JPH03258687A - Float coated with thermal shrinkage film - Google Patents

Float coated with thermal shrinkage film

Info

Publication number
JPH03258687A
JPH03258687A JP2059508A JP5950890A JPH03258687A JP H03258687 A JPH03258687 A JP H03258687A JP 2059508 A JP2059508 A JP 2059508A JP 5950890 A JP5950890 A JP 5950890A JP H03258687 A JPH03258687 A JP H03258687A
Authority
JP
Japan
Prior art keywords
float
films
film
coated
cylindrical
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2059508A
Other languages
Japanese (ja)
Inventor
Kazuyuki Kawabata
和幸 川端
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Okura Industrial Co Ltd
Original Assignee
Okura Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Okura Industrial Co Ltd filed Critical Okura Industrial Co Ltd
Priority to JP2059508A priority Critical patent/JPH03258687A/en
Publication of JPH03258687A publication Critical patent/JPH03258687A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To prevent the lowering of buoyance and damage of a float caused by the sticking of seaweeds of the like in the float for a raft for breeding sea living things by coating the edge of the float with a bag-like shrinkage films and shrinking them by heating and in the next step coating the center of the float with cylindrical heat shrinkage films and shrinking them by heating. CONSTITUTION:Both ends of cylindrical float 1 are covered by baglike thermal shrinkage films 2, and the films 2 are heated and shrunk, as a result, both ends of the floating 1 are tightly coated by the films 2. In the next step the center section or center section and end sections of the float 1 are covered by cylindrical bag-like thermal shrinkage films 3, and the films 3 are heated and shrunk to tightly seal the bag-like films 2 and the float 1. These films 2 and 3 are made of polyethylene or the like. In addition, to these films 2 and 3 disinfectant, mildewproofing agent, paraffin, wax, etc. are added or applied for preventing from sticking of living things such as seaweeds, barnacles, or the like. This constitution can protect and prevent the float from being stuck by seaweeds or the like.

Description

【発明の詳細な説明】 [産業上の利用分野] 本発明は藻類又はフジッボ類等の生物の付着により生ず
る浮力低下を防止したフロートに関する。
DETAILED DESCRIPTION OF THE INVENTION [Field of Industrial Application] The present invention relates to a float that prevents a decrease in buoyancy caused by the attachment of living things such as algae or barnacles.

[従来の技術] 従来、海、湖、河川での養殖用いかだ又は浮き桟橋等に
使用されている合成樹脂発泡体製のフロートにはフロー
トの破損を防止するために合成樹脂の袋が被覆されてい
た。
[Prior Art] Conventionally, floats made of synthetic resin foam used for aquaculture rafts or floating piers in the sea, lakes, and rivers are covered with synthetic resin bags to prevent damage to the floats. was.

[発明が解決しようとする課題] 上記フロートを被覆した合成樹脂の袋はフロートに密着
していないために破損しやすく、破損部等から水が入り
フロートに藻類又はフジッボ等の生物が付着したり、前
記袋の表面にも生物が付着して該フロートの浮力を低下
させていた・。
[Problem to be solved by the invention] The synthetic resin bag covering the float is easily damaged because it does not adhere to the float, and water may enter from the damaged part and organisms such as algae or Fujibbo may adhere to the float. , Organisms also adhered to the surface of the bag, reducing the buoyancy of the float.

[課題を解決するための手段] 本発明は上記課題解決に鑑みなされた漫ので、以下本発
明の一実施例を示す図面に基づいて説明する。
[Means for Solving the Problems] The present invention was developed in view of solving the above problems, and therefore, an embodiment of the present invention will be described below based on the drawings.

第1図及び第2図は円柱状のフロートに熱収縮性フィル
ム(以下フィルムと言う)を密着被覆したものの断面図
を示し、第3図は球状のフロートにフィルムを密着被覆
したものの側面図である。
Figures 1 and 2 are cross-sectional views of a cylindrical float covered with a heat-shrinkable film (hereinafter referred to as film), and Figure 3 is a side view of a spherical float covered with a film. be.

請求項1に記載の如くフロートが柱状の場合、すなわち
第1図又は第2図の場合、まずポリエチレン、ボロプロ
ピレン、ポリスチレン等の発泡体よりなるフロート1の
両端を、一方が密封され他方が開口した袋状のフィルム
2で被覆した後加熱して収縮せしめ、次に両端が開口し
た円筒状のフィルム3でフロート1の中央部を被覆した
後加熱して収縮せしめ前記袋状のフィルム2と密着させ
る。
When the float is columnar as described in claim 1, that is, in the case of FIG. 1 or FIG. After covering the float 1 with a bag-shaped film 2, it is heated and shrunk, and then the center part of the float 1 is covered with a cylindrical film 3 with both ends open, and then heated and shrunk so that it is tightly attached to the bag-shaped film 2. let

フィルムとしてはポリエチレン、ポリプロピレン、ポリ
スチレン、ナイロン、ポリエチレンテレフタレート等が
使用できるがこれ・らに限定するものではない。
As the film, polyethylene, polypropylene, polystyrene, nylon, polyethylene terephthalate, etc. can be used, but the film is not limited to these.

