JPH01124568A - Cylindrical film package filled with processed food - Google Patents

Cylindrical film package filled with processed food

Info

Publication number
JPH01124568A
JPH01124568A JP62275282A JP27528287A JPH01124568A JP H01124568 A JPH01124568 A JP H01124568A JP 62275282 A JP62275282 A JP 62275282A JP 27528287 A JP27528287 A JP 27528287A JP H01124568 A JPH01124568 A JP H01124568A
Authority
JP
Japan
Prior art keywords
film
casing
seal line
edges
package
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP62275282A
Other languages
Japanese (ja)
Other versions
JP2594068B2 (en
Inventor
Munenobu Fujita
藤田 宗信
Minoru Yoshida
稔 吉田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kureha Corp
Original Assignee
Kureha Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kureha Corp filed Critical Kureha Corp
Priority to JP62275282A priority Critical patent/JP2594068B2/en
Priority to CN88108410A priority patent/CN1015795B/en
Priority to KR1019880014167A priority patent/KR940008008B1/en
Publication of JPH01124568A publication Critical patent/JPH01124568A/en
Application granted granted Critical
Publication of JP2594068B2 publication Critical patent/JP2594068B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

PURPOSE:To tear a film easily while increasing the film weld strength by a method wherein film rims of a cylindrical package are aligned together and welded so that the rims form the second weld line along the outer face of a cylindrical package, and a cut is made on the second weld line. CONSTITUTION:Rims 1a and 1b of a film 1 are joined with inner surfaces facing each other which is an extension of an inner wall of a cylindrical package 10, and aligned together. The aligned portion is welded along a first weld line S1. The film rims 1a and 1b protruding from the first weld line S1 are bent in one direction and aligned to an outer surface of the package 10. Three films, the film rims 1a and 1b and the film 1 which composes the package 10 are welded together on a second weld line S2 by high frequency or supersonic wave. The second weld line S2 has a cut 1 (a portion not welded) on its mid and a notch is placed at 1. This allows easy tearing of the film while strengthening the weld portion.

Description

【発明の詳細な説明】 〔技術分計〕 本発明はソーセージやチーズなどの加工食品が円筒状フ
ィルムの内部に充填されている包装体に係り、特に消費
者がフィルムを開放しやすいようにした円筒状フィルム
包装体に関する。
[Detailed Description of the Invention] [Technical Summary] The present invention relates to a package in which processed foods such as sausages and cheese are filled inside a cylindrical film, and in particular, the package is designed to make it easier for consumers to open the film. This invention relates to a cylindrical film package.

(発明の背景〕 第11図はソーセージなどの加工食品が充填された円筒
状フィルム包装体の従来例を示している。
(Background of the Invention) FIG. 11 shows a conventional example of a cylindrical film package filled with processed foods such as sausages.

この種の包装体では、第12図の断面図に示しているよ
うに、塩化ビニリデン系などのフィルム1の両縁部1a
と1bが合わされ、この合わせ部が高周波溶着あるいは
超音波溶着手段などにより溶着されてシール線Sが形成
されており、これによって円筒状のケーシング5が形成
されている。
In this type of package, as shown in the cross-sectional view of FIG.
and 1b are brought together, and this joint is welded by high frequency welding or ultrasonic welding means to form a seal line S, thereby forming a cylindrical casing 5.

ソーセージの場合にはこの円筒状ケーシング5内に加工
食肉が充填され、またスティックチーズの場合には、円
筒状ケーシング5内にプロセスチーズが充填される。モ
してケーシング5の長手方向両端部が絞られ、この絞り
部分がアルミニウムなどの金属製クランプ部材2によっ
て締付けられて閉じられている。
In the case of sausage, the cylindrical casing 5 is filled with processed meat, and in the case of stick cheese, the cylindrical casing 5 is filled with processed cheese. Both ends of the casing 5 in the longitudinal direction are constricted, and the constricted portions are tightened and closed by clamp members 2 made of metal such as aluminum.

