adhesion of rust preventive oil, a method disclosed in Japanese Patent Laid-Open No. 5-269525, in which a steel plate is cut by a cutting shear and then the steel plate is pressed against an Euler roll by a pinch roll. It has been known. According to this method, since the plate is immediately wound up after the oiling without interposing a threading roll, it is possible to completely prevent the rust preventive oil from adhering to the surface of the steel plate only by stopping the oiling device. it can.

【0010】しかしながら、この方法の場合、塗油装置
から発生する霧滴の、他の設備への飛散を防止する排気
設備の設置を考慮すると、塗油装置自体が大型にならざ
るを得ないばかりか、このような塗油装置を、時々刻々
変化するコイル外径に応じて変化する、搬送パスライン
に追従させるのは設備的に非常に困難であった。
However, in the case of this method, considering the installation of the exhaust equipment for preventing the spray of mist generated from the oil coating device from scattering to other equipment, the oil coating device itself must be large. However, it was very difficult in terms of equipment to make such an oiling device follow the transfer path line that changes depending on the coil outer diameter that changes from moment to moment.

【0011】[0011]

【発明が解決しようとする課題】この発明の目的は、塗
油装置を有するプロセスラインにおける上述したような
問題を有利に解決できる精整設備を提案するところにあ
る。この発明の他の目的は、表面状態が異なる圧延材を
処理する場合に、品質低下あるいは生産性低下を招くこ
となく操業することができる精整設備を提案するところ
にある。
SUMMARY OF THE INVENTION An object of the present invention is to propose a refining equipment which can advantageously solve the above problems in a process line having an oiling device. Another object of the present invention is to propose a refining facility that can be operated without causing quality deterioration or productivity deterioration when processing rolled materials having different surface conditions.

【0012】[0012]

【課題を解決するための手段】この発明は、圧延材を巻
き取るリールに向けて、塗油装置、少なくとも一組のピ
ンチロール、シャー、デフレクタロールを順次配設して
なる精整設備であって、前記設備は、圧延材の表面状況
に応じて搬送ラインへ入替えできる複数本のデフレクタ
ロールを有する、ことを特徴とする圧延材の精整設備で
ある。そして、この精整設備は、調質圧延ラインや連続
焼鈍−調質圧延ライン等の下流に接続することができる
ほか、熱間圧延−酸洗ライン、電気錫めっきライン、電
気亜鉛めっきライン、溶融亜鉛めっきライン等種々のラ
インに接続できるものである。
SUMMARY OF THE INVENTION The present invention is a conditioning equipment in which an oiling device, at least one set of pinch rolls, shears, and deflector rolls are sequentially arranged toward a reel for winding rolled material. In addition, the above-mentioned facility is a facility for adjusting rolled material, characterized in that it has a plurality of deflector rolls that can be switched to a conveyor line according to the surface condition of the rolled material. And this refinement equipment can be connected to the downstream of a temper rolling line, a continuous annealing-tempering rolling line, etc., as well as a hot rolling-pickling line, an electric tin plating line, an electric zinc plating line, a melting It can be connected to various lines such as a galvanizing line.

【0013】[0013]

【作用】この発明における設備配列上のポイントは次の
とおりに集約することができる。
The points on the equipment arrangement in the present invention can be summarized as follows.

【0014】塗油装置〜シャー間にデフレクタロール
が配置されていないこと。 塗油装置〜シャー間に一組以上のピンチロールが配置
されていること。 シャー〜巻き取りリール間に必要最小個数のデフレク
ターロールが配置され、このロールは複数本からなるも
のとし、そのいずれもが、必要に応じて適宜、圧延材の
搬送パスラインへ入替えできる構造になっていること。
No deflector roll is arranged between the oiling device and the shear. One or more sets of pinch rolls should be placed between the oiling device and the shear. The minimum required number of deflector rolls are arranged between the shear and the take-up reel, and this roll shall consist of multiple rolls, each of which has a structure that can be appropriately replaced with a rolled material transport path line as required. That

【0015】これらについて、次に説明する。ラインが
運転状態にあるとき、塗油装置〜シャー間には常に圧延
材が存在するため、その状態でデフレクタロールを入替
えることは困難であるから、この間にデフレクタロール
が配置されていないことが肝要である。
These will be described below. When the line is in the operating state, it is difficult to replace the deflector roll in that state because there is always rolled material between the oiling device and the shear.Therefore, the deflector roll may not be placed between them. It is essential.

