JP6371506B2 - Washi-style shrink label for decoration of cylindrical containers and its continuum - Google Patents

Washi-style shrink label for decoration of cylindrical containers and its continuum Download PDF

Info

Publication number
JP6371506B2
JP6371506B2 JP2013189718A JP2013189718A JP6371506B2 JP 6371506 B2 JP6371506 B2 JP 6371506B2 JP 2013189718 A JP2013189718 A JP 2013189718A JP 2013189718 A JP2013189718 A JP 2013189718A JP 6371506 B2 JP6371506 B2 JP 6371506B2
Authority
JP
Japan
Prior art keywords
japanese paper
shrink label
paper
decorative layer
joining
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2013189718A
Other languages
Japanese (ja)
Other versions
JP2015055791A (en
Inventor
吉田 忠雄
忠雄 吉田
岡田 豊
豊 岡田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Osaka Sealing Printing Co Ltd
Original Assignee
Osaka Sealing Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Osaka Sealing Printing Co Ltd filed Critical Osaka Sealing Printing Co Ltd
Priority to JP2013189718A priority Critical patent/JP6371506B2/en
Publication of JP2015055791A publication Critical patent/JP2015055791A/en
Application granted granted Critical
Publication of JP6371506B2 publication Critical patent/JP6371506B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、酒類などの液体を収容するのに適した筒状容器を装飾するシュリンクラベルに関し、詳しくは、和風の高級感を観者に与える、和紙調シュリンクラベルに関する。   The present invention relates to a shrink label for decorating a cylindrical container suitable for containing a liquid such as liquor, and more particularly to a Japanese paper-like shrink label that gives a viewer a sense of Japanese-style luxury.

近年の社会的な環境意識の高まりに伴い、焼却処理や再利用を容易かつ安価に行える紙パックを液体用容器として用いることが多くなってきている。そこで、酒類用容器としても、紙パックを用いることが検討されている。しかし、紙パックの装飾は、紙パックの外面にオフセット印刷法やグラビア印刷法などで文字や絵柄を施したものであり、和紙調の視覚感や触感が得られず、容器の外観が高級感に欠けるものとなる。そこで、熱収縮性フィルムと和紙調レーヨン紙との積層シートで、紙パックの底部から側部を覆い、加熱により熱収縮性フィルムを収縮させて、容器に密着させることが提案されている(特許文献1参照)。   With the recent increase in social awareness of the environment, paper packs that can be incinerated and reused easily and inexpensively are increasingly used as liquid containers. Therefore, it has been studied to use a paper pack as a container for alcoholic beverages. However, the decoration of the paper pack is made by applying letters and patterns to the outer surface of the paper pack by the offset printing method or gravure printing method. It will be lacking. Therefore, it has been proposed to cover the side from the bottom of the paper pack with a laminated sheet of heat-shrinkable film and Japanese paper-like rayon paper, and shrink the heat-shrinkable film by heating to make it adhere to the container (patent) Reference 1).

一方、ガラス瓶を化粧装飾する方法としても、熱収縮性フィルムと和紙調レーヨン紙からなる一枚の積層シートを、ガラス瓶の側面に押し付けながら捲きつけ、その後、加熱により熱収縮性フィルムを収縮させて、ガラス瓶に密着させることが提案されている(特許文献2参照)。   On the other hand, as a method of decoratively decorating a glass bottle, a laminated sheet made of a heat-shrinkable film and Japanese paper rayon paper is squeezed against the side of the glass bottle, and then the heat-shrinkable film is shrunk by heating. It has been proposed to make it adhere to a glass bottle (see Patent Document 2).

特開平6−345132号公報JP-A-6-345132 特開平3−14432号公報Japanese Patent Laid-Open No. 3-14432

しかし、特許文献1、2のように、熱収縮性フィルムと和紙調レーヨン紙との積層シートを用いて容器を包装する場合、熱収縮性フィルムを収縮させて容器に密着させる前の、積層シートの容器への装着状態が重要である。装着状態が適切でない場合には、積層シートに歪みが生じたり、和紙調レーヨン紙に印刷された模様が正規位置から外れたりして、装飾の効果が低減することになる。そして、特許文献1、2の場合、積層シートの容器への適切な装着状態を得るためには、積層シートを容器の特定の位置に位置合わせして捲き付けるとともに、積層シートの両端部を固定する作業が必要である。   However, as in Patent Documents 1 and 2, when packaging a container using a laminated sheet of heat-shrinkable film and Japanese paper-like rayon paper, the laminated sheet before the heat-shrinkable film is shrunk and adhered to the container The state of mounting on the container is important. When the mounting state is not appropriate, the laminated sheet is distorted or the pattern printed on the Japanese paper rayon paper is out of the normal position, thereby reducing the decoration effect. In the case of Patent Documents 1 and 2, in order to obtain an appropriate mounting state of the laminated sheet to the container, the laminated sheet is aligned and positioned at a specific position of the container, and both ends of the laminated sheet are fixed. Work is necessary.

また、特許文献1、2は、紙パックやガラス瓶のような容器の全体を被覆するための包装材料を提案するものである。包装材料で被覆された商品の購入者は、通常、購入した商品を使用もしくは消費する際には、包装材料を剥ぎ取ってしまい、包装材料で覆われていた容器を取り出してしまうことが多い。その場合、容器を修飾するものは、容器に直接印刷されている装飾か、あるいは容器に貼り付けられている紙ラベルだけとなる。従って、包装材料を剥ぎ取った時点で、高級感が失われてしまう。一方、酒類を提供する飲食店などでは、包装材料を剥ぎ取った状態で、商品を顧客に見える状態で陳列することも多い。従って、紙パックやガラス瓶のような容器の全体を被覆するための包装材料を使用しても、筒状容器が高級感を継続的に維持することは困難である。   Patent Documents 1 and 2 propose a packaging material for covering an entire container such as a paper pack or a glass bottle. In many cases, a purchaser of a product covered with a packaging material usually peels off the packaging material and takes out the container covered with the packaging material when using or consuming the purchased product. In that case, the only thing that modifies the container is a decoration that is printed directly on the container or a paper label that is affixed to the container. Therefore, when the packaging material is peeled off, the sense of quality is lost. On the other hand, in restaurants and the like that provide alcoholic beverages, products are often displayed in a state that customers can see them with the packaging material removed. Therefore, it is difficult for the cylindrical container to continuously maintain a high-class feeling even when a packaging material for covering the entire container such as a paper pack or a glass bottle is used.

更に、安価な酒類などは、そのまま飲用者の口と接触させるのに適したカップ状の筒状容器で販売されることも多い。このような商品は、安価で提供することが前提となっており、コスト面の制約が大きいため、包装材料で被覆されることなく提供されるのが通常である。従って、包装材料によって商品に高級感を付与することはできない。   Furthermore, cheap liquors and the like are often sold in cup-shaped cylindrical containers that are suitable for direct contact with the mouth of the drinker. Such goods are presupposed to be provided at a low cost, and are largely provided with no covering with a packaging material because of great cost constraints. Therefore, it is not possible to give the product a high-class feeling with the packaging material.

本発明は、上記に鑑み、包装材料を用いることなく、酒類などを収容する筒状容器に和風の高級感を与えるとともに、容器の内容物がなくなるまで高級感を継続的に維持することができるような、和紙調シュリンクラベルを提供することを目的とする。   In view of the above, the present invention can provide a Japanese-style luxury feeling to a cylindrical container containing alcoholic beverages without using a packaging material, and can continuously maintain a sense of quality until the contents of the container disappear. An object of the present invention is to provide a Japanese paper-like shrink label.

