JPH0614343U - Floor material - Google Patents

Floor material

Info

Publication number
JPH0614343U
JPH0614343U JP5267292U JP5267292U JPH0614343U JP H0614343 U JPH0614343 U JP H0614343U JP 5267292 U JP5267292 U JP 5267292U JP 5267292 U JP5267292 U JP 5267292U JP H0614343 U JPH0614343 U JP H0614343U
Authority
JP
Japan
Prior art keywords
veneer
cross plywood
thickness
cross
plywood
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP5267292U
Other languages
Japanese (ja)
Other versions
JP2582092Y2 (en
Inventor
守男 林
博 柴崎
栄 小山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panasonic Electric Works Co Ltd
Original Assignee
Matsushita Electric Works Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Matsushita Electric Works Ltd filed Critical Matsushita Electric Works Ltd
Priority to JP1992052672U priority Critical patent/JP2582092Y2/en
Publication of JPH0614343U publication Critical patent/JPH0614343U/en
Application granted granted Critical
Publication of JP2582092Y2 publication Critical patent/JP2582092Y2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

(57)【要約】 【目的】床材、特に耐熱床材における反りを防止する。 【構成】クロス合板1の表面に化粧薄単板2を接着して
積層すると共にクロス合板1の裏面側に切り溝3を形成
した床材である。クロス合板1の表面のフェイス単板1
aの厚さをクロス合板1の他の単板1bの厚さよりも充
分に薄くしてある。
(57) [Summary] [Purpose] To prevent warpage in floor materials, especially heat-resistant floor materials. [Structure] A floor material in which a decorative thin veneer 2 is adhered and laminated on the surface of a cross plywood 1 and a cut groove 3 is formed on the back surface side of the cross plywood 1. Face veneer 1 on the surface of cross plywood 1
The thickness of a is made sufficiently smaller than the thickness of the other veneer 1b of the cross plywood 1.

Description

【考案の詳細な説明】[Detailed description of the device]

【0001】[0001]

【産業上の利用分野】[Industrial applications]

本考案は、床材、特に耐熱床材における反り防止のための技術に関するもので ある。 The present invention relates to a technique for preventing warpage in a floor material, particularly a heat resistant floor material.

【0002】[0002]

【従来の技術】[Prior art]

従来からクロス合板の表面に化粧薄単板を積層すると共にクロス合板の裏面側 に切り溝を形成した床材が知られている。この床材は、図2に示すように、5プ ライまたは7プライのクロス合板1の表面に化粧薄単板2を接着して積層した直 貼り用の床材が知られている。このクロス合板1の表面に化粧薄単板2を接着す るに当たり、クロス合板1上に水溶性接着剤を塗布し、その上にラワン単板のよ うな化粧薄単板2を載せ、加熱プレスして接着するのであるが、この場合、11 0℃〜130℃で加熱プレスするものである。 BACKGROUND ART Conventionally, there is known a flooring material in which a decorative thin veneer is laminated on the surface of a cross plywood and a cut groove is formed on the back surface side of the cross plywood. As this floor material, as shown in FIG. 2, there is known a floor material for direct bonding in which a decorative thin veneer 2 is bonded and laminated on the surface of a 5-ply or 7-ply cross plywood 1. When adhering the decorative thin veneer 2 to the surface of the cross plywood 1, a water-soluble adhesive is applied on the cross plywood 1, and the decorative thin veneer 2 such as the Lauan veneer is placed on the cross plywood 1 and heated and pressed. In this case, hot pressing is performed at 110 ° C to 130 ° C.

【0003】[0003]

【考案が解決しようとする課題】[Problems to be solved by the device]

ところが、クロス合板1上に水溶性接着剤を塗布してその上に化粧薄単板2を 載せてセットすると水溶性接着剤の水分を化粧薄単板1が吸収して化粧薄単板1 が膨張(伸びる)し、そのままプレスするとプレス後の放熱状態において水分も 蒸発するため元の寸法に収縮する力が働いて全体として図2に示すように反ると いう問題がある。クロス合板1の裏面側に不陸に対応するために切り溝3を形成 しておくと、いっそう図2のように反りやすいという問題があった。 However, if the water-soluble adhesive is applied on the cross plywood 1 and the decorative thin veneer 2 is placed on it and set, the water of the water-soluble adhesive is absorbed by the decorative thin veneer 1 and the decorative thin veneer 1 is removed. When expanded (expanded) and pressed as it is, water also evaporates in the heat-dissipated state after pressing, and the force of contracting to the original dimension acts, causing a problem that the whole warps as shown in FIG. If the kerfs 3 are formed on the back side of the cross plywood 1 to deal with the unevenness, there is a problem that the warp is more likely to occur as shown in FIG.

