JPH0474409B2 - - Google Patents
Info
- Publication number
- JPH0474409B2 JPH0474409B2 JP57226599A JP22659982A JPH0474409B2 JP H0474409 B2 JPH0474409 B2 JP H0474409B2 JP 57226599 A JP57226599 A JP 57226599A JP 22659982 A JP22659982 A JP 22659982A JP H0474409 B2 JPH0474409 B2 JP H0474409B2
- Authority
- JP
- Japan
- Prior art keywords
- metal
- arc column
- arc
- particles
- ultrafine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B22—CASTING; POWDER METALLURGY
- B22F—WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER; APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B22F9/00—Making metallic powder or suspensions thereof
- B22F9/02—Making metallic powder or suspensions thereof using physical processes
- B22F9/14—Making metallic powder or suspensions thereof using physical processes using electric discharge
Landscapes
- Manufacture Of Metal Powder And Suspensions Thereof (AREA)
- Physical Vapour Deposition (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP22659982A JPS59118803A (ja) | 1982-12-27 | 1982-12-27 | 金属超微粒子の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP22659982A JPS59118803A (ja) | 1982-12-27 | 1982-12-27 | 金属超微粒子の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS59118803A JPS59118803A (ja) | 1984-07-09 |
JPH0474409B2 true JPH0474409B2 (enrdf_load_stackoverflow) | 1992-11-26 |
Family
ID=16847712
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP22659982A Granted JPS59118803A (ja) | 1982-12-27 | 1982-12-27 | 金属超微粒子の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS59118803A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60228604A (ja) * | 1984-04-27 | 1985-11-13 | Hitachi Ltd | 超微粒子の製造方法 |
WO2011054113A1 (en) * | 2009-11-05 | 2011-05-12 | Ap&C Advanced Powders & Coatings Inc. | Methods and apparatuses for preparing spheroidal powders |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5117167A (ja) * | 1974-08-03 | 1976-02-10 | Nippon Steel Corp | Purazumajetsutonyoru kinzokufuntaino seizohoho |
JPS5544123A (en) * | 1978-09-20 | 1980-03-28 | Kamiichi Denshi Kk | Device for automatically shutting off main valve |
JPS5854166B2 (ja) * | 1981-12-17 | 1983-12-03 | 科学技術庁金属材料技術研究所長 | 金属微粒子の製造法およびその製造装置 |
JPS607682B2 (ja) * | 1982-01-29 | 1985-02-26 | 科学技術庁金属材料技術研究所長 | 金属微粒子製造装置における電極装置 |
-
1982
- 1982-12-27 JP JP22659982A patent/JPS59118803A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS59118803A (ja) | 1984-07-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Anders et al. | Macroparticle‐free thin films produced by an efficient vacuum arc deposition technique | |
JPH06508235A (ja) | アークソース用大粒子フィルター | |
Methling et al. | Magnetic studies on mass-selected iron particles | |
US4419381A (en) | Method of making magnetic material layer | |
JPH0474409B2 (enrdf_load_stackoverflow) | ||
JPS6116793B2 (enrdf_load_stackoverflow) | ||
JP4000764B2 (ja) | 真空アーク蒸発装置 | |
JPS59140303A (ja) | 金属超微粒子の製造方法 | |
JPH0227806B2 (ja) | Kohowajikajiseizairyooyobisonoseizohoho | |
JPS6367328B2 (enrdf_load_stackoverflow) | ||
JPS5836908A (ja) | 窒化物薄膜軟質磁性体の製造法 | |
JPS60130103A (ja) | 磁性粉末及びその製造法 | |
JPS59140307A (ja) | 金属超微粒子の製造装置 | |
JPS5887272A (ja) | プレ−ナマグネトロンスパツタ装置 | |
JPS60228609A (ja) | 超微粒子の製造方法 | |
JPS59140305A (ja) | 金属超微粒子の製造装置 | |
JP2752179B2 (ja) | 垂直磁気記録媒体及びその製造方法 | |
JPH02180003A (ja) | 強磁性超微粒子、その製造方法、磁気記録媒体および熱磁気記録媒体 | |
Shevchenko et al. | Granular thin film deposition by simultaneous spark erosion and sputtering | |
JPS60228608A (ja) | 超微粒子の製造方法と製造装置 | |
Calugaru et al. | Structure and magnetic properties of Al–Ni–Co fine particles produced by spark erosion | |
Hiraga et al. | Low Temperature Magnetic Properties of Austenitic Iron-Based Alloys Containing gamma' Particles | |
JPS5840248B2 (ja) | 磁気記録媒体およびその製造方法 | |
JPS60228606A (ja) | 超微粒子製造用の電極 | |
Tsuno | 4 Magnetic Lenses for |