例えばソーセージの場合には、ケーシング5内に加工食
肉が充填された後に、ボイル工程に容性する。このボイ
ル工程ではケーシングの内圧が上昇するため、フィルム
1に張力が作用する。この張力はシール線Sに作用する
ことになるが、従来は第12図に示すように、フィルム
縁部1aと1bが互いにほぼ平面状態に重ね合わされて
溶着されている。よってフィルム張力によフてシール線
Sに対しFで示す力が作用しても、この力Fに対するシ
ール線Sの溶着強度は高く、ボイル工程にてケーシング
5の破壊が生じにくくなっている。
For example, in the case of sausages, processed meat is filled into the casing 5 and then subjected to a boiling process. In this boiling process, the internal pressure of the casing increases, so tension acts on the film 1. This tension acts on the seal line S, and conventionally, as shown in FIG. 12, the film edges 1a and 1b are overlapped and welded in a substantially planar state. Therefore, even if a force indicated by F acts on the seal line S due to the film tension, the welding strength of the seal line S against this force F is high, making it difficult for the casing 5 to break during the boiling process.

〔発明が解決しようとする問題点〕[Problem that the invention seeks to solve]

しかしながら上記の円筒状フィルム包装体では、ケーシ
ング5の外側に突出するフィルム縁部1bが短いために
このフィルム縁部1aを指によって十分につかむことが
できず、しかも全長にわたって形成されているシール線
Sを破るためのきっかけとなる部分がないため、フィル
ム縁部1aの部分からフィルム1を剥すことは不可能と
なっている。よって消費者がフィルム1を剥そうとする
ときには、例えばナイフなどによってフィルム1に切込
みを入れこの切込みをきっかけとして内容物から剥すこ
とになるが、手元にナイフなどがない場合にはフィルム
1を剥すことが非常に困難である。
However, in the above-mentioned cylindrical film package, the film edge 1b protruding to the outside of the casing 5 is short, so the film edge 1a cannot be grasped sufficiently with fingers, and furthermore, the seal line is formed over the entire length. Since there is no trigger for tearing the film S, it is impossible to peel off the film 1 from the film edge 1a. Therefore, when a consumer wants to peel off the film 1, he or she will make a cut in the film 1 with a knife, for example, and use this cut as a trigger to peel it off from the contents, but if the consumer does not have a knife at hand, he or she will peel off the film 1. It is extremely difficult to do so.

またスティックチーズなどのように、比較的小さい包装
体の場合には、赤などに着色された開封テープが取付け
られており、この開封テープを引っ張ることによってフ
ィルム1に破れを生じさせるようにしている。しかしな
がら開封テープは高価であるため、これを長い寸法にて
使用している従来の包装体はコストが高くなっており不
経済である。また開封テープは、包装体の長手方向全長
にわたって取付けられており、その両端部がクランプ部
材2によってフィルム1と共に締付けられているのが一
般的である。したがって、開封テープをケーシング5か
ら引き剥した場合、その両端がクランプ部材2を引き付
けることになって包装体全体が曲がってしまい、内容物
が変形する欠点もある。
In addition, in the case of relatively small packages such as stick cheese, a tearing tape colored red or the like is attached, and by pulling this tearing tape, the film 1 is torn. . However, since tear tape is expensive, conventional packaging using long tapes is expensive and uneconomical. Further, the tear tape is generally attached over the entire length of the package in the longitudinal direction, and both ends thereof are fastened together with the film 1 by the clamp members 2. Therefore, when the tear tape is peeled off from the casing 5, both ends of the tape will attract the clamp member 2, causing the entire package to bend and the contents to be deformed.

本発明は上記従来の問題点を解決するものであり、開封
テープを設けなくても、フィルムを容易に剥すことがで
きるようになり且つ、シールを十分に強くできて、ソー
セージの場合のボイル工程などにおいて内圧の上昇に十
分に耐え得る円筒状フィルム包装体を提供することを目
的としている。
The present invention solves the above-mentioned conventional problems, and makes it possible to easily peel off the film without providing a tear tape, and to make the seal strong enough to improve the boiling process for sausages. It is an object of the present invention to provide a cylindrical film package that can sufficiently withstand increases in internal pressure.

