JPH0691692A - Container and production thereof - Google Patents

Container and production thereof

Info

Publication number
JPH0691692A
JPH0691692A JP24381992A JP24381992A JPH0691692A JP H0691692 A JPH0691692 A JP H0691692A JP 24381992 A JP24381992 A JP 24381992A JP 24381992 A JP24381992 A JP 24381992A JP H0691692 A JPH0691692 A JP H0691692A
Authority
JP
Japan
Prior art keywords
label
container body
mold
container
heat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP24381992A
Other languages
Japanese (ja)
Inventor
Masaaki Fujio
正明 藤尾
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fuji Seal Inc
Original Assignee
Fuji Seal Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fuji Seal Inc filed Critical Fuji Seal Inc
Priority to JP24381992A priority Critical patent/JPH0691692A/en
Publication of JPH0691692A publication Critical patent/JPH0691692A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To prevent the positional shift of a label and molding inferiority and to simplify a manufacturing process. CONSTITUTION:A label 5 composed of a heat shrinkable film formed into a cylindrical shape is externally fitted to a male mold 8 and shrunk under heating along the male mold 8 and, thereafter, the male mold 8 and the female mold 11 are closed so as to provide a predetermined gap 19 between the label 5 and the female mold 11. Next, a transparent or translucent molten resin material is injected in the gap 19 to form a container main body 3.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【産業上の利用分野】本発明は、食品等を収容する容器
及びその製造方法に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a container for containing food and the like and a method for manufacturing the container.

【0002】[0002]

【従来の技術】食品等を収容する容器として、図5
(ハ)に示す如く合成樹脂製の容器本体30の外周面に文
字絵柄等の印刷が施されたラベル31が装着されたものが
ある。この容器32の製造方法は、先ず、熱収縮性を有す
るフィルムからなるラベル31を円筒状に形成した後に、
該ラベル31を予備成形用型33に外嵌し、更に、該ラベル
31を予備成形用型33に沿うように熱収縮させることによ
り、ラベル31の予備成形品34を制作する(図5(イ)参
照)。
2. Description of the Related Art FIG.
As shown in (c), there is a container body 30 made of a synthetic resin with a label 31 attached to the outer peripheral surface of which is printed a character pattern or the like. The manufacturing method of this container 32 is, first, after forming the label 31 made of a film having heat shrinkability into a cylindrical shape,
The label 31 is fitted onto the preforming die 33, and the label 31 is further fitted.
By heat shrinking 31 along the preforming die 33, a preformed product 34 of the label 31 is produced (see FIG. 5A).

【0003】次に、この予備成形品34を雌型36の内周面
36a に内嵌させた状態で、該雌型36と雄型37とで型閉じ
を行い、型閉じされた状態で雌型37の注入路38を介して
両型36,37 間に溶融樹脂を注入して容器本体30を形成し
ている。
Next, the preform 34 is attached to the inner peripheral surface of the female die 36.
The mold 36 is closed with the female mold 36 and the male mold 37 in the state of being fitted in the 36a, and the molten resin is injected between the molds 36 and 37 through the injection passage 38 of the female mold 37 in the mold closed state. It is injected to form the container body 30.

【0004】[0004]

【発明が解決しようとする課題】しかしながら、上記従
来のような製造方法は、予め予備成形用型33にてラベル
31を予備成形した後に、予備成形品34を予備成形用型33
から取り外し、更に、雌型36に装着するため、予備成形
品34と雌型36との嵌合誤差が生じ易く、この嵌合誤差は
ラベル31の位置ずれ、あるいは、成形不良の原因となっ
ていた。
However, in the conventional manufacturing method described above, the label is preliminarily labeled with the preforming die 33.
31 is preformed, then preform 34 is preformed 33
Since the preform 34 and the female die 36 are fitted to the female die 36, a fitting error between the preform 34 and the female die 36 is likely to occur, which causes a misalignment of the label 31 or defective molding. It was

【0005】また、上記容器は、ラベル31が容器本体30
の外周面に装着されていることから、該ラベル31が不慮
に剥がれたり、更には脱落するおそれがあった。しか
も、予備成形品34を予備成形用型33から雌型36へ移す工
程が不可欠なため、製造工程が複雑になる欠点もあっ
た。
In the above container, the label 31 has a container body 30.
Since the label 31 is mounted on the outer peripheral surface, there is a risk that the label 31 may be inadvertently peeled off or even dropped off. In addition, the step of transferring the preform 34 from the preforming die 33 to the female die 36 is indispensable, so that the manufacturing process is complicated.