本発明の一局面は、熱収縮性フィルムと、前記熱収縮性フィルムの一方の面を被覆する装飾層と、前記熱収縮性フィルムと前記装飾層との間に介在する第一粘着層とを有し、互いに対向する第一端部および第二端部を有する形状の積層シートと、前記熱収縮フィルムの前記第一端部に対応する部分に設けられた第一接合代と、前記装飾層の前記第二端部に対応する部分に設けられた第二接合代との間に介在し、前記装飾層が外側になるように前記第一接合代と前記第二接合代とを接合する第二粘着層と、を具備し、前記装飾層が、レーヨン紙(雲龍紙を除く)の層を含み、前記レーヨン紙の坪量は、8〜40g/m2 であり、前記第一端部と前記第二端部との重なりの幅Wは、5〜20mmである、筒状容器装飾用の和紙調シュリンクラベルに関する。 One aspect of the present invention includes a heat-shrinkable film, a decorative layer that covers one surface of the heat-shrinkable film, and a first adhesive layer that is interposed between the heat-shrinkable film and the decorative layer. A laminated sheet having a shape having a first end and a second end facing each other, a first joining margin provided at a portion corresponding to the first end of the heat shrink film, and the decorative layer A second joining margin provided at a portion corresponding to the second end of the first joining margin and the second joining margin such that the decorative layer is on the outside . An adhesive layer, and the decorative layer includes a layer of rayon paper (excluding Yunlong paper), and the basis weight of the rayon paper is 8 to 40 g / m 2 , The width W of the overlap with the second end is 5 to 20 mm, and is a Japanese paper-like shrink label for decorating cylindrical containers. About.

本発明の好ましい形態において、積層シートは、第一端部と平行であり、かつ第二端部よりも第一端部に近い位置に形成された第一折り目と、第二端部と平行であり、かつ第一端部よりも第二端部に近い位置に形成された第二折り目とを有する。そして、積層シートが、第一折り目において、装飾層が外側になるように2つ折りにされ、かつ第二折り目において、装飾層が外側になるように2つ折りにされることにより、第一接合代と第二接合代との重なりが形成される。   In a preferred embodiment of the present invention, the laminated sheet is parallel to the first end and parallel to the second end and the first fold formed at a position closer to the first end than the second end. And a second fold formed at a position closer to the second end than the first end. The laminated sheet is folded in two so that the decorative layer is on the outer side at the first fold, and is folded in two on the second fold so that the decorative layer is on the outer side. And the second joint allowance are formed.

本発明のより好ましい形態において、積層シートは、第二端部と第二折り目との間のみに形成された、相対的強度の小さい破断予定部を有する。 In a more preferred embodiment of the present invention, the laminated sheet has a portion to be ruptured that is formed only between the second end portion and the second fold line and has a small relative strength.

本発明の他の局面は、長尺の帯状形状を有し、前記第一端部および前記第二端部が、前記帯状形状の長手方向に平行である、上記のいずれかに記載の筒状容器装飾用の和紙調シュリンクラベルの連続体に関する。   Another aspect of the present invention has a long belt-like shape, and the first end and the second end are parallel to the longitudinal direction of the belt-like shape according to any one of the above. The present invention relates to a continuum of Japanese paper-like shrink labels for container decoration.

本発明の好ましい形態において、上記筒状容器装飾用の和紙調シュリンクラベルの連続体は、前記帯状形状の長手方向が、捲回方向と平行になるように、ロール状に捲回されている。   In a preferred embodiment of the present invention, the continuous body of Japanese paper-like shrink labels for decorating the cylindrical container is wound in a roll shape so that the longitudinal direction of the belt-like shape is parallel to the winding direction.

本発明の和紙調シュリンクラベルを用いることにより、包装材料を用いることなく、酒類などを収容する筒状容器に和風の高級感を与えるとともに、容器の内容物がなくなるまで高級感を継続的に維持することができる。   By using the Japanese paper-like shrink label of the present invention, a high-class Japanese-style feeling is given to a cylindrical container that contains alcoholic beverages, etc., without using packaging materials, and the high-quality feeling is continuously maintained until the contents of the container disappear. can do.

第一実施形態に係る和紙調シュリンクラベルを構成する積層シートの断面図である。It is sectional drawing of the lamination sheet which comprises the Japanese paper style shrink label which concerns on 1st embodiment. 第一実施形態に係る展開された和紙調シュリンクラベルの上面図である。It is a top view of the developed Japanese paper-like shrink label according to the first embodiment. 略四角形の積層シートの形状を概念的に例示する上面図である。It is a top view which illustrates notionally the shape of a substantially square lamination sheet. 第一接合代と第二接合代とを第二粘着層により接合する前の和紙調シュリンクラベルを概念的に示す断面図である。It is sectional drawing which shows notionally the Japanese paper style shrink label before joining a 1st joining allowance and a 2nd joining allowance with a 2nd adhesion layer. 第一接合代と第二接合代とを第二粘着層により接合した後の和紙調シュリンクラベルの要部断面図である。It is principal part sectional drawing of a Japanese paper style shrink label after joining the 1st joining margin and the 2nd joining margin with the 2nd adhesion layer. 第一実施形態に係る和紙調シュリンクラベルを、第一接合代と第二接合代との接合部側から見た上面図である。It is the top view which looked at the Japanese paper style shrink label which concerns on 1st embodiment from the junction part side of the 1st joining allowance and the 2nd joining allowance. 第二実施形態に係る展開された和紙調シュリンクラベルの上面図である。It is a top view of the developed Japanese paper-like shrink label according to the second embodiment. 第一折り目と第二折り目で折り曲げ、かつ第一接合代と第二接合代とを第二粘着層により接合する前の和紙調シュリンクラベルを概念的に示す断面図である。It is sectional drawing which shows notionally the Japanese paper-style shrink label before bending by a 1st crease | fold and a 2nd crease | fold and joining a 1st joining allowance and a 2nd joining allowance with a 2nd adhesion layer. 第二実施形態に係る和紙調シュリンクラベルを、第一接合代と第二接合代との接合部側から見た上面図である。It is the top view which looked at the Japanese paper style shrink label which concerns on 2nd embodiment from the junction part side of the 1st joining allowance and the 2nd joining allowance. 瓶形状の筒状容器に、和紙調シュリンクラベルを装着し、その後、加熱により和紙調シュリンクラベルを収縮させて筒状容器に密着させた状態を示す図である。It is a figure which shows the state which mounted | worn the Japanese paper-like shrink label to the bottle-shaped cylindrical container, and contracted the Japanese paper-like shrink label by heating, and was made to closely_contact | adhere to a cylindrical container after that. カップ状の筒状容器に、和紙調シュリンクラベルを装着し、その後、加熱により和紙調シュリンクラベルを収縮させて筒状容器に密着させた状態を示す図である。It is a figure which shows the state which mounted | worn the Japanese paper style shrink label to the cup-shaped cylindrical container, and contracted the Japanese paper style shrink label by heating, and was made to contact | adhere to the cylindrical container after that. 第三実施形態に係る和紙調シュリンクラベルの連続体を、第一接合代と第二接合代との接合部側から見た上面図である。It is the top view which looked at the continuous body of the Japanese paper style shrink label which concerns on 3rd embodiment from the junction part side of the 1st joining allowance and the 2nd joining allowance. ロール状に捲回された連続体を、個別に切り出して、筒状容器に装着する工程を示す概念図である。It is a conceptual diagram which shows the process of cutting out the continuous body wound by roll shape separately, and mounting | wearing a cylindrical container.

