JPH02248568A - Surface treatment of tile joint - Google Patents
Surface treatment of tile jointInfo
- Publication number
- JPH02248568A JPH02248568A JP6884589A JP6884589A JPH02248568A JP H02248568 A JPH02248568 A JP H02248568A JP 6884589 A JP6884589 A JP 6884589A JP 6884589 A JP6884589 A JP 6884589A JP H02248568 A JPH02248568 A JP H02248568A
- Authority
- JP
- Japan
- Prior art keywords
- tile
- metal
- tiles
- tile joint
- joint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【発明の詳細な説明】
産業上の利用分野
本発明は床や壁などに形成したタイル面のタイル目地の
表面処理方法に関する。DETAILED DESCRIPTION OF THE INVENTION Field of the Invention The present invention relates to a method for surface treatment of tile joints on tile surfaces formed on floors, walls, etc.
従来の技術
浴槽、浴室、洗面所、台所など火気、水気を利用する場
所には、第2図(a)、 (b)に示すようにタイル1
が多く使用され、その固着に目地材が用いられ、隣合う
2個のタイル1の間にタイル目地2を形成している。Conventional technology Tile 1 is used in areas where fire and moisture are used, such as bathtubs, bathrooms, washrooms, and kitchens, as shown in Figures 2 (a) and (b).
are often used, and a joint material is used to fix them, forming a tile joint 2 between two adjacent tiles 1.
発明が解決しようとする課題
しかしながら、このタイル1を固着したタイル目地2は
、高温、高湿条件下に長時間さらされると表面にかびが
発生し、また固着力が減少してタイル1がはがれたり、
タイル目地2がひび割れして水滴が混入し壁材が腐蝕す
るなどの欠点があり、また寒冷地などでの建物外壁のタ
イルの目地の場合も、昼夜の温度差による水分の凍結、
融解により、上記のかび発生時と同様にタイル目地のひ
び割れおよび剥離が少なからず発生する。そこでこれら
を予防するために定期的な補修工事が必要である。Problems to be Solved by the Invention However, if the tile joints 2 to which the tiles 1 are fixed are exposed to high temperature and high humidity conditions for a long time, mold will form on the surface, and the adhesion strength will decrease, causing the tiles 1 to peel off. Or,
There are drawbacks such as the tile joints 2 cracking and water droplets entering and corroding the wall material.Also, in the case of tile joints on the exterior walls of buildings in cold regions, water freezes due to temperature differences between day and night.
As a result of the melting, cracking and peeling of the tile joints occur to some extent, similar to the above-mentioned mold outbreak. Therefore, regular repair work is necessary to prevent these problems.
本発明は、上記のタイル目地のかびの発生、タイル目地
のひび割れ部への水滴混入による腐蝕および凍結、融解
によるひび割れなどの課題を解決し、補修工事を軽減で
きるタイル目地の表面処理方法を提供することを目的と
している。The present invention provides a surface treatment method for tile joints that can solve the above-mentioned problems such as the occurrence of mold in tile joints, corrosion caused by water droplets entering cracks in tile joints, and cracks caused by freezing and thawing, and can reduce repair work. It is intended to.
課題を解決するための手段
上記課題を解決するために本発明のタイル目地の表面処
理方法は、タイル目地の表面に金属を溶射して金属溶射
被膜を形成することを特徴とするものである。Means for Solving the Problems In order to solve the above problems, the method for surface treatment of tile joints of the present invention is characterized in that a metal is thermally sprayed onto the surface of the tile joints to form a metal sprayed coating.
作用
上記構成により、タイル目地の表面に金属溶射被膜を形
成するので、タイル目地にかびが発生したり、ひび割れ
が生じたりすることがなく、長期間にわたって補修工事
を軽減できる。Function: With the above configuration, a metal spray coating is formed on the surface of the tile joints, so mold and cracks do not occur in the tile joints, and repair work can be reduced over a long period of time.
実施例 以下、本発明の実施例を図面に基づいて説明する。Example Embodiments of the present invention will be described below based on the drawings.
