JP6550311B2 - Peeling method - Google Patents

Peeling method Download PDF

Info

Publication number
JP6550311B2
JP6550311B2 JP2015189429A JP2015189429A JP6550311B2 JP 6550311 B2 JP6550311 B2 JP 6550311B2 JP 2015189429 A JP2015189429 A JP 2015189429A JP 2015189429 A JP2015189429 A JP 2015189429A JP 6550311 B2 JP6550311 B2 JP 6550311B2
Authority
JP
Japan
Prior art keywords
polarizing plate
adhesive tape
adhered
peeling
protective film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2015189429A
Other languages
Japanese (ja)
Other versions
JP2017065812A (en
Inventor
阿部 浩幸
浩幸 阿部
大悟 鈴木
大悟 鈴木
宜弘 中村
宜弘 中村
曜彰 大沢
曜彰 大沢
知広 原
知広 原
前田 実
実 前田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nitto Denko Corp
Original Assignee
Nitto Denko Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nitto Denko Corp filed Critical Nitto Denko Corp
Priority to JP2015189429A priority Critical patent/JP6550311B2/en
Priority to TW105125385A priority patent/TWI697712B/en
Priority to KR1020160119752A priority patent/KR20170037821A/en
Priority to CN201610833625.5A priority patent/CN106985499B/en
Publication of JP2017065812A publication Critical patent/JP2017065812A/en
Application granted granted Critical
Publication of JP6550311B2 publication Critical patent/JP6550311B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、積層体から偏光板を剥離する剥離方法に関する。   The present invention relates to a peeling method for peeling a polarizing plate from a laminate.

従来、液晶表示パネルや有機EL表示パネルといった画像表示装置の画像表示部に適用されるパネルとして、硬質ガラス板等により形成された基板と、該基板の少なくとも一方の面に接着された偏光板(偏光フィルム)とを備えたものが用いられている。流通段階においては、かかるパネルは、該パネルと、偏光板上に剥離可能に接着された表面保護フィルムとを有する積層体の状態で流通されている。   Conventionally, as a panel applied to an image display portion of an image display device such as a liquid crystal display panel or an organic EL display panel, a substrate formed of a hard glass plate or the like and a polarizing plate adhered to at least one surface of the substrate And a polarizing film are used. In the distribution stage, such a panel is distributed in the form of a laminate having the panel and a surface protective film releasably adhered on the polarizing plate.

この種の積層体は、例えば、基板に接着剤を介して偏光板を接着し、該偏光板の上に、該接着剤よりも接着力が小さい、剥離可能な接着剤を介して表面保護フィルムを接着することによって製造され、製造後に検査されるようになっている。この検査では、接着された偏光板の汚れや破損、該偏光板と基板との間への空気や異物の混入等の不具合が発見される場合がある。このように不具合が発見された場合、積層体から表面保護フィルムと共に偏光板を剥離することによって、得られた基板を別の積層体の製造に再利用することが行われている。このように偏光板を剥離することは、一般に、リワークと呼ばれている。   In this type of laminate, for example, a polarizing plate is adhered to a substrate via an adhesive, and a surface protective film on the polarizing plate via a releasable adhesive having smaller adhesion than the adhesive. It is manufactured by bonding and is to be inspected after manufacture. In this inspection, defects such as contamination or breakage of the adhered polarizing plate and mixing of air and foreign matter between the polarizing plate and the substrate may be found. When such a defect is found, the obtained substrate is reused to manufacture another laminate by peeling off the polarizing plate together with the surface protective film from the laminate. Such peeling of the polarizing plate is generally called rework.

ところで、このように積層体から偏光体を剥離する際、剥離時に偏光フィルムが裂け(破断し)、その一部が基板上に残ってしまう場合がある。   By the way, when peeling a polarizing body from a laminated body in this way, a polarizing film may tear at the time of peeling (rupture), and the one part may remain on a substrate.

そこで、フィルムの破断を抑制しつつ、積層体から該フィルムを剥離する方法が提案されている。
例えば、基板と、該基板に接着された破断し易いフィルムとを備えた積層体から該フィルムを剥離する方法であって、該破断し易いフィルムの全面に粘着シートを貼り付け、該粘着シートと共に該フィルムを剥離する方法が提案されている(特許文献1参照)。
Then, the method of peeling this film from a laminated body is proposed, suppressing the fracture | rupture of a film.
For example, a method of peeling the film from a laminate comprising a substrate and a breakable film adhered to the substrate, wherein an adhesive sheet is attached to the entire surface of the breakable film, together with the adhesive sheet. A method of peeling the film has been proposed (see Patent Document 1).

特開2014−88256号公報JP, 2014-88256, A

ここで、上記のように基板に偏光板と表面保護フィルムとが積層されてなる積層体から、表面保護フィルムと共に偏光板を剥離する際に、特許文献1に記載された剥離方法を適用すると、表面保護フィルムの全面に粘着シートを接着し、該粘着シート及び表面フィルムと共に偏光板を剥離することになる。
しかし、このように表面保護フィルムの全面に粘着シートを接着しても、偏光板を剥離する際、該偏光板が裂ける場合がある。このように偏光板が裂け、裂けた一部が基板に残ると、残った偏光板を別途剥離する必要が生じるため、その結果、偏光板を剥離する作業が困難となる。
Here, when the polarizing plate is peeled together with the surface protective film from the laminate in which the polarizing plate and the surface protective film are laminated on the substrate as described above, the peeling method described in Patent Document 1 is applied, An adhesive sheet is adhered to the entire surface of the surface protective film, and the polarizing plate is peeled off together with the adhesive sheet and the surface film.
However, even if the pressure-sensitive adhesive sheet is adhered to the entire surface of the surface protective film as described above, the polarizing plate may be torn when the polarizing plate is peeled off. As described above, when the polarizing plate is torn and a part of the torn is left on the substrate, it is necessary to separate the remaining polarizing plate separately. As a result, the operation of peeling the polarizing plate becomes difficult.

本発明は、上記事情に鑑み、偏光板が裂けることを抑制しつつ、該偏光板を表面保護フィルムと共に基板から簡便に剥離することを可能とする剥離方法を提供することを課題とする。   An object of the present invention is to provide a peeling method capable of easily peeling the polarizing plate from the substrate together with the surface protective film while suppressing the tearing of the polarizing plate in view of the above-mentioned circumstances.

本発明者らが、鋭意研究したところ、以下の知見を得た。
一般的によく知られているように、液晶表示パネル等において基板に接着された偏光板は、本来剥離されることが予定されていないものである。すなわち、本来剥離されることを前提として一のフィルムが他の部材に接着されるような場合よりも、遥かに強い接着力で偏光板が基板に接着されている。
これに対し、偏光板に接着された表面保護フィルムは、本来剥離されることが予定されているものである。すなわち、基板に対する偏光板の接着力よりも遥かに小さな接着力で、偏光板に表面保護フィルムが接着されている。
図19に、積層体30から、このような偏光板33と表面保護フィルム37とを一緒に剥離しようとして、両者を掴んで引っ張る状態を示す(図19中、白抜き矢印は、引っ張り方向を示す)。上記の通り、偏光板33と基板31との間の接着力よりも表面保護フィルム37と偏光板33との間の接着力の方が遥かに小さいため、基板31からの偏光板33の剥がれが進行するよりも速く、偏光板33からの表面保護フィルム37の剥がれが進行する。その結果、図19に示すように、偏光板33の未だ剥がれていない部分から表面保護フィルム37が剥がれること、すなわち、偏光板33からの表面保護フィルム37の乖離が発生することを見出した。
また、かかる乖離が発生すると、この乖離した部分において偏光板が裂け易くなることを見出した。
さらに、矩形状の偏光板を表面保護フィルムと共に剥離する際、通常、これらは、1つの角部から対角線を描くような方向に剥離される。そこで、この剥離起点を構成する2つの端縁(2辺)に沿うように、表面保護フィルムを剥離して偏光板に粘着テープを接着し、表面保護フィルムをこの粘着テープに被せてこれに接着し、偏光板を、表面保護フィルム及び粘着テープと共に引っ張ることによって、偏光板に対する表面保護フィルムの乖離を抑制することができ、これによって、偏光板の裂けを抑制しつつ、偏光板と表面保護フィルムとを剥離し得ることを見出した。
また、このようにすることによって、表面保護フィルムを全て剥離して偏光板を露出させ、露出した偏光板の全面に粘着シートを貼る必要がないため、その分、剥離作業が簡便になることも見出して、本発明を完成するに至った。
The present inventors earnestly studied and obtained the following findings.
As is generally well known, a polarizing plate adhered to a substrate in a liquid crystal display panel or the like is one which is not originally intended to be peeled off. That is, the polarizing plate is adhered to the substrate with much stronger adhesion than in the case where one film is adhered to another member on the premise that it is originally peeled off.
On the other hand, the surface protection film adhered to the polarizing plate is originally intended to be peeled off. That is, the surface protective film is adhered to the polarizing plate with an adhesive force much smaller than the adhesive force of the polarizing plate to the substrate.
FIG. 19 shows a state in which the polarizing plate 33 and the surface protective film 37 are separated and grasped and pulled from the laminate 30 together (white arrows in FIG. 19 indicate a pulling direction). ). As described above, since the adhesion between the surface protective film 37 and the polarization plate 33 is much smaller than the adhesion between the polarization plate 33 and the substrate 31, peeling of the polarization plate 33 from the substrate 31 is Peeling of the surface protection film 37 from the polarizing plate 33 proceeds faster than proceeding. As a result, as shown in FIG. 19, it has been found that the surface protection film 37 peels off from the portion of the polarizing plate 33 which has not been peeled yet, that is, the separation of the surface protection film 37 from the polarizing plate 33 occurs.
In addition, it has been found that when such a deviation occurs, the polarizing plate is easily torn at the part where the separation occurs.
Furthermore, when the rectangular polarizing plates are peeled together with the surface protective film, they are usually peeled in a direction that draws a diagonal line from one corner. Therefore, the surface protection film is peeled off along the two edges (two sides) constituting the peeling origin, the adhesive tape is adhered to the polarizing plate, and the surface protective film is covered on the adhesive tape and adhered thereto And by pulling the polarizing plate together with the surface protective film and the adhesive tape, it is possible to suppress the separation of the surface protective film from the polarizing plate, thereby suppressing the tearing of the polarizing plate, the polarizing plate and the surface protective film It was found that it was possible to exfoliate.
Moreover, since it is not necessary to peel all the surface protection films and to expose a polarizing plate and to stick an adhesive sheet on the whole surface of the exposed polarizing plate by doing in this way, the parting work becomes easy by that much. It found out and came to complete this invention.

すなわち、本発明に係る剥離方法は、
基板と、該基板の一方の面上に接着された偏光板とを備えた矩形状の積層体から前記偏光板を剥離する剥離方法であって、
前記積層体は、前記偏光板の上面に剥離可能に接着された表面保護フィルムをさらに備えており、
前記偏光板の上面に粘着テープを接着すべく前記表面保護フィルムを剥離し、
前記偏光板の4つの端縁のうち、少なくとも一の角部を構成する2つの端縁に粘着テープが沿うように、前記偏光板の上面に前記粘着テープを接着し、
前記表面保護フィルムを前記粘着テープに被せて接着し、
前記角部を剥離起点として前記表面保護フィルム及び前記粘着テープと共に前記偏光板を剥離する。
That is, the peeling method according to the present invention is
A peeling method for peeling the polarizing plate from a rectangular laminate including a substrate and a polarizing plate adhered on one surface of the substrate,
The laminate further includes a surface protection film releasably adhered to the upper surface of the polarizing plate,
Peeling off the surface protective film to adhere an adhesive tape to the upper surface of the polarizing plate;
The adhesive tape is adhered to the upper surface of the polarizing plate such that the adhesive tape is along two edges constituting at least one corner of the four edges of the polarizing plate,
Bonding the surface protective film to the adhesive tape and bonding;
The polarizing plate is peeled off together with the surface protective film and the pressure-sensitive adhesive tape, using the corner as a peeling starting point.