本発明の筒状容器装飾用の和紙調シュリンクラベルは、熱収縮性フィルムと、熱収縮性フィルムの一方の面を被覆する装飾層と、熱収縮性フィルムと装飾層との間に介在する第一粘着層と、を有する積層シートにより形成されている。装飾層は、高級感を付与する観点から、レーヨン紙の層を含んでいる。 The Japanese paper-like shrink label for decorating a cylindrical container according to the present invention includes a heat-shrinkable film, a decorative layer covering one surface of the heat-shrinkable film, and a first layer interposed between the heat-shrinkable film and the decorative layer. And an adhesive layer. The decorative layer includes a layer of rayon paper from the viewpoint of imparting a sense of quality.

和紙調シュリンクラベルが展開された状態では、積層シートの形状は、互いに対向する第一端部と第二端部とを有する形状(例えば長方形)である。熱収縮フィルムの第一端部に対応する部分には第一接合代が設けられており、装飾層の第二端部に対応する部分には第二接合代が設けられている。第一接合代と第二接合代とは、第二粘着層により接合されている。   In a state where the Japanese paper-style shrink label is developed, the shape of the laminated sheet is a shape having a first end portion and a second end portion facing each other (for example, a rectangle). A portion corresponding to the first end portion of the heat shrink film is provided with a first joining allowance, and a portion corresponding to the second end portion of the decorative layer is provided with a second joining allowance. The first joining allowance and the second joining allowance are joined by the second adhesive layer.

上記和紙調シュリンクラベルは、構造が簡易であるため、一枚の長方形の積層シートから容易に製造することができる。よって、製造コストが小さいため、安価で高級感のある装飾を筒状容器に付与することができる。   Since the Japanese paper-like shrink label has a simple structure, it can be easily manufactured from a single rectangular laminated sheet. Therefore, since the manufacturing cost is low, inexpensive and high-quality decoration can be imparted to the cylindrical container.

また、上記和紙調シュリンクラベルは、積層シートの第一端部に設けられた第一接合代と第二端部に設けられた第二接合代とが、第二粘着層により接合されていることから、筒状容器を和紙調シュリンクラベルに貫挿するだけで、容易に、筒状容器に和紙調シュリンクラベルを装着することができる。そのため、和紙調シュリンクラベルの筒状容器への位置合わせが容易で、装飾が斜めに歪んだりすることもない。   Moreover, as for the said Japanese paper-like shrink label, the 1st joining margin provided in the 1st end part of the lamination sheet and the 2nd joining margin provided in the 2nd end part are joined by the 2nd adhesion layer Therefore, the Japanese paper-style shrink label can be easily attached to the cylindrical container simply by inserting the cylindrical container into the Japanese paper-style shrink label. For this reason, it is easy to align the Japanese paper-like shrink label with the cylindrical container, and the decoration is not obliquely distorted.

更に、第一接合代が熱収縮フィルムの表面であり、第二接合代が網目構造を有するレーヨン紙で構成された装飾層の表面であることから、熱収縮フィルムの装飾層に対する密着性が適度なものとなる。よって、第一接合代と第二接合代との接合部を剥がして、筒状容器と和紙調シュリンクラベルとを分離することが容易である。そのため、容器に粘着剤を介して貼り付ける紙ラベルなどに比べて、筒状容器だけを回収したり、和紙調シュリンクラベルを廃棄したりする際の分別が容易となる。 Furthermore, since the first bonding margin is the surface of the heat shrinkable film and the second bonding margin is the surface of the decorative layer made of rayon paper having a network structure, the heat shrinkable film has an appropriate adhesion to the decorative layer. It will be something. Therefore, it is easy to peel off the joining portion between the first joining allowance and the second joining allowance to separate the cylindrical container and the Japanese paper-style shrink label. Therefore, compared with a paper label or the like attached to the container via an adhesive, it becomes easier to collect only the cylindrical container or discard the Japanese paper-like shrink label.

本発明の好ましい形態において、積層シートは、第一端部と平行であり、かつ第二端部よりも第一端部に近い位置に形成された第一折り目と、第二端部と平行であり、かつ第一端部よりも第二端部に近い位置に形成された第二折り目とを有する。そして、積層シートが、第一折り目において、装飾層が外側になるように2つ折りにされ、かつ第二折り目において、装飾層が外側になるように2つ折りにされることにより、第一接合代と第二接合代との重なりが形成されている。   In a preferred embodiment of the present invention, the laminated sheet is parallel to the first end and parallel to the second end and the first fold formed at a position closer to the first end than the second end. And a second fold formed at a position closer to the second end than the first end. The laminated sheet is folded in two so that the decorative layer is on the outer side at the first fold, and is folded in two on the second fold so that the decorative layer is on the outer side. And the second joining allowance are formed.

上記構成によれば、筒状の和紙調シュリンクラベルを、事実上、一枚のシート状物として扱うことができる。従って、複数の和紙調シュリンクラベルを重ねて保存したり、重ねて輸送したりすることができ、取り扱いの利便性が向上する。   According to the said structure, a cylindrical Japanese paper-like shrink label can be handled as one sheet-like thing in fact. Accordingly, a plurality of Japanese paper-like shrink labels can be stored and transported in an overlapping manner, and the convenience of handling is improved.

また、上記構成によれば、和紙調シュリンクラベルの形状が安定化するため、第二粘着層による第一接合代と第二接合代との接合部には、余計な応力が印加されにくくなる。よって、被装飾物である筒状容器に和紙調シュリンクラベルを装着する前に、第一接合代と第二接合代との接合部が剥がれたり、筒状容器に和紙調シュリンクラベルを密着させるときに、接合部が剥がれたりする可能性が低減する。   Moreover, according to the said structure, since the shape of a Japanese paper-like shrink label is stabilized, it becomes difficult to apply an extra stress to the junction part of the 1st joining margin and 2nd joining margin by a 2nd adhesion layer. Therefore, before attaching the Japanese paper-style shrink label to the cylindrical container that is to be decorated, when the joint portion between the first joint allowance and the second joint allowance is peeled off, or when the Japanese paper-style shrink label is brought into close contact with the tubular container In addition, the possibility that the joint is peeled off is reduced.

本発明のより好ましい形態において、積層シートは、第二端部と第二折り目との間に形成された、相対的強度の小さい破断予定部を有する。   In a more preferred embodiment of the present invention, the laminated sheet has a portion to be ruptured that is formed between the second end portion and the second fold line and has a small relative strength.

上記構成によれば、第一接合代と第二接合代との接合部の強度が、高くなり過ぎた場合でも、筒状容器を回収したり、和紙調シュリンクラベルを廃棄したりする際には、破断予定部が容易に破断する。よって、筒状容器と和紙調シュリンクラベルとを分離する作業が更に容易になる。   According to the above configuration, even when the strength of the joining portion between the first joining allowance and the second joining allowance becomes excessively high, when collecting the cylindrical container or discarding the Japanese paper-like shrink label, The portion to be broken is easily broken. Therefore, the operation | work which isolate | separates a cylindrical container and a Japanese paper-like shrink label becomes still easier.

また、第二端部は第一端部に覆われた状態であるため、破断予定部を、第一端部と第一折り目との間に形成するよりも、第二端部と第二折り目との間に形成する方が、接合部における面方向の摩擦力が働きやすい。よって、破断予定部を第二端部と第二折り目との間に形成することで、外力を付与したときの破断予定部の破断が促進される。   In addition, since the second end portion is covered with the first end portion, the second end portion and the second fold line are formed rather than forming the planned fracture portion between the first end portion and the first fold line. The frictional force in the surface direction at the joint is more likely to work between the two. Therefore, by forming the planned fracture portion between the second end portion and the second fold, the fracture of the planned fracture portion when an external force is applied is promoted.

