JPH03255244A - 低伸縮ベルト - Google Patents

低伸縮ベルト

Info

Publication number
JPH03255244A
JPH03255244A JP5540890A JP5540890A JPH03255244A JP H03255244 A JPH03255244 A JP H03255244A JP 5540890 A JP5540890 A JP 5540890A JP 5540890 A JP5540890 A JP 5540890A JP H03255244 A JPH03255244 A JP H03255244A
Authority
JP
Japan
Prior art keywords
belt
fiber
glass fiber
contraction
low
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP5540890A
Other languages
English (en)
Inventor
Kiyoshi Suzuki
清 鈴木
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NEC Corp
Original Assignee
NEC Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NEC Corp filed Critical NEC Corp
Priority to JP5540890A priority Critical patent/JPH03255244A/ja
Publication of JPH03255244A publication Critical patent/JPH03255244A/ja
Pending legal-status Critical Current

Abstract

(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は、低伸縮ベルト、特に動力伝達機構に使用する
ための低伸縮ベルトに関する。
〔従来の技術〕
従来のゴムベルトやプラスチックベルト等のベルトは芯
線にガラスファイバー繊維かテルミッド繊維のいづれか
一つを使用しており低温および高温時においてそれぞれ
特有の伸縮が発生していた。
〔発明が解決しようとする課題〕
しかしながら、このような上述した従来のベルトは、芯
線にガラスファイバー繊維を使用した場合、低温時に収
縮し高温時に伸び、あるいは、またテルミッド繊維を使
用した場合、低温時に伸び高温時に収縮する傾向が有り
、ベルト長が変化することにより、ベルト張力の変化が
発生し、特に印字装置の印字ユニット走行系において位
置精度の変化が発生する等の欠点があった。
〔課題を解決するための手段〕
本発明の低伸縮ベルトは、ベルトの芯線にガラスファイ
バー繊維とテルミッド繊維とをより合わせた芯線を使用
し、低温時に収縮し高温時に伸びるガラスファイバー繊
維と、逆の特性を示すテルミッド繊維により各温度域に
おける伸縮の変化量を少なくさせることができ、芯線に
上述した2種の繊維を使用することにより、それぞれ固
有の特性を有する繊維の絶対量が少なくなることにより
収縮力を弱め、また膨張時においてもいづれかの芯線に
おいて収縮力が発生するため伸び量を少なく押えること
が期待てき、各温度域におけるベルト張力の変化を少く
することが可能となるように構成される。
口実施例〕 次に、本発明の実施例について、図面を参照して説明す
る。
第1図は本発明の一実旅例を示す側断面図、第2図は第
1図に示す芯線の拡大斜視図である。
第1図に示す低伸縮ベルトは、例えば歯付ベルトのよう
なベルト1と、ベルト1の補強のため内部に一体化して
組込まれている芯線とで構成される。
第2図は第1図に示す芯線の拡大斜視図であり、ガラス
ファイバー繊維aと、テルミッド繊維すとで構成される
。このガラスファイバー繊維aは低温時に収縮し高温時
に伸びる。これに対してテルミッド繊維すは逆の特性を
示す。このため、ガラスファイバー繊維aとテルミッド
繊維すとをより合せて、芯線2としベルト1の中に組み
込むことにより各温度域における伸縮の変化を少なくす
ることができる。
〔発明の効果〕
本発明の低伸縮ベルトは、コムベルトやプラスチックベ
ルトの補強用に使用する芯線の材料に、低温、高温時に
発生する伸縮特性において逆の特性をもつグラスファイ
バー繊維とテルミ、ラド繊維をより合せて芯線とするこ
とにより、各温度域における伸縮を少なくすることがで
きるとともに一ベルト張力の変化を少なくすることが可
能となり、ベルト張力を一定にするためのテンション機
構を無くすことができるので原価低減を達成できるとい
う効果がある。
【図面の簡単な説明】
第1図は本発明の一実旅例を示す側断面図、第ド繊維。

Claims (1)

    【特許請求の範囲】
  1. 低温時に収縮し高温時に伸びるガラスファイバー繊維と
    低温時に伸び高温時に収縮するテルミッド繊維とをより
    合せて線状にした芯線と、前記芯線を内部に収容するた
    めのベルトとを含むことを特徴とする低伸縮ベルト。
JP5540890A 1990-03-06 1990-03-06 低伸縮ベルト Pending JPH03255244A (ja)