【0006】本発明は、上記従来の問題点に鑑みてなさ
れもので、ラベルの位置ずれ及び成形不良を防止でき、
製造工程の簡略化を図ることのできる容器及びその製造
方法を提供することを課題とする。
The present invention has been made in view of the above-mentioned problems of the prior art, and can prevent misalignment of labels and molding defects.
An object of the present invention is to provide a container and a manufacturing method thereof, which can simplify the manufacturing process.

【0007】[0007]

【課題を解決するための手段】本発明は、上記課題を解
決するために容器及びその製造方法としてなされたもの
で、容器の製造方法としての特徴は、筒状に形成された
熱収縮性フィルムからなるラベル5を雄型8に外嵌し、
該ラベル5を雄型8に沿うように加熱収縮した後に、該
ラベル5と雌型11とが所定の間隙19を有するように雄型
8と雌型11とを型閉じ、次に、透明又は半透明の溶融樹
脂材料を前記間隙19に注入して容器本体3を形成するこ
とにある。
The present invention has been made as a container and a method for manufacturing the same in order to solve the above-mentioned problems. The characteristic of the method for manufacturing the container is that the heat-shrinkable film formed in a tubular shape. The label 5 consisting of
After the label 5 is heated and shrunk along the male mold 8, the male mold 8 and the female mold 11 are closed so that the label 5 and the female mold 11 have a predetermined gap 19, and then the transparent or A semi-transparent molten resin material is injected into the gap 19 to form the container body 3.

【0008】また、容器としての特徴は、透明又は半透
明の合成樹脂材料からなる容器本体3と、該容器本体3
の内周面側に設けられ、且つ熱収縮性フィルムからなる
ラベル5とを備え、該ラベル5の容器本体3に面する外
表面には、文字,絵柄等の印刷が施されてなることにあ
る。
The container is characterized by a container body 3 made of a transparent or translucent synthetic resin material, and the container body 3
And a label 5 made of a heat-shrinkable film, which is provided on the inner peripheral surface side of the label. The outer surface of the label 5 facing the container body 3 is provided with characters, patterns, etc. is there.

【0009】[0009]

【作用】本発明の容器の製造方法において、筒状ラベル
5を雄型8に外嵌して密着状に加熱収縮し、その状態に
て雄型8と雌型11とを閉じて合成樹脂を注入することに
より容器本体3を形成するので、ラベル5の型8,11に対
する精度が何ら問題となることなくラベル5が一体に設
けられた容器本体3を形成でき、ラベル5は位置ずれし
たり、成形不良となることはない。
In the container manufacturing method of the present invention, the cylindrical label 5 is externally fitted to the male mold 8 and heat-shrinked in a close contact manner, and in that state, the male mold 8 and the female mold 11 are closed to remove the synthetic resin. Since the container body 3 is formed by pouring, the accuracy of the label 5 with respect to the molds 8 and 11 does not pose any problem, so that the container body 3 integrally provided with the label 5 can be formed. It does not cause molding failure.

【0010】しかも、本発明の容器においては、容器本
体3は透明又は半透明であることから、その内周面側の
ラベル5に記載された文字等を目視することができる。
また、容器本体3はラベル5を保護し、該ラベル5が不
慮に剥がれたり、脱落するのを防止でき、ラベル5の印
刷は、該ラベル5の外側に設けられていることから、容
器本体3に収容される内容物が食品であっても、印刷イ
ンキが食品に触れることがないため無害である。
Moreover, in the container of the present invention, since the container body 3 is transparent or translucent, the characters and the like written on the label 5 on the inner peripheral surface side can be visually observed.
Further, the container body 3 protects the label 5 and can prevent the label 5 from being peeled off or dropped off accidentally. Since the label 5 is printed on the outside of the label 5, the container body 3 Even if the contents contained in the food are food, the printing ink does not touch the food and is harmless.

【0011】[0011]

【実施例】以下、本発明の一実施例について図面に基づ
いて説明する。図1において、1は例えば食品が収容さ
れる容器を示し、該容器1は、合成樹脂製の容器本体3
と、該容器本体3の内側周面3aに装着された熱収縮性の
ラベル5とから構成されている。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will be described below with reference to the drawings. In FIG. 1, reference numeral 1 denotes a container for containing food, for example, and the container 1 is a container body 3 made of synthetic resin.
And a heat-shrinkable label 5 attached to the inner peripheral surface 3a of the container body 3.