本発明の和紙調シュリンクラベルは、長尺の帯状形状を有する連続体とすることもできる。このとき、和紙調シュリンクラベルの第一端部および第二端部は、帯状形状の連続体の長手方向と平行となる。   The Japanese paper-like shrink label of the present invention may be a continuous body having a long strip shape. At this time, the first end and the second end of the Japanese paper-like shrink label are parallel to the longitudinal direction of the belt-like continuous body.

上記構成によれば、和紙調シュリンクラベルを連続体から、順次、切り出して使用することができる。よって、多数の和紙調シュリンクラベルを使用する際の作業効率が向上する。また、和紙調シュリンクラベルを連続体とすることで、和紙調シュリンクラベルの製造コストを低減することができる。   According to the said structure, a Japanese paper style shrink label can be cut out and used from a continuous body sequentially. Therefore, the working efficiency when using a number of Japanese paper-like shrink labels is improved. Moreover, the manufacturing cost of a Japanese paper-like shrink label can be reduced by using a Japanese paper-like shrink label as a continuous body.

和紙調シュリンクラベルの連続体は、事実上、一枚のシート状物として取り扱うことができる。よって、連続体は、その長手方向が、捲回方向と平行になるように、ロール状に捲回することができる。これにより、和紙調シュリンクラベルの輸送、管理、保存および取り扱いが容易となる。   The continuum of Japanese paper-like shrink labels can be handled as a single sheet in nature. Therefore, the continuous body can be wound in a roll shape so that its longitudinal direction is parallel to the winding direction. This facilitates the transport, management, storage and handling of Japanese paper-like shrink labels.

以下、本発明の筒状容器装飾用の和紙調シュリンクラベルの実施形態について、より具体的に説明するが、以下の実施形態は本発明を限定するものではない。   Hereinafter, although the embodiment of the Japanese paper-like shrink label for decorating a cylindrical container of the present invention will be described more specifically, the following embodiments do not limit the present invention.

(第一実施形態)
図1に、本実施形態に係る筒状容器装飾用の和紙調シュリンクラベルを構成する積層シート10の断面図を示す。積層シート10は、展開されたときの形状が長方形であり、熱収縮性フィルム11と、熱収縮性フィルム11の一方の面を被覆する装飾層12と、熱収縮性フィルム11と装飾層12との間に介在する第一粘着層13とを具備する。なお、展開されたときの形状とは、積層シート10を平坦に引き延ばし、積層シート10を、その主面に対して垂直な方向からみたときの外形である。
(First embodiment)
In FIG. 1, sectional drawing of the lamination sheet 10 which comprises the Japanese paper style shrink label for cylindrical container decoration which concerns on this embodiment is shown. The laminated sheet 10 has a rectangular shape when unfolded, a heat-shrinkable film 11, a decorative layer 12 that covers one surface of the heat-shrinkable film 11, a heat-shrinkable film 11, and a decorative layer 12 And a first adhesive layer 13 interposed therebetween. In addition, the shape when unfolded is an outer shape when the laminated sheet 10 is stretched flat and the laminated sheet 10 is viewed from a direction perpendicular to the main surface.

熱収縮性フィルム11は、加熱することによって収縮し、容器に密着するフィルムである。熱収縮性フィルムの材質は、特に限定されないが、例えば、ポリ塩化ビニル、ポリ塩化ビニリデン、ポリスチレン、ポリプロピレン、ポリエチレン、ポリエチレンテレフタレートなどを用いることができる。   The heat-shrinkable film 11 is a film that shrinks by heating and adheres to the container. The material of the heat-shrinkable film is not particularly limited. For example, polyvinyl chloride, polyvinylidene chloride, polystyrene, polypropylene, polyethylene, polyethylene terephthalate, or the like can be used.

装飾層12は、和風の高級感を表現するのに適することから、レーヨン紙14(特に和紙調レーヨン紙)の層を含んでいる。装飾層12は、例えば、レーヨン紙14と、その表面に形成された印刷層15とで構成されている。 The decorative layer 12 includes a layer of rayon paper 14 (particularly Japanese paper-like rayon paper ) because it is suitable for expressing a Japanese-style luxury feeling. The decoration layer 12 is composed of, for example, rayon paper 14 and a printing layer 15 formed on the surface thereof.

印刷層15は、筒状容器を装飾するための様々な図形、文字、模様等を含んでいる。印刷層15は、図1のように、レーヨン紙等14の第一粘着層13側とは反対側の面に設けることが好ましいが、レーヨン紙等14と第一粘着層13との間に設けてもよいし、レーヨン紙等14の両面に設けてもよい。また、印刷層15は、必ずしも、装飾層12に設ける必要はなく、熱収縮性フィルム11の一方の面に形成してもよい。印刷層15は、その被形成面に対して、例えば、オフセット印刷法やグラビア印刷法などにより形成することができる。   The print layer 15 includes various figures, characters, patterns and the like for decorating the cylindrical container. As shown in FIG. 1, the printing layer 15 is preferably provided on the surface opposite to the first adhesive layer 13 side of the rayon paper 14, but provided between the rayon paper 14 and the first adhesive layer 13. Alternatively, it may be provided on both sides of the rayon paper 14 or the like. The printed layer 15 is not necessarily provided on the decorative layer 12 and may be formed on one surface of the heat-shrinkable film 11. The print layer 15 can be formed on the surface to be formed by, for example, an offset printing method or a gravure printing method.

レーヨン紙は、熱収縮性フィルム11が収縮しても、大きな皺を形成することがなく、網目構造の網目がより詰った状態になるため、シュリンクラベルの材料として特に適している。和紙調レーヨン紙は、表面に和紙のような繊維状の起伏を有する。和紙調レーヨン紙は、再生セルロースの人造繊維により形成することができる。和紙調レーヨン紙の坪量は、特に限定されないが、例えば8〜40g/m2 が好ましい。なお、レーヨン紙とは、溶解パルプを原料とするレーヨン(rayon)繊維を用いた不織布である。 Rayon paper is particularly suitable as a material for shrink labels because it does not form large wrinkles even when the heat-shrinkable film 11 contracts, and the mesh of the mesh structure becomes more clogged. Japanese paper-like rayon paper has a fibrous undulation like Japanese paper on its surface. Japanese paper rayon paper can be formed from artificial fibers of regenerated cellulose. Although the basic weight of Japanese paper-like rayon paper is not specifically limited, For example, 8-40 g / m < 2 > is preferable. The rayon paper is a non-woven fabric using rayon fibers made from dissolved pulp.

第一粘着層13を形成する粘着剤としては、所望の接着強度を発現する材料を用いればよく、特に限定されない。例えば、デンプンなどの糊剤、アクリル樹脂、ウレタン樹脂などの樹脂を主成分とする粘着剤などを用いることができる。   The pressure-sensitive adhesive that forms the first pressure-sensitive adhesive layer 13 may be any material that exhibits desired adhesive strength, and is not particularly limited. For example, a paste such as starch, an adhesive mainly composed of a resin such as an acrylic resin or a urethane resin can be used.

