JPH0330505Y2 - - Google Patents
Info
- Publication number
- JPH0330505Y2 JPH0330505Y2 JP10033687U JP10033687U JPH0330505Y2 JP H0330505 Y2 JPH0330505 Y2 JP H0330505Y2 JP 10033687 U JP10033687 U JP 10033687U JP 10033687 U JP10033687 U JP 10033687U JP H0330505 Y2 JPH0330505 Y2 JP H0330505Y2
- Authority
- JP
- Japan
- Prior art keywords
- side wall
- pool
- panel
- deck
- finishing panel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【考案の詳細な説明】
〔産業上の利用分野〕
本考案は老朽化したプールの側壁を改修するそ
の構造に関するものである。[Detailed Description of the Invention] [Industrial Application Field] The present invention relates to a structure for repairing the side wall of a dilapidated swimming pool.
従来、プールの材質はコンクリート製、金属
製、FRP製、に大別できるが、長期間の使用に
よりコンクリート製の場合はひび割れや、風化浸
食による表面の凹凸化が発生し使用不能となつた
り、金属製の場合はプールに使用される塩素滅菌
剤の影響も受け特に溶接部分で激しく局部腐蝕が
起ると共に、地面との電位差との関係で腐蝕が促
進され漏水を生じ、さらに、FRP製の場合は前
記塩素滅菌剤や紫外線により表面色が退色した
り、傷や微細なひび割れが発生し、漏水はないも
のの外観上見苦しいという問題があるいずれの場
合も改修が必要となる。
Traditionally, swimming pools can be broadly classified into concrete, metal, and FRP materials, but after long-term use, concrete can become unusable due to cracks and uneven surfaces due to weathering and erosion. If it is made of metal, it will be affected by the chlorine sterilizer used in swimming pools, and severe local corrosion will occur, especially in the welded parts, and the corrosion will be accelerated due to the potential difference with the ground, resulting in water leakage. In any case, the surface color may fade due to the chlorine sterilizer or ultraviolet rays, or scratches or minute cracks may occur, and even if there is no water leakage, the appearance is unsightly, and repair is required.
これ等諸欠陥は主にプール底部分に発生する
が、例外なくプール側壁部分にも発生する。この
プール側壁を改修する場合、プール側壁の全体に
亘つて不飽和ポリエステルやエポキシ系の樹脂を
塗布し、この上にガラス繊維を敷いて脱泡し、ま
た上記の樹脂を塗布するという作業が何回も繰り
返される方法が主として行なわれている(これに
より形成されるものが所謂FRPである)。 These defects mainly occur on the bottom of the pool, but without exception they also occur on the side walls of the pool. When renovating this pool side wall, it is necessary to apply an unsaturated polyester or epoxy resin to the entire side wall, lay glass fiber on top to defoam, and then apply the above resin. The method that is repeated many times is mainly used (the product formed by this method is the so-called FRP).
しかしこのような先行技術の場合、作業が繁雑
で手間がかかり、従つて工期を要するためコスト
が高くなるという問題点がある。 However, in the case of such prior art, there is a problem that the work is complicated and time-consuming, and therefore the cost is high because it requires a long construction period.
本考案の技術的課題は老朽化したプール側壁の
改修に際し、短い工期で手間のかからない経済的
なプール側壁の改修構造を提供する為に、FRP
等の合成樹脂製ライニング材の塗布面積を最小限
度に抑えることにある。
The technical problem of this invention is to provide an economical pool side wall repair structure that requires less time and effort in a short construction period when repairing aging pool side walls.
The objective is to minimize the area of synthetic resin lining material applied.