【0012】前記容器本体3はポリプロピレン、ポリエ
チレン、ポリスチレン、ポリ塩化ビニル等の合成樹脂材
料からなり、所定の剛性を有するように射出成形により
形成されている。
The container body 3 is made of a synthetic resin material such as polypropylene, polyethylene, polystyrene and polyvinyl chloride, and is formed by injection molding so as to have a predetermined rigidity.

【0013】前記ラベル5は、例えば一軸延伸のポリプ
ロピレンの熱収縮性を有する合成樹脂性フィルム6から
なり、容器本体3に面する外側表面に文字,絵柄等の印
刷7が施されたラベルである。尚、容器本体3とラベル
5との材質が、ポリプロピレン等のように同種の場合や
印刷インキが接着性を有する場合には、ラベル5と容器
本体3とを接着するための接着樹脂層17は不要である
が、容器本体3とラベル5との材質が異なったり、両者
が同種の樹脂であってもラベル5の全面にインキ層が設
けられている場合には、これらラベル5と容器本体3と
を接着する接着性樹脂層17が必要となる。
The label 5 is made of, for example, a uniaxially stretched polypropylene synthetic resin film 6 having a heat-shrinking property, and is a label having a print 7 of characters, a pattern or the like on the outer surface facing the container body 3. . If the container body 3 and the label 5 are made of the same material such as polypropylene or the printing ink has adhesiveness, the adhesive resin layer 17 for bonding the label 5 and the container body 3 is Although not necessary, if the container body 3 and the label 5 are made of different materials, or if the ink layers are provided on the entire surface of the label 5 even if both are the same type of resin, the label 5 and the container body 3 An adhesive resin layer 17 for adhering and is required.

【0014】本発明の一実施例は以上の構成からなり、
次にその製造方法について説明する。先ず、図2(イ)
に示すようにフィルム6の両縁部を接合して予め筒状の
ラベル5を制作した後に、該筒状のラベル5を雄型8に
外嵌する。次に、例えば熱風を送風する装置、あるい
は、加熱ヒータからなる加熱装置9にてラベル5を加熱
すると、ラベル5は雄型8に密着して皺及び弛みのない
状態に収縮する。
An embodiment of the present invention has the above-mentioned configuration,
Next, the manufacturing method will be described. First, Fig. 2 (a)
As shown in FIG. 2, both edges of the film 6 are joined to produce a tubular label 5 in advance, and then the tubular label 5 is externally fitted to the male die 8. Next, when the label 5 is heated by, for example, a device that blows hot air or a heating device 9 that is a heater, the label 5 is brought into close contact with the male mold 8 and contracts without wrinkles and slack.

【0015】次に、熱収縮されたラベル5を備える雄型
8と雌型11とを接近させて型閉じを行う。このように型
閉じ状態において前記ラベル5と雌型11の内周面11aと
は、所定の間隙12が設けられており、該間隙12に溶融状
態にある樹脂材料を雌型11の注入路13を介して注入し、
ラベル5と一体的に容器本体3を形成する(図2
(ハ))参照。
Next, the male mold 8 and the female mold 11 having the heat-shrinkable label 5 are brought close to each other to close the mold. In this manner, in the mold closed state, a predetermined gap 12 is provided between the label 5 and the inner peripheral surface 11a of the female mold 11, and the resin material in a molten state is injected into the gap 12 of the female mold 11. Injected through
The container body 3 is integrally formed with the label 5 (see FIG. 2).
See (c)).

【0016】図3は本発明の他の実施例を示し、上記実
施例がラベル5を雄型8に沿うように熱収縮した後に、
型閉じを行ったのに対して、本実施例は、型閉じと同時
にラベル5を熱収縮するようにしたものである。即ち、
雌型11には、加熱装置9が一体的に設けられており、該
雌型11と雄型8との接近時にラベル5を加熱するように
構成されているのである。従って、このように両型8,11
を接近させる際に、同時にラベル5も加熱するので、更
に作業時間の短縮を図ることが可能となる。
FIG. 3 shows another embodiment of the present invention. In the above embodiment, after the label 5 is heat-shrinked along the male mold 8,
In contrast to the mold closing, in this embodiment, the label 5 is heat-shrinked simultaneously with the mold closing. That is,
The female die 11 is integrally provided with a heating device 9 so that the label 5 is heated when the female die 11 and the male die 8 approach each other. Therefore, in this way both types 8,11
Since the label 5 is heated at the same time when the two are brought close to each other, the working time can be further shortened.

