JPH071057A - Method for correcting expanded end part of pipe and tool for correcting the expanded part - Google Patents

Method for correcting expanded end part of pipe and tool for correcting the expanded part

Info

Publication number
JPH071057A
JPH071057A JP15076293A JP15076293A JPH071057A JP H071057 A JPH071057 A JP H071057A JP 15076293 A JP15076293 A JP 15076293A JP 15076293 A JP15076293 A JP 15076293A JP H071057 A JPH071057 A JP H071057A
Authority
JP
Japan
Prior art keywords
pipe
die
punch
tube
outer diameter
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP15076293A
Other languages
Japanese (ja)
Other versions
JP2673651B2 (en
Inventor
Toshimitsu Fukihara
俊光 吹原
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yutaka Giken Co Ltd
Original Assignee
Yutaka Giken Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yutaka Giken Co Ltd filed Critical Yutaka Giken Co Ltd
Priority to JP15076293A priority Critical patent/JP2673651B2/en
Publication of JPH071057A publication Critical patent/JPH071057A/en
Application granted granted Critical
Publication of JP2673651B2 publication Critical patent/JP2673651B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

PURPOSE:To precisely finish the end part of a pipe by expanding the end part of the pipe a little larger than the original diameter and the outer diameter of the expanded pipe part and the roundness of the outer peripheral surface by only forming. CONSTITUTION:A tool 1 for correcting the expanded pipe integrally provides a punch 3 having a forming part 8 in the inner part of a die 2 having a forming part 5. To the pipe 13 to be worked, the tool 1 is advanced in the A1 direction and the punch 3 is pressed in the hole 13a to expand the pipe. At this time, the forming part 5 of the die 2 does not contact with the outer periphery of the pipe 13. Successively, at the time of retreating the tool 1 in the arrow mark A2 direction, the expanded pipe part 14 is contracted with the forming part 5 of the die 2 to form the corrected part 15 having the precise outer surface.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【産業上の利用分野】本発明は、管の端部の外面を所定
の外径を持つ真円に仕上げるための手段に関し、例え
ば、フランジ材や板材に一定寸法の穴を穿設しておき、
該穴に管の端部を挿入して溶接する場合に、その前工程
として、管の端部を該穴に密嵌できる正確な外径に修正
加工するための手段に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a means for finishing the outer surface of an end portion of a pipe into a perfect circle having a predetermined outer diameter. For example, a flange material or a plate material is provided with a hole having a predetermined size. ,
The present invention relates to a means for correcting the end portion of a pipe into an accurate outer diameter capable of being tightly fitted in the hole when the end portion of the pipe is inserted into the hole and welded.

【0002】[0002]

【従来の技術】板材に設けた穴に管を固定する手段とし
て、板材の穴に管を挿入し、該管の孔にパンチを圧入し
て拡管し、穴面に管の外面を密着させるようにすること
は、多数の放熱フィンを管体に固定する手段として従来
知られている(例えば特開昭62−144829)。
2. Description of the Related Art As a means for fixing a pipe in a hole provided in a plate material, the tube is inserted into the hole of the plate material, a punch is pressed into the hole of the plate to expand the tube, and the outer surface of the tube is closely adhered to the hole surface. This is conventionally known as a means for fixing a large number of heat radiation fins to the tube body (for example, Japanese Patent Laid-Open No. 62-144829).

【0003】この従来技術を管端の拡管用に利用する
と、図3に示す手段となる。図3(a)でWはワークと
してのパイプであり、パンチpの作動線上に保持され、
該パイプWの内径より大径のパンチpが図3(b)
(c)に示すように前進してパイプW中に圧入され、こ
れを拡径する。
When this conventional technique is used for expanding the pipe end, the means shown in FIG. 3 is obtained. In FIG. 3A, W is a pipe as a work, which is held on the operating line of the punch p,
A punch p having a diameter larger than the inner diameter of the pipe W is shown in FIG.
As shown in (c), it moves forward and is press-fitted into the pipe W to expand it.