本考案の技術的手段は平面四角状を呈し裏面に
充填材を塗布したFRP等の合成樹脂製側壁仕上
パネルと、断面形を呈し裏面に充填材を塗布し
たFRP等の合成樹脂製デツキボーダー仕上パネ
ルとを用意し、上記側壁仕上パネルをプール側壁
全長に渉り平行に圧着すると共に、その側壁仕上
パネル上端との間に充填材の洩材確認間隔をおい
てプール側壁全長に渉りデツキボーダー仕上パネ
ルを端縁を当接させて平行に圧着し、側壁仕上パ
ネル相互間に、FRP等の合成樹脂製ライニング
材を埋込固定したことである。
The technical means of this invention is a side wall panel made of synthetic resin such as FRP which has a square planar shape and has a filler applied to the back side, and a deck border finish made of synthetic resin such as FRP which has a cross-sectional shape and has a filler applied to the back side. Prepare a panel and crimp the side wall finishing panel in parallel across the entire length of the pool side wall, and at the same time, leave a space between the top edge of the side wall finishing panel to check for leakage of filler material, and spread it across the entire length of the pool side wall to create a deck border. The finished panels are pressed together in parallel with their edges abutting, and a synthetic resin lining material such as FRP is embedded and fixed between the side wall finished panels.
次に、本考案の実施例を図面に基づいて説明す
る。
Next, embodiments of the present invention will be described based on the drawings.
図面は既設プールとしてアルミ製のプールを示
している。このプールはデツキa1−1を上端に水
平に延設したアルミ製の側壁パネルa1−2多数枚
を溶接等で接合することによつて形成したプール
側壁a1の下端にアルミ製の底用パネルa2−1多数
枚を敷設してプール底a2が形成されている。 The drawings show an aluminum pool as the existing pool. This pool consists of an aluminum side wall panel A 1 - 1 that extends horizontally from the upper end of the pool side wall A 1 - 2, which is formed by joining a number of panels A 1 - 2 by welding, etc., and an aluminum bottom at the lower end of the pool side wall A 1 . The pool bottom A2 is formed by laying a large number of panels A2-1 .
この既設プールにおいてプール側壁a1はデツキ
a1−1を改修するデツキボーダー仕上パネル1
と、プール側面a1−3を改修する側壁仕上パネル
2と、FRP等の合成樹脂製のライニング材5と
を用いて改修され、プール底a2は底壁仕上パネル
3及び上記と同様なライニング材5を用いて改修
される。 In this existing pool, pool side wall a1 is decked.
Deck border finishing panel 1 to repair a 1-1
The pool bottom a 2 is renovated using a side wall finishing panel 2 that repairs the pool side surface a 1 - 3 and a lining material 5 made of synthetic resin such as FRP, and the pool bottom a 2 is renovated using a bottom wall finishing panel 3 and a lining similar to the above. It will be renovated using material 5.
デツキボーダー仕上パネル1は既設プールのデ
ツキa1−1を仕上げるデツキ面部1−1と、その
デツキ面部1−1先端から垂設しプール側面a1−
3上端部分を仕上げる上隅面部1−2とで形成さ
れたFRP等の合成樹脂製のもので、長さ数十cm
〜数m、デツキ面部1−1の幅を50〜100mm、上
隅面部1−2の高さを20〜50mm程度にしてなり、
デツキ面部1−1の長さ方向に125mm等の適当な
ピツチ間隔をもつて逆円錐台状の凹所1−3を多
数凹設すると共に、デツキ面部1−1と、上隅面
部−2とのコーナー裏面を既設プールのデツキa1
−1とプール側面a1−3との境界部の曲率よりも
小さくしてその部分に図示するように全長に渉つ
て隙間10が形成されるようにすると共に上隅面
部1−2裏面下縁部分にプール内方向に傾斜する
傾斜面11を形成している。 The deck border finishing panel 1 includes a deck surface portion 1-1 that finishes the deck a 1 -1 of an existing pool, and a deck surface portion 1-1 that is hung vertically from the tip of the deck surface portion 1-1 to finish the deck surface a 1 -1 of the existing pool.
3.It is made of synthetic resin such as FRP and is several tens of centimeters long, formed by the upper corner surface 1-2 that finishes the upper end part.
~ several meters, the width of the deck surface part 1-1 is about 50 to 100 mm, and the height of the upper corner surface part 1-2 is about 20 to 50 mm,
A large number of inverted truncated cone-shaped recesses 1-3 are provided in the length direction of the deck surface 1-1 at appropriate pitch intervals such as 125 mm, and the deck surface 1-1 and the upper corner surface 2 are The back of the corner of the existing swimming pool A 1
The curvature of the boundary between -1 and the pool side a 1 -3 is made smaller than the curvature of the boundary, so that a gap 10 is formed in that part over the entire length as shown in the figure, and the lower edge of the back surface of the upper corner part 1-2. A sloped surface 11 that slopes toward the inside of the pool is formed in the portion.
