JPH0644805Y2 - Blow molding container - Google Patents
Blow molding containerInfo
- Publication number
- JPH0644805Y2 JPH0644805Y2 JP4244388U JP4244388U JPH0644805Y2 JP H0644805 Y2 JPH0644805 Y2 JP H0644805Y2 JP 4244388 U JP4244388 U JP 4244388U JP 4244388 U JP4244388 U JP 4244388U JP H0644805 Y2 JPH0644805 Y2 JP H0644805Y2
- Authority
- JP
- Japan
- Prior art keywords
- container
- reinforcing
- blow molding
- strength
- molding container
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
【考案の詳細な説明】 〔産業上の利用分野〕 本考案はブロー成型容器に係り、特に補強面を形成して
強度を向上させたものに関する。[Detailed Description of the Invention] [Industrial field of application] The present invention relates to a blow-molded container, and more particularly to a container in which a reinforcing surface is formed to improve strength.
一般に、ブロー成型容器は胴部が肉薄となるため、その
胴部に周辺が他の面と段差を有する補強面を複数個所定
の間隔を以て形成し、強度を向上させるようにしてあ
る。In general, since the body of a blow-molded container is thin, a plurality of reinforcing surfaces are formed around the body at a predetermined distance from other surfaces so as to improve the strength.
このようなものとしては、例えば実開昭57-199511号公
報に記載されているものがあり、第4図に示すように、
凹部で縁どった補強面3を角型胴部の周囲に4箇所設
け、胴部を補強するようになっている。As such a thing, for example, there is one described in Japanese Utility Model Publication No. 57-199511, and as shown in FIG.
Reinforcing surfaces 3 framed by the recesses are provided at four places around the rectangular body to reinforce the body.
しかし、前記した従来のものにおいては、胴部の強度は
向上するが、強度的な不連続性が生じて局部的に強度不
足の部分が発生することがある。However, in the above-mentioned conventional one, although the strength of the body portion is improved, a discontinuity in strength may occur and a portion with insufficient strength may locally occur.
即ち、容器に内容物を充填するに際して、殺菌のため果
汁等を加熱した状態で行うことがあるが、この場合、内
容物が冷えると内圧が低下し容器を変形させる力が発生
する。この力は容器の強度が急変する部位、例えば、リ
ブを形成した部分と肩部との境目等に集中することがあ
る。That is, when the contents are filled in the container, the juice or the like may be heated for sterilization, but in this case, when the contents are cooled, the internal pressure is lowered and a force for deforming the container is generated. This force may be concentrated on a portion where the strength of the container suddenly changes, for example, a boundary between a rib-formed portion and a shoulder portion.
このため当該部分が座屈しこれが全体に波及して大きな
変形に至る場合がある。For this reason, the part may buckle, which may spread to the whole and cause large deformation.
本考案は前記事項に鑑みてなされたもので、筒状に形成
した胴部に、その周辺が他の面と段差を有する補強面を
所定の間隔を以て複数個形成したものにおいて、容器の
強度分布が急変する部分を補強し、容器全体の強度を向
上させることができるようにしたブロー成型容器を提供
することを技術的課題とする。The present invention has been made in view of the above-mentioned matters, and in the case where a plurality of reinforcing surfaces having a step difference with other surfaces are formed at a predetermined interval on a cylindrical body portion, the strength distribution of the container It is a technical object to provide a blow-molded container in which the strength of the entire container can be improved by reinforcing the portion where the temperature suddenly changes.
本考案は前記技術的課題を解決するために、以下のよう
な構成とした。The present invention has the following configuration in order to solve the above technical problems.
即ち、筒状に形成した胴部2に、その周辺が他の面と段
差を有する補強面3を所定の間隔を以て複数個形成す
る。That is, a plurality of reinforcing surfaces 3 having a step difference with other surfaces around the periphery of the barrel-shaped body 2 are formed at predetermined intervals.
これにより各補強面3の間に縦長面4を形成する。Thereby, the vertically long surface 4 is formed between the reinforcing surfaces 3.
この縦長面4の両端部分に凹所5を夫々形成してブロー
成型容器とした。Recesses 5 were formed at both ends of the vertically long surface 4 to obtain a blow molded container.