装飾層12および第一粘着層13は、いずれも熱収縮性フィルム11の全面に形成されていることが好ましいが、装飾層12および第一粘着層13が形成されていない領域を有してもよい。ただし、筒状容器に十分な高級感を付与する観点から、例えば、熱収縮性フィルム11の一方の面の面積の90%以上に、装飾層12および第一粘着層13が形成されていることが好ましい。   Both the decorative layer 12 and the first adhesive layer 13 are preferably formed on the entire surface of the heat-shrinkable film 11, but may have a region where the decorative layer 12 and the first adhesive layer 13 are not formed. Good. However, the decorative layer 12 and the first adhesive layer 13 are formed on, for example, 90% or more of the area of one surface of the heat-shrinkable film 11 from the viewpoint of imparting a sufficient luxury to the cylindrical container. Is preferred.

積層シート10は、ドライラミネーション法、無溶剤型ラミネーション法、ウエットラミネーション法などの積層法によって作製することができる。上記のように、本発明の和紙調シュリンクラベルは、一枚の積層シート10から容易に製造することができる。よって、安価でありながら、高級感のある装飾を筒状容器に付与することが可能である。   The laminated sheet 10 can be produced by a lamination method such as a dry lamination method, a solventless lamination method, or a wet lamination method. As described above, the Japanese paper-like shrink label of the present invention can be easily manufactured from one laminated sheet 10. Therefore, it is possible to give a high-quality decoration to the cylindrical container while being inexpensive.

次に、図2に、展開された状態の和紙調シュリンクラベル20の上面図を示す。和紙調シュリンクラベル20の形状は長方形であり、互いに対向する第一端部16および第二端部17を有するとともに、第一端部16および第二端部17に対して垂直かつ互いに平行な第三端部18および第四端部19を有する。   Next, FIG. 2 shows a top view of the Japanese paper-like shrink label 20 in a developed state. The shape of the Japanese paper-like shrink label 20 is rectangular, and has a first end portion 16 and a second end portion 17 facing each other, and is perpendicular to the first end portion 16 and the second end portion 17 and parallel to each other. It has a three end portion 18 and a fourth end portion 19.

図2の一点鎖線は、第一端部16に設けられる第一接合代16aの境界および第二端部に設けられる第二接合代17aの境界を示している。装飾層12の表面からなる第二接合代17aには、第二粘着層21が設けられている。なお、第二粘着層21は、第一接合代16aに設けてもよく、第一接合代16aと第二接合代17aの両方に設けてもよい。   2 indicates the boundary of the first joint allowance 16a provided at the first end portion 16 and the boundary of the second joint allowance 17a provided at the second end portion. A second adhesive layer 21 is provided in the second bonding allowance 17 a made of the surface of the decorative layer 12. In addition, the 2nd adhesion layer 21 may be provided in the 1st joining allowance 16a, and may be provided in both the 1st joining allowance 16a and the 2nd joining allowance 17a.

積層シート10の形状は、完全な四角形である必要はなく、略四角形であればよい。従って、長方形の四隅は鋭角であってもよく、丸みを帯びていてもよい。また、長方形の各辺は、曲線部を含んでもよく、長方形は、非対称な形状であってもよい。なお、長方形には、正方形も含まれる。   The shape of the laminated sheet 10 does not have to be a perfect rectangle, but may be a substantially rectangle. Therefore, the four corners of the rectangle may be acute or rounded. Each side of the rectangle may include a curved portion, and the rectangle may have an asymmetric shape. Note that the rectangle includes a square.

図3に、略四角形の積層シート10A〜10Cの形状を上面図により例示する。図3(a)は、四隅が面取りされた略四角形であり、図3(b)は、四隅が丸みを帯びている略四角形であり、図3(c)は、四隅が丸みを帯びるとともに、第三端部18および第四端部19が曲線からなる略四角形である。なお、略四角形は、上記に限定されるものではない。   In FIG. 3, the shape of the substantially square laminated sheets 10A to 10C is illustrated by a top view. 3A is a substantially quadrangle with four corners chamfered, FIG. 3B is a substantially quadrangle with four corners rounded, and FIG. 3C is rounded with four corners, The 3rd end part 18 and the 4th end part 19 are the substantially squares which consist of a curve. The substantially square shape is not limited to the above.

和紙調シュリンクラベル20を形成する際には、装飾層12が外側に配置されるように、かつ、互いに対向する第一端部16と第二端部17とが互いに重なり合うように、積層シート10が折り曲げられ、または屈曲される。そして、第一端部16に設けられた第一接合代16aと、第二端部17に設けられた第二接合代17aとが、これらの間に介在する第二粘着層により接合される。   When the Japanese paper-like shrink label 20 is formed, the laminated sheet 10 is arranged so that the decorative layer 12 is disposed on the outside and the first end 16 and the second end 17 facing each other overlap each other. Is bent or bent. And the 1st joining margin 16a provided in the 1st end part 16 and the 2nd joining allowance 17a provided in the 2nd end part 17 are joined by the 2nd adhesion layer interposed between these.

ここで、第一接合代16aは、熱収縮フィルム11の表面であり、第二接合代17aは網目構造を有するレーヨン紙で構成された装飾層の表面である。従って、熱収縮フィルム11の装飾層12に対する密着性は適度なものとなる。そのため、筒状容器を廃棄等する際には、第一接合代16aと第二接合代17aとの接合部を剥がして、筒状容器と和紙調シュリンクラベルを分離することが容易となる。 Here, the first joining allowance 16a is the surface of the heat-shrinkable film 11, and the second joining allowance 17a is the surface of the decorative layer made of rayon paper having a network structure. Therefore, the adhesiveness of the heat shrink film 11 to the decorative layer 12 is appropriate. Therefore, when discarding the cylindrical container, it becomes easy to separate the cylindrical container and the Japanese paper-style shrink label by peeling the joint portion between the first joint allowance 16a and the second joint allowance 17a.

図4Aは、第一接合代16aと第二接合代17aとを第二粘着層(図示せず)により接合する前の和紙調シュリンクラベルを、概念的に断面で示している。図4Bは、第一接合代16aと第二接合代17aとを第二粘着層21により接合した後の和紙調シュリンクラベルの要部断面図を示している。第一接合代16aは、熱収縮フィルム11の第一端部16に対応する部分に設けられる。また、第二接合代17aは、装飾層12の第二端17部に対応する部分に設けられる。   FIG. 4A conceptually shows a cross section of a Japanese paper-like shrink label before joining the first joining allowance 16a and the second joining allowance 17a with a second adhesive layer (not shown). FIG. 4B shows a cross-sectional view of the main part of the Japanese paper-style shrink label after the first joining allowance 16a and the second joining allowance 17a are joined by the second adhesive layer 21. FIG. The first bonding allowance 16 a is provided at a portion corresponding to the first end portion 16 of the heat shrink film 11. The second joining allowance 17 a is provided at a portion corresponding to the second end 17 portion of the decorative layer 12.

図5は、和紙調シュリンクラベル20を、第一接合代16aと第二接合代17aとの接合部側から見た上面図である。第一端部16と第二端部17との重なりの幅Wは、特に限定されないが、積層シート10を有効に利用するとともに、十分な面積の接合代を確保する観点から、例えば5〜20mmであることが好ましい。第一接合代16aと第二接合代17aの幅は同じでも異なってもよく、例えば、第一端部16と第二端部17との重なりの幅W以下であればよい。   FIG. 5 is a top view of the Japanese paper-like shrink label 20 as viewed from the joint portion side between the first joint allowance 16a and the second joint allowance 17a. Although the width W of the overlap between the first end portion 16 and the second end portion 17 is not particularly limited, it is 5 to 20 mm, for example, from the viewpoint of effectively using the laminated sheet 10 and securing a bonding area with a sufficient area. It is preferable that The widths of the first joint allowance 16a and the second joint allowance 17a may be the same or different. For example, the width may be equal to or less than the overlap width W of the first end portion 16 and the second end portion 17.