【0004】ところが、パイプpの肉厚の均等度すなわ
ち偏肉については、一般に10%程度の許容値があり、
偏肉のあるワークを図3のように加工すると、薄い部分
の伸び率が高くなるため薄肉部aと厚肉部bとの差が更
に拡大される上、外周面の真円度が低下して嵌合する穴
との間に隙間ができる。また、肉厚が均等で外径が規定
値であっても、内径が規定値と異なれば、拡管量も異な
って拡管後の外径がばらつき、例えば図3(c)にfと
して示すフランジ材の穴に挿入するとき、穴との寸法差
が生じる。
However, there is generally a permissible value of about 10% for the uniformity of the wall thickness of the pipe p, that is, the uneven thickness.
When a work with uneven thickness is machined as shown in FIG. 3, the elongation rate of the thin portion is increased, so that the difference between the thin portion a and the thick portion b is further expanded, and the roundness of the outer peripheral surface is reduced. There is a gap between the holes that fit together. Further, even if the wall thickness is uniform and the outer diameter is the specified value, if the inner diameter is different from the specified value, the pipe expansion amount is also different and the outer diameter after pipe expansion varies. For example, the flange material shown as f in FIG. 3C. When inserting into the hole, there is a dimensional difference from the hole.

【0005】このような不都合を防止するためには、研
摩代を設けて拡管したのち研摩して一定外径に修正しな
ければならず、高コストとなる不都合がある。また、外
径及び内径を正確に成形するために、外径と内径に同時
にしごき絞り加工を施すものがあり、その一例が特開昭
63−248521号に示されている。この技術は、ワ
ークが有底の缶体であり、外ダイスと内ダイスを、その
加工面を前後に僅かにずらせて配置し、パンチでワーク
の底部を内側から加圧して両ダイスを通過させ、胴部を
外ダイスで外側から絞りながら内ダイスで内側からしご
いて缶胴を薄くするものであり、両ダイスで同時に加工
が行われるため、大きい引抜き力を作用させなければな
らず、また拡径は実質上行われない。
In order to prevent such an inconvenience, it is necessary to provide a polishing allowance, expand the pipe, and then polish the pipe to correct it to a constant outer diameter, resulting in a high cost. Further, in order to accurately form the outer diameter and the inner diameter, there is a method in which the outer diameter and the inner diameter are simultaneously subjected to ironing and drawing, and an example thereof is disclosed in JP-A-63-248521. In this technology, the work is a bottomed can, and the outer die and inner die are arranged with their working surfaces slightly offset from each other in the front and back, and the bottom of the work is pressed with a punch from the inside to pass both dies. The body of the can is thinned by squeezing the body from the outside with the outer die and squeezing from the inside with the inner die.Since both dies are processed at the same time, a large drawing force must be applied. There is virtually no expansion.

【0006】[0006]

【発明が解決しようとする課題】本発明は、管の端部
に、正確な外径寸法をもつ拡径した部分を簡単な手段で
形成することを課題とする。
SUMMARY OF THE INVENTION An object of the present invention is to form an enlarged portion having an accurate outer diameter dimension at the end of a pipe by a simple means.

【0007】[0007]

【課題を解決するための手段】本発明における加工方法
は、加工すべき管の外径より大径の成形部をもつダイ
を、管端部の加工範囲を越えて管に嵌め、該管の内径よ
り大きい外径をもつパンチを管端部に圧入して拡管し、
該パンチを抜取りながら前記ダイで拡管部を絞り加工す
ることを特徴とする。
According to the processing method of the present invention, a die having a forming portion having a diameter larger than the outer diameter of the pipe to be processed is fitted into the pipe beyond the processing range of the pipe end, A punch with an outer diameter larger than the inner diameter is pressed into the pipe end to expand the pipe,
The pipe expanding portion is drawn by the die while removing the punch.

【0008】また、本発明に使用する工具は、拡管前の
管の外径より大径で、拡管後の管の外径より小径の成形
部を前端にもつ筒状のダイと、該ダイの成形部より後方
に前端部をもち、前記管の内径より外径が大きい拡管用
のパンチと、を同心に固定したことを特徴とする。
Further, the tool used in the present invention is a tubular die having a front end with a molding portion having a diameter larger than the outer diameter of the pipe before pipe expansion and smaller than the outer diameter of the pipe after pipe expansion. A punch for expanding a pipe having a front end portion rearward of the forming portion and having an outer diameter larger than the inner diameter of the pipe is fixed concentrically.