かかる構成によれば、表面保護フィルムを剥離して、偏光板の4つの端縁のうち、少なくとも一の角部を構成する2つの端縁に粘着テープが沿うように、偏光板の上面に粘着テープを接着し、表面保護フィルムを粘着テープに接着し、上記角部を剥離起点として表面保護フィルム及び粘着テープと共に偏光板を剥離することによって、偏光板を剥離する際に、表面保護フィルムが偏光板から乖離することを抑制できる。これにより、剥離の間、表面保護フィルムと偏光板とが接着された状態が維持されることになる(図18参照)。その結果、偏光板が表面保護フィルムで補強された状態が維持されつつ基板から剥離されるため、偏光板の裂けを抑制することが可能となる。
ここで、偏光板の上面の全面に特許文献1に記載されたような粘着シートを接着しようとすれば、表面保護フィルムを全て剥離して偏光板を露出させた後、露出した偏光板の上面の全面に粘着シートを接着させる必要がある。このため、偏光板の上面の全面に粘着シートを接着する分だけ手間がかかり、また、別途の粘着シートを用いて偏光板を補強することになる分だけ、手間がかかる。
しかし、上記構成によれば、偏光板の上面における端縁側の部分に粘着テープを接着するため、表面保護フィルムを全て剥離する必要がなく、その分、手間が省ける。また、表面保護フィルムで偏光板を補強することができるため、表面保護フィルムの有効利用を図ることができ、別途の部材で偏光板を補強する手間も省ける。
このように、偏光板が裂けることを抑制しつつ、該偏光板を表面保護フィルムと共に基板から簡便に剥離することが可能となる。
According to this configuration, the surface protection film is peeled off, and the adhesive tape adheres to the upper surface of the polarizing plate so that the adhesive tape is along the two edges constituting at least one corner of the four edges of the polarizing plate. The surface protective film is polarized when the polarizing plate is peeled off by bonding the tape, bonding the surface protective film to the pressure-sensitive adhesive tape, and peeling the polarizing plate together with the surface protective film and the pressure-sensitive adhesive tape with the corner as a peeling origin. It can control that it separates from a board. Thereby, the state in which the surface protection film and the polarizing plate are adhered is maintained during peeling (see FIG. 18). As a result, since the polarizing plate is peeled from the substrate while maintaining the state of being reinforced by the surface protective film, it is possible to suppress the tearing of the polarizing plate.
Here, if an adhesive sheet as described in Patent Document 1 is adhered to the entire surface of the upper surface of the polarizing plate, the entire surface protective film is peeled off to expose the polarizing plate, and then the upper surface of the exposed polarizing plate It is necessary to adhere the adhesive sheet to the entire surface of the Therefore, it takes time and effort to bond the pressure-sensitive adhesive sheet to the entire upper surface of the polarizing plate, and it takes time and effort to reinforce the polarizing plate using a separate pressure-sensitive adhesive sheet.
However, according to the above configuration, since the pressure-sensitive adhesive tape is adhered to the edge side portion of the upper surface of the polarizing plate, it is not necessary to peel off the surface protection film altogether, and labor can be saved accordingly. In addition, since the polarizing plate can be reinforced with the surface protective film, effective use of the surface protective film can be achieved, and the time and effort of reinforcing the polarizing plate with a separate member can be saved.
Thus, it is possible to easily peel the polarizing plate from the substrate together with the surface protective film while suppressing the tearing of the polarizing plate.

また、上記構成の剥離方法においては、
前記偏光板の前記粘着テープが沿うように接着される各端縁と、該各端縁に対応する前記粘着テープの外側の端縁とが面一に位置するように、または、前記偏光板の前記粘着テープが沿うように接着される各端縁から、該各端縁に対応する前記粘着テープの外側の端縁が前記偏光板の厚み未満の長さで突出するように、前記偏光板の上面に前記粘着テープを接着することが好ましい。
Moreover, in the peeling method of the said structure,
Each edge of the polarizing plate to be adhered along the adhesive tape and the outer edge of the adhesive tape corresponding to each edge are flush with each other, or The outer edge of the pressure-sensitive adhesive tape corresponding to each edge protrudes from each edge to be adhered along the pressure-sensitive adhesive tape with a length less than the thickness of the polarizing plate, It is preferable to adhere the adhesive tape on the top surface.

ここで、通常、基板は偏光板よりも大きく形成されているため、粘着テープの外側の端縁が偏光板の端縁よりも厚み以上の長さで外側にはみ出していると、該粘着テープが基板と接着し、基板からの偏光板の剥離を妨げるという不具合が発生するおそれがある。また、通常、偏光板は所定の形状となるように切断されて形成されており、微視的にはその端縁に一直線となっていない部分があるため、粘着テープの外側の端縁が偏光板の端縁よりも内側に引っ込んでいると、この一直線上となっていない部分を起点として裂けが生じるという不具合が発生するおそれがある。
しかし、かかる構成によれば、上記したような粘着テープのはみ出しによる不具合や、引っ込みによる不具合の発生を抑制し得るため、より確実に、偏光板が裂けることを抑制しつつ、偏光板を表面保護フィルムと共に基板から剥離することが可能となる。
Here, since the substrate is usually formed to be larger than the polarizing plate, when the outer edge of the pressure-sensitive adhesive tape protrudes beyond the edge of the polarizing plate by a length greater than the thickness of the edge of the polarizing plate, the pressure-sensitive adhesive tape There is a possibility that a defect may occur that adheres to the substrate and prevents peeling of the polarizing plate from the substrate. Also, usually, the polarizing plate is cut and formed to have a predetermined shape, and microscopically, there is a portion that is not straight at the end edge, so the outer edge of the adhesive tape is polarized If it is recessed inside the edge of the plate, there is a possibility that a failure may occur from the part which is not on the straight line as a starting point.
However, according to such a configuration, it is possible to suppress the occurrence of the problem due to the protrusion of the pressure-sensitive adhesive tape as described above and the problem due to the retraction, so the surface protection of the polarizing plate is performed while suppressing the tearing of the polarizing plate more reliably. It becomes possible to exfoliate from a substrate with a film.

また、上記構成の剥離方法においては、
前記偏光板の4つの端縁に沿うように、前記偏光板の上面に前記粘着テープを接着することが好ましい。
Moreover, in the peeling method of the said structure,
It is preferable to adhere the pressure-sensitive adhesive tape to the upper surface of the polarizing plate along the four edges of the polarizing plate.

かかる構成によれば、偏光板を剥離する際、偏光板から表面保護フィルムが乖離することをより確実に抑制し得るため、より確実に、偏光板が裂けることを抑制しつつ、偏光板を表面保護フィルムと共に基板から剥離することが可能となる。   According to this configuration, when peeling off the polarizing plate, it is possible to more reliably suppress the separation of the surface protection film from the polarizing plate, so it is possible to more reliably suppress the tearing of the polarizing plate while the surface of the polarizing plate is It becomes possible to peel from a substrate with a protective film.

また、上記構成の剥離方法においては、
前記表面保護フィルムを介して前記粘着テープと重なるように、前記表面保護フィルムの上面に粘着シートを接着し、
前記表面保護フィルム、前記粘着テープ及び前記粘着シートと共に前記偏光板を剥離することが好ましい。
Moreover, in the peeling method of the said structure,
An adhesive sheet is adhered to the upper surface of the surface protective film so as to overlap with the adhesive tape via the surface protective film,
It is preferable to peel the said polarizing plate with the said surface protection film, the said adhesive tape, and the said adhesive sheet.

かかる構成によれば、表面保護フィルムの上面に、さらに粘着シートを接着することによって、偏光板を剥離する際、該偏光板を一層補強し得るため、より確実に、偏光板が裂けることを抑制しつつ、偏光板を表面保護フィルムと共に基板から剥離することが可能となる。   According to this configuration, when the polarizing plate is peeled off by further adhering the pressure-sensitive adhesive sheet to the upper surface of the surface protective film, the polarizing plate can be further reinforced, so that the tearing of the polarizing plate is suppressed more surely. In addition, it becomes possible to peel the polarizing plate from the substrate together with the surface protective film.

以上の通り、本発明によれば、偏光板が裂けることを抑制しつつ、該偏光板を表面保護フィルムと共に基板から簡便に剥離することを可能とする剥離方法が提供される。   As described above, according to the present invention, there is provided a peeling method capable of easily peeling the polarizing plate from the substrate together with the surface protective film while suppressing the tearing of the polarizing plate.

本実施形態の剥離装置および剥離方法が適用される積層体を示す概略上面図Schematic top view which shows the laminated body to which the peeling apparatus and peeling method of this embodiment are applied 図1の積層体の層構成の一例を示す概略側面図Schematic side view showing an example of the layer configuration of the laminate of FIG. 1 図1の積層体のうち偏光板の層構成の一例を示す概略側面図The schematic side view which shows an example of the laminated constitution of a polarizing plate among the laminated bodies of FIG. 偏光板における剥離起点を構成する2つの端縁のうち一方の端縁が露出するように、表面保護フィルムの端縁側を偏光板から剥離した状態を示す概略上面図A schematic top view showing a state in which the edge side of the surface protective film is peeled from the polarizing plate so that one of the two edges constituting the peeling starting point of the polarizing plate is exposed. 露出した偏光板の端縁に沿うように粘着テープを接着した状態を示す概略上面図A schematic top view showing the adhesive tape adhered along the exposed edge of the polarizing plate 図5の状態から、表面保護フィルムを粘着テープに被せ、これに接着した状態を示す概略上面図From the state of FIG. 5, a surface protection film is covered on an adhesive tape, and the schematic top view which shows the state adhere | attached on this 偏光板における剥離起点となる角部を構成する2つの端縁のうち他方の端縁が露出するように、表面保護フィルムの端縁側を偏光板から剥離した状態を示す概略上面図A schematic top view showing a state in which the edge side of the surface protective film is peeled from the polarizing plate so that the other edge of the two edges constituting the corner serving as the peeling starting point of the polarizing plate is exposed 露出した偏光板の端縁に沿うように粘着テープを接着した状態を示す概略上面図A schematic top view showing the adhesive tape adhered along the exposed edge of the polarizing plate 図8の状態から、表面保護フィルムを粘着テープに被せ、これに接着した状態を示す概略上面図From the state of FIG. 8, a surface protection film is covered on an adhesive tape, and the schematic top view which shows the state adhere | attached on this 偏光板の4つの端縁に沿うように粘着テープを接着した後、表面保護フィルムを粘着テープに被せ、これに接着した状態を示す概略上面図After adhering the adhesive tape along the four edges of the polarizing plate, a surface protection film is put on the adhesive tape and it is a schematic top view showing the adhesive tape. 図5で接着した粘着シートと表面保護フィルム介して重なるように、表面保護フィルムに粘着シートを接着した状態を示す概略上面図The schematic top view which shows the state which adhere | attached the adhesive sheet to the surface protection film so that the adhesive sheet and the surface protection film which were adhered in FIG. 5 may overlap. 図8で接着した粘着シートと表面保護フィルム介して重なるように、表面保護フィルムに粘着シートを接着した状態を示す概略上面図The schematic top view which shows the state which adhere | attached the adhesive sheet to the surface protection film so that the adhesive sheet and the surface protection film which were adhered in FIG. 8 may overlap. 図10に示す4つの粘着シートと表面保護フィルム介して重なるように、表面保護フィルムに4つの粘着シートを接着した状態を示す概略上面図A schematic top view showing a state in which four pressure-sensitive adhesive sheets are adhered to a surface protection film so as to overlap with the four pressure-sensitive adhesive sheets shown in FIG. 10 via the surface protection film. 本実施形態の剥離方法に用いる剥離装置に、剥離起点から剥離された偏光板が巻き掛けられた状態を示す概略上面図The schematic top view which shows the state by which the polarizing plate peeled from the peeling origin was wound by the peeling apparatus used for the peeling method of this embodiment 本実施形態の剥離方法に用いる剥離装置に、剥離起点から剥離された偏光板が表面保護フィルム、粘着テープ及び粘着シートと共に巻き掛けられた状態を示す概略側面図The peeling apparatus used for the peeling method of this embodiment WHEREIN: The schematic side view which shows the state by which the polarizing plate peeled from the peeling origin was wound by the surface protection film, the adhesive tape, and the adhesive sheet. 巻き取り部材の回転によって偏光板が表面保護フィルム、粘着テープ及び粘着シートと共にさらに剥離されつつ、剥離された偏光板が表面保護フィルム、粘着テープ及び粘着シートと共に順次巻き取られる状態を示す概略側面図A schematic side view showing a state in which the peeled polarizing plate is sequentially taken up with the surface protective film, the adhesive tape and the adhesive sheet while the polarizing plate is further peeled together with the surface protective film, the adhesive tape and the adhesive sheet by the rotation of the winding member. 巻き取り部材の回転によって偏光板が表面保護フィルム、粘着テープ及び粘着シートと共に全て剥離された状態を示す概略側面図The schematic side view which shows the state in which the polarizing plate was all peeled with the surface protection film, the adhesive tape, and the adhesive sheet by rotation of a winding-up member 本実施形態の剥離方法によって偏光板が表面保護フィルム、粘着テープ及び粘着シートと共に剥離される状態を拡大して示す概略側面図The schematic side view which expands and shows the state by which a polarizing plate is peeled with a surface protection film, an adhesive tape, and an adhesive sheet by the peeling method of this embodiment 従来の剥離方法によって偏光板が表面保護フィルムと共に剥離される状態を拡大して示す概略側面図The schematic side view which expands and shows the state by which the polarizing plate is peeled with a surface protection film by the conventional peeling method

以下、本発明の実施形態に係る剥離方法について図面を参照しつつ説明する。   Hereinafter, a peeling method according to an embodiment of the present invention will be described with reference to the drawings.

まず、本実施形態の剥離方法で偏光板が剥離される積層体について説明する。
図1及び図2に示すように、積層体30は、矩形状の基板31と、該基板31の一方の面31a上に接着された矩形状の偏光板33と、該偏光板33の上面33a上に剥離可能に接着された表面保護フィルム37とを有している。
基板31は、偏光板33及び表面保護フィルム37よりも大きく形成され、偏光板33と表面保護フィルム37とは同じ大きさに形成されている。
First, a laminate from which a polarizing plate is peeled by the peeling method of the present embodiment will be described.
As shown in FIGS. 1 and 2, the laminate 30 includes a rectangular substrate 31, a rectangular polarizing plate 33 adhered on one surface 31 a of the substrate 31, and an upper surface 33 a of the polarizing plate 33. And a surface protection film 37 releasably adhered thereto.
The substrate 31 is formed to be larger than the polarizing plate 33 and the surface protection film 37, and the polarizing plate 33 and the surface protection film 37 are formed to have the same size.

基板31としては、例えば、硬質ガラス等が挙げられる。   Examples of the substrate 31 include hard glass and the like.