【0016】また、圧延材の巻き取り中はコイルの外径
が時々刻々と変化するから、搬送パスラインのレベルを
常に一定にするには、巻き取りリールの手前にデフレク
タロールを配置しておくのが有用である。圧延材をシャ
ーによって切断したのちはシャー〜巻き取りリール間に
圧延材が存在しないことになるので、デフレクタロール
の入替えも容易となる。
Since the outer diameter of the coil changes from moment to moment during winding of the rolled material, a deflector roll is arranged in front of the winding reel in order to keep the level of the conveying path line constant. Is useful. Since the rolled material does not exist between the shear and the take-up reel after the rolled material is cut by the shear, the deflector rolls can be easily replaced.

【0017】上述したように、この発明においては、巻
き取りリールの直前に複数本のデフレクタロールを配置
して、圧延材の表面状況に応じて搬送パスラインに入替
えできるようにしたので、塗油の付着を避けたいような
場合には、ロールの入替えのみを行えばよく、余計な工
程を付加する必要がないだけでなく、品質の低下が避け
られ生産効率を著しく改善することができる。また、こ
の発明によって、前コイルと次コイルとで塗布する防錆
油の種類が異なり、防錆油が相互に混入するのを避けた
い場合(例えば、混入すると脱脂性やその後の化成処理
性に悪影響を及ぼす)にも、同様に、品質の低下や生産
効率を改善する効果が発揮される。
As described above, in the present invention, a plurality of deflector rolls are arranged immediately before the take-up reel so that the deflector rolls can be replaced with the conveying path line according to the surface condition of the rolled material. In the case where it is desired to avoid the adherence, it is only necessary to replace the rolls, it is not necessary to add an extra step, and it is possible to avoid the deterioration of the quality and significantly improve the production efficiency. Further, according to the present invention, when the type of rust preventive oil applied to the front coil and the next coil is different, and it is desired to avoid mixing the rust preventive oils with each other (for example, when mixed, the degreasing property and the subsequent chemical conversion processability can be improved. The adverse effect) similarly exerts the effect of reducing the quality and improving the production efficiency.

【0018】[0018]

【実施例】以下、図面を用いてこの発明を詳細に説明す
る。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention will be described in detail below with reference to the drawings.

【0019】図1は、この発明に従う設備の構成を示し
たものであり、図中1は圧延材、2は圧延材1の表面に
防錆油等を塗布する塗油装置、3はピンチロールであっ
て、このピンチロール3によってシャーSによる切断後
の圧延材を支持するとともに、それを前方に送り出す
が、上流工程での未処理の圧延材1につき、防錆油の付
着が心配されるような場合には迅速にロールを開放する
ことができるようになっている。
FIG. 1 shows a structure of equipment according to the present invention. In the figure, 1 is a rolled material, 2 is an oil coating device for applying rust preventive oil or the like to the surface of the rolled material 1, and 3 is a pinch roll. While the rolled material after being cut by the shear S is supported by the pinch rolls 3 and is fed forward, there is a concern that rust-preventing oil may be attached to the untreated rolled material 1 in the upstream process. In such a case, the roll can be released quickly.

【0020】また、4はエプロン、5は一端を油圧シリ
ンダ5aに接続し枢軸5bを中心にして揺動可能なリン
ク5cを備えたデフレクタロールであって、このデフレ
クタロール5は複数本からなり(この例では2本)、油
圧シリンダ5aの作動により搬送パスラインへ交互に入
替えできるようになっている。また、6はカローセルタ
イプの例で示した巻き取りリールであり、この巻き取り
リール6は複数個設けるようにしてもよく、この場合に
は、デフレクタロール5はそれぞれのリールに一組ずつ
配置するようにする。
Further, 4 is an apron, 5 is a deflector roll having one end connected to the hydraulic cylinder 5a and having a link 5c swingable about a pivot 5b. The deflector roll 5 is composed of a plurality of ( In this example, the number is two), and the transfer path line can be alternately switched by the operation of the hydraulic cylinder 5a. Further, 6 is a take-up reel shown as an example of a carousel type, and a plurality of take-up reels 6 may be provided. In this case, one set of deflector rolls 5 is arranged on each reel. To do so.