更にフィルムの重なり合う部分の密着性をよくするため
にエチレン酢酸ビニル樹脂等を積層した多層フィルム或
は感圧接着剤を塗布したフィルムを使用することもでき
る 又藻類、フジッボ類等の生物の付着を防止するために熱
収縮フィルムに殺菌剤、防カビ剤、パラフィン、ワック
ス等を添力汀したり塗布することができる。
Furthermore, in order to improve the adhesion of the overlapping parts of the films, a multilayer film laminated with ethylene vinyl acetate resin, etc., or a film coated with a pressure-sensitive adhesive can also be used. To prevent this, a bactericide, a fungicide, a paraffin, a wax, etc. can be applied or applied to the heat-shrinkable film.

上記フロートの形状としては円柱状、多角形の柱状など
がある。
The shape of the float includes a cylindrical shape, a polygonal column shape, and the like.

請求項2に記載の如くフロートが球状の場合は、まず最
初に両端が開口した円筒状のフィルム4でフロート1を
被覆した後加熱して収縮せしめ、次に両端の開口したフ
ィルム4で最初のフィルムと直角方向にフロートを被覆
した後加熱して収縮せしめる。前記フィルム4の長さは
収縮後フィルムの両端がフロートに密着する程度のもの
が好ましい。
When the float is spherical as described in claim 2, the float 1 is first covered with a cylindrical film 4 with both ends open, and then heated and shrunk, and then the first After coating the float in a direction perpendicular to the film, it is heated and shrunk. The length of the film 4 is preferably such that both ends of the film are in close contact with the float after shrinkage.

請求項3に記載の如く、フロートを熱収縮フィルムで二
重以上の被覆を行うことにより最外層のフィルムが汚染
したり、傷ついた場合そのフィルムを取り除くだけで使
用が継続できるものである。
As described in claim 3, by covering the float with heat-shrinkable films or more twice, if the outermost film becomes contaminated or damaged, use can be continued by simply removing the film.

使用済みのフィルムを取り除きやすくするためにフィル
ムにミシン目を入れることができる。
The film can be perforated to facilitate removal of the used film.

[発明の効果コ 3− 以上述べた如く本発明の熱収縮性フィルムで被覆された
フロートは、フィルムがフロートに密着しているためよ
り強固に保護され、しかもフロートへの生物の付着によ
る浮力の低下、フィルムの破損が抑止できるものである
[Effect of the invention 3- As described above, the float coated with the heat-shrinkable film of the present invention is more strongly protected because the film is in close contact with the float, and moreover, the buoyancy caused by the attachment of organisms to the float is reduced. This can prevent deterioration and damage to the film.

更にフロートを多数回フィルムで被覆した場合は最外層
のフィルムが汚染したり、傷ついた際そのフィルムを取
り除くだけで継続使用できるものである。
Furthermore, if the float is coated with a film many times, if the outermost film becomes contaminated or damaged, it can be used continuously by simply removing the film.

【図面の簡単な説明】[Brief explanation of drawings]

第1図及び第2図は円柱状のフロートに熱収縮性フィル
ムを被覆したものの断面図を示し、第34− ものの側面図である。 1・・・フロート 2・・・袋状の熱収縮性フィルム 3・・・円筒状の熱収縮性フィルム 4・・・円筒状の熱収縮フィルム
1 and 2 are cross-sectional views of a cylindrical float coated with a heat-shrinkable film, and a side view of the cylindrical float. 1...Float 2...Bag-shaped heat-shrinkable film 3...Cylindrical-shaped heat-shrinkable film 4...Cylindrical-shaped heat-shrinkable film

Claims (1)

【特許請求の範囲】 1 柱状のフロートの両端を、一方が密封され他方が開
口している袋状の熱収縮性フィルムで被覆後加熱して収
縮せしめ、次に円筒状の熱収縮性フィルムで前記フロー
トの中央部を被覆後加熱して収縮せしめたことを特徴と
する熱収縮性フィルムで被覆したフロート。2 球状の
フロートを、両端が開口した円筒状の熱収縮性フィルム
で被覆後加熱して収縮せしめ、次に前記円筒状の熱収縮
性フィルムと直角方向に、両端が開口した円筒状の熱収
縮性フィルムを被覆後加熱して収縮せしめたことを特徴
とする熱収縮性フィルムで被覆したフロート。 3 熱収縮性フィルムが二重以上被覆されていることを
特徴とする請求項1又は2記載の熱収縮性フィルムで被
覆されたフロート。
[Claims] 1. Both ends of a columnar float are covered with a bag-shaped heat-shrinkable film that is sealed on one side and open on the other, and then heated and contracted, and then covered with a cylindrical heat-shrinkable film. A float coated with a heat-shrinkable film, characterized in that the center portion of the float is coated and then heated to shrink. 2. A spherical float is covered with a cylindrical heat-shrinkable film that is open at both ends and then heated to shrink it, and then a cylindrical heat-shrinkable film that is open at both ends is coated in a direction perpendicular to the cylindrical heat-shrinkable film. 1. A float coated with a heat-shrinkable film, characterized in that the film is coated with a heat-shrinkable film and then shrunk by heating. 3. The float coated with a heat-shrinkable film according to claim 1 or 2, characterized in that the heat-shrinkable film is coated twice or more.
JP2059508A 1990-03-08 1990-03-08 Float coated with thermal shrinkage film Pending JPH03258687A (en)