偏光板33は、基板31の上面31aに、第1の接着剤(不図示)によって接着されている。偏光板33は、4つの端縁34a、34b、34c、34dを、この順に隣接して有しており、これら端縁の交点が、4つの角部35a、35b、35c、35dを構成している。   The polarizing plate 33 is adhered to the upper surface 31 a of the substrate 31 by a first adhesive (not shown). The polarizing plate 33 has four edges 34a, 34b, 34c, 34d adjacent in this order, and the intersection of these edges constitutes four corners 35a, 35b, 35c, 35d. There is.

また、図3に示すように、本実施形態では、偏光板33は、具体的には、偏光子41と、偏光子41の両面にそれぞれ形成された第2の接着剤を有する接着剤層43と、これら接着剤層43にそれぞれ積層された保護フィルム45とを備えている。
なお、このように、本実施形態では、偏光板33が、偏光子41と、その両面に積層された保護フィルム45とを有する態様を示すが、その他、本発明では、偏光板33が、偏光子41と、その一方の面のみに積層された保護フィルム45とを有する態様を採用することもできる。
Further, as shown in FIG. 3, in the present embodiment, the polarizing plate 33 is specifically an adhesive layer 43 having a polarizer 41 and a second adhesive formed on both sides of the polarizer 41. And a protective film 45 laminated on each of the adhesive layers 43.
As described above, in the present embodiment, the polarizing plate 33 is an example having the polarizer 41 and the protective films 45 laminated on both sides thereof, but in the present invention, the polarizing plate 33 is polarized light. It is also possible to adopt an embodiment having the child 41 and the protective film 45 laminated on only one side thereof.

かかる偏光板33の厚みは、特に限定されるものではなく、適宜設定し得る。ただし、例えば、偏光板33の厚みが小さい程、強度が低下して破れ易くなる傾向にあり、一方、厚みが大きい程、強度が増加して破れ難くなる傾向にある。従って、例えば、偏光板33の厚みが、200μm以下、好ましくは90μm以下、さらに好ましくは50μm以下である場合に、本実施形態の剥離方法を好ましく適用できる。このように、厚みが比較的小さい場合であっても、偏光板30を補強して、剥離時に偏光板33を破れ難くすることができるため、本実施形態の剥離方法がより有用となるからである。   The thickness of the polarizing plate 33 is not particularly limited, and can be set as appropriate. However, for example, the smaller the thickness of the polarizing plate 33, the lower the strength and the easier it is to break. On the other hand, the larger the thickness, the higher the strength and the more difficult to break. Therefore, for example, when the thickness of the polarizing plate 33 is 200 μm or less, preferably 90 μm or less, more preferably 50 μm or less, the peeling method of the present embodiment can be preferably applied. As described above, even when the thickness is relatively small, it is possible to reinforce the polarizing plate 30 and make it difficult to break the polarizing plate 33 at the time of peeling, so the peeling method of the present embodiment becomes more useful. is there.

また、偏光板33の材質は、特に限定されるものではない。ただし、後述するように、偏光板33、特に、そのうち保護フィルム45の材質が破れ易いものである場合に、本実施形態の剥離方法を好ましく適用し得る。   Further, the material of the polarizing plate 33 is not particularly limited. However, as described later, the peeling method of the present embodiment can be preferably applied when the polarizing plate 33, particularly, the material of the protective film 45 among them is easy to tear.

偏光子41としては、ポリビニルアルコール系フィルムが染色、延伸されることによって形成されたものが挙げられる。
偏光子41の厚みは、通常、2〜30μm程度である。
Examples of the polarizer 41 include those formed by dyeing and stretching a polyvinyl alcohol-based film.
The thickness of the polarizer 41 is usually about 2 to 30 μm.

第1及び第2の接着剤としては、従来公知の接着剤が挙げられる。   The first and second adhesives include conventionally known adhesives.

保護フィルム45としては、トリアセチルセルロース等のセルロース樹脂、ポリエステル樹脂、ポリエーテルスルホン樹脂、ポリスルホン樹脂、ポリカーボネート樹脂、ポリアミド樹脂、ポリイミド樹脂、ポリオレフィン樹脂、(メタ)アクリル樹脂、環状ポリオレフィン樹脂(ノルボルネン樹脂)、ポリアリレート樹脂、ポリスチレン樹脂、ポリビニルアルコール樹脂、及び、これらの混合物等から形成されたフィルムが挙げられる。   As the protective film 45, cellulose resin such as triacetyl cellulose, polyester resin, polyether sulfone resin, polysulfone resin, polycarbonate resin, polycarbonate resin, polyamide resin, polyimide resin, polyolefin resin, (meth) acrylic resin, cyclic polyolefin resin (norbornene resin) And films formed from polyarylate resins, polystyrene resins, polyvinyl alcohol resins, and mixtures thereof.

上記したような保護フィルム45の厚みは、通常、20〜60μm程度である。   The thickness of the protective film 45 as described above is usually about 20 to 60 μm.

本実施形態の剥離方法で用いられる積層体30では、上記の通り、偏光板33が第1の接着剤によって基板31の上面31a上に接着されており、基板31に対する偏光板33の接着力(すなわち、第1の接着剤の接着力)は、通常、5〜15N/25mmである。かかる接着力であれば、基板31に対して偏光板33が比較的強固に接着され得る。また、このように強固に接着された偏光板33を剥離するときであっても、偏光板33の裂けを抑制し得る。よって、本実施形態の剥離方法は、上記範囲の接着力を有する積層体30に好適である。
かかる接着力は、オートグラフ(精密万能試験機、島津製作所製)によって、基板31から偏光板33を、引張速度300mm/minで90°方向に引き剥がして測定される値である。
In the laminate 30 used in the peeling method of the present embodiment, as described above, the polarizing plate 33 is adhered on the upper surface 31 a of the substrate 31 by the first adhesive, and the adhesion of the polarizing plate 33 to the substrate 31 ( That is, the adhesive force of the first adhesive is usually 5 to 15 N / 25 mm. With such an adhesive force, the polarizing plate 33 can be relatively firmly adhered to the substrate 31. Further, even when the polarizing plate 33 firmly bonded in this manner is peeled off, the tearing of the polarizing plate 33 can be suppressed. Therefore, the peeling method of this embodiment is suitable for the laminated body 30 which has the adhesive force of the said range.
The adhesive strength is a value measured by peeling off the polarizing plate 33 from the substrate 31 in a 90 ° direction at a tensile speed of 300 mm / min by an autograph (manufactured by Shimadzu Corporation, a precision universal tester).

表面保護フィルム37は、偏光板33の上面33aに、すなわち、保護フィルム45の上面に、上記第1の接着剤よりも弱い接着力を有する第3の接着剤(不図示)によって剥離可能に接着されている。
表面保護フィルム37は、偏光板33の4つの端縁34a〜34dにそれぞれ対応して(重なるように)、4つの端縁38a、38b、38c、38dを、この順に隣接して有しており、これら端縁の交点が、角部39a、39b、39c、39dを構成している。
本実施形態では、偏光板33に対する表面保護フィルム37の接着力(すなわち、第3の接着剤の接着力)は、通常、0.3〜2.0N/25mmである。かかる接着力であれば、偏光板33に対して表面保護フィルム37が剥離可能に接着され得る。
かかる接着力は、オートグラフ(精密万能試験機、島津製作所製)によって、偏光板33から表面保護フィルム37を、引張速度300mm/minで90°方向に引き剥がして測定される値である。
The surface protective film 37 is releasably adhered to the upper surface 33 a of the polarizing plate 33, that is, to the upper surface of the protective film 45 by a third adhesive (not shown) having weaker adhesion than the first adhesive. It is done.
The surface protection film 37 has four edges 38a, 38b, 38c and 38d adjacent to each other in this order, corresponding (overlapping) to the four edges 34a to 34d of the polarizing plate 33, respectively. The intersections of these edge parts constitute corner portions 39a, 39b, 39c, 39d.
In the present embodiment, the adhesion of the surface protection film 37 to the polarizing plate 33 (that is, the adhesion of the third adhesive) is usually 0.3 to 2.0 N / 25 mm. With such an adhesive force, the surface protection film 37 can be releasably adhered to the polarizing plate 33.
The adhesive strength is a value measured by peeling off the surface protective film 37 from the polarizing plate 33 in a 90 ° direction at a tensile speed of 300 mm / min by an autograph (manufactured by Shimadzu Corporation, a precision universal tester).

本実施形態の剥離方法は、
基板31と、該基板31の一方の面(上面)31a上に接着された偏光板33とを備えた矩形状の積層体30から前記偏光板33を剥離する剥離方法であって、
前記積層体30は、前記偏光板33の上面33aに剥離可能に接着された表面保護フィルム37をさらに備えており、
前記偏光板33の上面33aに粘着テープ51を接着すべく前記表面保護フィルム37を剥離し、
前記偏光板33の4つの端縁34a、34b、34c、34dのうち、少なくとも一の角部35aを構成する2つの端縁34a、34bに前記粘着テープ51が沿うように、前記偏光板33の上面33aに前記粘着テープ51を接着し、
前記表面保護フィルム37を前記粘着テープ51に被せて接着し、
前記角部35を剥離起点Pとして前記表面保護フィルム37及び前記粘着テープ51と共に前記偏光板33を剥離する。
また、本実施形態では、
前記偏光板33の前記粘着テープ51が沿うように接着される各端縁と、該各端縁に対応する前記粘着テープ51の外側の端縁とが面一に位置するように、または、前記偏光板33の前記粘着テープ51が沿うように接着される各端縁34a〜34dから、該各端縁34a〜34dに対応する前記粘着テープ51の外側の端縁が前記偏光板33の厚み未満の長さで突出するように、前記粘着テープ51を接着する。
より具体的には、本実施形態では、
前記偏光板33の4つの端縁34a〜34dに沿うように、前記偏光板33に前記粘着テープ51を接着する。
また、本実施形態では、
前記表面保護フィルム37を介して前記粘着テープ51と重なるように、前記表面保護フィルム37の上面37aに粘着シート53を接着し、
前記表面保護フィルム37、前記粘着テープ51及び前記粘着シート53と共に前記偏光板33を剥離する。
The peeling method of the present embodiment is
A peeling method for peeling the polarizing plate 33 from a rectangular laminate 30 including a substrate 31 and a polarizing plate 33 adhered on one surface (upper surface) 31 a of the substrate 31.
The laminate 30 further includes a surface protection film 37 releasably adhered to the upper surface 33 a of the polarizing plate 33,
The surface protection film 37 is peeled off to adhere the adhesive tape 51 to the upper surface 33a of the polarizing plate 33,
Of the four edges 34a, 34b, 34c, 34d of the polarizer 33, the adhesive tape 51 is placed along the two edges 34a, 34b that constitute at least one corner 35a. The adhesive tape 51 is adhered to the upper surface 33a,
Bonding the surface protection film 37 onto the adhesive tape 51;
The polarizing plate 33 is peeled off together with the surface protection film 37 and the adhesive tape 51 with the corner portion 35 as the peeling start point P.
Also, in the present embodiment,
Each edge of the polarizing plate 33 to be adhered along the adhesive tape 51 and the outer edge of the adhesive tape 51 corresponding to each edge are flush with each other, or From the edges 34a to 34d of the polarizing plate 33 adhered along the adhesive tape 51, the outer edges of the adhesive tape 51 corresponding to the respective edges 34a to 34d are less than the thickness of the polarizing plate 33 The adhesive tape 51 is adhered so as to protrude with a length of.
More specifically, in the present embodiment,
The adhesive tape 51 is adhered to the polarizing plate 33 along the four edges 34 a to 34 d of the polarizing plate 33.
Also, in the present embodiment,
An adhesive sheet 53 is adhered to the upper surface 37 a of the surface protective film 37 so as to overlap with the adhesive tape 51 via the surface protective film 37,
The polarizing plate 33 is peeled off together with the surface protection film 37, the pressure-sensitive adhesive tape 51 and the pressure-sensitive adhesive sheet 53.

本実施形態の剥離方法においては、偏光板33の角部35aを剥離起点Pとして、偏光板33を基板31から剥離することとする。
また、偏光板33の4つの端縁34a〜34dにそれぞれ沿うように、粘着テープ51を接着することとする。
In the peeling method of the present embodiment, the polarizing plate 33 is peeled from the substrate 31 with the corner 35 a of the polarizing plate 33 as the peeling starting point P.
Also, the adhesive tape 51 is adhered along the four edges 34 a to 34 d of the polarizing plate 33.

本実施形態では、偏光板33の各端縁34a、34b、34c、34dに沿うように、粘着テープ51を偏光板33の上面33aに接着する。また、粘着テープ51としては、両面側に粘着剤(第1の粘着剤、不図示)を有しているテープ、具体的には両面テープを用いる。かかる粘着テープ51の一面側の粘着剤は露出しており、他面側の粘着剤には剥離ライナー(不図示)が貼着されている。   In the present embodiment, the adhesive tape 51 is adhered to the upper surface 33 a of the polarizing plate 33 along the edges 34 a, 34 b, 34 c, 34 d of the polarizing plate 33. Further, as the adhesive tape 51, a tape having an adhesive (a first adhesive, not shown) on both sides, specifically, a double-sided tape is used. The adhesive on one side of the adhesive tape 51 is exposed, and a release liner (not shown) is attached to the adhesive on the other side.