側壁仕上パネル2は上記デツキボーダー仕上パ
ネル1の上隅面部1−2下縁と相対する上縁を除
く他3縁に一段低い取付鍔部2−1を段設すると
共に裏面にクツシヨン材7を収容する所定高さの
凹部2−2を凹設した所望長さで且つ、その巾を
プールの深さに準じた所望巾とするFRP等の合
成樹脂で成形されたシート状物であり、裏面上縁
部分に上記上隅面部1−2の傾斜面11とでハの
字を形成する傾斜面2−3を形成し、上縁近傍部
分に長さ方向全長にわたつて125mm等の適当なピ
ツチ間隔をもつて逆円錐台状の凹所2−4が多数
凹設されている。 The side wall finishing panel 2 has lower mounting flanges 2-1 stepped on three edges other than the upper edge opposite to the lower edge of the upper corner 1-2 of the deck border finishing panel 1, and a cushion material 7 on the back side. It is a sheet-like object molded from synthetic resin such as FRP with a desired length and a desired width corresponding to the depth of the pool, with a recessed portion 2-2 of a predetermined height for accommodating the pool. An inclined surface 2-3 forming a V-shape with the inclined surface 11 of the upper corner surface 1-2 is formed on the upper edge, and a suitable pitch such as 125 mm is formed in the vicinity of the upper edge along the entire length. A large number of inverted truncated cone-shaped recesses 2-4 are provided at intervals.
斯るデツキボーダー仕上パネル1は裏面及び前
記隙間10内にシリコン等の充填材6を充填した
状態で、この充填材6が固化する前にデツキa1−
1に沿い長さ方向に必要枚圧着し、更に凹所1−
3内においてデツキa1−1にリベツト8で縫着す
ることによつて固定する。 Such a deck border finished panel 1 is provided with a filler 6 such as silicone filled on the back side and in the gap 10, and before the filler 6 hardens, the deck border finish panel 1 is finished with a deck a 1 -.
Crimp the necessary sheets in the length direction along 1, and then press the recess 1-
It is fixed by sewing it to the deck a 1 -1 in 3 with rivets 8.
この時、圧着行為に伴ないデツキボーダー仕上
パネル1の四方から充填材6が洩れ出るが、上隅
面部1−2下縁を除いてその洩材をふきとること
とする。 At this time, the filler material 6 leaks from all sides of the deck border finished panel 1 due to the crimping operation, but the leakage material is wiped off except for the lower edge of the upper corner portion 1-2.
側壁仕上パネル2はクツシヨン材7部分を除く
裏面全面あるいは、デツキボーダー仕上パネル1
の上隅面部1−2に近接する上域面裏面のみに充
填材6を塗布し、この充填材6が固化する前にデ
ツキボーダー仕上パネル1の上隅面部1−2下縁
との間に2〜3mm程度の洩材確認間隔4を確保す
る位置に上縁を位置させてプール側面a1−3長さ
方向に必要枚圧着し、更に凹所2−4内及び取付
鍔部2−1をリベツト8でプール側面a1−3に縫
着することによつて固定する。 The side wall finish panel 2 is the entire back surface except for the cushion material 7, or the deck border finish panel 1
The filler 6 is applied only to the back surface of the upper area near the upper corner 1-2, and before the filler 6 hardens, it is applied between the lower edge of the upper corner 1-2 of the deck border finishing panel 1. Position the upper edge at a position that ensures a leakage confirmation interval 4 of about 2 to 3 mm, and crimp the necessary pieces in the length direction of the pool side surface a 1 - 3, and then press the inside of the recess 2-4 and the mounting collar 2-1. are fixed by sewing them to the pool side surfaces a1-3 with rivets 8.
この時圧着行為に伴なつて側壁仕上パネル2の
四方から充填材6が洩れ出るか、あるいは上縁面
のみから益れ出るが、洩材確認間隔4から洩材が
溢れると少なくともデツキボーダー仕上パネル1
と、側壁仕上パネル2との接続部分においては完
全にシールされたことが確認されたことになり溢
れた洩材はその場でふき取る。 At this time, the filling material 6 leaks from all sides of the side wall finishing panel 2 due to the crimping action, or leaks only from the upper edge surface, but if the filling material 6 overflows from the leakage material confirmation interval 4, at least the deck border finishing panel 1
Then, it is confirmed that the connection part with the side wall finishing panel 2 is completely sealed, and any overflowing material is wiped off on the spot.