【0004】 本考案は上記の従来例の問題点に鑑みて考案したものであって、その目的とす るところは、反りを防止できる床材を提供するにある。The present invention has been devised in view of the above-mentioned problems of the conventional example, and an object thereof is to provide a floor material capable of preventing warpage.

【0005】[0005]

【課題を解決するための手段】[Means for Solving the Problems]

本考案の床材は、クロス合板1の表面に化粧薄単板2を接着して積層すると共 にクロス合板1の裏面側に切り溝3を形成した床材であって、クロス合板1の表 面のフェイス単板1aの厚さをクロス合板1の他の単板1bの厚さよりも充分に 薄くしてあることを特徴とするものである。 The flooring material of the present invention is a flooring material in which a decorative thin veneer 2 is adhered and laminated on the surface of a cross plywood 1 and a cut groove 3 is formed on the back side of the cross plywood 1. It is characterized in that the thickness of the face veneer 1a of the surface is made sufficiently thinner than the thickness of the other veneer 1b of the cross plywood 1.

【0006】[0006]

【作用】[Action]

化粧薄単板2を接着して積層する影響で反ろうとするが、クロス合板のフェイ ス単板1aの厚さをクロス合板1の他の単板1bの厚さよりも充分に薄くするに より、反りを防止する。そして反り防止をフェイス単板1aを薄くするとの簡単 な改良でよいものである。 The decorative thin veneer 2 tends to warp due to the adhesion and lamination, but by making the thickness of the face veneer 1a of the cross plywood sufficiently thinner than the thickness of the other veneer 1b of the cross plywood 1, Prevent warpage. The warp can be prevented simply by improving the thickness of the face single plate 1a.

【0007】[0007]

【実施例】【Example】

以下本考案を添付図面に示す実施例に基づいて詳述する。クロス合板1は単板 を繊維方向が交差するように積層一体化したもので、5プライあるいは7プライ のものが用いられる。このクロス合板1には表面側に化粧薄単板2が接着して積 層してある。ここで、化粧薄単板2は0.25mm厚のものが使用され、またク ロス合板1としては9mm厚のものが使用される。クロス合板1には裏面側に多 数の切り溝3が形成してあり、この切り溝3は図1に示すようにクロス合板1の 上から2層目の単板1bに至るように形成してある。化粧薄単板2の繊維方向は クロス合板1の表層のフェイス単板1aの繊維方向に対して略直交するようにク ロスさせて、耐クラック性を高めてある。 Hereinafter, the present invention will be described in detail with reference to the embodiments shown in the accompanying drawings. The cross plywood 1 is made by laminating and integrating single plates so that the fiber directions cross each other, and 5 ply or 7 ply is used. A thin laminated veneer 2 is adhered and laminated on the front side of the cross plywood 1. Here, the decorative thin veneer 2 having a thickness of 0.25 mm is used, and the cross plywood 1 having a thickness of 9 mm is used. A large number of cut grooves 3 are formed on the back surface of the cross plywood 1, and the cut grooves 3 are formed so as to extend from the top of the cross plywood 1 to the second-layer veneer 1b as shown in FIG. There is. The decorative thin veneer 2 is crossed so that the fiber direction thereof is substantially orthogonal to the fiber direction of the face veneer 1a of the surface layer of the cross plywood 1 to enhance crack resistance.

【0008】 そして、クロス合板1の表層のフェイス単板1aと他の単板1bの厚さは、通 常は1.2mm(合板メーカーにおける厚さ)であるが、このようなクロス合板 1を使用する場合には、クロス合板1に化粧薄単板2を接着して積層する場合に は反りが生じるのであるが、かかる反りを抑制するべく、本考案においては、フ ェイス単板1aに0.7mm以上のサンディングをおこなってフェイス単板1a の厚さを0.5mm以下にする。しかして、クロス合板1の表面に化粧薄単板2 を接着積層することで、化粧薄単板2の影響で従来のように反りが発生しようと するが、クロス合板1のフェイス単板1aの厚さをクロス合板1の他の単板1b の厚さに比べて充分に薄く、つまり、0.5mm以下にすることで、クロス合板 1に化粧薄単板2を接着することにより反りが生じようとするのを抑制して、床 材全体としては反りのない状態とすることができる。なお、本考案において、ク ロス合板1の裏面側に切り溝3を設けたのは床材に全体として「腰」のある柔軟 性を持たせてコンクリートスラブ等の施工下地の不陸に対応できるようにするた めである。The thickness of the face veneer 1a on the surface layer of the cross plywood 1 and the other veneer 1b is normally 1.2 mm (thickness at the plywood maker). In the case of use, a warp occurs when the thin laminated veneer 2 is adhered and laminated on the cross plywood 1, but in the present invention, in order to suppress such warp, the face veneer 1a has no warp. The thickness of the face single plate 1a is reduced to 0.5 mm or less by performing sanding of 7 mm or more. Then, when the decorative thin veneer 2 is adhered and laminated on the surface of the cross plywood 1, warping is likely to occur due to the influence of the decorative thin veneer 2 as in the conventional case. By making the thickness sufficiently smaller than the thickness of the other veneer 1b of the cross plywood 1, that is, by setting it to 0.5 mm or less, a warp is caused by bonding the decorative thin veneer 2 to the cross plywood 1. It is possible to prevent the above from happening and to make the floor material as a whole without warpage. In the present invention, the grooving 3 is provided on the back surface side of the cross plywood 1 so that the flooring material as a whole has a "flexible" flexibility and can cope with the unevenness of the construction base such as the concrete slab. To do so.