粘着テープ51の接着力、すなわち、両面テープの接着力(上記第1の粘着剤の接着力)は、偏光板33の上面33aに対する表面保護フィルム37の接着力(上記第3の接着剤の接着力)よりも大きい。かかる粘着テープ51の接着力は、10.0N/25mm以上であることが好ましく、15.0N/25mm以上がより好ましい。
接着力が10.0N/25mm以上であることによって、基板31から偏光板33を剥離している間に、粘着テープ51が偏光板33から乖離することを抑制し得るため、より確実に、偏光板33裂けることなく該偏光板33を表面保護フィルム37と共に基板31から剥離し得る。
なお、上記接着力は、オートグラフ(精密万能試験機、島津製作所製)によって、偏光板33から表面保護フィルム37を、引張速度300mm/minで90°方向に引き剥がして測定される値である。
The adhesion of the adhesive tape 51, that is, the adhesion of the double-sided tape (the adhesion of the first adhesive) is the adhesion of the surface protection film 37 to the upper surface 33a of the polarizing plate 33 (the adhesion of the third adhesive Greater than force). The adhesive strength of the adhesive tape 51 is preferably 10.0 N / 25 mm or more, and more preferably 15.0 N / 25 mm or more.
When the adhesive strength is 10.0 N / 25 mm or more, separation of the adhesive tape 51 from the polarizing plate 33 can be suppressed while the polarizing plate 33 is peeled from the substrate 31, so polarization can be more reliably performed. The polarizing plate 33 can be peeled off from the substrate 31 together with the surface protective film 37 without tearing the plate 33.
The adhesive strength is a value measured by peeling off the surface protection film 37 from the polarizing plate 33 in a 90 ° direction at a tensile speed of 300 mm / min by an autograph (manufactured by Shimadzu Corporation, a precision universal tester). .

本実施形態の剥離方法においては、具体的には、まず、図4に示すように、偏光板33の端縁34aに沿うように粘着テープ51を接着するために、表面保護フィルム37の端縁38a側を部分的に剥離する。
この剥離によって露出した偏光板33の上面33aの領域に、図5に示すように、端縁34aに沿うように粘着テープ51を接着する。接着後、粘着テープ51に貼着されている剥離ライナー(不図示)を剥離し、図6に示すように、露出した粘着テープ51の接着剤(不図示)に表面保護フィルム37を被せて接着する。なお、ここでは、偏光板33の端縁34b、34d側に粘着テープ51を接着すべく該端縁34b、34d側の表面保護フィルム37を部分的に剥離できるような剥離しろを設けるように、偏光板33の端縁34a側に粘着テープ51を接着する。
Specifically, in the peeling method of the present embodiment, first, as shown in FIG. 4, in order to bond the adhesive tape 51 along the edge 34 a of the polarizing plate 33, the edge of the surface protection film 37 Partially peel off the 38a side.
As shown in FIG. 5, an adhesive tape 51 is adhered along the edge 34a to the area of the upper surface 33a of the polarizing plate 33 exposed by this peeling. After bonding, the release liner (not shown) attached to the pressure-sensitive adhesive tape 51 is peeled off, and as shown in FIG. 6, the surface protective film 37 is covered on the exposed adhesive (not shown) of the pressure-sensitive adhesive tape 51 Do. Here, in order to bond the adhesive tape 51 to the edges 34b and 34d of the polarizing plate 33, a peeling margin is provided so that the surface protection film 37 on the edges 34b and 34d can be partially peeled off. The adhesive tape 51 is adhered to the edge 34 a side of the polarizing plate 33.

次に、図7に示すように、偏光板33の端縁34bに沿うように粘着テープ51を接着するために、表面保護フィルム37の端縁38b側を部分的に剥離する。
この剥離によって露出した偏光板33の上面33aの領域に、図8に示すように、端縁34bに沿うように粘着テープ51を接着する。接着後、粘着テープ51に貼着されている剥離ライナー(不図示)を剥離し、図9に示すように、露出した粘着テープ51の接着剤(不図示)に表面保護フィルム37を被せて接着する。なお、ここでは、上記偏光板33の端縁34a側への粘着フィルム51の接着で形成された剥離しろを埋めるように、且つ、偏光板33の端縁34c側に粘着テープ51を接着すべく該端縁34c側の表面保護フィルム37を部分的に剥離できるような剥離しろを設けるように、偏光板33の端縁34b側に粘着テープ51を接着する。
Next, as shown in FIG. 7, in order to adhere the adhesive tape 51 along the edge 34 b of the polarizing plate 33, the edge 38 b side of the surface protective film 37 is partially peeled off.
An adhesive tape 51 is adhered to the area of the upper surface 33a of the polarizing plate 33 exposed by this peeling, as shown in FIG. 8, along the edge 34b. After bonding, the release liner (not shown) attached to the adhesive tape 51 is peeled off, and as shown in FIG. 9, the surface protective film 37 is covered on the exposed adhesive (not shown) of the adhesive tape 51 to adhere Do. Here, the adhesive tape 51 is adhered to the edge 34 c side of the polarizing plate 33 so as to fill the peeling margin formed by the adhesion of the adhesive film 51 to the edge 34 a side of the polarizing plate 33. The adhesive tape 51 is adhered to the edge 34 b side of the polarizing plate 33 so as to provide a peeling margin so that the surface protection film 37 on the edge 34 c side can be partially peeled off.

これらと同様にして、偏光板33の端縁34cに沿うように粘着テープ51を接着するために、表面保護フィルム37の端縁38c側を剥離し、この剥離によって露出した偏光板33の上面33aの領域に、端縁34cに沿うように粘着テープ51を接着する。接着後、粘着テープ51に貼着されている剥離ライナーを剥離し、露出した粘着テープ51の粘着剤に表面保護フィルム37を被せて接着する。なお、ここでは、上記偏光板33の端縁34b側への粘着フィルム51の接着で形成された剥離しろを埋めるように、且つ、偏光板33の端縁34d側に粘着テープ51を接着すべく該端縁34d側の表面保護フィルム37を部分的に剥離できるような剥離しろを設けるように、偏光板33の端縁34c側に粘着テープ51を接着する。
さらに、端縁34dに沿うように粘着テープ51を接着するために、表面保護フィルム37の端縁38d側を部分的に剥離し、この剥離によって露出した偏光板33の上面33aの領域に、端縁34dに沿うように粘着テープ51を接着する。接着後、粘着テープ51に貼着されている剥離ライナーを剥離し、露出した粘着テープ51の粘着剤に表面保護フィルム37を被せて接着する。なお、ここでは、上記偏光板33の端縁34a、34c側への粘着フィルム51の接着で形成された剥離しろを埋めるように、偏光板33の端縁34d側に粘着テープ51を接着する。
Similarly to the above, in order to bond the adhesive tape 51 along the edge 34c of the polarizing plate 33, the edge 38c side of the surface protective film 37 is peeled off, and the upper surface 33a of the polarizing plate 33 exposed by this peeling. The adhesive tape 51 is adhered along the edge 34 c in the area of After bonding, the release liner attached to the pressure-sensitive adhesive tape 51 is peeled off, and the exposed surface of the pressure-sensitive adhesive tape 51 is covered with the surface protective film 37 for adhesion. Here, the adhesive tape 51 is adhered to the edge 34 d side of the polarizing plate 33 so as to fill the peeling margin formed by the adhesion of the adhesive film 51 to the edge 34 b side of the polarizing plate 33. The adhesive tape 51 is adhered to the edge 34c side of the polarizing plate 33 so as to provide a peeling margin so as to partially peel off the surface protection film 37 on the edge 34d side.
Furthermore, in order to adhere the adhesive tape 51 along the edge 34d, the edge 38d side of the surface protection film 37 is partially peeled off, and the edge is in the region of the upper surface 33a of the polarizing plate 33 exposed by this peeling. The adhesive tape 51 is adhered along the edge 34d. After bonding, the release liner attached to the pressure-sensitive adhesive tape 51 is peeled off, and the exposed surface of the pressure-sensitive adhesive tape 51 is covered with the surface protective film 37 for adhesion. Here, the adhesive tape 51 is adhered to the edge 34 d side of the polarizing plate 33 so as to fill the peeling margin formed by the adhesion of the adhesive film 51 to the edge 34 a, 34 c side of the polarizing plate 33.

このように、偏光板33の4つの端縁34a〜34dに沿うように偏光板33の上面33aに粘着テープ51を接着すべく、表面保護フィルム37を部分的に剥離し、剥離によって露出した偏光板33の上面33aに粘着テープ51を接着した後、各粘着テープ51に貼着されている剥離ライナーを剥離し、図10に示すように、露出した粘着テープ51の粘着剤に表面保護フィルム37を被せて接着する。   Thus, in order to adhere the adhesive tape 51 to the upper surface 33a of the polarizing plate 33 along the four edges 34a to 34d of the polarizing plate 33, the surface protection film 37 is partially peeled off, and the polarized light is exposed by peeling. After adhering the adhesive tape 51 to the upper surface 33a of the plate 33, the release liner attached to each adhesive tape 51 is peeled off, and as shown in FIG. 10, the surface protective film 37 is made of the adhesive of the exposed adhesive tape 51. Cover and bond.

本実施形態では、偏光板33の粘着テープ51が沿うように接着される各端縁と(すなわち4つの各端縁34a〜34d)と、各端縁に対応する粘着テープ51の外側の端縁とが面一に位置される(すなわち、偏光板33の各端縁と、各粘着テープ51の外側の端縁とが一致する)ように、または、前記偏光板33の前記粘着テープ51が沿うように接着される各端縁34a〜34dから、該各端縁34a〜34dに対応する前記粘着テープ51の外側の端縁が前記偏光板33の厚み未満の長さで突出するように、偏光板33の上面33aに粘着テープ51を接着する。   In the present embodiment, each edge to which the adhesive tape 51 of the polarizing plate 33 is adhered along (i.e., each of four edges 34a to 34d) and the outer edge of the adhesive tape 51 corresponding to each edge Such that each edge of the polarizing plate 33 and the outer edge of each adhesive tape 51 coincide, or the adhesive tape 51 of the polarizing plate 33 is aligned So that the outer edges of the adhesive tape 51 corresponding to the respective edges 34a to 34d protrude with a length less than the thickness of the polarizing plate 33 from the respective edges 34a to 34d to be bonded The adhesive tape 51 is adhered to the upper surface 33 a of the plate 33.

ここで、図1に示すように、通常、基板31は偏光板33よりも大きく形成されているため、粘着テープ51の外側の端縁が偏光板33の端縁よりも外側にはみ出していると、該粘着テープ51が基板31と接着し、基板31からの偏光板33の剥離を妨げるという不具合が発生するおそれがある。また、通常、偏光板33は所定の形状となるように切断されて形成されており、微視的にはその端縁に一直線となっていない部分(例えばギザギザになっている部分)があるため、粘着テープ51の外側の端縁が偏光板33の端縁よりも内側に引っ込んでいると、この一直線となっていない部分を起点として裂けが生じるという不具合が発生するおそれがある。   Here, as shown in FIG. 1, since the substrate 31 is usually formed larger than the polarizing plate 33, it is assumed that the outer edge of the adhesive tape 51 protrudes outside the edge of the polarizing plate 33. The adhesive tape 51 adheres to the substrate 31, which may cause a problem that the peeling of the polarizing plate 33 from the substrate 31 is hindered. Also, normally, the polarizing plate 33 is cut and formed to have a predetermined shape, and microscopically, there is a portion (for example, a jagged portion) that is not a straight line at the end edge When the outer edge of the adhesive tape 51 is recessed inward of the edge of the polarizing plate 33, there is a possibility that a tear may occur starting from the portion which is not straight.

しかし、上記のように、偏光板33の粘着テープ51が沿うように接着される各端縁と、各端縁に対応する粘着テープ51の外側の端縁とが面一に位置するように、または、前記偏光板33の前記粘着テープ51が沿うように接着される各端縁34a〜34dから、該各端縁34a〜34dに対応する前記粘着テープ51の外側の端縁が前記偏光板33の厚み未満の長さで突出するように、偏光板33の上面33aに粘着テープ51を接着することによって、上記したような粘着テープ51のはみ出しによる不具合や、引っ込みによる不具合の発生を抑制し得るため、より確実に、偏光板33が裂けることを抑制しつつ、前記偏光板33を表面保護フィルム37と共に基板31から剥離することが可能となる。
なお、粘着テープ51の外側の端縁が偏光板33の端縁34a〜34dよりも外側に、該偏光板33の厚み未満の長さで突出している場合には、粘着テープ51が基材31に接着することなく、上記と同様に、より確実に、偏光板33が裂けることを抑制しつつ、前記偏光板33を表面保護フィルム37と共に基板31から剥離することが可能となる。
However, as described above, each edge to which the adhesive tape 51 of the polarizing plate 33 is adhered along and the outer edge of the adhesive tape 51 corresponding to each edge are flush with each other. Alternatively, from the edges 34a to 34d of the polarizing plate 33 adhered along the adhesive tape 51, the outer edges of the adhesive tape 51 corresponding to the respective edges 34a to 34d are the polarizing plate 33. By sticking the adhesive tape 51 to the upper surface 33a of the polarizing plate 33 so as to project with a length less than the thickness of the above, occurrence of defects due to the above-mentioned sticking of the adhesive tape 51 or defects due to retraction can be suppressed. Therefore, it is possible to peel off the polarizing plate 33 together with the surface protection film 37 from the substrate 31 while suppressing the tearing of the polarizing plate 33 more reliably.
When the outer edge of the adhesive tape 51 protrudes outside the edges 34 a to 34 d of the polarizing plate 33 by a length less than the thickness of the polarizing plate 33, the adhesive tape 51 is the substrate 31. It becomes possible to peel off the polarizing plate 33 together with the surface protection film 37 from the substrate 31 while suppressing the tearing of the polarizing plate 33 more reliably, as described above, without adhering to the above.