また、側壁仕上パネル2,2相互間、側壁仕上
パネル2、底壁仕上パネル3相互間は取付鍔部2
−1,2−1間、取付鍔部2−1,3−1間に発
泡性のポリエチレン、ウレタン等のテープ9を全
長に渉つて貼着してガラス繊維の落下を防止した
状態でライニング材5の埋め込み作業を遂行して
プール側壁の回収は終了する。 In addition, between the side wall finishing panels 2 and 2, and between the side wall finishing panels 2 and the bottom wall finishing panels 3, the mounting flange 2 is
-1, 2-1 and between the mounting flanges 2-1, 3-1, a tape 9 made of foamed polyethylene, urethane, etc. is pasted along the entire length to prevent the glass fibers from falling. After performing the embedding work in step 5, the recovery of the pool side wall is completed.
ライニング材5は、従来周知の如く、硬化剤、
促進剤等の添加剤を含む不飽和ポリエステルやエ
ポキシ系の熱硬化性樹脂剤とガラス繊維より成つ
ている。 As is conventionally known, the lining material 5 includes a curing agent,
It is made of unsaturated polyester or epoxy thermosetting resin containing additives such as accelerators and glass fiber.
底壁仕上パネル3は周縁に取付鍔部3−1を残
して裏面に所定高さの凹部3−2を設けることに
よつて周縁部に段部3−3(間隙)を間接的に形
成し、プール底a2の短手巾に対して所望長さで且
つ所望巾とするFRP等の合成樹脂等で成形した
平面矩形状のシート状物であり、凹部3−2内に
クツシヨン材7を収容した状態で取付鍔部3−1
をリベツト8止めすることによつてプール底a2全
面に、それぞれ平行に敷設固定されている。 The bottom wall finishing panel 3 leaves the mounting flange 3-1 on the periphery and provides a recess 3-2 of a predetermined height on the back surface, thereby indirectly forming a step 3-3 (gap) on the periphery. , is a planar rectangular sheet-like material molded from synthetic resin such as FRP with a desired length and desired width relative to the short width of the pool bottom A2 , and the cushion material 7 is accommodated in the recessed portion 3-2. Mounting flange 3-1 in the state
They are laid and fixed parallel to each other on the entire surface of the pool bottom A2 by fixing them with 8 rivets.
クツシヨン材7は若干の弾力性を有する合成樹
脂等の発泡材料を用いて、上記凹部2−2,3−
2の高さよりやや高い高さを有するシート状に形
成したもので、凹部2−2,3−2内に粘着収容
するか或は図示するように側壁仕上パネル2底壁
仕上パネル3が敷設される予め箇所に配置し、そ
のパネル2,3を敷設した際、自動的にその凹部
2−2,3−2内に収容できるようにする。 The cushion material 7 is made of a foamed material such as a synthetic resin having some elasticity, and is made of a foam material such as a synthetic resin having some elasticity.
It is formed into a sheet shape having a height slightly higher than the height of 2, and is adhesively accommodated in the recesses 2-2 and 3-2, or the side wall finishing panel 2 and the bottom wall finishing panel 3 are laid as shown in the figure. When the panels 2 and 3 are laid down, they can be automatically accommodated in the recesses 2-2 and 3-2.
この底壁仕上パネル3,3相互間においても側
壁仕上パネル2,2相互間と同様に発泡性のポリ
エチレン、ウレタン等のテープ9を全長に渉つて
貼着してライニング材5を塗布する。 Also between the bottom wall finishing panels 3, 3, the lining material 5 is applied by pasting a foaming polyethylene, urethane, etc. tape 9 over the entire length in the same way as between the side wall finishing panels 2, 2.