〔問題点を解決するための具体的な手段〕本発明は、フ
ィルムの縁部どうしが溶着されて円筒状のケーシングが
形成され、この円筒状のケーシング内に加工食品が充填
されているとともに、ケーシングの長手方向両端部が閉
じられているフィルム包装体において、前記フィルムの
縁部どうしは、ケーシングの内面に連続する面どうしが
接するような合掌状態に合わされてこの合掌部が第1の
シール線によって溶着されており、さらに第1のシール
線から外方向へ延びる2枚のフィルム縁部が共にケーシ
ングの外面に合わされて、2枚のフィルム縁部とケーシ
ングを形成しているフィルムとが一緒に第2のシール線
によって溶着されており且つ、この第2のシール線が間
欠部を有して形成されていることを特徴とするものであ
る。
[Specific Means for Solving the Problems] The present invention is characterized in that the edges of the film are welded together to form a cylindrical casing, and the cylindrical casing is filled with a processed food. In a film package in which both ends in the longitudinal direction of the casing are closed, the edges of the film are brought together in a state in which their palms are in contact with each other so that their continuous surfaces contact the inner surface of the casing, and this joined part forms the first seal line. and the two film edges extending outwardly from the first seal line are brought together to the outer surface of the casing such that the two film edges and the film forming the casing are welded together. It is characterized in that it is welded by a second seal line, and the second seal line is formed with intermittent portions.

〔作 用〕[For production]

この円筒状フィルム包装体では、第2のシール線の間欠
部分にてフィルム縁部を指でつかみ、この部分を引くこ
とによってケーシングの外面に接合されている2枚のフ
ィルム縁部が第2のシール線から剥れ、また場合によっ
ては第1のシール線部分からも剥れて、この部分のケー
シングを構成しているフィルムに破れを生じさせる。よ
フて2枚のフィルム縁部が従来の開封テープとほぼ同様
な機能を発揮することになり、フィルム縁部の剥れ部分
からケーシングを破るきっかけを作ることができるよう
になる。また好ましくは、第2のシール線の間欠部にて
フィルム縁部にノツチ(切込み)を入れておけば、この
部分からフィルム縁部を分断することができ、フィルム
縁部をさらに剥しやすくなる。
In this cylindrical film package, the edges of the two films joined to the outer surface of the casing are moved to the outer surface of the casing by grasping the edges of the film with your fingers at the intermittent portions of the second seal line and pulling this portion. It peels off from the seal line and, in some cases, from the first seal line portion, causing tears in the film constituting the casing in this portion. As a result, the two edges of the film function in much the same way as conventional tear tape, and the peeled portion of the edge of the film can be used to create an opportunity to tear the casing. Preferably, notches are made in the edge of the film at the intermittent portions of the second seal line, so that the edge of the film can be separated from these portions, making it easier to peel off the edge of the film.

また、フィルム縁部どつしは第1のシール線によって合
掌状態に合わされて溶着されているが、さらにこのシー
ル線か外方に延びているフィルム縁部がケーシングの外
面に対し第2のシール線によって溶着されているため、
ケーシングフィルムの溶着強度を十分に確保できる。よ
ってソーセージの場合のように、ボイル工程などにおい
てケーシングの内圧が上昇したとしても、シール線の部
分がケーシングの内圧の上昇に十分に耐え得るようにな
る。
In addition, the edges of the film are welded together by a first seal line, and the edges of the film extending outward from this seal line form a second seal against the outer surface of the casing. Because it is welded by wire,
Sufficient welding strength of the casing film can be ensured. Therefore, even if the internal pressure of the casing increases during the boiling process, as in the case of sausages, the seal line portion can sufficiently withstand the increase in internal pressure of the casing.

〔発明の実施例〕[Embodiments of the invention]

以下、本発明の実施例を第1図〜第1O図の図面によっ
て説明する。
Embodiments of the present invention will be described below with reference to the drawings of FIGS. 1 to 1O.

第1図は本発明の第1実施例による円筒状フィルム包装
体を示す正面図である。
FIG. 1 is a front view showing a cylindrical film package according to a first embodiment of the present invention.