【0009】 そして、上記床材の製造工程は、まずクロス合板1のフェイス単板1aをサン ディングして、クロス合板1の他の単板1bの厚さに比べて充分に薄くし、次に 化粧薄単板2を接着剤にて接着し、熱圧プレスをおこない、その後、フェイス単 板1aの表面を#180、#240のものでサンディングをおこない、次に実4 の加工をおこなう。そして、カラーリング、塗装をおこなった後、小割りをおこ ない、成型をおこなって製品化する。In the floor material manufacturing process, first, the face veneer 1a of the cross plywood 1 is sanded to be sufficiently thinner than the other veneer 1b of the cross plywood 1, and then The decorative thin veneer 2 is adhered with an adhesive and hot pressed, then the surface of the face veneer 1a is sanded with # 180 and # 240, and then the process of Ex. 4 is performed. After coloring and painting, the product is divided into small pieces and molded to produce a product.

【0010】 なお、上記の構成の床材はコンクリートスラブの上に直貼りされる場合、ある いは、暖房パネルの上に貼られる場合等、種々の用途があるが特に限定されるも のではない。しかしながら、上記のように構成することで反りの発生がないので 、特に熱の影響を受ける部分に使用する床材としても何ら問題がないものである 。The flooring material having the above-mentioned structure has various uses, such as a case where it is directly pasted on a concrete slab or a case where it is pasted on a heating panel, but it is not particularly limited. Absent. However, since the above structure does not cause warpage, there is no problem as a floor material used particularly in a portion affected by heat.

【0011】 そして、クロス合板1において、裏面のバック単板1cの厚さをフェイス単板 1aの厚さより更に薄くすると、化粧薄単板2を接着して積層するのに、一層反 りを抑制することができるものである。Then, in the cross plywood 1, if the thickness of the back veneer 1c on the back surface is made thinner than the thickness of the face veneer 1a, the decorative thin veneers 2 are bonded and laminated, further suppressing warpage. Is what you can do.

【0012】[0012]

【考案の効果】[Effect of device]

本考案にあっては、上述のように、クロス合板の表面のフェイス単板の厚さを クロス合板の他の単板の厚さよりも充分に薄くしてあるから、化粧薄単板側の影 響で反ろうとするのを、クロス合板のフェイス単板の厚さをクロス合板の他の単 板の厚さよりも充分に薄くするにより、反りを防止することができ、かつ反り防 止をフェイス単板を薄くするとの簡単な改良でよいものである。 In the present invention, as described above, the thickness of the face veneer on the surface of the cross plywood is made sufficiently thinner than the thickness of the other veneer of the cross plywood. If the thickness of the face veneer of the cross plywood is made sufficiently thinner than the thickness of the other veneer of the cross plywood, the warp can be prevented and the warp can be prevented from warping. A simple improvement by thinning the plate is good.

【図面の簡単な説明】[Brief description of drawings]

【図1】本考案の床材の断面図である。1 is a cross-sectional view of a flooring material of the present invention.

【図2】従来の床材において反っている状態を示す断面
図である。
FIG. 2 is a cross-sectional view showing a warped state of a conventional floor material.

【符号の説明】[Explanation of symbols]

1 クロス合板 1a フェイス単板 2 化粧薄単板 3 切り溝 1 Cross plywood 1a Face veneer 2 Decorative thin veneer 3 Cut groove

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 【請求項1】 クロス合板の表面に化粧薄単板を接着し
て積層すると共にクロス合板の裏面側に切り溝を形成し
た床材であって、クロス合板の表面のフェイス単板の厚
さをクロス合板の他の単板の厚さよりも充分に薄くして
あることを特徴とする床材。
1. A flooring material in which a decorative thin veneer is laminated on the surface of a cross plywood and a cut groove is formed on the back side of the cross plywood, and the thickness of the face veneer on the surface of the cross plywood is A flooring material characterized by being made sufficiently thinner than the thickness of other veneer of cross plywood.
JP1992052672U 1992-07-28 1992-07-28 Floor material Expired - Lifetime JP2582092Y2 (en)