【0017】また、前記両型8,11の型閉じは左右方向、
上下方向等の任意な方向で行うことができるのである
が、図4に示す如く、雄型8を上向きに配置し、雌型11
をその上方から移動する構成とし、筒状のラベル5を該
雄型8に外嵌すると共に、雄型8の上面8aには、外面側
に文字等が印刷された円形等の任意な形状の補助ラベル
15を載置する。そして、該ラベル5の加熱収縮時に、雄
型8から突出するその一端部5aを、ヒートシールした
り、あるいは感熱接着剤により補助ラベル15に接着させ
るのである。
Further, the mold closing of the both molds 8 and 11 is performed in the left-right direction,
Although it can be performed in any direction such as the vertical direction, as shown in FIG. 4, the male mold 8 is arranged upward and the female mold 11
Is moved from above, and the cylindrical label 5 is fitted onto the male die 8 and the upper surface 8a of the male die 8 has an arbitrary shape such as a circle with characters or the like printed on the outer surface side. Auxiliary label
Place 15. When the label 5 is heated and contracted, its one end 5a protruding from the male mold 8 is heat-sealed or adhered to the auxiliary label 15 with a heat-sensitive adhesive.

【0018】このように、補助ラベル15を容器本体3の
底部に設けることにより、容器本体3の全面に文字等が
表示できる利点がある。尚、この補助ラベル15は、上記
の如くラベル5の内側に設ける以外に、図4(ロ)に示
す如くラベル5を加熱収縮した後に、その一端部5aの外
側に接着しても良い。
As described above, by providing the auxiliary label 15 on the bottom of the container body 3, there is an advantage that characters or the like can be displayed on the entire surface of the container body 3. The auxiliary label 15 may be attached to the outside of the one end 5a after the label 5 is heated and shrunk as shown in FIG. 4B, instead of being provided inside the label 5 as described above.

【0019】尚、本発明は上記実施例に限定されるもの
ではなく、例えば、前記ラベル5は、熱収縮性ポリプロ
ピレンフィルムに限らず、例えば、ポリスチレン、ポリ
エステル、ポリエチレン、ポリ塩化ビニル等の熱収縮性
を有するフィルムでも良く、これらを材料とする発泡フ
ィルムから構成して、断熱効果を付加することもでき
る。
The present invention is not limited to the above embodiment, and the label 5 is not limited to a heat-shrinkable polypropylene film, but may be a heat-shrinkable material such as polystyrene, polyester, polyethylene or polyvinyl chloride. A film having a property may be used, or a foamed film made of such a material may be used to add a heat insulating effect.

【0020】また、該ラベル5は、上記材料からなるフ
ィルムを適宜組み合わせた多層フィルムであっても良
い。しかも、雌型11の形状を任意に設定することによ
り、容器本体3の内側の形状と外側の形状とが異なるよ
うに形成することができ、また、図1(イ)に示す如く
取手18や脚部19を設けたり、容器本体3の表面を凹凸状
に形成することが可能である。
Further, the label 5 may be a multilayer film in which films made of the above materials are appropriately combined. Moreover, by arbitrarily setting the shape of the female mold 11, the inside shape and the outside shape of the container body 3 can be formed to be different, and as shown in FIG. It is possible to provide the leg portions 19 or form the surface of the container body 3 in an uneven shape.

【0021】[0021]

【発明の効果】本発明の容器の製造方法は以上のように
構成されているので、筒状ラベルを雄型に外嵌して密着
状に加熱収縮し、その状態にて雄型と雌型とを閉じて合
成樹脂を注入することにより容器本体を形成するので、
従来のように一端ラベルを予備成形用型にて予備成形し
た後に、該予備成形品を予備成形用型から取り外して成
形型に装着する工程が省略できる。従って、製造工程の
簡略化が図れ生産性を向上することができる。
EFFECT OF THE INVENTION Since the method for producing a container of the present invention is configured as described above, the cylindrical label is fitted onto the male mold and heat-shrinked in a close contact, and in that state, the male mold and the female mold are attached. Because the container body is formed by closing and and injecting synthetic resin,
It is possible to omit a step of removing the preformed product from the preforming mold and mounting it on the forming mold after preliminarily molding the one-end label with the preforming mold as in the conventional case. Therefore, the manufacturing process can be simplified and the productivity can be improved.

【0022】しかも、ラベルを雄型に収縮させた状態に
て容器本体を成形するので、従来のように予備成形品と
してのラベルの型に対する精度が何ら問題となることな
く、ラベルの位置ずれ及び成形不良を防止できる。
Moreover, since the container body is molded in a state where the label is contracted to the male mold, there is no problem in the accuracy of the label mold as a preformed product as in the conventional case, and there is no positional deviation of the label and Molding defects can be prevented.