この実施例では、塩化ビニリデン系などのフィルム1が
円筒状に巻かれてケーシング10が形成されている。こ
のケーシング10を構成するフィルム1は、その縁部1
aと1bが高周波または超音波によって溶着されている
が、この溶着は2箇所のシール線S1とS2によって行
なわれている。第2図に示すように、まずフィルム1の
縁部1aと1bどうしが、ケーシング10の内面と連続
する面どうしが接合される合掌状態に合わされ、この合
掌部が第1のシール線S1によって溶着シールされてい
る。さらに第3図に示すように、第1のシール線S1か
ら外側に突出しているフィルム縁部1aと1bが、ケー
シング10の外面に合わせられ、シール線S2において
フィルム縁部1a、1bとケーシング10を構成してい
るフィルム1とが3枚−緒になって高周波または超音波
によって溶着されている。第1図に示すように、第2の
シール線S2は、その途中に間欠部lを有している。そ
してこの間欠部文の部分にノツチ(切込み)3が設けら
れている。
In this embodiment, a casing 10 is formed by winding a film 1 made of vinylidene chloride or the like into a cylindrical shape. The film 1 constituting this casing 10 has an edge 1
A and 1b are welded by high frequency or ultrasonic waves, and this welding is performed by two seal lines S1 and S2. As shown in FIG. 2, first, the edges 1a and 1b of the film 1 are brought together in a state in which the faces that are continuous with the inner surface of the casing 10 are joined, and this joined part is welded by the first seal line S1. It is sealed. Further, as shown in FIG. 3, the film edges 1a and 1b projecting outward from the first seal line S1 are aligned with the outer surface of the casing 10, and the film edges 1a, 1b and the casing 10 are aligned at the seal line S2. The three films 1 forming the structure are welded together by high frequency or ultrasonic waves. As shown in FIG. 1, the second seal line S2 has an intermittent portion l in the middle thereof. A notch 3 is provided in this intermittent part.

ソーセージの場合には上記円筒状のケーシング10の内
部に加工食肉が充填され、またスティックチーズの場合
には、ケーシング10の内部にプロセスチーズが充填さ
れる。そしてケーシング10の長手方向両端部が絞られ
、アルミニウムなどによる金属製クランプ部材2により
締め付けられて閉じられる。
In the case of sausage, the cylindrical casing 10 is filled with processed meat, and in the case of stick cheese, the casing 10 is filled with processed cheese. Both ends in the longitudinal direction of the casing 10 are then squeezed and closed by tightening with metal clamp members 2 made of aluminum or the like.

第4図は上記ケーシング10を形成するための装置の一
例を示している。符号11はスタッファノズルであり、
このスタッファノズル11によって加工食肉などが充填
される。スタッファノズル11の外周には成形部材12
が設けられている。
FIG. 4 shows an example of an apparatus for forming the casing 10. Reference numeral 11 is a stuffer nozzle;
This stuffer nozzle 11 is used to fill processed meat and the like. A molded member 12 is provided on the outer periphery of the stuffer nozzle 11.
is provided.

フィルム1は供給ローラ13と14によって供給され、
成形部材12によって円筒状に成形される。成形部材1
2には隙間を開けて対向する一対のガイド片12aと1
2bが設けられており、このガイド片12aと12bと
によってフィルム1の縁部1aと1bが合掌状態に合わ
せられる。成形部材12の下側には高周波電極15と1
6が対向して設けられている。円筒状ケーシング10の
縁部1aと1bが前記ガイド片12aと12bによって
合掌合わせされた後に、この高周波電極15と16によ
フて溶着され、第2図に示した第1のシール線S1が形
成される。さらにその下方には他の高周波室[17と1
8が設けられている。
Film 1 is fed by feed rollers 13 and 14;
It is molded into a cylindrical shape by the molding member 12. Molding member 1
2 has a pair of guide pieces 12a and 1 facing each other with a gap.
2b, and these guide pieces 12a and 12b align the edges 1a and 1b of the film 1 so that their palms are joined. High frequency electrodes 15 and 1 are provided on the lower side of the molded member 12.
6 are provided facing each other. After the edges 1a and 1b of the cylindrical casing 10 are brought together by the guide pieces 12a and 12b, they are welded together by the high frequency electrodes 15 and 16, and the first seal line S1 shown in FIG. 2 is formed. It is formed. Further below, there are other high frequency chambers [17 and 1
8 is provided.