【0009】[0009]

【作用】前記の各発明において、まず、管の端部からパ
ンチが押込まれて拡管し、管外径を所定寸法以上にす
る。次に、パンチを抜取りながらダイを後退させ、その
成形部で管の外面をしごくと、ダイの成形面に一致した
正確な外径と真円度をもつ成形面が形成される。この
際、パンチによる加工とダイによる加工は別々に行われ
るので、小さい力で加工することができ、被加工部分の
残留応力や材料の劣化が少ない。
In each of the above inventions, first, the punch is pushed from the end of the pipe to expand the pipe, and the outer diameter of the pipe is made equal to or larger than the predetermined size. Next, the die is retracted while removing the punch, and the outer surface of the tube is squeezed at the forming portion to form a forming surface having an accurate outer diameter and roundness that match the forming surface of the die. At this time, since the punching and the die are separately performed, the processing can be performed with a small force, and the residual stress in the processed portion and the deterioration of the material are small.

【0010】[0010]

【実施例】以下、図面を参照して本発明の実施例を説明
する。図1において1は拡管修正工具であり、2はダ
イ、3はパンチである。ダイ2の中心孔4の前端には、
該中心孔4より僅かに小径で内径D1の成形部5がリン
グ状に設けられており、ダイ2の後端にはフランジ6と
固定穴6aが設けられている。
Embodiments of the present invention will be described below with reference to the drawings. In FIG. 1, 1 is a pipe expanding correction tool, 2 is a die, and 3 is a punch. At the front end of the center hole 4 of the die 2,
A molding portion 5 having a diameter slightly smaller than the center hole 4 and an inner diameter D 1 is provided in a ring shape, and a flange 6 and a fixing hole 6a are provided at the rear end of the die 2.

【0011】パンチ3には、前端のテーパ部7に続いて
成形部8が設けられ、更に前記中心穴4に密嵌する嵌合
部9及びフランジ10と固定穴10aが設けられる。そ
して、ダイ2とパンチ3は、固定穴6a、10aを通る
ボルトで油圧シリンダの作動部12に固定される。
The punch 3 is provided with a molding portion 8 following the front taper portion 7, and further with a fitting portion 9 for tightly fitting the central hole 4, a flange 10 and a fixing hole 10a. Then, the die 2 and the punch 3 are fixed to the working portion 12 of the hydraulic cylinder with bolts passing through the fixing holes 6a and 10a.

【0012】ダイ2の成形部5の内径をD1、パンチ3
の成形部8の外径をD2とし、管13の外径をd1、内径
をd2とすると、D1>d1>D2>d2の関係にあり、管
端部の加工後の外径は、すべてD1になる。
The inner diameter of the molding portion 5 of the die 2 is D 1 , and the punch 3 is
Assuming that the outer diameter of the molded portion 8 is D 2 , the outer diameter of the pipe 13 is d 1 , and the inner diameter is d 2 , there is a relation of D 1 > d 1 > D 2 > d 2 , and after the pipe end is processed. The outer diameters of all are D 1 .

【0013】図2(a)〜(c)は、前記拡管修正工具
1により管13の端部を拡管及び修正する工程を示し、
図3(a)で該拡管工具1を矢印A1方向に前進させる
と、ダイ2の成形部5は、管13に接触せず、パンチ3
が孔13aにテーパ部7から圧入され、成形部8による
拡管が行われて外径d3の拡管部14が形成され、該d3
は、ダイ2の成形部5の内径D1より大きい。
2 (a) to 2 (c) show a step of expanding and correcting the end portion of the pipe 13 by the pipe expanding correction tool 1,
When the tube expanding tool 1 is advanced in the direction of arrow A 1 in FIG. 3 (a), the forming part 5 of the die 2 does not contact the tube 13 and the punch 3
There is pressed from the tapered portion 7 into the hole 13a, is made expanded pipe by molding portion 8 is expanded pipe portion 14 of the outer diameter d 3 is formed, the d 3
Is larger than the inner diameter D 1 of the molding portion 5 of the die 2.