このように、積層シート10の第一端部16に設けられた第一接合代16aと第二端部17に設けられた第二接合代17aとが、予め第二粘着層21で接合されていることから、和紙調シュリンクラベル20自体が筒状であり、筒状容器に容易に装着することができる。そして、和紙調シュリンクラベル20を筒状容器に装着するだけで、和紙調シュリンクラベル20の筒状容器への位置合わせがほぼ完了する。   Thus, the first joining margin 16a provided at the first end 16 of the laminated sheet 10 and the second joining margin 17a provided at the second end 17 are joined together in advance by the second adhesive layer 21. Therefore, the Japanese paper-like shrink label 20 itself has a cylindrical shape and can be easily attached to the cylindrical container. Then, only by attaching the Japanese paper-style shrink label 20 to the cylindrical container, the alignment of the Japanese paper-style shrink label 20 to the cylindrical container is almost completed.

第二粘着層21を形成する粘着剤としても、所望の接着強度を発現する材料を用いればよく、特に限定されない。例えば、第一粘着層13としても使用可能な糊剤や粘着剤を用いることができる。   The pressure-sensitive adhesive forming the second pressure-sensitive adhesive layer 21 is not particularly limited as long as a material that exhibits desired adhesive strength is used. For example, a paste or adhesive that can be used as the first adhesive layer 13 can also be used.

(第二実施形態)
図6は、本実施形態に係る和紙調シュリンクラベル20Aを展開した状態の上面図である。本実施形態では、第一実施形態と同じ構成要素には、同じ符号を用いる。和紙調シュリンクラベル20Aを構成する積層シート10には、第一端部16と平行であり、かつ第二端部17よりも第一端部16に近い位置に形成された第一折り目22と、第二端部17と平行であり、かつ第一端部16よりも第二端部17に近い位置に形成された第二折り目23とを有する。
(Second embodiment)
FIG. 6 is a top view of the state in which the Japanese paper-style shrink label 20A according to the present embodiment is developed. In this embodiment, the same code | symbol is used for the same component as 1st embodiment. In the laminated sheet 10 constituting the Japanese paper-like shrink label 20A, the first fold line 22 is formed in a position parallel to the first end portion 16 and closer to the first end portion 16 than the second end portion 17; The second fold line 23 is formed in a position parallel to the second end portion 17 and closer to the second end portion 17 than the first end portion 16.

和紙調シュリンクラベル20Aを形成する際には、図7に示すように、積層シート10が、第一折り目22において、装飾層12が外側になるように2つ折りにされ、かつ第二折り目23において、装飾層12が外側になるように2つ折りにされる。これにより、第一接合代16aと第二接合代17aとの重なりが形成される。そして、第一接合代16aと第二接合代17aとが、第二粘着層21により接合される。   When forming the Japanese paper-like shrink label 20A, as shown in FIG. 7, the laminated sheet 10 is folded in two so that the decorative layer 12 is on the outer side at the first fold line 22, and at the second fold line 23. The decorative layer 12 is folded in half so that it is on the outside. Thereby, the overlap of the first joining allowance 16a and the second joining allowance 17a is formed. The first joining allowance 16 a and the second joining allowance 17 a are joined by the second adhesive layer 21.

図8は、完成した和紙調シュリンクラベル20Aを、第一接合代16aと第二接合代17aとの接合部側から見た上面図である。このように、積層シート10を明確な折り目22、23により完全に折り畳むことで、筒状の和紙調シュリンクラベル20Aを、事実上、一枚のシート状物として扱うことができ、和紙調シュリンクラベル20Aの保存や輸送の利便性が向上する。また、上記のように折り畳むことで、和紙調シュリンクラベル20Aの形状が安定化するため、第二粘着層21による第一接合代16aと第二接合代17aとの接合部に余計な応力が印加されにくくなる。よって、第一接合代と第二接合代との接合部の剥がれが低減される。   FIG. 8 is a top view of the completed Japanese paper-like shrink label 20A as viewed from the joint portion side between the first joint allowance 16a and the second joint allowance 17a. In this way, by completely folding the laminated sheet 10 with clear creases 22 and 23, the cylindrical Japanese paper-like shrink label 20A can be handled virtually as a single sheet-like product. The convenience of storage and transportation of 20A is improved. Moreover, since the shape of the Japanese paper-like shrink label 20A is stabilized by folding as described above, an extra stress is applied to the joint between the first joint allowance 16a and the second joint allowance 17a by the second adhesive layer 21. It becomes difficult to be done. Therefore, peeling of the joint portion between the first joint allowance and the second joint allowance is reduced.

図6および図8に示すように、積層シート10の第二端部と第二折り目との間には、破断予定部24を形成してもよい。これにより、第一接合代16aと第二接合代17aとの接合部の強度が高い場合でも、必要時には、破断予定部24を破断させて、筒状容器と和紙調シュリンクラベルとを分離することができる。   As shown in FIGS. 6 and 8, a planned fracture portion 24 may be formed between the second end of the laminated sheet 10 and the second fold. Thereby, even when the strength of the joint portion between the first joint allowance 16a and the second joint allowance 17a is high, when necessary, the breakable portion 24 is broken to separate the cylindrical container and the Japanese paper-like shrink label. Can do.

破断予定部24の構成は、特に限定されないが、例えば、積層シート10を貫通する貫通孔によるミシン目を設けることにより、和紙調シュリンクラベル20Aに、破断予定部24を付与することができる。また、熱収縮性フィルム11に、周囲よりも厚みの小さい溝部を設けてもよく、破断の契機となる切れ込みを積層シート10の第三端部18および第四端部19の少なくとも一方に設けてもよい。   The configuration of the planned fracture portion 24 is not particularly limited. For example, by providing a perforation by a through hole that penetrates the laminated sheet 10, the planned fracture portion 24 can be imparted to the Japanese paper-like shrink label 20A. Further, the heat-shrinkable film 11 may be provided with a groove portion having a thickness smaller than that of the surroundings, and a notch serving as a trigger for breaking is provided in at least one of the third end portion 18 and the fourth end portion 19 of the laminated sheet 10. Also good.

次に、和紙調シュリンクラベルの具体的な用途の例について説明する。
まず、筒状容器の具体的形状としては、横断面が円形もしくは楕円形である胴部を有する形状が好ましいが、横断面が多角形(例えば略矩形)である胴部を有する形状でもよい。円筒型の胴部の直径は一定であってもよく、軸方向に沿って変化してもよい。筒状容器は、注ぎ口の横断面の直径が胴部よりも小さくなる瓶形状でもよい。このような形状は、清酒、焼酎、ワインなどを収容するのに適している。また、筒状容器は、直径がほぼ一定であるカップ状でもよい。カップ状の容器は、清酒を収容するのに適している。ここで、カップ状とは、横断面がほぼ一定の直径D1を有する円形である円筒型の胴部を有し、開口の直径D2が胴部の直径D1とほぼ同じである形状をいう(例えば0.8×D1≦D2≦D1)。カップ状の容器は、筒状容器の開口を、液体を飲用する者の口と直に接触させるのに適している。
Next, an example of a specific use of the Japanese paper-like shrink label will be described.
First, the specific shape of the cylindrical container is preferably a shape having a trunk portion whose cross section is circular or elliptical, but may be a shape having a trunk portion whose cross section is polygonal (for example, substantially rectangular). The diameter of the cylindrical barrel may be constant or may vary along the axial direction. The cylindrical container may have a bottle shape in which the diameter of the cross section of the spout is smaller than that of the barrel. Such a shape is suitable for accommodating sake, shochu, wine and the like. Further, the cylindrical container may have a cup shape with a substantially constant diameter. The cup-shaped container is suitable for containing sake. Here, the cup shape refers to a shape having a cylindrical body having a circular cross section with a substantially constant diameter D1, and having an opening diameter D2 that is substantially the same as the diameter D1 of the body (for example, 0.8 × D1 ≦ D2 ≦ D1). The cup-shaped container is suitable for bringing the opening of the cylindrical container into direct contact with the mouth of the person who drinks the liquid.