一方の高周波電極17は送り出されるフィルム1の外側
に対向しており、他方の高周波電極18は送り出される
フィルム1の内側に対向している。
One high-frequency electrode 17 faces the outside of the film 1 being sent out, and the other high-frequency electrode 18 faces the inside of the film 1 being sent out.

上方に位置する高周波電極15と16とによって第1の
シール線Slが形成された後のフィルム縁部1aと1b
は、ケーシング10の外面に合わせられ、高周波電極1
7と18とによってこのフィルム縁部1a、lbとケー
シングを形成しているフィルム1とが3枚−緒に溶着さ
れ、第3図に示す第2のシール線S2が形成される。ま
た符号19と20は送りローラであり、この送りローラ
19と20とによってケーシング10が下方向へ連続的
に送り出される。上記第2のシール線S2を形成する際
、−時的に高周波電極17(プラス電極)に供給される
電流を停止することによって、第1図に示す間欠部1が
形成される。なお第4図では省略しているが、高周波電
極15.16と高周波電極17.18との間にガイド板
、を設け、第1のシール線S1が形成された後のフィル
ム縁部la、’lbをこのガイド板によってケーシング
を構成するフィルムの外面に倒すようにすれば、高周波
電極17と18とによって第2のシール線S2を形成し
やすくなる。
Film edges 1a and 1b after the first seal line Sl is formed by the high frequency electrodes 15 and 16 located above
is aligned with the outer surface of the casing 10, and the high frequency electrode 1
7 and 18, the three film edges 1a, lb and the film 1 forming the casing are welded together, forming a second seal line S2 shown in FIG. Further, reference numerals 19 and 20 indicate feed rollers, and the casing 10 is continuously fed downward by these feed rollers 19 and 20. When forming the second seal line S2, the intermittent portion 1 shown in FIG. 1 is formed by temporarily stopping the current supplied to the high frequency electrode 17 (positive electrode). Although not shown in FIG. 4, a guide plate is provided between the high-frequency electrode 15.16 and the high-frequency electrode 17.18, and the film edges la,' are provided after the first seal line S1 is formed. If the guide plate allows the guide plate to tilt the second seal line S2 toward the outer surface of the film constituting the casing, the high-frequency electrodes 17 and 18 can easily form the second seal line S2.

そして円筒状に形成されたケーシング10に対し、スタ
ッファノズル11から内容物が供給され、また送りロー
ラ19,20のさらに下方向に設けられたクランプ装置
によりクランプ部材2による締付けが行なわれ、第1図
に示すような包装体が形成される。なお、第1図に示す
ノツチ3は、包装体が完全に製造された後に付けること
もできるが、第4図に示す装置にノツチを成形する装置
を設け、第1のシール線S1が形成されてから第2のシ
ール線S2が形成されるまでの間にノツチ3を自動的に
形成することも可能である。
The contents are supplied from the stuffer nozzle 11 to the cylindrical casing 10, and the clamp member 2 is tightened by the clamp device provided further below the feed rollers 19, 20. A package as shown in FIG. 1 is formed. Note that the notch 3 shown in FIG. 1 can be added after the package is completely manufactured, but it is also possible to add a notch forming device to the device shown in FIG. 4 to form the first seal line S1. It is also possible to form the notch 3 automatically between the time the second seal line S2 is formed and the notch 3 formed.

第1図に示す円筒状フィルム包装体において、内容物か
らフィルム1を剥す方法の一例としてば、第2のシール
線S2の間欠部1に指を入れてノツチ3の部分からフィ
ルム縁部1aと1bを切断する。そして第5図に示すよ
うにフィルム縁部1aと1bをシール線S1ならびにS
2に沿フて引くと、フィルム縁部1aと1bはテープ状
となってフィルム1から分離されて引き剥される。
In the cylindrical film package shown in FIG. 1, an example of a method for peeling off the film 1 from the contents is to insert a finger into the intermittent portion 1 of the second seal line S2 and peel off the film edge 1a from the notch 3. Cut 1b. Then, as shown in FIG.
2, the film edges 1a and 1b become tape-like and are separated from the film 1 and peeled off.