尚、12は凹部1−3,2−4内に充填する充
填材、13はライニング材5上に塗布するゲルコ
ート層であり、14は段差をうめる為の樹脂製パ
テであり、この樹脂製パテ14を前記テープ9の
代りに充填し、その上にFRPライニング材5を
埋め込んでもよい。 In addition, 12 is a filler to be filled into the recesses 1-3 and 2-4, 13 is a gel coat layer applied on the lining material 5, and 14 is a resin putty for filling the steps. 14 may be filled instead of the tape 9, and the FRP lining material 5 may be embedded thereon.
ちなみに、本実施例においては底壁仕上パネル
3、側壁仕上パネル2、デツキボーダー仕上パネ
ル1の全高Xは全て6mmとし、改修壁を形成した
際、その改修壁が面一になるようになつており、
そして側壁仕上パネル2、デツキボーダー仕上パ
ネル1を圧着する際に、裏面の充填材6の反発圧
によつて側壁仕上パネル2自体が波をうつような
変形を起こすことがないように配慮され、また、
前記隙間10内にも充填材6が充填されて固化す
るから、永年使用によつて裏面の充填材に万が一
折損等が生じても、その隙間10内の厚肉な充填
材6部分が堰として作用し、プール水の流出や、
デツキa1−1に溢流した水の流入を阻止する利点
がある。 By the way, in this example, the total height X of the bottom wall finishing panel 3, side wall finishing panel 2, and deck border finishing panel 1 is all 6 mm, so that when the repaired wall is formed, the repaired wall is flush with the wall. Ori,
When the side wall finishing panel 2 and the deck border finishing panel 1 are crimped, care is taken to prevent the side wall finishing panel 2 itself from being deformed in a wave-like manner due to the repulsive pressure of the filler 6 on the back side. Also,
Since the filler 6 is also filled in the gap 10 and solidified, even if the filler on the back side breaks due to long-term use, the thick filler 6 in the gap 10 will still function as a dam. This will prevent pool water from flowing out,
This has the advantage of preventing overflowing water from flowing into the deck a 1 -1.
尚、プール側壁コーナーの改修については、図
面に示すように平面L形を呈するデツキボーダー
仕上パネル1、側壁仕上パネル2を用いること言
うまでもなく、実施例ではアルミ製のプールを対
象として説明しているが、コンクリート製や、そ
の他の金属製プール、FRP製プールも対象とし
ていること言うまでもない。 Regarding the renovation of the pool side wall corners, it goes without saying that deck border finishing panels 1 and side wall finishing panels 2, which have an L-shaped planar shape as shown in the drawings, are used, and in the examples, explanations are given for aluminum pools. However, it goes without saying that it also covers concrete, other metal pools, and FRP pools.
本考案は以上のように平面四角状を呈し裏面に
充填材を塗布したFRP等の合成樹脂製側壁仕上
パネルと、断面形を呈し裏面に充填材を塗布し
たFRP等の合成樹脂製デツキボーダー仕上パネ
ルとを用意し、上記側壁仕上パネルをプール側壁
全長に渉り平行に圧着すると共に、その側壁仕上
パネル上端との間に充填材の洩材確認間隔をおい
てプール側壁全長に渉りデツキボーダー仕上パネ
ルを端縁を当接させて平行に圧着し、側壁仕上パ
ネル相互間にFRP等の合成樹脂製ライニング材
を埋込固定したので、下記の作用効果がある。
As described above, the present invention consists of a side wall panel made of synthetic resin such as FRP that has a square planar shape and has a filler applied to the back side, and a deck border finish made of synthetic resin such as FRP that has a cross-sectional shape and has a filler applied to the back side. Prepare a panel and crimp the side wall finishing panel in parallel across the entire length of the pool side wall, and at the same time, leave a space between the top edge of the side wall finishing panel to check for leakage of filler material, and spread it across the entire length of the pool side wall to create a deck border. The finished panels are crimped in parallel with their edges abutting, and a synthetic resin lining material such as FRP is embedded and fixed between the side wall finished panels, resulting in the following effects.
側壁仕上パネル相互間にライニング材を埋込
み固定すれば、改修側壁を形成できるから、ラ
イニング材の塗布面積が最小ですむ。 By embedding and fixing the lining material between the side wall finishing panels, a repaired side wall can be formed, so the area to which the lining material is applied can be minimized.
