JPH04332440A - Core for deflecting york - Google Patents

Core for deflecting york

Info

Publication number
JPH04332440A
JPH04332440A JP10256091A JP10256091A JPH04332440A JP H04332440 A JPH04332440 A JP H04332440A JP 10256091 A JP10256091 A JP 10256091A JP 10256091 A JP10256091 A JP 10256091A JP H04332440 A JPH04332440 A JP H04332440A
Authority
JP
Japan
Prior art keywords
core
deflecting
york
film
core pieces
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP10256091A
Other languages
Japanese (ja)
Inventor
Masaaki Irie
入江 真明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Electric Corp
Original Assignee
Mitsubishi Electric Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Electric Corp filed Critical Mitsubishi Electric Corp
Priority to JP10256091A priority Critical patent/JPH04332440A/en
Publication of JPH04332440A publication Critical patent/JPH04332440A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To improve electromagnetic characteristics of a deflecting york and stabilize the characteristics by coating two core pieces of a core for the deflecting york divided into two after baking with a thermal shrink film, and shrinking the film thermally so as to be fixed in one united body. CONSTITUTION:Two core pieces 1a and 1b of a core for a deflecting york divided into two after baking are combined together, and are sandwiched between separators 2, and a conical cylinder shape heat-shrinkable film 5 is coated around the both core pieces 1a and 1b. Next, when the film 5 is shrunk after heat is applied, as for installation of the film 5, the core pieces 1a and 1b are fixed in one united body by means of shrinkage force. Then, a cross sectional area of the core 1 is uniformized all over its periphery, and magnetic flux density is uniformized, so that electromagnetic characteristics can be improved as the deflecting york. Furthermore, since a clip groove is used as a molding metal mold and a projection part does not exist in it, raw materials can flow smoothly, and molding density of the core 1 is uniformized, so that the characteristics can be stabilized as the deflecting york.

Description

【発明の詳細な説明】[Detailed description of the invention]

【0001】0001

【産業上の利用分野】この発明は、CRTに用いる偏向
ヨーク用コアに関するものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a core for a deflection yoke used in a CRT.

【0002】0002

【従来の技術】図2は、従来の偏向ヨーク用コアを示す
。図において、1a,1bは焼成後に2分割された偏向
ヨーク用コア1のコア片、2は組み合わされた2つのコ
ア片1a,1bを挟むセパレータ、3は2つのコア片1
a,1bを一体に固定するためのクリップ、4a,4b
はクリップ3を嵌めるためのクリップ用溝で、両コア片
1a,1bにあらかじめ設けたものである。両コア片1
a,1bは、クリップ3をクリップ用溝4a,4bに嵌
めることによって一体に固定されている。
2. Description of the Related Art FIG. 2 shows a conventional core for a deflection yoke. In the figure, 1a and 1b are the core pieces of the deflection yoke core 1 divided into two after firing, 2 is a separator that sandwiches the combined two core pieces 1a and 1b, and 3 is the two core pieces 1.
Clips 4a, 4b for fixing a, 1b together
A clip groove for fitting the clip 3 is provided in advance on both core pieces 1a and 1b. Both core pieces 1
a and 1b are fixed together by fitting the clip 3 into the clip grooves 4a and 4b.

【0003】0003

【発明が解決しようとする課題】しかし、従来の偏向ヨ
ーク用コアにあっては、2つのコア片1a,1bを固定
するためにクリップ用溝4a,4bを設けなければなら
ないので、次のような問題があった。 (1)クリップ用溝4a,4b部分の断面積が小さいた
め、コア中の磁束がこの部分に集中し、偏向ヨークの電
磁気特性が悪くなる。 (2)コアの成形時に、クリップ用溝4a,4bを形成
するための金型の凸部によって原料の顆粒粉末の動きが
部分的に阻害されるので、成形密度が不均一になり、焼
成後のコアの寸法精度、特に、真円度が低下する。この
ため、偏向ヨークの特性が不安定となる。
However, in the conventional core for a deflection yoke, clip grooves 4a and 4b must be provided in order to fix the two core pieces 1a and 1b. There was a problem. (1) Since the cross-sectional area of the clip grooves 4a and 4b is small, the magnetic flux in the core is concentrated in these parts, deteriorating the electromagnetic characteristics of the deflection yoke. (2) When molding the core, the movement of the raw material granule powder is partially obstructed by the protrusions of the mold for forming the clip grooves 4a and 4b, resulting in uneven molding density and The dimensional accuracy of the core, especially the roundness, decreases. Therefore, the characteristics of the deflection yoke become unstable.