これによってケーシング10のフィルム1が破られるこ
とになる。その詳細は、まずフィルム縁部1a、lbを
引くことによって第3図にてAで示す部分が破られる。
This causes the film 1 of the casing 10 to be torn. The details are as follows: First, by pulling the film edges 1a and lb, the portion indicated by A in FIG. 3 is torn.

すなわち指によって引かれる2枚のフィルム縁部1a、
lbに対しケーシング10側は1枚のフィルムであるた
め、フィルム縁部1a、1bを引くことによってケーシ
ング側の1枚のフィルム1がシール線S2の部分にて破
られる。続いて、フィルム縁部1aと1bが引かれるこ
とによって第3図にてBで示すシール線S1の部分にて
フィルム縁部1a、lbが分離され、よって第5図に示
すようにフィルム縁部1a、1bがテープ状に引き剥さ
れるようになる。場合によってはA部のみならず8部に
おいてもケーシング10を構成しているフィルム1に破
れが生じる。よってフィルム縁部1aと1bをテープ状
に引き剥していくにしたがって、ケーシング10を構成
しているフィルム1の破れが拡大していき、内容物が露
出する。
i.e. two film edges 1a drawn by fingers,
Since there is one film on the casing 10 side with respect to lb, by pulling the film edges 1a and 1b, the one film 1 on the casing side is torn at the seal line S2. Subsequently, the film edges 1a and 1b are pulled, and the film edges 1a and 1b are separated at the seal line S1 indicated by B in FIG. 1a and 1b come to be peeled off like a tape. In some cases, the film 1 constituting the casing 10 may be torn not only in the A section but also in the 8 section. Therefore, as the film edges 1a and 1b are peeled off in a tape-like manner, the tear in the film 1 constituting the casing 10 expands, and the contents are exposed.

またこの包装体のフィルム1を剥すには第6図に示す方
法も有効である。この方法は、まず指によってノツチ3
の部分からフィルム縁部1aと1bを分断する。フィル
ム縁部1a、lbのうちDで示す部分をケーシング10
から剥すと、前述のようにケーシング10を構成してい
るフィルム1が少なくとも第3図にてAで示す部分から
破られる。その後に包装体の端部を指で押して内容物を
膨らませると、第6図で示すように、フィルム1の破れ
部分が拡大していき、内容物が露出する。
The method shown in FIG. 6 is also effective for peeling off the film 1 of this package. In this method, first use your finger to open the notch 3.
The film edges 1a and 1b are separated from the part. The part indicated by D among the film edges 1a and lb is the casing 10
When it is peeled off, the film 1 constituting the casing 10 is torn at least from the part indicated by A in FIG. 3 as described above. When the end of the package is then pressed with a finger to inflate the contents, the torn portion of the film 1 expands and the contents are exposed, as shown in FIG.

なお第5図と第6図に示しているのは第1図に示す包装
体の開封方法の一例を示しているにすぎず、その他のど
のような方法で開封するにしろ、シール線S2の間欠部
1にてノツチ3からフィルム縁部1a、lbを破断する
ことによってケーシング10のフィルムを容易に剥すこ
とができる。
Note that what is shown in FIGS. 5 and 6 is only an example of how to open the package shown in FIG. The film of the casing 10 can be easily peeled off by breaking the film edges 1a, lb from the notch 3 at the intermittent portion 1.

第7図と第8図は本発明の第2実施例を示している。7 and 8 show a second embodiment of the invention.

この実施例では、第2のシール線S2の間欠部りに、第
1図にて符号3で示すノツチが、設けられていない。し
かしながらノツチ3が設けられていなくてもフィルム1
を剥す作業は容易である。その方法の一例としては、第
2のシール線S2の間欠部1の部分にてフィルム縁部1
a、lbを指でつかみ、第8図に示すようにこのフィル
ム縁部1a、lbを引く。これによってシール線S2の
部分、場合によってはシール線S1の部分にてケーシン
グ10のフィルム1が破れ、内容物が露出する。このよ
うにノツチ3を設けない構造であってもフィルムを剥す
作業は容易である。
In this embodiment, the notches indicated by reference numeral 3 in FIG. 1 are not provided at the intermittent portions of the second seal line S2. However, even if notch 3 is not provided, film 1
Peeling it off is easy. As an example of the method, the film edge 1 is
Grasp a and lb with your fingers and pull the film edges 1a and lb as shown in FIG. As a result, the film 1 of the casing 10 is torn at the seal line S2, or in some cases at the seal line S1, and the contents are exposed. Even with this structure without the notch 3, the work of peeling off the film is easy.