従つて、プール側壁の改修作業が容易であ
り、従来のように含浸、脱泡操作を有する
FRPのライニング材塗布作業を全面に渉つて
繰り返して行なう作業に比べて手間がかから
ず、工期が短くてすみ、経済的である。 Therefore, the renovation work of the pool side wall is easy, and it does not require impregnation and defoaming operations as in the past.
Compared to the work of repeatedly applying FRP lining material over the entire surface, it is less labor-intensive, takes less time, and is more economical.
側壁仕上パネルと、デツキボーダー仕上パネ
ルとに分割しているから、嵩ばらず、対象とす
る改修用プールが室内設置型であつても楽に出
入口から搬入でき、持ち運び作業が簡単であ
る。 Since it is divided into a side wall finishing panel and a deck border finishing panel, it is not bulky, and even if the target pool for renovation is installed indoors, it can be easily carried in from the entrance and exit, making it easy to carry.
更に、デツキボーダー仕上パネルと、側壁仕
上パネルは夫々デツキボーダー部分及びプール
側面部分に洩材確認間隔をおいて圧着される
が、その際、その洩材確認間隔から洩材が洩れ
でることを確認できるようにしているので、プ
ール水の流出や、デツキ面へ溢流した水の流入
に最も機能する側壁仕上パネル上縁と、デツキ
ボーダー仕上パネル下縁との接続部のシール度
を確認でき、漏水を確実に防止して耐久性の劣
化も招かない。 Furthermore, the deck border finishing panels and side wall finishing panels are crimped to the deck border and pool side parts, respectively, at intervals to check for leakage material, but at that time, it was confirmed that there was no leakage material leaking from the gaps to check for leakage material. This allows you to check the degree of sealing at the connection between the upper edge of the side wall finishing panel, which is most effective in preventing the outflow of pool water and the inflow of water that overflows to the deck surface, and the lower edge of the deck border finishing panel. It reliably prevents water leakage and does not cause deterioration of durability.
依つて、所期の目的を達成できる。 Thus, the intended purpose can be achieved.
図面は本考案プール側壁の改修構造の実施例を
示し、第1図は断面斜視図で一部切欠して示す、
第2図は2−2拡大断面図で中間省略して示す、
第3図は3−3拡大断面図、第4図は4−4拡大
断面図、第5図は5−5拡大断面図である。
尚図中、a1:プール側壁、a2:プール底、6:
充填材、2:側壁仕上パネル、1:デツキボーダ
ー仕上パネル、4:洩材確認間隔、5:ライニン
グ材。
The drawings show an embodiment of the pool side wall repair structure of the present invention, and FIG. 1 is a cross-sectional perspective view with a part cut away.
Figure 2 is a 2-2 enlarged sectional view with the middle omitted,
3 is an enlarged sectional view 3-3, FIG. 4 is an enlarged sectional view 4-4, and FIG. 5 is an enlarged sectional view 5-5. In the figure, a1 : pool side wall, a2 : pool bottom, 6:
Filling material, 2: Side wall finishing panel, 1: Deck border finishing panel, 4: Leakage confirmation interval, 5: Lining material.
Claims (1)
FRP等の合成樹脂製側壁仕上パネルと、断面
形を呈し裏面に充填材を塗布したFRP等の合成
樹脂製デツキボーダー仕上パネルとを用意し、上
記側壁仕上パネルをプール側壁全長に渉り平行に
圧着すると共に、その側壁仕上パネル上端との間
に充填材の洩材確認間隔をおいてプール側壁全長
に渉りデツキボーダー仕上パネルを端縁を当接さ
せて平行に圧着し、側壁仕上パネル相互間に、
FRP等の合成樹脂製ライニング材を埋込固定し
たことを特徴とするプール側壁の改修構造。 It has a rectangular shape and a filler is applied to the back side.
Prepare a side wall finish panel made of synthetic resin such as FRP and a deck border finish panel made of synthetic resin such as FRP which has a cross-sectional shape and has a filler applied to the back side.The side wall finish panel is placed parallel to the entire length of the pool side wall. At the same time, the deck border finishing panel is crimped in parallel with the top edge of the side wall finishing panel across the entire length of the pool side wall with a gap to check for leakage of filler between the top edge of the side wall finishing panel and the side wall finishing panel is pressed together in parallel. Between,
A pool side wall repair structure characterized by embedded and fixed synthetic resin lining material such as FRP.