図9は、注ぎ口の横断面の直径が胴部よりも小さくなる瓶形状の筒状容器25に、和紙調シュリンクラベル20を装着し、その後、加熱により和紙調シュリンクラベル20を収縮させて筒状容器25に密着させた状態を示している。このような瓶形状の容器を修飾するラベルとしては、従来、紙ラベルを、粘着剤を介して容器に貼り付けることが常法となっている。しかし、紙ラベルを容器に貼り付ける際には、ラベルが歪まないように位置合わせしたり、ラベルに皺がよらないように配慮したりする必要があり、作業には、ある程度の熟練を要する。しかも、内容物が空になった容器を廃棄する際には、ラベルを取り外すことが困難である。一方、和紙調シュリンクラベル20は、容器に対する位置合わせが容易であり、かつ容器を廃棄する際には、容易に容器から取り外すことができる。   FIG. 9 shows a case in which a Japanese paper-like shrink label 20 is attached to a bottle-shaped cylindrical container 25 whose cross-sectional diameter of the spout is smaller than that of the barrel, and then the Japanese paper-like shrink label 20 is contracted by heating. The state which was stuck to the cylindrical container 25 is shown. Conventionally, as a label for modifying such a bottle-shaped container, a paper label is usually attached to the container via an adhesive. However, when a paper label is affixed to a container, it is necessary to align the label so that the label is not distorted or to prevent the label from wrinkling, and the work requires some skill. In addition, it is difficult to remove the label when the container whose contents are empty is discarded. On the other hand, the Japanese paper-like shrink label 20 is easily aligned with the container, and can be easily removed from the container when the container is discarded.

図10は、カップ状の筒状容器26に、和紙調シュリンクラベル20を装着し、その後、加熱により和紙調シュリンクラベル20を収縮させて筒状容器26に密着させた状態を示している。カップ状の筒状容器26は、包装材料で包装されることは稀であり、粘着剤を介して紙ラベルを容器に貼り付けることが常法となっている。しかし、このような商品は安価で販売されるものであり、紙ラベルに高級な和紙を使用することはできない。一方、和紙調シュリンクラベル20を用いることにより、安価なコストで高級感を商品に付与することが可能となる。   FIG. 10 shows a state in which the Japanese paper-style shrink label 20 is attached to the cup-shaped cylindrical container 26 and then the Japanese paper-style shrink label 20 is contracted by heating to be in close contact with the cylindrical container 26. The cup-shaped cylindrical container 26 is rarely packaged with a packaging material, and it is a common practice to attach a paper label to the container via an adhesive. However, such products are sold at low cost, and high-grade Japanese paper cannot be used for paper labels. On the other hand, by using the Japanese paper-like shrink label 20, it is possible to give a high-class feeling to the product at a low cost.

また、このような商品は、図10に示すように、上下方向に重ねて陳列されることも多い。従って、全ての商品のラベルの位置が揃わないと、見栄えが低下し、商品の高級感が損なわれることとなる。一方、和紙調シュリンクラベル20を用いる場合には、ラベルの位置合わせが容易であり、ラベルが斜めに歪むこともないため、商品の陳列状態に関わらず、高級感を維持しやすい。   In addition, as shown in FIG. 10, such merchandise is often displayed in the vertical direction. Accordingly, if the positions of all the product labels are not aligned, the appearance will be deteriorated, and the quality of the product will be impaired. On the other hand, when the Japanese paper-style shrink label 20 is used, label alignment is easy and the label is not distorted obliquely, so that a high-class feeling is easily maintained regardless of the display state of the product.

(第三実施形態)
図11は、本実施形態に係る和紙調シュリンクラベルの連続体20Bを、第一接合代16aと第二接合代17aとの接合部側から見た上面図である。本実施形態でも、第一実施形態と同じ構成要素には、同じ符号を用いる。
(Third embodiment)
FIG. 11 is a top view of the continuous body 20B of Japanese paper-like shrink labels according to the present embodiment as viewed from the joint portion side between the first joint allowance 16a and the second joint allowance 17a. Also in this embodiment, the same code | symbol is used for the same component as 1st embodiment.

連続体20Bは、第二実施形態に係る和紙調シュリンクラベル20Aの連続体に相当する。すなわち、連続体20Bを構成する積層シート10には、第一端部16と平行であり、かつ第二端部17よりも第一端部16に近い位置に形成された第一折り目22と、第二端部17と平行であり、かつ第一端部16よりも第二端部17に近い位置に形成された第二折り目23とを有する。長尺で帯状の積層シート10が、その長手方向と平行な第一折り目22において、装飾層12が外側になるように2つ折りにされ、かつその長手方向と平行な第二折り目23において、装飾層12が外側になるように2つ折りにされる。これにより、第一接合代16aと第二接合代17aとの重なりが形成される。そして、第一接合代16aと第二接合代17aとが、第二粘着層21により接合される。   The continuous body 20B corresponds to a continuous body of the Japanese paper-like shrink label 20A according to the second embodiment. That is, in the laminated sheet 10 constituting the continuous body 20B, the first fold line 22 is formed in a position parallel to the first end portion 16 and closer to the first end portion 16 than the second end portion 17; The second fold line 23 is formed in a position parallel to the second end portion 17 and closer to the second end portion 17 than the first end portion 16. The elongate belt-like laminated sheet 10 is folded in two so that the decorative layer 12 faces outside at a first fold 22 parallel to the longitudinal direction, and at a second fold 23 parallel to the longitudinal direction, the decoration is made. Folded in half so that layer 12 is on the outside. Thereby, the overlap of the first joining allowance 16a and the second joining allowance 17a is formed. The first joining allowance 16 a and the second joining allowance 17 a are joined by the second adhesive layer 21.

和紙調シュリンクラベルの連続体は、長尺で帯状の積層シート10を原料として、容易に製造することができる。また、連続体によれば、多数の筒状容器に必要な和紙調シュリンクラベルを同時に供給することができる。よって、和紙調シュリンクラベルの製造コストを低減することができる。更に、和紙調シュリンクラベルを連続体とすることにより、必要時に必要な数(または長さ)の和紙調シュリンクラベルを連続体から順次切り出して使用することができる。   The continuous body of a Japanese paper-like shrink label can be easily manufactured using a long and belt-like laminated sheet 10 as a raw material. Moreover, according to a continuous body, a Japanese paper-style shrink label required for many cylindrical containers can be supplied simultaneously. Therefore, the manufacturing cost of a Japanese paper-like shrink label can be reduced. Furthermore, by using a Japanese paper-like shrink label as a continuous body, a necessary number (or length) of Japanese paper-like shrink labels can be cut out from the continuous body and used when necessary.