【0021】デフレクタロール5の入替えはコイル分割
ののち行う。すなわち、入替えは図2に示すような手順
で行えばよい。
The deflector roll 5 is replaced after the coil is divided. That is, the replacement may be performed in the procedure as shown in FIG.

【0022】缶用材料T4〜T5CA相当の鋼板を対象
として、上掲図1に示したような本発明設備を使用して
処理した場合、および図3に示すような従来設備を使用
して処理した場合の各々について、その過程で発生した
ノースキンパス材を、他ラインで改めて調質圧延(ドラ
イスキンパス、伸び率1.5%)を行ったときの不良品
の発生率を調査した。ここで、本発明設備を使用するに
あたっては、調質圧延・塗油の実施材と、調質圧延・塗
油の未実施材とで、デフレクタロールを交互に使い分け
して処理し、従来設備では、そのまま同じデフレクタロ
ールによって処理した。なお、これらいずれの場合も塗
油量は100mg/m2 とした。
Steel plates corresponding to can materials T4 to T5CA are treated by using the equipment of the present invention as shown in FIG. 1 and by using conventional equipment as shown in FIG. In each of the above cases, the occurrence rate of defective products was examined when the North Kinpas material generated in the process was subjected to another temper rolling (dry skin pass, elongation rate 1.5%) in another line. Here, in using the equipment of the present invention, the material subjected to the temper rolling / oiling and the material not subjected to the temper rolling / oiling are processed by selectively using deflector rolls, and the conventional equipment is used. , Treated with the same deflector roll as is. In each of these cases, the amount of oil applied was 100 mg / m 2 .

【0023】その結果を図4に示す。図4より明らかな
ように、従来設備の使用では、不良製品(汚れ、伸び率
不良)が25%も発生したのに対し、この発明に従う設
備を使用すれば、極めて少なくなることが確認できた。
このように、この発明にしたがう設備を適用することに
より不良製品が従来設備による場合に比べて激減した理
由は、これまでも述べたように、調質圧延鋼板に塗布し
た防錆油が後続のノースキンパス材に付着しなかったか
らである。
The results are shown in FIG. As is clear from FIG. 4, 25% of defective products (dirt, poor elongation) were generated by using the conventional equipment, but it was confirmed that the number of defective products was extremely reduced by using the equipment according to the present invention. .
As described above, the reason why the defective product is drastically reduced by applying the equipment according to the present invention as compared with the case of the conventional equipment is that the rust preventive oil applied to the temper rolled steel sheet is This is because it did not adhere to the North Kinpus material.

【0024】なお、上掲図1発明例においては、デフレ
クターロールが2本の場合を示したが、この数が3本以
上とすることもできる。また、デフレクターロールを洗
浄する機構を設け、かかるロールの待機中に洗浄するこ
とがでるようにしておけば、3種類以上の用途(表面状
態)にも適用することができ、適用範囲はさらに広が
る。また、図1では、圧延材の搬送パスラインが水平と
なる場合についての例を示したが、搬送パスラインが必
ずしも水平である必要はなく、垂直であってもよく、こ
れに塗油装置、シャー等を配置した構成としてもよい。
ただし、塗油装置〜シャー間にデフレクタロールを配置
することはできないので、垂直搬送パスラインに塗油装
置を、これに続く水平搬送パスラインにシャーを配置す
るような組み合わせは不可能である。
In the example of the invention shown in FIG. 1 above, the case where the number of deflector rolls is two is shown, but the number may be three or more. Further, if a mechanism for cleaning the deflector rolls is provided so that the rolls can be cleaned while the rolls are on standby, the deflector rolls can be applied to three or more kinds of uses (surface condition), and the application range is further expanded. . Further, although FIG. 1 shows an example in which the transport path line of the rolled material is horizontal, the transport path line does not necessarily have to be horizontal, and may be vertical. A configuration in which a shear or the like is arranged may be used.
However, since the deflector roll cannot be arranged between the oil coating device and the shear, a combination in which the oil coating device is arranged on the vertical conveying path line and the shear is arranged on the horizontal conveying path line subsequent thereto is impossible.