上記第1図〜第8図に示す実施例では、ケーシング10
を構成しているフィルム縁部1aと1bが第1のシール
線S1と第2のシール線S2とによって2箇所にて溶着
されている。第2図に示すようにフィルム縁部1a、l
bを合掌合せし、1つのシール線Stだけで溶着した場
合にはFで示す方向の力に対するシール線S1の強度は
弱いが、上記実施例では、第3図に示すように第1のシ
ール線S1に加えて第2のシール線S2が設けられてい
るため溶着強度は高められている。したがって、ソーセ
ージの場合のように包装完了後にボイル工程に8行され
、内部圧力が高まってフィルム張力によるFの方向への
力が作用したとしても十分な強度を発揮できるようにな
る。
In the embodiment shown in FIGS. 1 to 8 above, the casing 10
Film edges 1a and 1b constituting the film are welded at two locations by a first seal line S1 and a second seal line S2. As shown in FIG.
If the palms of the seal line S1 are joined together and welded with only one seal line St, the strength of the seal line S1 against the force in the direction F is weak, but in the above embodiment, as shown in FIG. Since the second seal line S2 is provided in addition to the line S1, the welding strength is increased. Therefore, as in the case of sausages, the product is subjected to eight boiling steps after packaging is completed, and even if the internal pressure is increased and a force in the direction of F due to film tension is applied, sufficient strength can be exerted.

またシール部分の強度をさらに高める必要がある場合に
は、第9図に示すように、フィルム縁部1aと1bとの
間に補強用のフィルムテープ11を介在させ、シール線
S1とSlにて、このフィルムテープ11を一緒に溶着
することも可能である。このフィルムテープ11として
は従来使用されている開封テープをそのまま用いること
が可能である。このように補強用のフィルムテープ11
を設けることによって、シール線S1と32部分にて溶
着されるフィルムの枚数を増加することができ、高周波
などによる溶着強度を高めることが可能になる。あるい
は第10図に示すように補強用のフィルムテープ11を
フィルム縁部1aの外側に添付し、このフィルムテープ
11をシール線StとSlにて溶着することによっても
、シール部の強度を高めることが可能になる。
In addition, if it is necessary to further increase the strength of the sealing part, as shown in FIG. It is also possible to weld this film tape 11 together. As the film tape 11, it is possible to use a conventional tear-opening tape as is. In this way, the reinforcing film tape 11
By providing this, it is possible to increase the number of films to be welded at the seal lines S1 and 32, and it is possible to increase the welding strength by high frequency or the like. Alternatively, as shown in FIG. 10, the strength of the seal portion can be increased by attaching a reinforcing film tape 11 to the outside of the film edge 1a and welding this film tape 11 to the seal lines St and Sl. becomes possible.