図12に示すように、和紙調シュリンクラベルの連続体20Bは、ロール状に捲回することができるため、輸送、管理、保存および取り扱いに便利である。また、取り扱いが容易であることから、連続して多数の筒状容器に和紙調シュリンクラベルを装着する際の作業効率も向上する。   As shown in FIG. 12, since the continuous body 20B of a Japanese paper-like shrink label can be wound in a roll shape, it is convenient for transportation, management, storage and handling. In addition, since the handling is easy, the working efficiency is improved when the Japanese paper-style shrink labels are continuously attached to a large number of cylindrical containers.

図12では、ロール状に捲回された連続体20Bから、和紙調シュリンクラベルが一枚のシート状物として捲き出され、所定の長さで切り出される((a))。次に、和紙調シュリンクラベルが一枚のシート状から筒状に形成され((b))、筒状容器に装着される((c))。その後、和紙調シュリンクラベルに含まれる熱収縮性フィルムを収縮させることで、筒状容器に和紙調の装飾が施される((d))。このような一連の工程は、ライン状の装置を用いて、連続的に、筒状容器に和紙調シュリンクラベルの装飾を施すのに適している。   In FIG. 12, a Japanese paper-like shrink label is rolled out as a single sheet from the continuous body 20B wound in a roll shape, and is cut out to a predetermined length ((a)). Next, a Japanese paper-like shrink label is formed from a single sheet shape into a cylindrical shape ((b)) and attached to the cylindrical container ((c)). Thereafter, the heat-shrinkable film contained in the Japanese paper-style shrink label is shrunk to give Japanese-style decoration to the cylindrical container ((d)). Such a series of processes is suitable for continuously decorating a Japanese paper-like shrink label on a cylindrical container using a line-shaped device.

本発明の筒状容器装飾用の和紙調シュリンクラベルは、筒状容器の内容物に関わらず、様々な筒状容器に適用することができるが、特に、日本酒(清酒)、焼酎などの酒類を収容する筒状容器を装飾するのに適している。   The Japanese paper-like shrink label for decorating a cylindrical container of the present invention can be applied to various cylindrical containers regardless of the contents of the cylindrical container, and in particular, alcoholic beverages such as Japanese sake (sake) and shochu. It is suitable for decorating the cylindrical container to be accommodated.

10:積層シート、11:熱収縮性フィルム、12:装飾層、13:第一粘着層、14:レーヨン紙等、15:印刷層、16:第一端部、16a:第一接合代、17:第二端部、17a:第二接合代、18:第三端部、19:第四端部、20,20A:和紙調シュリンクラベル、20B:和紙調シュリンクラベルの連続体、21:第二粘着層、22:第一折り目、23:第二折り目、24:破断予定部、25,26:筒状容器   10: laminated sheet, 11: heat-shrinkable film, 12: decorative layer, 13: first adhesive layer, 14: rayon paper, 15: printed layer, 16: first end, 16a: first joining margin, 17 : Second end portion, 17a: second joining margin, 18: third end portion, 19: fourth end portion, 20, 20A: Japanese paper-like shrink label, 20B: continuum of Japanese paper-like shrink label, 21: second Adhesive layer, 22: first fold, 23: second fold, 24: part to be broken, 25, 26: cylindrical container

Claims (6)

熱収縮性フィルムと、前記熱収縮性フィルムの一方の面を被覆する装飾層と、前記熱収縮性フィルムと前記装飾層との間に介在する第一粘着層とを有し、互いに対向する第一端部および第二端部を有する形状の積層シートと、
前記熱収縮フィルムの前記第一端部に対応する部分に設けられた第一接合代と、前記装飾層の前記第二端部に対応する部分に設けられた第二接合代との間に介在し、前記装飾層が外側になるように前記第一接合代と前記第二接合代とを接合する第二粘着層と、を具備し、
前記装飾層が、レーヨン紙(雲龍紙を除く)の層を含み、
前記レーヨン紙の坪量は、8〜40g/m2 であり、
前記第一端部と前記第二端部との重なりの幅Wは、5〜20mmである、筒状容器装飾用の和紙調シュリンクラベル。
A heat-shrinkable film, a decorative layer covering one surface of the heat-shrinkable film, and a first adhesive layer interposed between the heat-shrinkable film and the decorative layer and facing each other. A laminated sheet having a shape having one end and a second end;
It is interposed between a first joining margin provided at a portion corresponding to the first end portion of the heat shrink film and a second joining margin provided at a portion corresponding to the second end portion of the decorative layer. And a second adhesive layer that joins the first joining allowance and the second joining allowance so that the decorative layer is on the outside ,
The decorative layer includes a layer of rayon paper (excluding Yunlong paper),
The basis weight of the rayon paper is 8 to 40 g / m 2 ,
The width W of the overlap between the first end and the second end is 5 to 20 mm, and is a Japanese paper-like shrink label for decorating a cylindrical container.
前記装飾層は、前記レーヨン紙の前記第一粘着層側とは反対側の表面に形成された印刷層を含む、請求項1に記載の筒状容器装飾用の和紙調シュリンクラベル。   2. The Japanese paper-like shrink label for decorating cylindrical containers according to claim 1, wherein the decorative layer includes a printed layer formed on a surface of the rayon paper opposite to the first adhesive layer side. 前記積層シートが、前記第一端部と平行であり、かつ前記第二端部よりも前記第一端部に近い位置に形成された第一折り目と、前記第二端部と平行であり、かつ前記第一端部よりも前記第二端部に近い位置に形成された第二折り目とを有し、
前記積層シートが、前記第一折り目において、前記装飾層が外側になるように2つ折りにされ、かつ前記第二折り目において、前記装飾層が外側になるように2つ折りにされることにより、前記第一接合代と前記第二接合代との重なりが形成される、請求項1または2に記載の筒状容器装飾用の和紙調シュリンクラベル。
The laminated sheet is parallel to the first end, and is formed in a position closer to the first end than the second end, and parallel to the second end, And a second fold formed at a position closer to the second end than the first end,
In the first fold, the laminated sheet is folded in two so that the decorative layer is on the outside, and in the second fold, the laminated sheet is folded in two so that the decorative layer is on the outside. The Japanese paper-like shrink label for decorating a cylindrical container according to claim 1 or 2, wherein an overlap between the first joining allowance and the second joining allowance is formed.
前記第二端部と前記第二折り目との間のみに形成された、相対的強度の小さい破断予定部を有する、請求項3に記載の筒状容器装飾用の和紙調シュリンクラベル。   The Japanese paper-like shrink label for decorating a cylindrical container according to claim 3, further comprising a portion to be ruptured that is formed only between the second end portion and the second fold line and has a relatively low strength. 長尺の帯状形状を有し、
前記第一端部および前記第二端部が、前記帯状形状の長手方向に平行である、請求項1〜4のいずれか1項に記載の筒状容器装飾用の和紙調シュリンクラベルの連続体。
Has a long strip shape,
The continuous body of the Japanese paper-like shrink label for cylindrical container decoration of any one of Claims 1-4 whose said 1st end part and said 2nd end part are parallel to the longitudinal direction of the said strip | belt shape. .
前記帯状形状の長手方向が、捲回方向と平行になるようにロール状に捲回された、請求項5に記載の筒状容器装飾用の和紙調シュリンクラベルの連続体。   The continuous body of Japanese paper-style shrink labels for decorating a cylindrical container according to claim 5, wherein the longitudinal direction of the belt-like shape is wound in a roll shape so as to be parallel to the winding direction.
JP2013189718A 2013-09-12 2013-09-12 Washi-style shrink label for decoration of cylindrical containers and its continuum Active JP6371506B2 (en)