粘着テープ51の幅は、特に限定されるものではなく、適宜設定し得る。例えば、粘着テープ51の幅が大きくなれば、表面保護フィルム37と偏光板33との乖離をより抑制し得る傾向にある一方、コストが高くなる傾向にある。従って、例えば、かかる観点を考慮して、粘着テープ51の幅は、10〜50mmであることが好ましい。   The width of the adhesive tape 51 is not particularly limited, and may be set as appropriate. For example, when the width of the adhesive tape 51 is increased, the separation between the surface protective film 37 and the polarizing plate 33 tends to be further suppressed, but the cost tends to be increased. Therefore, for example, in consideration of this point of view, the width of the adhesive tape 51 is preferably 10 to 50 mm.

次に、偏光板33の端縁34a、34b、34c、34dに沿って接着された粘着テープ51と表面保護フィルム37を介して重なるように、該表面保護フィルム37の上面37aに、さらに粘着シート53を接着する。   Next, on the upper surface 37a of the surface protective film 37, the adhesive sheet 51 is further adhered so that the adhesive tape 51 adhered along the edges 34a, 34b, 34c, 34d of the polarizing plate 33 and the surface protective film 37 overlap. Glue 53

本実施形態では、一面側にのみ粘着剤が露出した粘着シートを用いる。かかる粘着シート53として、例えば、粘着テープ51と同様の、両面テープの一面側に剥離ライナーが貼着されてなるものを(剥離ライナーを剥離することなく)用いる。
この粘着シート53の表面(表面保護フィルム37に接着される側とは反対の側の面、ここでは剥離ライナーの表面)は、表面保護フィルム37よりも滑り性が高いことが好ましい。具体的には、粘着シート53の表面の摩擦係数が、表面保護フィルム37の上面37aの摩擦係数よりも小さいことが好ましい。
In the present embodiment, a pressure-sensitive adhesive sheet in which the pressure-sensitive adhesive is exposed only on one side is used. As the pressure-sensitive adhesive sheet 53, for example, one having a release liner attached to one surface side of the double-sided tape similar to the pressure-sensitive adhesive tape 51 is used (without releasing the release liner).
It is preferable that the surface of the pressure-sensitive adhesive sheet 53 (the surface on the side opposite to the side to be adhered to the surface protective film 37, here, the surface of the release liner) has higher slipperiness than the surface protective film 37. Specifically, the coefficient of friction of the surface of the adhesive sheet 53 is preferably smaller than the coefficient of friction of the upper surface 37 a of the surface protective film 37.

具体的には、図11に示すように、偏光板33の端縁34aに沿うように接着した粘着テープ51と、表面保護フィルム37を介して重なるように、すなわち、該表面保護フィルム37の端縁38aに沿うように、該表面保護フィルム37の上面37aに、さらに粘着シート53を接着する。   Specifically, as shown in FIG. 11, the adhesive tape 51 adhered along the edge 34 a of the polarizing plate 33 and the surface protection film 37 overlap, that is, the end of the surface protection film 37. An adhesive sheet 53 is further adhered to the upper surface 37a of the surface protective film 37 along the edge 38a.

また、図12に示すように、偏光板33の端縁34bに沿うように接着した粘着テープ51と、表面保護フィルム37を介して重なるように、すなわち、該表面保護フィルム37の端縁38bに沿うように、該表面保護フィルム37の上面37aに、さらに粘着シート53を接着する。   Further, as shown in FIG. 12, the adhesive tape 51 adhered along the edge 34 b of the polarizing plate 33 and the surface protection film 37 overlap with each other, that is, the edge 38 b of the surface protection film 37. An adhesive sheet 53 is further adhered to the upper surface 37 a of the surface protective film 37 so as to be along.

さらに、これらと同様にして、偏光板33の端縁34cに沿うように接着した粘着テープ51と、表面保護フィルム37を介して重なるように、すなわち、該表面保護フィルム37の端縁38cに沿うように、該表面保護フィルム37の上面37aに、さらに粘着シート53を接着する。
また、偏光板33の端縁34dに沿うように接着した粘着テープ51と、表面保護フィルム37を介して重なるように、すなわち、該表面保護フィルム37の端縁38dに沿うように、該表面保護フィルム37の上面37aに、さらに粘着シート53を接着する。
Furthermore, in the same manner as above, the adhesive tape 51 adhered along the edge 34 c of the polarizing plate 33 is overlapped with the surface protection film 37 via the surface protection film 37, that is, along the edge 38 c of the surface protection film 37. Thus, the adhesive sheet 53 is further adhered to the upper surface 37 a of the surface protective film 37.
The surface protection film 51 is adhered to the edge 34 d of the polarizing plate 33 so as to overlap with the adhesive tape 51 via the surface protection film 37, that is, along the edge 38 d of the surface protection film 37. The adhesive sheet 53 is further adhered to the upper surface 37 a of the film 37.

このようにして、図13に示すように、表面保護フィルム37を介して粘着テープ51と重なるように、表面保護フィルム37の上面37aに、その4つの端縁38a〜38dに沿うように、粘着シート53を接着する。   In this manner, as shown in FIG. 13, the upper surface 37a of the surface protection film 37 is adhered to the upper surface 37a of the surface protection film 37 so as to overlap with the adhesive tape 51 via the surface protection film 37. The sheet 53 is adhered.

引き続き、剥離装置1を用いて、前記表面保護フィルム37、粘着テープ51及び粘着シート53と共に前記偏光板33を、偏光板33の角部35aを剥離起点Pとして順次剥離する。   Subsequently, the surface protection film 37, the pressure-sensitive adhesive tape 51, and the pressure-sensitive adhesive sheet 53 are sequentially peeled off using the peeling device 1 with the corner portion 35a of the polarizing plate 33 as the peeling start point P.

本実施形態の剥離方法に用いる好ましい剥離装置1について説明する。   The preferable peeling apparatus 1 used for the peeling method of this embodiment is demonstrated.

図14、図15に示すように、本実施形態の剥離装置1は、積層体30が載置されるステージ部材3と、ローラ状の剥離用部材7と、積層体30から剥離され且つ剥離用部材7によって剥離された偏光板33の角部35aを、これと重なる表面保護フィルム39の角部39a、粘着テープ51及び粘着シート53を保持して、偏光板33をさらに順次剥離する剥離部材5とを備えている。
より具体的には、本実施形態の剥離装置1は、剥離部材5として、積層体30から剥離され且つ剥離用部材7によって湾曲された偏光板33の角部35aが、これと重なっている粘着テープ51、粘着シート53及び表面保護フィルムの角部39aと共に巻き架けられて、回転することにより偏光板33をさらに剥離しながら順次巻き取る巻き取り部材5を備えている。
As shown in FIG. 14 and FIG. 15, the peeling apparatus 1 of this embodiment peels from the stage member 3 on which the laminated body 30 is placed, the roller-like peeling member 7 and the laminated body 30 and is for peeling A peeling member 5 which holds the corner portion 35a of the polarizing plate 33 peeled off by the member 7 and the corner portion 39a of the surface protection film 39 overlapping with this, the adhesive tape 51 and the adhesive sheet 53, and peels the polarizing plate 33 further sequentially. And have.
More specifically, in the peeling apparatus 1 of the present embodiment, as the peeling member 5, an adhesive in which the corner 35 a of the polarizing plate 33 peeled from the laminate 30 and curved by the peeling member 7 overlaps with this. A winding member 5 is provided which is wound along with the tape 51, the adhesive sheet 53 and the corner portion 39a of the surface protective film, and is further wound while sequentially peeling the polarizing plate 33 by rotating.

ステージ部材3は、積層体30から全ての偏光板33が剥離されるまでの間、積層体30が載置される台である。   The stage member 3 is a stage on which the stacked body 30 is mounted until all the polarizing plates 33 are peeled from the stacked body 30.

剥離用部材7は、偏光板33を基板31から剥離させると共に、剥離された偏光板33を表面保護フィルム37、粘着テープ51及び粘着シート53と共に湾曲させながら後端側へと案内するものである。かかる剥離用部材7として、ローラ体が挙げられる。   The peeling member 7 peels the polarizing plate 33 from the substrate 31 and guides the peeled polarizing plate 33 along with the surface protection film 37, the adhesive tape 51 and the adhesive sheet 53 to the rear end side while curving. . A roller body may be mentioned as the peeling member 7.

巻き取り部材5は、剥離された偏光板33の角部35aが、これと重なっている粘着テープ51、粘着シート53及び表面保護フィルム37の角部39aと共に巻き架けられ、この状態で回転することによって、偏光板33を、粘着テープ51、粘着シート53及び表面保護フィルム37と共に、さらに剥離しつつ順次巻き取るものである。
このような巻き取り部材5としては、例えば、モーター等の駆動装置17による駆動を受けて回転するローラ等が挙げられる。
また、巻き取り部材5には、上記剥離された偏光板33の角部35aが、これと重なっている粘着テープ51、粘着シート53及び表面保護フィルム37の角部39aと共に、接着テープ(不図示)等によって固定されるようになっている。
なお、図14では、偏光板33は、上記第1の接着剤(不図示)と共に基板31から剥離される。
The winding member 5 is wound with the adhesive tape 51, the adhesive sheet 53, and the corner 39a of the surface protective film 37, which are overlapped with the corner 35a of the separated polarizing plate 33, and is rotated in this state. Thus, the polarizing plate 33 is sequentially taken up with the pressure-sensitive adhesive tape 51, the pressure-sensitive adhesive sheet 53 and the surface protective film 37 while being further peeled off.
As such a winding member 5, for example, a roller that rotates in response to a drive by a drive device 17 such as a motor can be mentioned.
Further, in the winding member 5, an adhesive tape (not shown) together with the adhesive tape 51, the adhesive sheet 53, and the corner 39a of the surface protection film 37 where the corner 35a of the separated polarizing plate 33 is overlapped. And so on).
In FIG. 14, the polarizing plate 33 is peeled from the substrate 31 together with the first adhesive (not shown).

本実施形態では、上記剥離装置1を用い、積層体30から偏光板33の角部35aを、表面保護フィルム37の角部39a、粘着テープ51及び粘着シート53と共に剥離して、この剥離した部分を、剥離用部材7に巻き架けながら、さらに剥離部材5に巻き架ける。この状態で、剥離部材51で巻き取ることによって、剥離された偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に、剥離用部材7によって湾曲させながら剥離部材5へと案内しつつ、剥離部材5で巻き取ることによって、偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に、さらに基板31から順次剥離し、巻き取る。   In this embodiment, using the peeling apparatus 1, the corner 35a of the polarizing plate 33 is peeled off from the laminate 30 together with the corner 39a of the surface protective film 37, the adhesive tape 51 and the adhesive sheet 53, and the peeled portion Is further wound around the peeling member 5 while being wound around the peeling member 7. In this state, by winding with the peeling member 51, the peeled polarizing plate 33 is guided to the peeling member 5 while being curved by the peeling member 7 together with the surface protection film 37, the adhesive tape 51 and the adhesive sheet 53. While being wound by the peeling member 5, the polarizing plate 33 is further peeled off sequentially from the substrate 31 together with the surface protection film 37, the pressure-sensitive adhesive tape 51 and the pressure-sensitive adhesive sheet 53, and is wound.

積層体30から偏光板33の角部35aを剥離することは、例えば以下のようにして行う。すなわち、先端に刃部を有する剥離用ナイフ(不図示)等を作業者の手指で掴み、積層体30の基板31と偏光板33の角部35aとの間に上記剥離用ナイフを挿入することによって偏光板33の角部35aを剥離する。より具体的には、偏光板33の基板31側の面33bに接着された上記第1の接着剤(不図示)と、基板31との間に上記剥離用ナイフを挿入し、上記第1の接着剤と共に偏光板33を剥離する。   The peeling of the corner 35 a of the polarizing plate 33 from the laminate 30 is performed, for example, as follows. That is, hold a peeling knife (not shown) or the like having a blade portion at the tip with an operator's finger, and insert the peeling knife between the substrate 31 of the laminate 30 and the corner 35a of the polarizing plate 33. As a result, the corner 35 a of the polarizing plate 33 is peeled off. More specifically, the peeling knife is inserted between the substrate 31 and the first adhesive (not shown) adhered to the surface 33b of the polarizing plate 33 on the substrate 31 side, and The polarizing plate 33 is peeled off together with the adhesive.

また、剥離された偏光板33の角部35aを、表面保護フィルム37の角部39a、粘着テープ51、粘着シート53と共に巻き取り部材5に巻き掛けることを、例えば以下のようにして行う。すなわち、剥離された偏光板33の角部35aを、巻き取り部材5の周面に巻き架けるようにして該周面に接着テープ(不図示)等で固定することによって行う。   The corner 35a of the peeled polarizing plate 33 is wound around the winding member 5 together with the corner 39a of the surface protective film 37, the adhesive tape 51, and the adhesive sheet 53 as follows, for example. That is, the corner 35 a of the peeled polarizing plate 33 is wound around the peripheral surface of the winding member 5 and fixed to the peripheral surface with an adhesive tape (not shown) or the like.