第1図(a)、 (b)、 (C)は本発明の一実施例
のタイル目地の表面処理方法により処理したタイル面の
要部を示し、(a)は一部切欠き概略正面図、(b)は
(a)のA−A線断面図、(C)は(a)の要部の拡大
図である。第1図(a)、 (b)、 (c)に示すよ
うに、タイル面11の隣合うタイル12の間のタイル目
地13の表面に、低温溶射のアーク溶射方法によってア
ルミニウム(,11)を溶射して金属溶射被膜14を形
成した。このとき、溶射金属はタイル12の表面上にも
一旦は付着するが、タイル12の表面が平滑な面である
ため溶射金属の固哲力は極めて弱く、布などでふきとれ
ば簡単に取り除くことができ、溶射金属はタイル目地1
3の表面のみに同者し、タイル12の表面状態はもとど
おりに保たれる。また別の方法としては、タイル12の
表面を紙やテープ材などで覆って溶射作業してもよい。Figures 1 (a), (b), and (C) show the main parts of a tile surface treated by the tile joint surface treatment method of one embodiment of the present invention, and (a) is a partially cutaway schematic front view. , (b) is a sectional view taken along the line A-A of (a), and (C) is an enlarged view of the main part of (a). As shown in FIGS. 1(a), (b), and (c), aluminum (,11) is applied to the surface of the tile joint 13 between adjacent tiles 12 on the tile surface 11 by a low-temperature arc spraying method. A metal spray coating 14 was formed by thermal spraying. At this time, the sprayed metal also adheres to the surface of the tile 12 once, but since the surface of the tile 12 is smooth, the stickiness of the sprayed metal is extremely weak, and it can be easily removed by wiping it off with a cloth. Thermal sprayed metal can be used for tile joints 1
The surface condition of the tiles 12 is maintained as before. Alternatively, the surface of the tile 12 may be covered with paper, tape, or the like and thermal spraying may be carried out.
金属としてはAΩのばか亜鉛(Zn )なども用い得る
。As the metal, AΩ stupid zinc (Zn) or the like may be used.
上記のようにして処理したタイル面11のタイル目地1
3は、表面に金属溶射被11!14が形成されているの
で、高温、高湿条件下においても長期間にわたって、か
びが発生したり、ひび割れたり、また凍結、融解が繰返
される環境下でもひび割れや剥離を発生することがなく
、補修工事が大幅に減少した。Tile joint 1 of tile surface 11 treated as above
3 has metal sprayed coatings 11 and 14 formed on the surface, so it will not cause mold or cracks even under high temperature and high humidity conditions for a long period of time, and will not crack even in environments where freezing and thawing are repeated. No peeling or peeling occurred, and repair work was significantly reduced.
発明の効果
以上のように本発明のタイル目地の表面処理方法におい
ては、タイル目地の表面に金属溶射被膜を形成すること
により、タイル表面を傷つけることなく容易に長期間に
わたってタイル目地表面におけるかびの発生やひび割れ
などの発生を防止することができ、補修工事費を大幅に
低減することができる。Effects of the Invention As described above, in the tile joint surface treatment method of the present invention, by forming a metal spray coating on the tile joint surface, mold and mildew on the tile joint surface can be easily prevented over a long period of time without damaging the tile surface. It is possible to prevent the occurrence of cracks, cracks, etc., and the cost of repair work can be significantly reduced.
第1図(a)、 (b)、 (c)は本発明の一実施例
のタイル目地の表面処理方法により処理したタイル面の
要部を示し、(a)は一部切欠き概略正面図、(11)
は(a)のA−Al!断面図、(C) ハ(a ) (
7) 要部(7) K入園、第2図(a)、(b)は従
来のタイル面を示し、(a)は概略正面図、(b) ハ
(a) I) B −B I!!断面図である。
12・・・タイル、13・・・タイル目地、14・・・
金属溶射被膜。
代理人 森 本 義 弘
第1図
第2図FIGS. 1(a), (b), and (c) show the main parts of a tile surface treated by the tile joint surface treatment method of one embodiment of the present invention, and (a) is a partially cutaway schematic front view. , (11)
is (a) A-Al! Cross-sectional view, (C) C (a) (
7) Main part (7) K entrance, Figures 2 (a) and (b) show the conventional tile surface, (a) is a schematic front view, (b) C (a) I) B -B I! ! FIG. 12...Tile, 13...Tile joint, 14...
Metal spray coating. Agent Yoshihiro Morimoto Figure 1 Figure 2
Claims (1)
成することを特徴とするタイル目地の表面処理方法。1. A method for surface treatment of tile joints, which comprises spraying metal onto the surface of tile joints to form a metal spray coating.