【0014】拡管工具1を図2(b)の位置から(c)
のように矢印A2方向に後退させると、拡管部14は、
成形部5でしごき加工されて縮径し、外径D1の修正部
15が形成され、孔13aの内径は、拡管時のD2より
は小さくなるが、元の内径d2よりは大きく、流通路の
縮小は防止される。このしごき加工においては、修正部
15の外面は、真円の成形部5の形状に従うから、拡管
部14の肉厚が不均一であっても、それと無関係に真円
の修正部15が形成される。
The pipe expanding tool 1 is moved from the position shown in FIG. 2 (b) to (c).
When retracted in the direction of the arrow A 2 as shown in FIG.
The molding portion 5 is ironed to reduce the diameter to form the correction portion 15 having the outer diameter D 1 , and the inner diameter of the hole 13a is smaller than D 2 at the time of pipe expansion, but larger than the original inner diameter d 2 . The reduction of the flow passage is prevented. In this ironing process, the outer surface of the correction portion 15 follows the shape of the rounded molding portion 5, so that even if the wall thickness of the expanded portion 14 is uneven, the correction portion 15 of a perfect circle is formed regardless of that. It

【0015】[0015]

【発明の効果】以上のように本発明の方法又は工具によ
れば、管の端部をパンチで一旦拡管したのちダイで絞り
加工をするので、管の内面で形成される流路の面積を縮
小することなく、正確な外径と真円度をもつ外周面が形
成できる効果を有し、かつ拡管と外面の絞り加工を別工
程で行うので小さい力で加工でき、これにより被加工部
分に生じる残留応力が小さく、材質の劣化も殆ど生じな
い利点を有する。
As described above, according to the method or tool of the present invention, since the end portion of the tube is once expanded with the punch and then drawn with the die, the area of the flow path formed on the inner surface of the tube is reduced. It has the effect of forming an outer peripheral surface with an accurate outer diameter and roundness without reducing it, and since the expansion and drawing of the outer surface are performed in separate steps, it can be processed with a small force, which allows the work piece to be processed. It has an advantage that the residual stress generated is small and the deterioration of the material hardly occurs.

【図面の簡単な説明】[Brief description of drawings]

【図1】 本発明の実施に用いる工具及びワークの断面
FIG. 1 is a sectional view of a tool and a work used for carrying out the present invention.

【図2】 本発明の加工方法の説明図FIG. 2 is an explanatory diagram of a processing method of the present invention.

【図3】 従来の加工方法の説明図FIG. 3 is an explanatory view of a conventional processing method.

【符号の説明】[Explanation of symbols]

1 拡管修正工具 2 ダイ 3 パン
チ 5、8 成形部 13 管 14
拡管部 15 修正部
1 Tube expansion correction tool 2 Die 3 Punch 5, 8 Forming part 13 Tube 14
Expansion section 15 Correction section

Claims (2)

【特許請求の範囲】[Claims] 【請求項1】 加工すべき管(13)の外径(d1)よ
り大径の成形部(D1)をもつダイ(2)を、管端部の
加工範囲を越えて管に嵌め、 該管(13)の内径(d2)より大きい外径(D2)をも
つパンチ(3)を管(13)端部に圧入して拡管し、 該パンチ(3)を抜取りながら前記ダイ(2)で拡管部
(14)を絞り加工すること、を特徴とする管端部の拡
管修正方法。
1. A die (2) having a forming portion (D 1 ) having a diameter larger than the outer diameter (d 1 ) of the pipe (13) to be processed is fitted into the pipe beyond the processing range of the pipe end. and the inner diameter (d 2) by press-fitting a punch having a larger outer diameter (D 2) (3) to the tube (13) end tube expansion of the tube (13), said die while withdrawing the punch (3) ( A method for expanding a pipe end portion, wherein the pipe expanding portion (14) is drawn in step 2).
【請求項2】 拡管前の管(13)の外径(d1)より
大径で、拡管後の管(13)の外径(d3)より小径
(D1)の成形部(5)を前端にもつ筒状のダイ(2)
と、 該ダイ(2)の成形部(5)より後方に前端部をもち、
前記管(13)の内径(d2)より外径(D2)が大きい
拡管用のパンチ(3)と、 を同心に固定したこと、を特徴とする管端部の拡管修正
工具。
In larger diameter than the outer diameter (d 1) of 2. A tube expanding front of the tube (13), forming part of the small-diameter (D 1) than the outer diameter (d 3) of the tube after tube expansion (13) (5) Cylindrical die with a front end (2)
And having a front end portion behind the molding portion (5) of the die (2),
A pipe expansion correction tool for a pipe end, comprising: a pipe expansion punch (3) having an outer diameter (D 2 ) larger than an inner diameter (d 2 ) of the pipe (13) and being fixed concentrically with each other.
JP15076293A 1993-06-22 1993-06-22 Pipe end expansion method and pipe expansion correction tool Expired - Lifetime JP2673651B2 (en)