そして、図15に示す状態から、巻き取り部材5によって、偏光板33をさらに剥離しつつ順次巻き取ると、偏光板33の剥離が進むにつれて、図16、図17に示すように、積層体30が剥離方向Xとは反対の側(図16、図17の白抜き矢印参照)に順次移動する。すなわち、ステージ部材3に対して積層体30が相対的に移動する。より具体的には、積層体30がステージ部材3上を摺動する。図17に示すように、最終的に全ての偏光板33が剥離されて基板31が完全に露出すると、積層体30は移動を停止する。
このようにして、積層体30から偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に剥離する。
Then, from the state shown in FIG. 15, when the polarizing plate 33 is further taken up while being further peeled off by the winding member 5, as the peeling of the polarizing plate 33 proceeds, as shown in FIG. 16 and FIG. Move sequentially to the side opposite to the peeling direction X (see open arrows in FIG. 16 and FIG. 17). That is, the stacked body 30 moves relative to the stage member 3. More specifically, the stacked body 30 slides on the stage member 3. As shown in FIG. 17, when all the polarizing plates 33 are finally peeled off and the substrate 31 is completely exposed, the laminate 30 stops moving.
Thus, the polarizing plate 33 is peeled off from the laminate 30 together with the surface protection film 37, the adhesive tape 51 and the adhesive sheet 53.

上記の通り、本実施形態の剥離方法は、
基板31と、該基板31の一方の面31a上に接着された偏光板33とを備えた矩形状の積層体30から前記偏光板33を剥離する剥離方法であって、
前記積層体30は、前記偏光板33の上面33aに剥離可能に接着された表面保護フィルム37をさらに備えており、
前記偏光板33の上面33aに粘着テープ51を接着すべく前記表面保護フィルム37を剥離し、
前記偏光板33の4つの端縁34a、34b、34c、34dのうち、少なくとも一の角部35aを構成する2つの端縁34a、34bに粘着テープ51が沿うように、前記偏光板33の上面33aに前記粘着テープ51を接着し、
前記表面保護フィルム37を前記粘着テープ51に被せて接着し、
前記角部35を剥離起点Pとして前記表面保護フィルム37及び前記粘着テープ51と共に前記偏光板33を剥離する。
As described above, the peeling method of the present embodiment is
A peeling method for peeling the polarizing plate 33 from a rectangular laminated body 30 including a substrate 31 and a polarizing plate 33 adhered on one surface 31 a of the substrate 31,
The laminate 30 further includes a surface protection film 37 releasably adhered to the upper surface 33 a of the polarizing plate 33,
The surface protection film 37 is peeled off to adhere the adhesive tape 51 to the upper surface 33a of the polarizing plate 33,
The upper surface of the polarizing plate 33 such that the adhesive tape 51 is along the two edges 34a, 34b that constitute at least one corner 35a among the four edges 34a, 34b, 34c, 34d of the polarizing plate 33 The adhesive tape 51 is adhered to 33a,
Bonding the surface protection film 37 onto the adhesive tape 51;
The polarizing plate 33 is peeled off together with the surface protection film 37 and the adhesive tape 51 with the corner portion 35 as the peeling start point P.

かかる構成によれば、表面保護フィルム37を剥離して、偏光板33の4つの端縁34a〜34dのうち、少なくとも一の角部35aを構成する2つの端縁34a、34bに粘着テープ51が沿うように、偏光板33の上面33aに粘着テープ51を接着し、該角部35aを剥離起点Pとして表面保護フィルム37及び粘着テープ51と共に偏光板33を剥離することによって、偏光板33を剥離する際に、表面保護フィルム37が偏光板33から乖離することを抑制できる。これにより、図18に示すように、剥離の間、表面保護フィルム37と偏光板33とが接着された状態が維持されることになる。その結果、偏光板33が表面保護フィルム37で補強された状態が維持されつつ基板31から剥離されるため、偏光板33の裂けを抑制することが可能となる。
ここで、偏光板33の上面33aの全面に特許文献1に記載されたような粘着シートを接着しようとすれば、表面保護フィルム37を全て剥離して偏光板33を露出させた後、露出した偏光板33の上面33aの全面に粘着シートを接着させる必要がある。このため、偏光板33の上面の33aの全面に粘着シートを接着する分だけ手間がかかり、また、別途の粘着シートを用いて偏光板33を補強することになる分だけ、手間がかかる。
しかし、上記構成によれば、偏光板33の上面33aにおける端縁側の部分に粘着テープ51を接着するため、その分、手間が省ける。また、表面保護フィルム37で偏光板33を補強することができるため、表面保護フィルム37の有効利用を図ることができ、別途の部材で偏光板33を補強する手間も省ける。
このように、偏光板33が裂けることを抑制しつつ、該偏光板33を表面保護フィルム37と共に基板31から簡便に剥離することが可能となる。
According to this configuration, the surface protection film 37 is peeled off, and the adhesive tape 51 is attached to the two edges 34 a and 34 b constituting at least one corner 35 a of the four edges 34 a to 34 d of the polarizing plate 33. The adhesive tape 51 is adhered to the upper surface 33a of the polarizing plate 33 along the surface, and the polarizing plate 33 is peeled off by peeling the polarizing plate 33 together with the surface protection film 37 and the adhesive tape 51 with the corner 35a as the peeling starting point P. At the same time, separation of the surface protection film 37 from the polarizing plate 33 can be suppressed. Thereby, as shown in FIG. 18, the state in which the surface protection film 37 and the polarizing plate 33 are adhered is maintained during peeling. As a result, the polarizing plate 33 is peeled off from the substrate 31 while maintaining the state in which the polarizing plate 33 is reinforced by the surface protective film 37, so that it is possible to suppress the tearing of the polarizing plate 33.
Here, if an adhesive sheet as described in Patent Document 1 is adhered to the entire surface of the upper surface 33a of the polarizing plate 33, the entire surface protection film 37 is peeled off to expose the polarizing plate 33 and then exposed. The adhesive sheet needs to be adhered to the entire surface of the upper surface 33 a of the polarizing plate 33. Therefore, it takes time and effort to bond the pressure-sensitive adhesive sheet to the entire surface 33a of the upper surface of the polarizing plate 33, and also takes time and effort to reinforce the polarizing plate 33 using a separate pressure-sensitive adhesive sheet.
However, according to the above configuration, since the adhesive tape 51 is adhered to the end edge side portion of the upper surface 33a of the polarizing plate 33, labor can be saved accordingly. Further, since the polarizing plate 33 can be reinforced by the surface protective film 37, the surface protective film 37 can be effectively used, and the time and effort of reinforcing the polarizing plate 33 with a separate member can be saved.
Thus, it is possible to easily peel the polarizing plate 33 from the substrate 31 together with the surface protective film 37 while suppressing the tearing of the polarizing plate 33.

また、本実施形態の剥離方法においては、
前記偏光板33の前記粘着テープ51が沿うように接着される各端縁34〜34dと、該各端縁34a〜34dに対応する前記粘着テープ51の外側の端縁とが面一に位置するように、または、前記偏光板33前記粘着テープ51が沿うように接着される各端縁34a〜34dから、該各端縁34a〜34dに対応する前記粘着テープ51の外側の端縁が前記偏光板33の厚み未満の長さで突出するように、前記粘着テープ51を接着する。
Moreover, in the peeling method of this embodiment,
The edges 34 to 34 d of the polarizing plate 33 adhered along the adhesive tape 51 are flush with the outer edges of the adhesive tape 51 corresponding to the edges 34 a to 34 d. Or, from the edges 34a to 34d to which the polarizing plate 33 is adhered along the adhesive tape 51, the outer edges of the adhesive tape 51 corresponding to the respective edges 34a to 34d are the polarized light The adhesive tape 51 is adhered so as to protrude with a length less than the thickness of the plate 33.

ここで、通常、基板31は偏光板33よりも大きく形成されているため、粘着テープ51の外側の端縁が偏光板33の端縁34a〜34dよりも偏光板33の厚み以上の長さで外側にはみ出していると、該粘着テープ51が基板31と接着し、基板31からの偏光板33の剥離を妨げるという不具合が発生するおそれがある。また、通常、偏光板33は所定の形状となるように切断されて形成されており、微視的にはその端縁に一直線となっていない部分(例えばギザギザになっている部分)があるため、粘着テープ51の外側の端縁が偏光板33の端縁34a〜34dよりも内側に引っ込んでいると、この一直線となっていない部分を起点として裂けが生じるという不具合が発生するおそれがある。
しかし、かかる構成によれば、上記したような粘着テープ51のはみ出しによる不具合や、引っ込みによる不具合の発生を抑制し得るため、より確実に、偏光板33が裂けることを抑制しつつ、偏光板33を表面保護フィルム37と共に基板31から剥離することが可能となる。
Here, since the substrate 31 is usually formed to be larger than the polarizing plate 33, the outer edge of the adhesive tape 51 has a length greater than the thickness of the polarizing plate 33 than the edges 34 a to 34 d of the polarizing plate 33. When the adhesive tape 51 protrudes outside, the adhesive tape 51 adheres to the substrate 31 and there is a possibility that a problem may occur that the peeling of the polarizing plate 33 from the substrate 31 is hindered. Also, normally, the polarizing plate 33 is cut and formed to have a predetermined shape, and microscopically, there is a portion (for example, a jagged portion) that is not a straight line at the end edge When the outer edge of the adhesive tape 51 is recessed inward from the edges 34a to 34d of the polarizing plate 33, there is a possibility that a failure may occur starting from a portion which is not in a straight line.
However, according to such a configuration, it is possible to suppress the occurrence of the failure due to the sticking out of the adhesive tape 51 as described above and the failure due to the retraction, and thus the polarization plate 33 is more reliably suppressed while the tearing of the polarization plate 33 is suppressed. And the surface protection film 37 can be peeled off from the substrate 31.

また、本実施形態の剥離方法においては、
前記偏光板33の4つの端縁34a〜34dに沿うように、前記偏光板33の上面33aに前記粘着テープ51を接着する。
Moreover, in the peeling method of this embodiment,
The adhesive tape 51 is adhered to the upper surface 33 a of the polarizing plate 33 along the four edges 34 a to 34 d of the polarizing plate 33.

かかる構成によれば、偏光板33を剥離する際、偏光板33から表面保護フィルム37が乖離することをより確実に抑制し得るため、より確実に、偏光板33が裂けることを抑制しつつ、偏光板33を表面保護フィルム37と共に基板31から剥離することが可能となる。   According to this configuration, when the polarizing plate 33 is peeled off, the separation of the surface protection film 37 from the polarizing plate 33 can be more reliably suppressed, so the tearing of the polarizing plate 33 is suppressed more reliably while: It becomes possible to peel off the polarizing plate 33 from the substrate 31 together with the surface protection film 37.

また、本実施形態の剥離方法においては、
前記表面保護フィルム37を介して前記粘着テープ51と重なるように、前記表面保護フィルム37の上面37aに粘着シート53を接着し、
前記表面保護フィルム37、前記粘着テープ51及び前記粘着シート53と共に前記偏光板33を剥離する。
Moreover, in the peeling method of this embodiment,
An adhesive sheet 53 is adhered to the upper surface 37 a of the surface protective film 37 so as to overlap with the adhesive tape 51 via the surface protective film 37,
The polarizing plate 33 is peeled off together with the surface protection film 37, the pressure-sensitive adhesive tape 51 and the pressure-sensitive adhesive sheet 53.

かかる構成によれば、表面保護フィルム37の上面37aに、さらに粘着シート53を接着することによって、偏光板33を剥離する際、該偏光板33を一層補強し得るため、より確実に、偏光板33が裂けることを抑制しつつ、偏光板33を表面保護フィルム37と共に基板31から剥離することが可能となる。   According to this configuration, when the polarizing plate 33 is peeled off by further adhering the pressure-sensitive adhesive sheet 53 to the upper surface 37a of the surface protection film 37, the polarizing plate 33 can be further reinforced. It becomes possible to peel off the polarizing plate 33 from the substrate 31 together with the surface protective film 37 while suppressing the tearing of the plate 33.

以上の通り、本実施形態によれば、偏光板33が裂けることを抑制しつつ、該偏光板33を表面保護フィルム37と共に基板31から簡便に剥離することが可能となる。   As described above, according to the present embodiment, it is possible to easily peel the polarizing plate 33 from the substrate 31 together with the surface protective film 37 while suppressing the tearing of the polarizing plate 33.

本実施形態の剥離方法は上記の通りであるが、本発明の剥離方法は、上記実施形態に限定されるものではない。   The peeling method of the present embodiment is as described above, but the peeling method of the present invention is not limited to the above embodiment.

例えば、上記実施形態では、偏光板33上に粘着テープ51、表面保護フィルム37上に粘着シート53を接着する態様を示したが、その他、粘着シート53を接着することなく、偏光板33を表面保護フィルム37及び粘着テープ51と共に剥離する態様を採用し得る。   For example, in the embodiment described above, the adhesive tape 51 is adhered to the polarizing plate 33 and the adhesive sheet 53 is adhered to the surface protection film 37. In addition, the polarizing plate 33 is surfaced without adhering the adhesive sheet 53. A mode of peeling together with the protective film 37 and the adhesive tape 51 can be adopted.

また、上記実施形態では、偏光板33の4つ端縁34a〜34dに沿うように粘着テープ51を接着したが、少なくとも角部35aを構成する2つの端縁34a、34bに沿うように粘着テープ51を接着すればよく、偏光板33上において該粘着テープ51を接着する領域の数量は、特に限定されない。   In the above embodiment, the adhesive tape 51 is adhered along the four edges 34a to 34d of the polarizing plate 33. However, the adhesive tape 51 is disposed along at least the two edges 34a and 34b constituting the corner 35a. 51 may be adhered, and the number of areas for adhering the adhesive tape 51 on the polarizing plate 33 is not particularly limited.