【0025】図5は、この発明に従う精整設備を連続焼
鈍−調質圧延ラインの下流に配置した例である。このほ
かに、この発明に従う精整設備は、最近冷延鋼板の代替
として使用されつつある熱延鋼板の製造のための、熱間
圧延−酸洗−調質圧延−精整ラインとか、溶融亜鉛めっ
き−調質圧延−精整ラインなどにおいて、塗油装置を伴
う精整設備として、適宜配置し使用することが可能であ
る。さらに、塗油に限らずクロメート処理等、鋼板に液
体を塗布する場合にも、この発明を応用することが可能
である。
FIG. 5 shows an example in which the refining equipment according to the present invention is arranged downstream of the continuous annealing-temper rolling line. In addition to the above, the refining equipment according to the present invention is a hot rolling-pickling-tempering rolling-refining line for producing hot-rolled steel sheets, which has recently been used as an alternative to cold-rolled steel sheets, or molten zinc. In a plating-temper rolling-refining line or the like, it can be appropriately arranged and used as a refining equipment accompanied by an oil coating device. Furthermore, the present invention can be applied not only to oil application but also to the case where a liquid is applied to a steel plate such as chromate treatment.

【0026】[0026]

【発明の効果】この発明によれば、巻き取りリールの入
側に配置したデフレクタロールの入替えのみで、圧延材
の表面状況に応じた対応が可能となり、品質の良好な圧
延材を安定的に供給できるだけでなく、生産効率の改善
にも極めて有用である。また、この発明によれば、デフ
レクターロールを洗浄する機構を設け、かかるロールの
待機中に洗浄することによって3種類以上の用途にも適
用することができ、適用範囲は極めて広い。
According to the present invention, by simply replacing the deflector rolls arranged on the entrance side of the take-up reel, it is possible to respond to the surface condition of the rolled material, and to stabilize the rolled material of good quality. Not only can it be supplied, but it is extremely useful for improving production efficiency. Further, according to the present invention, a mechanism for cleaning the deflector rolls is provided, and by cleaning the rolls while they are on standby, the deflector rolls can be applied to three or more kinds of uses, and the application range is extremely wide.

【図面の簡単な説明】[Brief description of drawings]

【図1】この発明に従う精整設備の構成を示した図であ
る。
FIG. 1 is a diagram showing a configuration of a refining facility according to the present invention.

【図2】デフレクタロールの入替え要領を示した図であ
る。
FIG. 2 is a diagram showing how to replace a deflector roll.

【図3】従来設備の構成を示した図である。FIG. 3 is a diagram showing a configuration of conventional equipment.

【図4】製品不良発生率を比較して示した図である。FIG. 4 is a diagram showing a comparison of product defect occurrence rates.

【図5】連続焼鈍炉、調質圧延設備および精整設備を接
続したプロセスラインを示した図である。
FIG. 5 is a diagram showing a process line in which a continuous annealing furnace, temper rolling equipment, and conditioning equipment are connected.

【符号の説明】[Explanation of symbols]

1 圧延材 2 塗油装置 3 ピンチロール 4 エプロン 5 デフレクタロール 6 リール S シャー 1 rolled material 2 oil coating device 3 pinch roll 4 apron 5 deflector roll 6 reel S shear

Claims (2)

【特許請求の範囲】[Claims] 【請求項1】 圧延材を巻き取るリールに向けて、塗油
装置、少なくとも一組のピンチロール、シャー、デフレ
クタロールを順次配設してなる精整設備であって、 この精整設備は、圧延材の表面状況に応じて搬送パスラ
インへ入替えできる複数のデフレクタロールを有する、
ことを特徴とする圧延材の精整設備。
1. A refining facility in which an oiling device, at least one set of pinch rolls, shears, and deflector rolls are sequentially arranged toward a reel for winding rolled material. Having a plurality of deflector rolls that can be switched to the transport path line according to the surface condition of the rolled material,
This is a facility for adjusting rolled material.
【請求項2】 調質圧延設備に接続してなる、請求項1
に記載の設備。
2. The method according to claim 1, which is connected to a temper rolling equipment.
Equipment described in.
JP08708594A 1994-04-26 1994-04-26 Rolled material refinement equipment Expired - Fee Related JP3392937B2 (en)