JPH0323494B2 - - Google Patents
Info
- Publication number
- JPH0323494B2 JPH0323494B2 JP56012030A JP1203081A JPH0323494B2 JP H0323494 B2 JPH0323494 B2 JP H0323494B2 JP 56012030 A JP56012030 A JP 56012030A JP 1203081 A JP1203081 A JP 1203081A JP H0323494 B2 JPH0323494 B2 JP H0323494B2
- Authority
- JP
- Japan
- Prior art keywords
- bottle
- treatment
- ion exchange
- glass
- glass bottle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Surface Treatment Of Glass (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1203081A JPS57129845A (en) | 1981-01-29 | 1981-01-29 | Glass bottle provided with both mechanical strength and chemical durability and its manufacture |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1203081A JPS57129845A (en) | 1981-01-29 | 1981-01-29 | Glass bottle provided with both mechanical strength and chemical durability and its manufacture |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57129845A JPS57129845A (en) | 1982-08-12 |
JPH0323494B2 true JPH0323494B2 (enrdf_load_stackoverflow) | 1991-03-29 |
Family
ID=11794199
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1203081A Granted JPS57129845A (en) | 1981-01-29 | 1981-01-29 | Glass bottle provided with both mechanical strength and chemical durability and its manufacture |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57129845A (enrdf_load_stackoverflow) |
Families Citing this family (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB2199318B (en) * | 1986-12-04 | 1990-11-14 | Glaverbel | Dealkalised sheet glass and method of producing same |
GB2206878B (en) * | 1987-07-11 | 1991-07-17 | Glaverbel | Pyrolytically coated sheet glass and process of manufacturing same |
JPH0678181B2 (ja) * | 1988-10-27 | 1994-10-05 | セントラル硝子株式会社 | ガラス表面の処理方法 |
ATE151390T1 (de) * | 1993-08-19 | 1997-04-15 | Cardinal Ig Co | Anlaufbeständiges glas und methode zu seiner herstellung |
JP2008044834A (ja) * | 2006-07-19 | 2008-02-28 | Asahi Glass Co Ltd | フラットパネルディスプレイ用ガラス基板およびその製造方法、ならびにそれを用いたディスプレイパネル |
US9499434B1 (en) | 2012-08-31 | 2016-11-22 | Owens-Brockway Glass Container Inc. | Strengthening glass containers |
FR3017613B1 (fr) * | 2014-02-18 | 2020-03-13 | Glass Surface Technology | Procede et dispositif de passivation de la surface interne d'un flacon en verre et flacon obtenu avec un tel procede. |
TWI709541B (zh) * | 2018-03-16 | 2020-11-11 | 雅士晶業股份有限公司 | 抗菌玻璃及其製備方法 |
CN110498616A (zh) * | 2018-05-18 | 2019-11-26 | 雅士晶业股份有限公司 | 抗菌玻璃及其制备方法 |
DE102018127528A1 (de) * | 2018-11-05 | 2020-05-07 | Schott Ag | Behälter aus Glas sowie Verfahren zu dessen Herstellung |
CN111960694B (zh) * | 2020-07-24 | 2022-12-02 | 北方夜视技术股份有限公司 | 倒像器用吸收玻璃表面化学稳定性处理方法及应用 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS49101405A (enrdf_load_stackoverflow) * | 1972-12-18 | 1974-09-25 | ||
JPS54142226A (en) * | 1978-04-28 | 1979-11-06 | Nippon Taisanbin Kougiyou Kk | Treatment of soda lime glass surface layer |
-
1981
- 1981-01-29 JP JP1203081A patent/JPS57129845A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS57129845A (en) | 1982-08-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4164402A (en) | Strengthening of thin-walled, light glass containers | |
US4021218A (en) | Chemical method of strengthening glass articles subjected to abrasion resistance treatment | |
AU2004232803B2 (en) | Method and apparatus for strengthening glass | |
US3473906A (en) | Method of strengthening glass | |
US3791809A (en) | Method of strengthening glass articles using powdered salts for ion exchange | |
GB1076603A (en) | Glass articles and preparation thereof | |
US3844754A (en) | Process of ion exchange of glass | |
US2779136A (en) | Method of making a glass article of high mechanical strength and article made thereby | |
JPH0323494B2 (enrdf_load_stackoverflow) | ||
GB1292539A (en) | Method of strengthening a silicate glass article | |
US4206253A (en) | Method of strengthening chemically a glass container | |
GB2195332A (en) | Chemically strengthened glass article and method of producing same | |
ES2886100T3 (es) | Proceso de tratamiento de superficie para recipientes de vidrio | |
US3451796A (en) | Method of treating strengthened glass surface to increase acid durability | |
GB1220292A (en) | Process for tempering vitreous and vitro-crystalline bodies | |
JP2022543044A (ja) | ガラス物品を強化するための塩浴組成物、ガラス物品を強化するためにその塩浴組成物を使用する方法、およびそれにより強化されたガラス物品 | |
JPS60180936A (ja) | 高強度耐熱ガラス製品の製造方法 | |
JPH11228186A (ja) | ガラス、ガラスの製造方法、及び強化抗菌ガラス用組成物 | |
JPS62270439A (ja) | 化学強化用ガラス | |
US3556757A (en) | Alkali metal salt bath with alkali metal acetate additive for treatment of glasses and glass-ceramics | |
JPS5864248A (ja) | ガラスびんの表面処理方法 | |
US3697242A (en) | Strengthening borosilicate glass by crowding surface layer with lioh and/or koh | |
JPS632906B2 (enrdf_load_stackoverflow) | ||
JPS6022662B2 (ja) | 安定した化学的耐久性・機械的強度を有する軽量びんの製造方法 | |
SU1293134A1 (ru) | Способ повышени химической устойчивости полых стеклоизделий |