縦長面4の両端部分に凹所5を夫々形成することによ
り、容器の強度が急変する部位を補強することができ
る。By forming the recesses 5 at both end portions of the vertically long surface 4, it is possible to reinforce the portion where the strength of the container suddenly changes.
本考案の実施例を第1図ないし第3図に基づいて説明す
る。An embodiment of the present invention will be described with reference to FIGS.
容器本体1はポリエチレンテレフタレート(PET)製の
プリフォームをブロー成型したものであり、筒状に形成
した胴部2に、その周辺が他の面と段差を有する補強面
3が所定の間隔を以て6個形成されている。この補強面
3は第2図に示すように、胴部2の基準面に対して凹ま
せて凹部3aを形成するとともに、この凹部3aの中央部分
を胴部2の基準面付近にまで隆起させて凸部3bを形成し
たものである。The container body 1 is formed by blow molding a preform made of polyethylene terephthalate (PET), and a cylindrical body portion 2 has a reinforcing surface 3 having a step difference from other surfaces around the body portion 6 at a predetermined interval. Individually formed. As shown in FIG. 2, the reinforcing surface 3 is recessed from the reference surface of the body portion 2 to form a recessed portion 3a, and the central portion of the recessed portion 3a is raised up to near the reference surface of the body portion 2. To form the convex portion 3b.
これにより各補強面3の間に6本の縦長面4が形成され
ている。この縦長面4は胴部2の基準面となっており、
第3図に示すようにその両端部分に凹所5が形成されて
いる。この凹所5は長円形をなしており、その長径は補
強面3の高さの1/8程度に設定してある。また凹所5は
各補強面3の上下端を結んだ線よりも少許外側に位置せ
しめてあり、容器の強度分布が急変する部位を補強する
ようにしてある。As a result, six vertically long surfaces 4 are formed between the reinforcing surfaces 3. This vertically long surface 4 serves as a reference surface for the body portion 2,
As shown in FIG. 3, recesses 5 are formed at both ends thereof. The recess 5 has an oval shape, and its major axis is set to about 1/8 of the height of the reinforcing surface 3. The recess 5 is located slightly outside the line connecting the upper and lower ends of each reinforcing surface 3 so as to reinforce the portion where the strength distribution of the container suddenly changes.
このように、内容物充填後に内圧が降下して応力が局部
的に集中しても、容器の変形を最小限に抑えることがで
きる。In this way, even if the internal pressure drops and the stress is locally concentrated after filling the contents, the deformation of the container can be minimized.
本考案によれば、胴部に形成した複数個の補強面3の間
に縦長の縦長面4を形成し、この縦長面4の両端部分に
凹所5を夫々形成したので、局部的に強度不足となる部
分を補強することができ、容器全体の強度を向上させる
ことができた。According to the present invention, the vertically long surface 4 is formed between the plurality of reinforcing surfaces 3 formed on the body, and the recesses 5 are formed at both end portions of the vertically long surface 4, respectively. It was possible to reinforce the insufficient portion and improve the strength of the entire container.
第1図ないし第3図は本考案の一実施例を示し、第1図
は要部の側面図、第2図はそのA−A断面図、第3図は
そのB−B断面図、第4図は従来のブロー成型容器を示
す側面図である。 1……容器本体、2……胴部、 3……補強面、4……縦長面、 5……凹部。1 to 3 show an embodiment of the present invention. FIG. 1 is a side view of a main part, FIG. 2 is a sectional view taken along the line AA, and FIG. 3 is a sectional view taken along the line BB. FIG. 4 is a side view showing a conventional blow molding container. 1 ... Container body, 2 ... Body, 3 ... Reinforcing surface, 4 ... Longitudinal surface, 5 ... Concave part.
Claims (1)
面と段差を有する補強面3を所定の間隔を以て複数個形
成し、これにより各補強面3の間に縦長面4を形成し、
この縦長面4の両端部分に凹所5を夫々形成したことを
特徴とするブロー成型容器。1. A cylindrical body 2 is formed with a plurality of reinforcing surfaces 3 having a step on the periphery thereof with other surfaces at predetermined intervals, whereby vertical surfaces 4 are provided between the reinforcing surfaces 3. To form
A blow molding container characterized in that recesses 5 are formed at both ends of the vertically long surface 4, respectively.