【0004】この発明は、上記のような問題点を解消す
るためになされたもので、偏向ヨークの電磁気特性の向
上と特性の安定化を図ることができる偏向ヨーク用コア
を提供することを目的とする。
The present invention was made to solve the above-mentioned problems, and an object thereof is to provide a core for a deflection yoke that can improve the electromagnetic characteristics of the deflection yoke and stabilize the characteristics. shall be.

【0005】[0005]

【課題を解決するための手段】この発明が提供する偏向
ヨーク用コアは、焼成後に2分割された偏向ヨーク用コ
アの2つのコア片を、両コア片に被せて熱収縮させた熱
収縮性フィルムで一体に固定してなる構成としたもので
ある。
[Means for Solving the Problems] The core for a deflection yoke provided by the present invention has a heat-shrinkable structure in which two core pieces of a core for a deflection yoke, which are divided into two parts after firing, are placed over both core pieces and heat-shrinked. It has a structure in which it is fixed together with a film.

【0006】[0006]

【作用】この発明による偏向ヨーク用コアは、従来不可
欠であったクリップ用溝を設けないので、コアの断面積
がどの部分も全周にわたって均一になり、磁束密度も均
一になる。このため、偏向ヨークの電磁気特性が向上す
る。また、成形用金型に上記クリップ用溝に対応する凸
部を設けなくてよいので、金型のキャビティ内において
原料の顆粒粉末がスムーズに動き、特定個所に偏在しな
くなる。このため、コアの成形密度が均一になり、焼成
後のコアの寸法精度、特に、その真円度が向上し、偏向
ヨークの特性が安定する。
[Operation] Since the core for a deflection yoke according to the present invention does not have a clip groove, which was conventionally indispensable, the cross-sectional area of the core is uniform throughout the entire circumference, and the magnetic flux density is also uniform. Therefore, the electromagnetic characteristics of the deflection yoke are improved. Furthermore, since it is not necessary to provide a convex portion corresponding to the clip groove on the molding die, the raw material granule powder moves smoothly within the cavity of the die and is not unevenly distributed in a specific location. Therefore, the molding density of the core becomes uniform, the dimensional accuracy of the core after firing, especially its roundness, improves, and the characteristics of the deflection yoke become stable.

【0007】[0007]

【実施例】図において、1a,1bは焼成後に2分割さ
れた偏向ヨーク用コア1のコア片、2は組み合わされた
2つのコア片1a,1bを挟むセパレータである。いず
れも、図2におけると同一の部分を示す。5は、組み合
わせた2つのコア片1a,1bに被せ、熱収縮させるこ
とによって、両コア片1a,1bの外周面に帯状に一体
に取り付けたコア固定用の熱収縮性フィルムである。
DESCRIPTION OF THE PREFERRED EMBODIMENTS In the figure, 1a and 1b are core pieces of the deflection yoke core 1 which is divided into two parts after firing, and 2 is a separator that sandwiches the combined two core pieces 1a and 1b. Both show the same parts as in FIG. Reference numeral 5 denotes a heat-shrinkable film for fixing the core, which is integrally attached in a band shape to the outer peripheral surfaces of both the core pieces 1a and 1b by covering the two combined core pieces 1a and 1b and heat-shrinking the film.