また、上記実施形態では、表面保護フィルム37を介して4つの粘着テープ51と重なるように4つの粘着シート53を接着したが、粘着シート51と重なるように粘着シート53を接着するのであれば、粘着シート53の形状、大きさ、数量は特に限定されるものではなく、粘着シート51の数量に応じて、適宜設定すればよい。
例えば、粘着シート53として、表面保護フィルム37と同じ大きさに形成されたものを用い、この粘着シートを、表面保護フィルム37の上面37aの全面に接着する態様を採用し得る。
Moreover, in the said embodiment, although the four adhesive sheets 53 were adhere | attached so that it might overlap with the four adhesive tapes 51 via the surface protection film 37, if it adhere | attaches the adhesive sheet 53 so that it may overlap with the adhesive sheet 51, The shape, size, and number of the adhesive sheet 53 are not particularly limited, and may be appropriately set according to the number of the adhesive sheet 51.
For example, as the adhesive sheet 53, one formed in the same size as the surface protective film 37 may be employed, and the adhesive sheet may be adhered to the entire surface of the upper surface 37a of the surface protective film 37.

また、上記実施形態では、基板31の方が偏光板33及び表面保護フィルム37よりも大きく形成され、偏光板33と表面保護フィルム37とが同じ大きさに形成されている態様を採用したが、本発明では、これらの大きさは、必ずしも上記実施形態に限定されるものではない。   In the above embodiment, the substrate 31 is larger than the polarizing plate 33 and the surface protective film 37, and the polarizing plate 33 and the surface protective film 37 are formed to have the same size. In the present invention, these sizes are not necessarily limited to the above embodiment.

また、粘着テープ51同士の接着順序、及び、粘着シート53同士の接着順序も、特に限定されるものではない。   Moreover, the adhesion | attachment order of adhesive tape 51 comrades and the adhesion | attachment order of adhesive sheet 53 comrades are not specifically limited, either.

また、上記実施形態では、偏光板33の端縁34a〜34dについて、1つずつ表面保護フィルム37の部分的な剥離、粘着フィルム51の接着、この粘着フィルム51への表面保護フィルム37の被せ及び接着を行い、これを繰り返したが、その他、偏光板33の端縁34a〜34dに対応する表面保護フィルム37の端縁38a〜38d側を同時に部分的に剥離し、これによって偏光板33の全ての端縁34a〜34d側を露出させ、この状態で剥離した端縁38a〜38d側を仮固定し、偏光板33の端縁34a〜34dに沿うように粘着テープ51を接着した後、仮固定を解除して、表面保護フィルム37の端縁38a〜38d側を粘着テープ51に被せて接着してもよい。   Further, in the above embodiment, partial peeling of the surface protective film 37, adhesion of the adhesive film 51, covering of the surface protective film 37 on the adhesive film 51, and one for each of the edges 34a to 34d of the polarizing plate 33 Bonding is performed, and this is repeated, but in addition, the edges 38a to 38d of the surface protection film 37 corresponding to the edges 34a to 34d of the polarizing plate 33 are partially peeled simultaneously at the same time. The end edges 34a to 34d side of the sheet are exposed, and the peeled off end edges 38a to 38d side are temporarily fixed in this state, and the adhesive tape 51 is adhered along the end edges 34a to 34d of the polarizing plate 33, and then temporarily fixed. , And the edges 38a to 38d of the surface protection film 37 may be adhered to the adhesive tape 51 by covering them.

また、上記実施形態では、複数の粘着テープ51を用い、偏光板33の端縁ごとに各粘着テープ51を接着したが、その他、予め、複数の端縁に沿うように形成された1つの粘着テープを用い、これを偏光板33の各端縁に沿うように接着してもよい。また、粘着シート53についても、同様に、予め、複数の端縁に沿うように形成された1つの粘着シートを用いてもよい。   In the above embodiment, the plurality of adhesive tapes 51 are used to bond each adhesive tape 51 to each edge of the polarizing plate 33. In addition, one adhesive previously formed along the plurality of edges A tape may be used and adhered along each edge of the polarizing plate 33. Also, as for the pressure-sensitive adhesive sheet 53, similarly, one pressure-sensitive adhesive sheet formed in advance along a plurality of edges may be used.

次に、実施例を示しつつ、本発明をさらに詳細に説明する。   The present invention will now be described in more detail by way of examples.

図1〜3に示すような積層板30を用いた。
具体的には、偏光板33として、偏光子41の両面に、第2の接着剤を有する接着剤層43を介して保護フィルム45が積層されて形成された偏光板33(厚み:約100μm)を用いた。積層体30として、かかる偏光板33の一方の保護フィルム45に第1の接着剤を介して基板31が積層され、他方の保護フィルム45に第3の接着剤を介して表面保護フィルム37が積層されて形成された積層体30を用いた。
より具体的には、偏光子41の両面に第2の接着剤を有する接着剤層43を介して保護フィルム45が積層され、該保護フィルム45のうち一方の保護フィルム45に第1の接着剤を介してセパレータ(不図示)が積層され、他方の保護フィルム45に第3の接着剤を介して表面保護フィルム37が積層されて形成された市販品(TEG1465DU、日東電工社製)から、セパレータを剥離して基材31に積層することによって、積層体30を形成した。
The laminated board 30 as shown to FIGS. 1-3 was used.
Specifically, as the polarizing plate 33, the polarizing plate 33 (thickness: about 100 μm) is formed by laminating the protective film 45 on both sides of the polarizer 41 via the adhesive layer 43 having the second adhesive. Was used. As the laminate 30, the substrate 31 is laminated on one protective film 45 of the polarizing plate 33 via the first adhesive, and the surface protective film 37 is laminated on the other protective film 45 via the third adhesive. The laminated body 30 thus formed was used.
More specifically, the protective film 45 is laminated on both sides of the polarizer 41 via the adhesive layer 43 having the second adhesive, and a first adhesive is applied to one of the protective films 45 of the protective films 45. From a commercial product (TEG 1465DU, manufactured by Nitto Denko Corp.), in which a separator (not shown) is laminated via the adhesive layer and the surface protective film 37 is laminated on the other protective film 45 via the third adhesive. Was peeled off and laminated on the substrate 31 to form a laminate 30.

粘着テープ51として、一面側に剥離ライナーが貼着されている両面テープ(No.500、日東電工社製)を用いた。   As the adhesive tape 51, a double-sided tape (No. 500, manufactured by Nitto Denko Corporation) having a release liner attached to one side was used.

粘着シート53として、粘着テープ51と同様の剥離ライナーが貼着されている両面テープ、及び、表面保護フィルム37(すなわち偏光板33)と同じ大きさに形成された粘着シート53を用いた。具体的には、粘着シート53として、上記市販品(TEG1465DU、日東電工社製)の品質検査(接着力を除く)で除かれた規格外品を用いた。
粘着シート53としての上記両面テープの上面(剥離ライナーの上面)の摩擦係数は、表面保護フィルム37の上面37aの摩擦係数よりも小さかった。
As the adhesive sheet 53, a double-sided tape to which a release liner similar to the adhesive tape 51 is attached, and an adhesive sheet 53 formed in the same size as the surface protective film 37 (that is, the polarizing plate 33) were used. Specifically, as the adhesive sheet 53, a nonstandard product removed in the quality inspection (except for the adhesive strength) of the above-mentioned commercial product (TEG1465DU, manufactured by Nitto Denko Corporation) was used.
The friction coefficient of the upper surface (the upper surface of the release liner) of the double-sided tape as the adhesive sheet 53 was smaller than the friction coefficient of the upper surface 37 a of the surface protective film 37.

(実施例1)
偏光板33の4つの端縁34a〜34dに沿うように粘着テープ51を接着すべく、表面保護フィルム37を部分的に剥離し、該端縁34a〜34dに沿うように、且つ、各端縁34a〜34dと粘着テープ51の外側の端縁とが面一に位置するように、偏光板33の上面33aに、剥離ライナーが貼着されている粘着テープ51としての両面テープを接着した後、該剥離ライナーを剥離して、粘着テープ51の粘着剤(不図示)に表面保護フィルム37を被せて接着した。
さらに、表面保護フィルム37を介して粘着テープ51と重なるように、且つ、表面保護フィルム37の4つの端縁38a〜38dに粘着シート53が沿うように、しかも、各端縁38a〜38dと粘着シート53の外側の端縁とが面一に位置するように、表面保護フィルム37の上面37aに、粘着シート53としての、剥離ライナーが貼着されている両面テープを接着した。なお、この剥離ライナーは剥離しなかった。
そして、図14、15に示す剥離装置1を用いて、偏光板33の角部35aを剥離起点Pとして、偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に剥離した。このときの、偏光板33からの表面保護フィルム37の乖離状況と、偏光板33の裂けの状況とを、目視によって観察した。
これを50回繰り返し、成功率が90%以上の場合を良好と判断して、「〇」と表し、成功率が50%以上90%未満の場合をやや良好であると判断して、「△」と表し、50%未満の場合を不良であるとして、「×」と評価した。結果を表1に示す。
Example 1
In order to adhere the adhesive tape 51 along the four edges 34a to 34d of the polarizing plate 33, the surface protection film 37 is partially peeled off, and along the edges 34a to 34d, and each edge After adhering a double-sided tape as the adhesive tape 51 to which the release liner is attached to the upper surface 33a of the polarizing plate 33 so that the edge 34a to 34d and the outer edge of the adhesive tape 51 are flush with each other The release liner was peeled off, and the adhesive (not shown) of the adhesive tape 51 was covered with the surface protective film 37 and adhered.
Furthermore, the adhesive sheet 53 is adhered to the four edges 38 a to 38 d of the surface protection film 37 so as to overlap with the adhesive tape 51 via the surface protection film 37, and to adhere to the respective edges 38 a to 38 d A double-sided tape to which a release liner as a pressure-sensitive adhesive sheet 53 is attached is adhered to the upper surface 37a of the surface protective film 37 so that the outer edge of the sheet 53 is flush with the outer edge. The release liner did not peel off.
Then, using the peeling device 1 shown in FIGS. 14 and 15, the polarizing plate 33 was peeled together with the surface protection film 37, the pressure-sensitive adhesive tape 51, and the pressure-sensitive adhesive sheet 53, with the corner 35a of the polarizing plate 33 as the peeling starting point P. At this time, the separation state of the surface protection film 37 from the polarizing plate 33 and the tearing state of the polarizing plate 33 were visually observed.
This is repeated 50 times, and the case where the success rate is 90% or more is judged as good, represented as “o”, and the case where the success rate is 50% or more and less than 90% is judged as somewhat good, “Δ It was evaluated as "x" on the assumption that the case of less than 50% was inferior. The results are shown in Table 1.

(実施例2)
表面保護フィルム37に粘着シート53を接着しなかったこと以外は実施例1と同様にして、剥離装置1を用いて、偏光板33を、表面保護フィルム37及び粘着テープ51と共に剥離し、実施例1と同様に評価した。結果を表1に示す。
(Example 2)
In the same manner as in Example 1 except that the adhesive sheet 53 was not adhered to the surface protective film 37, the polarizing plate 33 was peeled together with the surface protective film 37 and the adhesive tape 51 using the peeling apparatus 1, It evaluated similarly to 1. The results are shown in Table 1.

(実施例3)
偏光板33の2つの端縁34a、34bに沿うように、且つ、各端縁34a、34bと粘着テープ51の外側の端縁とが面一に位置するように、偏光板33の上面33aに粘着テープ51を接着し、表面保護フィルム37を介して粘着テープ51と重なるように、且つ、表面保護フィルム37の端縁38a、38bに粘着シート53が沿うように、しかも、粘着シート53の外側の端縁が各端縁38a、38bと面一に位置するように、粘着シート53としての、剥離ライナーが貼着されている両面テープを接着したこと以外は実施例1と同様にして、剥離装置1を用いて、偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に剥離し、実施例1と同様に評価した。結果を表1に示す。
(Example 3)
On the upper surface 33a of the polarizing plate 33 along the two edges 34a and 34b of the polarizing plate 33 and so that each edge 34a and 34b is flush with the outer edge of the adhesive tape 51. The adhesive tape 51 is adhered, and the adhesive sheet 53 is placed along the edges 38 a and 38 b of the surface protective film 37 so as to overlap with the adhesive tape 51 via the surface protective film 37. Peeling in the same manner as in Example 1 except that a double-sided adhesive tape as a pressure-sensitive adhesive sheet 53 is adhered such that the edges of the adhesive are positioned flush with the respective edges 38a, 38b. Using the apparatus 1, the polarizing plate 33 was peeled together with the surface protective film 37, the pressure-sensitive adhesive tape 51 and the pressure-sensitive adhesive sheet 53, and evaluated in the same manner as in Example 1. The results are shown in Table 1.

(実施例4)
表面保護フィルム37の上面37aの全面にわたって、表面保護フィルム37(すなわち偏光板33)と同じ大きさに形成された粘着シート53を接着したこと以外は実施例1と同様にして、剥離装置1を用いて、偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に剥離し、実施例1と同様に評価した。結果を表1に示す。
(Example 4)
In the same manner as in Example 1 except that an adhesive sheet 53 formed in the same size as the surface protective film 37 (that is, the polarizing plate 33) is adhered over the entire upper surface 37a of the surface protective film 37. The polarizing plate 33 was peeled off together with the surface protective film 37, the pressure-sensitive adhesive tape 51 and the pressure-sensitive adhesive sheet 53, and evaluated in the same manner as in Example 1. The results are shown in Table 1.