【0023】しかも、本発明の容器においては、容器本
体は透明又は半透明であることから、その内周面側のラ
ベルに記載された文字等を目視することができると共
に、容器本体の内側にラベルが設けられているので、該
ラベルは剥がれたり、脱落することはない。
Moreover, in the container of the present invention, since the container body is transparent or translucent, the characters and the like written on the label on the inner peripheral surface side can be visually observed and the inside of the container body can be seen. Since the label is provided, the label does not come off or fall off.

【0024】更に、ラベルの印刷は、該ラベルの外側に
設けられていることから、容器本体に収容される内容物
が食品であっても無害である。
Further, since the label is printed on the outside of the label, it is harmless even if the content contained in the container body is food.

【図面の簡単な説明】[Brief description of drawings]

【図1】本発明の一実施例を示し、(イ)は容器の断面
図、(ロ)は同要部断面図。
FIG. 1 shows an embodiment of the present invention, in which (a) is a sectional view of a container and (b) is a sectional view of the relevant part.

【図2】本発明の一実施例を示し、(イ)はラベルを雄
型に外嵌した状態の断面図、(ロ)はラベルを加熱収縮
する状態の断面図、(ハ)は型閉じ状態の断面図。
FIG. 2 shows an embodiment of the present invention, in which (a) is a cross-sectional view of a label fitted onto a male mold, (b) is a cross-sectional view of a label in which heat shrinks, and (c) is a mold closure. Sectional drawing of a state.

【図3】本発明の他の実施例を示す断面図。FIG. 3 is a sectional view showing another embodiment of the present invention.

【図4】本発明の他の実施例を示し、(イ)はラベルを
雄型に外嵌した状態の断面図、、(ロ)はラベルの加熱
収縮後の断面図、(ハ)は容器の要部断面図。
4A and 4B show another embodiment of the present invention, in which FIG. 4A is a cross-sectional view of the label externally fitted to the male mold, FIG. 4B is a cross-sectional view of the label after heat shrinkage, and FIG. FIG.

【図5】従来例を示し、(イ)は予備成形時の断面図、
(ロ)は成形時の断面図、(ハ)は一部断面を含む容器
の斜視図。
FIG. 5 shows a conventional example, (a) is a cross-sectional view during preforming,
(B) is a cross-sectional view at the time of molding, and (C) is a perspective view of the container including a partial cross-section.

【符号の説明】[Explanation of symbols]

3…容器本体、5…ラベル、8…雄型、11…雌型 3 ... Container body, 5 ... Label, 8 ... Male type, 11 ... Female type

───────────────────────────────────────────────────── フロントページの続き (51)Int.Cl.5 識別記号 庁内整理番号 FI 技術表示箇所 B29L 22:00 4F ─────────────────────────────────────────────────── ─── Continuation of the front page (51) Int.Cl. 5 Identification code Office reference number FI technical display location B29L 22:00 4F

Claims (2)

【特許請求の範囲】[Claims] 【請求項1】 筒状に形成された熱収縮性フィルムから
なるラベル(5)を雄型(8)に外嵌し、該ラベル
(5)を雄型(8)に沿うように加熱収縮した後に、該
ラベル(5)と雌型(11)とが所定の間隙(19)を有す
るように雄型(8)と雌型(11)とを型閉じ、次に、透
明又は半透明の溶融樹脂材料を前記間隙(19)に注入し
て容器本体(3)を形成することを特徴とする容器の製
造方法。
1. A label (5) made of a heat-shrinkable film formed in a tubular shape is fitted onto a male die (8), and the label (5) is heat-shrinked along the male die (8). After that, the male mold (8) and the female mold (11) are closed so that the label (5) and the female mold (11) have a predetermined gap (19), and then the transparent or translucent melting is performed. A method of manufacturing a container, characterized by injecting a resin material into the gap (19) to form a container body (3).
【請求項2】 透明又は半透明の合成樹脂材料からなる
容器本体(3)と、該容器本体(3)の内周面側に設け
られ、且つ熱収縮性フィルムからなるラベル(5)とを
備え、該ラベル(5)の容器本体3に面する外表面に
は、文字,絵柄等の印刷が施されてなることを特徴とす
る容器。
2. A container body (3) made of a transparent or translucent synthetic resin material, and a label (5) provided on the inner peripheral surface side of the container body (3) and made of a heat-shrinkable film. A container comprising the label (5), wherein an outer surface of the label (5) facing the container body 3 is printed with characters, patterns and the like.
JP24381992A 1992-09-11 1992-09-11 Container and production thereof Pending JPH0691692A (en)