【0008】帯状の熱収縮性フィルムの取り付けは、例
えば、次の要領で行う。まず、焼成後2分割された偏向
ヨーク用コア1の2つのコア片1a,1bを組み合わせ
てセパレータ2で挟み、両コア片1a,1bの周囲に円
錐筒状の熱収縮性フィルム5を被せる。次いで、フィル
ム5に熱を加えて、これを収縮させる。このようにする
と、上記2つのコア片1a,1bは、熱収縮性フィルム
5の収縮力によって、一体に固定される。
[0008] The belt-shaped heat-shrinkable film is attached, for example, in the following manner. First, the two core pieces 1a and 1b of the deflection yoke core 1, which has been divided into two parts after firing, are combined and sandwiched between separators 2, and a conical cylindrical heat-shrinkable film 5 is placed around both core pieces 1a and 1b. Next, heat is applied to the film 5 to shrink it. In this way, the two core pieces 1a and 1b are fixed together by the shrinkage force of the heat-shrinkable film 5.

【0009】なお、実施例では、フィルム5をコア片1
a,1bの外周面全域に被せる場合について説明したが
、外周面に部分的に帯状に被せるようにしてもよい。
In the embodiment, the film 5 is attached to the core piece 1.
Although the case has been described in which the entire outer peripheral surfaces of the parts a and 1b are covered, the outer peripheral surfaces may be partially covered in a band-like manner.

【0010】上記のように、この実施例においては、従
来必要としたクリップ用溝をコア1に設けないで、コア
1の断面積がどの部分をとっても全周にわたって均一に
なり、したがって磁束密度も均一になる。このため、偏
向ヨークとしての電磁気特性が向上する。
As described above, in this embodiment, the core 1 is not provided with the groove for the clip, which is conventionally required, so that the cross-sectional area of the core 1 is uniform throughout the entire circumference, and therefore the magnetic flux density is also increased. It becomes uniform. Therefore, the electromagnetic characteristics of the deflection yoke are improved.

【0011】また、成形用の金型に上記クリップ用溝を
形成するための凸部を設けなくてよいので、金型のキャ
ビティ内において、原料の顆粒粉末がスムーズに流れ、
特定個所に偏在しなくなる。このため、コア1の成形密
度が均一になり、焼成後の寸法精度、特に真円度が向上
し、偏向ヨークとしての特性が安定する。
[0011] Furthermore, since there is no need to provide a protrusion for forming the above-mentioned clip groove in the molding die, the granular powder of the raw material flows smoothly in the cavity of the die.
It will no longer be unevenly distributed in specific locations. Therefore, the molding density of the core 1 becomes uniform, the dimensional accuracy after firing, especially the roundness, improves, and the characteristics as a deflection yoke become stable.

【0012】0012

【発明の効果】以上のように、この発明によれば、2つ
のコア片を熱収縮性フィルムで固定するようにし、クリ
ップ用溝を設けなくて済むようにしたので、偏向ヨーク
の電磁気特性の向上と、特性の安定化を図ることができ
る。
[Effects of the Invention] As described above, according to the present invention, the two core pieces are fixed with a heat-shrinkable film, and there is no need to provide a clip groove, so that the electromagnetic characteristics of the deflection yoke can be improved. It is possible to improve the performance and stabilize the characteristics.

【図面の簡単な説明】[Brief explanation of the drawing]

【図1】実施例の偏向ヨーク用コアの側面図[Fig. 1] Side view of the deflection yoke core of the embodiment

【図2】従
来の偏向ヨーク用コアの側面図
[Figure 2] Side view of a conventional deflection yoke core

【符号の説明】[Explanation of symbols]

1    偏向ヨーク用コア 1a,1b  偏向ヨーク用コア1のコア片2    
セパレータ
1 Deflection yoke core 1a, 1b Core piece 2 of deflection yoke core 1
separator

Claims (1)

【特許請求の範囲】[Claims] 【請求項1】  焼成後に2分割された偏向ヨーク用コ
アの2つのコア片を、両コア片に被せて熱収縮させた熱
収縮性フィルムで一体に固定してなる偏向ヨーク用コア
1. A core for a deflection yoke, in which two core pieces of the core for a deflection yoke, which are divided into two after firing, are fixed together with a heat-shrinkable film that is covered with both core pieces and heat-shrinked.
JP10256091A 1991-05-08 1991-05-08 Core for deflecting york Pending JPH04332440A (en)