(実施例5)
偏光板33の上面33aの4つの端縁34a〜34dに沿うように、且つ、該各粘着テープ51の外側の端縁が、各端縁34a〜34dから2mm内側に位置するように粘着テープ51を接着したこと以外は実施例1と同様に、剥離装置1を用いて、偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に剥離し、実施例1と同様に評価した。結果を表1に示す。
(Example 5)
Adhesive tape 51 along the four edges 34a to 34d of the upper surface 33a of the polarizing plate 33 and so that the outer edges of the adhesive tape 51 are positioned 2 mm from the respective edges 34a to 34d. The polarizing plate 33 was peeled together with the surface protective film 37, the pressure-sensitive adhesive tape 51 and the pressure-sensitive adhesive sheet 53 using the peeling apparatus 1 in the same manner as in Example 1 except that the adhesive was adhered. The results are shown in Table 1.

(実施例6)
偏光板33の上面33aの4つの端縁34a〜34dに沿うように、且つ、該各粘着テープ51の外側の端縁が、各端縁34a〜34dから外側に50μm突出するように粘着テープ51を接着したこと以外は実施例1と同様に、剥離装置1を用いて、偏光板33を、表面保護フィルム37、粘着テープ51及び粘着シート53と共に剥離し、実施例1と同様に評価した。結果を表1に示す。
(Example 6)
Adhesive tape 51 along the four edges 34a to 34d of the upper surface 33a of the polarizing plate 33 and so that the outer edges of the respective adhesive tapes 51 protrude 50 μm outward from the respective edges 34a to 34d. The polarizing plate 33 was peeled together with the surface protective film 37, the pressure-sensitive adhesive tape 51 and the pressure-sensitive adhesive sheet 53 using the peeling apparatus 1 in the same manner as in Example 1 except that the adhesive was adhered. The results are shown in Table 1.

(比較例1)
偏光板33の上面33aに粘着テープ51を接着しなかったこと以外は実施例1と同様に、剥離装置1を用いて、偏光板33を、表面保護フィルム37及び粘着シート53と共に剥離し、実施例1と同様に評価した。結果を表1に示す。
(Comparative example 1)
As in Example 1, except that the adhesive tape 51 was not adhered to the upper surface 33a of the polarizing plate 33, the polarizing plate 33 was peeled together with the surface protective film 37 and the adhesive sheet 53 using the peeling device 1 It evaluated similarly to Example 1. The results are shown in Table 1.

(比較例2)
偏光板33の上面33aに粘着テープ51を接着しなかったこと以外は実施例4と同様にして、剥離装置1を用いて、偏光板33を、表面保護フィルム37及び粘着シート53と共に剥離し、実施例1と同様に評価した。結果を表1に示す。
(Comparative example 2)
Using the peeling apparatus 1, the polarizing plate 33 is peeled together with the surface protective film 37 and the adhesive sheet 53 in the same manner as in Example 4 except that the adhesive tape 51 is not adhered to the upper surface 33a of the polarizing plate 33. It evaluated similarly to Example 1. The results are shown in Table 1.

(比較例3)
偏光板33の上面33aに粘着テープ51を接着しなかったこと以外は実施例2と同様にして、剥離装置1を用いて、偏光板33を、表面保護フィルム37と共に剥離し、実施例1と同様に評価した。結果を表1に示す。

Figure 0006550311
(Comparative example 3)
The polarizing plate 33 is peeled together with the surface protection film 37 using the peeling apparatus 1 in the same manner as in Example 2 except that the adhesive tape 51 is not adhered to the upper surface 33 a of the polarizing plate 33. It evaluated similarly. The results are shown in Table 1.
Figure 0006550311

表1に示すように、偏光板33の少なくとも2つの端縁34a、34bに沿うように、偏光板33の上面33aに粘着テープ51を接着することによって、偏光板33の裂けを抑制しつつ、基板31から偏光板33を良好に剥離し得ることがわかった。
偏光板33の4つの端縁34a〜34dに沿うように、偏光板33の上面33aに粘着テープ51を接着することによって、基板31から偏光板33をより良好に剥離し得ることがわかった。
偏光板33の粘着テープ51が沿うように接着される各端縁と、各端縁に対応する粘着テープ51の外側の端縁とが面一に位置していることによって、基板31から偏光板33をより良好に剥離し得ることがわかった。
また、偏光板33の粘着テープ51が沿うように接着される各端縁34a〜34dから、該各端縁34a〜34dに対応する粘着テープ51の外側の端縁が偏光板33の厚み未満の長さで突出していることによっても、基板31から偏光板33をより良好に剥離し得ることがわかった。
表面保護フィルム37の上面37aの全面に粘着シート53を接着することによって、基板31から偏光板33をより良好に剥離し得ることがわかった。
As shown in Table 1, the adhesive tape 51 is adhered to the upper surface 33a of the polarizing plate 33 along the at least two edges 34a and 34b of the polarizing plate 33, thereby suppressing the tearing of the polarizing plate 33, It has been found that the polarizing plate 33 can be peeled well from the substrate 31.
It has been found that by adhering the adhesive tape 51 to the upper surface 33 a of the polarizing plate 33 along the four edges 34 a to 34 d of the polarizing plate 33, the polarizing plate 33 can be peeled better from the substrate 31.
Since each edge to which adhesive tape 51 of polarizing plate 33 is adhered along and the outer edge of adhesive tape 51 corresponding to each edge are flush with each other, the substrate 31 is separated from the polarizing plate It turned out that 33 can be exfoliated better.
Further, from each of the edges 34a to 34d to which the adhesive tape 51 of the polarizing plate 33 is adhered, the outer edge of the adhesive tape 51 corresponding to each of the edges 34a to 34d is less than the thickness of the polarizing plate 33 It was also found that the polarizing plate 33 can be peeled off from the substrate 31 more satisfactorily by protruding in the length.
It was found that by adhering the adhesive sheet 53 to the entire surface of the upper surface 37a of the surface protective film 37, the polarizing plate 33 can be more favorably peeled from the substrate 31.

実施例2のように表面保護フィルム37の上面37aに粘着シート53が接着されていない場合よりも、2つの端縁38a、38bに沿うように表面保護フィルム37の上面37aに粘着シート53が接着されている場合の方が、剥離用部材7に対する滑り性が良好であった。また、2つの端縁38a、38bに沿うように表面保護フィルム37の上面37aに粘着シート53が接着されている場合よりも、4つの端縁38a〜38dに沿うように表面保護フィルム37の上面37aに粘着シート53が接着されている場合、及び、表面保護フィルム37の上面37aの全面に粘着シート53が接着されている場合の方が、剥離用部材7に対する滑り性が良好であった。   The adhesive sheet 53 adheres to the upper surface 37 a of the surface protective film 37 along the two edges 38 a and 38 b than when the adhesive sheet 53 is not adhered to the upper surface 37 a of the surface protective film 37 as in Example 2. The slidability with respect to the peeling member 7 was better in the case where it was carried out. In addition, the upper surface of the surface protection film 37 follows the four edges 38a to 38d than when the adhesive sheet 53 is adhered to the upper surface 37a of the surface protection film 37 along the two edges 38a and 38b. The slidability with respect to the peeling member 7 was better in the case where the adhesive sheet 53 was adhered to 37a and in the case where the adhesive sheet 53 was adhered to the entire surface of the upper surface 37a of the surface protective film 37.

実施例4のように表面保護フィルム37の上面37aの全面に粘着シート53を接着する場合よりも、表面保護フィルム37の端縁に沿うように表面保護フィルム37の上面37aに粘着シート53を接着する方が、設備面、作業面で簡便であった。   The adhesive sheet 53 is adhered to the upper surface 37a of the surface protective film 37 along the edge of the surface protective film 37 than when the adhesive sheet 53 is adhered to the entire upper surface 37a of the surface protective film 37 as in Example 4. It was easier in terms of equipment and work if it was done.

用いた偏光板33の端縁が粗い状態(微視的にギザギザになっている状態)であったため、実施例5のように偏光板33の端縁よりも内側に粘着テープ51を接着した場合よりも、実施例1〜4、6のように、偏光板33の粘着テープ51が沿うように接着される各端縁と、各端縁に対応する粘着テープ51の外側の端縁とが面一に位置するように粘着テープ51を接着した場合の方が、この粗い部分を粘着テープ51で補強できるため、裂けがより抑制された。
また、実施例6のように、偏光板33の粘着テープ51が沿うように接着される各端縁34a〜34dから、該各端縁34a〜34dに対応する粘着テープ51の外側の端縁が偏光板33の厚み未満の長さで突出している場合であっても、実施例1〜4と同様、偏光板33の端縁が粗い部分を粘着テープ51で補強できる。よって、実施例5よりも実施例6の方が、裂けがより抑制された。
Since the edge of the polarizing plate 33 used was in a rough state (microscopically jagged), the case where the adhesive tape 51 was adhered inside the edge of the polarizing plate 33 as in Example 5 Further, as in the first to fourth and sixth embodiments, each edge to which the adhesive tape 51 of the polarizing plate 33 is adhered along the surface and the outer edge of the adhesive tape 51 corresponding to each edge are surfaces In the case where the adhesive tape 51 is bonded so as to be located at one position, this rough portion can be reinforced by the adhesive tape 51, so that the tearing is further suppressed.
Further, as in the sixth embodiment, the outer edges of the adhesive tape 51 corresponding to the respective edges 34a to 34d are obtained from the respective edges 34a to 34d to which the adhesive tape 51 of the polarizing plate 33 is adhered along. Even when protruding with a length less than the thickness of the polarizing plate 33, the adhesive tape 51 can reinforce a portion where the edge of the polarizing plate 33 is rough as in the first to fourth embodiments. Therefore, tearing was more suppressed in Example 6 than in Example 5.

1:剥離装置、3:ステージ部材、5:剥離部材、7:剥離用部材、30:積層体、31:基板、31a:一方の面、33:偏光板、33a:上面、34a〜34d:端縁、35a〜35d:角部、37:表面保護フィルム、37a:上面、38a〜38d:端縁、39a〜39d:角部、51:粘着テープ、53:粘着シート   1: Peeling device, 3: Stage member, 5: Peeling member, 7: Peeling member, 30: laminate, 31: substrate, 31a: one surface, 33: polarizing plate, 33a: upper surface, 34a to 34d: end Edge, 35a to 35d: corner, 37: surface protective film, 37a: upper surface, 38a to 38d: edge, 39a to 39d: corner, 51: adhesive tape, 53: adhesive sheet

Claims (4)

基板と、該基板の一方の面上に接着された偏光板とを備えた矩形状の積層体から前記偏光板を剥離する剥離方法であって、
前記積層体は、前記偏光板の上面に剥離可能に接着された表面保護フィルムをさらに備えており、
前記偏光板の上面に粘着テープを接着すべく前記表面保護フィルムを剥離し、
前記偏光板の4つの端縁のうち、少なくとも一の角部を構成する2つの端縁に粘着テープが沿うように、前記偏光板の上面に前記粘着テープを接着し、
前記表面保護フィルムを前記粘着テープに被せて接着し、
前記角部を剥離起点として前記表面保護フィルム及び前記粘着テープと共に前記偏光板を剥離する、剥離方法。
A peeling method for peeling the polarizing plate from a rectangular laminate including a substrate and a polarizing plate adhered on one surface of the substrate,
The laminate further includes a surface protection film releasably adhered to the upper surface of the polarizing plate,
Peeling off the surface protective film to adhere an adhesive tape to the upper surface of the polarizing plate;
The adhesive tape is adhered to the upper surface of the polarizing plate such that the adhesive tape is along two edges constituting at least one corner of the four edges of the polarizing plate,
Bonding the surface protective film to the adhesive tape and bonding;
The peeling method which peels the said polarizing plate with the said surface protection film and the said adhesive tape by making the said corner | angular part into a peeling origin.
前記偏光板の前記粘着テープが沿うように接着される各端縁と、該各端縁に対応する前記粘着テープの外側の端縁とが面一に位置するように、または、前記偏光板の前記粘着テープが沿うように接着される各端縁から、該各端縁に対応する前記粘着テープの外側の端縁が前記偏光板の厚み未満の長さで突出するように、前記偏光板の上面に前記粘着テープを接着する、請求項1に記載の剥離方法。   Each edge of the polarizing plate to be adhered along the adhesive tape and the outer edge of the adhesive tape corresponding to each edge are flush with each other, or The outer edge of the pressure-sensitive adhesive tape corresponding to each edge protrudes from each edge to be adhered along the pressure-sensitive adhesive tape with a length less than the thickness of the polarizing plate, The peeling method of Claim 1 which adhere | attaches the said adhesive tape on an upper surface. 前記偏光板の4つの端縁に沿うように、前記偏光板の上面に前記粘着テープを接着する、請求項1または2に記載の剥離方法。   The peeling method of Claim 1 or 2 which adheres the said adhesive tape on the upper surface of the said polarizing plate so that four edges of the said polarizing plate may be followed. 前記表面保護フィルムを介して前記粘着テープと重なるように、前記表面保護フィルムの上面に粘着シートを接着し、
前記表面保護フィルム、前記粘着テープ及び前記粘着シートと共に前記偏光板を剥離する、請求項1〜3のいずれかに記載の剥離方法。
An adhesive sheet is adhered to the upper surface of the surface protective film so as to overlap with the adhesive tape via the surface protective film,
The peeling method in any one of Claims 1-3 which peels the said polarizing plate with the said surface protection film, the said adhesive tape, and the said adhesive sheet.
JP2015189429A 2015-09-28 2015-09-28 Peeling method Active JP6550311B2 (en)