〔発明の効果) 以上のように本発明によれば、円筒状ケーシングを形成
するフィルムの縁部どうじを、合掌状態に合せてシール
するとともにさらにフィルム縁部をケーシングのフィル
ム外面に沿わせて第2のシール線を形成し、この第2の
シール線の途中に欠損部を設けているので、この第2の
シール線の欠損部にてフィルム縁部を指でつかみ、これ
を引き剥すことによってフィルムを容易に破ることがで
き、フィルムを内容物から剥しやすくなる。また2つの
シール線を形成しているため、合掌合せシールのみによ
る場合に比べてシール部の強度を高くできるようになる
。したがってソーセージの場合のボイル工程などにおい
て内部圧力が上昇しても、シール部からケーシングが破
壊されることはない。
[Effects of the Invention] As described above, according to the present invention, the edges of the film forming the cylindrical casing are sealed in accordance with the state of palms together, and the edges of the film are further aligned along the outer surface of the film of the casing. 2 seal line is formed, and a defect is provided in the middle of this second seal line, so by grasping the edge of the film with your fingers at the defect part of this second seal line and peeling it off. The film can be easily torn and the film can be easily peeled off from the contents. Furthermore, since two seal lines are formed, the strength of the seal portion can be increased compared to a case where only a palm-to-face seal is used. Therefore, even if the internal pressure increases during the boiling process for sausages, the casing will not be destroyed from the sealed portion.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は本発明の第1実施例による円筒状フィルム包装
体を示す正面図、第2図と第3図はシール線による溶着
部を示す断面拡大図、第4図は円筒状フィルム包装体の
製造装置の一例を示す斜視図、第5図と第6図は第1実
施例による円筒状フィルム包装体の開封方法の例を示す
正面図、第7図は本発明の第2実施例による円筒状フィ
ルム包装体を示す部分正面図、第8図は第2実施例によ
る円筒状フィルム包装体の開封方法の一例を示す部分正
面図、第9図と第1θ図は各々他の実施例による円筒状
フィルム包装体の断面拡大図、第11図は従来の円筒状
フィルム包装体を示す正面図、第12図は従来の円筒状
フィルム包装体の断面図である。 1・・・フィルム、la、lb・・・フィルム縁部、2
・・・クランプ部材、3・・・ノツチ、10・・・円筒
状ケーシング、Sl・・・第1のシール線、Sl・・・
第2のシール線、1・・・第2のシール線の間欠部。 第4図 第7図    第8図 第9図 第10図 第11図 ら 第12図
FIG. 1 is a front view showing a cylindrical film package according to a first embodiment of the present invention, FIGS. 2 and 3 are enlarged cross-sectional views showing a welded part by a seal line, and FIG. 4 is a cylindrical film package. 5 and 6 are front views showing an example of the method for opening the cylindrical film package according to the first embodiment, and FIG. 7 is a perspective view showing an example of the manufacturing apparatus according to the second embodiment of the present invention. FIG. 8 is a partial front view showing an example of the method for opening the cylindrical film package according to the second embodiment; FIG. 9 and FIG. 1θ are each according to other embodiments. FIG. 11 is a front view of a conventional cylindrical film package, and FIG. 12 is a cross-sectional view of a conventional cylindrical film package. 1... Film, la, lb... Film edge, 2
... Clamp member, 3... Notch, 10... Cylindrical casing, Sl... First seal line, Sl...
Second seal line, 1... Intermittent portion of the second seal line. Figure 4 Figure 7 Figure 8 Figure 9 Figure 10 Figure 11 and Figure 12

Claims (1)

【特許請求の範囲】[Claims]  フィルムの縁部どうしが溶着されて円筒状のケーシン
グが形成され、この円筒状のケーシング内に加工食品が
充填されているとともに、ケーシングの長手方向両端部
が閉じられているフィルム包装体において、前記フィル
ムの縁部どうしは、ケーシングの内面に連続する面どう
しが接するような合掌状態に合わされてこの合掌部が第
1のシール線によって溶着されており、さらに第1のシ
ール線から外方向へ延びる2枚のフィルム縁部が共にケ
ーシングの外面に合わされて、2枚のフィルム縁部とケ
ーシングを形成しているフィルムとが一緒に第2のシー
ル線によって溶着されており且つ、この第2のシール線
が間欠部を有して形成されていることを特徴とする加工
食品が充填された円筒状フィルム包装体。
In a film packaging body in which the edges of the film are welded together to form a cylindrical casing, the cylindrical casing is filled with a processed food, and both longitudinal ends of the casing are closed. The edges of the film are aligned in such a way that their continuous surfaces touch the inner surface of the casing, and this joined part is welded by a first seal line, and further extends outward from the first seal line. The two film edges are brought together on the outer surface of the casing, and the two film edges and the film forming the casing are welded together by a second seal line, and this second seal A cylindrical film package filled with a processed food, characterized in that lines are formed with intermittent parts.
JP62275282A 1987-10-30 1987-10-30 Cylindrical film package filled with processed food Expired - Lifetime JP2594068B2 (en)