JP5695618B2 - Equipment for plating articles - Google Patents

Equipment for plating articles Download PDF

Info

Publication number
JP5695618B2
JP5695618B2 JP2012202956A JP2012202956A JP5695618B2 JP 5695618 B2 JP5695618 B2 JP 5695618B2 JP 2012202956 A JP2012202956 A JP 2012202956A JP 2012202956 A JP2012202956 A JP 2012202956A JP 5695618 B2 JP5695618 B2 JP 5695618B2
Authority
JP
Japan
Prior art keywords
anode
piston
plating
article
central axis
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP2012202956A
Other languages
Japanese (ja)
Other versions
JP2012246573A (en
Inventor
トス,ジェイムズ・アール
アゼベド,ミゲール
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Federal Mogul LLC
Original Assignee
Federal Mogul LLC
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Federal Mogul LLC filed Critical Federal Mogul LLC
Priority to JP2012202956A priority Critical patent/JP5695618B2/en
Publication of JP2012246573A publication Critical patent/JP2012246573A/en
Application granted granted Critical
Publication of JP5695618B2 publication Critical patent/JP5695618B2/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本願は、2005年7月26日付米国仮出願第60/702,483号の権利を主張し、ここにその全体を引用によって援用する。   This application claims the rights of US Provisional Application No. 60 / 702,483, Jul. 26, 2005, which is hereby incorporated by reference in its entirety.

発明の背景
1.技術分野
本発明は概して、物品、たとえば限定はしないが燃焼機関用ピストンをめっきするための方法および装置に関する。
Background of the Invention TECHNICAL FIELD The present invention relates generally to methods and apparatus for plating articles, such as but not limited to combustion engine pistons.

2.関連技術
めっき槽に物品を浸漬して、アノード/カソード配置を設けることによって物品をめっきし、それにより物品の1つ以上の面を電解槽溶液の材料でめっきすることが知られている。たとえば、一部の物品は、この一般的な技術を用いてクロムでめっきされる。
2. Related Art It is known to plate an article by immersing the article in a plating bath and providing an anode / cathode arrangement, thereby plating one or more sides of the article with the material of the electrolytic cell solution. For example, some articles are plated with chromium using this general technique.

起伏した表面および/または鋭角を有する物品をめっきする際に生じる課題の1つは、物品の形状がコーティングの均一な発現を妨げ、所望される以上にコーティングされる部分と、所望されるほどコーティングされない部分とが生じ得る点である。   One of the challenges that arises when plating articles with undulating surfaces and / or sharp angles is that the shape of the article prevents the uniform appearance of the coating, and the more coated parts are desired and the more coatings are desired. This is a point that may occur.

発明の概要
本発明は、めっき槽からのコーティングで物品をめっきするための装置および方法、たとえばクロムベースのコーティングをピストンの表面に塗布することに関する。当該装置は、物品の外側輪郭形状の少なくとも一部に輪郭を合わせた成形アノードを含む。物品自体がカソードとなり、カソードおよびアノードをめっき中に互いに対して移動させ、物品に対するめっきの塗布を制御する。
SUMMARY OF THE INVENTION The present invention relates to an apparatus and method for plating articles with a coating from a plating bath, such as applying a chromium-based coating to the surface of a piston. The apparatus includes a molded anode contoured to at least a portion of the outer contour shape of the article. The article itself becomes the cathode and moves the cathode and anode relative to each other during plating to control the application of plating to the article.

特定の実施形態によれば、成形アノードは静止して保持され、ピストンは成形アノードに対してめっき槽内で回転される。この相対的な移動、特に相対的な回転移動によって、コーティングが必要なピストンの所望の領域へのコーティングの塗布をより良く制御することができる。この点に関し、本発明は、アノードの形状を固定することができ、かつ物品がアノードに対して回転して、めっき中に物品とアノードの輪郭との間に一定の間隔を維持するような回転対称性を有する物品に特に良く適する。この点に関し、ピストンの外側面と、環状溝と、上面と、多くの場合燃焼ボウルとを含む特徴のうちの多くがピストン本体の中心長手軸に対する対称性、または少なくともおおよその対称性を有する点で、ピストンが特に良く適する。   According to a particular embodiment, the shaped anode is held stationary and the piston is rotated in the plating tank relative to the shaped anode. This relative movement, in particular relative rotational movement, allows better control of the application of the coating to the desired area of the piston that requires coating. In this regard, the present invention is such that the anode shape can be fixed and the article rotates relative to the anode to maintain a constant spacing between the article and the anode profile during plating. Particularly well suited for articles having symmetry. In this regard, many of the features, including the outer surface of the piston, the annular groove, the upper surface, and often the combustion bowl, have symmetry with respect to the central longitudinal axis of the piston body, or at least approximate symmetry. The piston is particularly well suited.

ピストンのコーティングに関して、外側面がコーティングされるだけでなく、上側環状溝の表面、上面および燃焼ボウルもコーティングされる利点がある。一部のピストン構造では、燃焼ボウルがボウルの外周上側リップをアンダーカットするように、燃焼ボウルは凹状のボウル構造を有しているため、従来のめっき槽装置では、これらの領域をめっきするのは特に困難である。本発明は、上側環状溝の場合は、アノードの一部分を環状溝内に延在させ、アノードを上面を横切って燃焼ボウルに入るように、かつ必要であれば燃焼ボウルの凹状の構成を含むように成形することによって、このような難しい輪郭に対応することができる。したがって、成形アノードに関連付けられた所望の領域においてめっき材料を均一に堆積させるために、ピストンの長手軸を中心にアノードに対してピストンが回転するにつれて、めっき処理中に所望量のコーティングが所望通りに表面に塗布される。   With regard to the coating of the piston, there is the advantage that not only the outer surface is coated, but also the surface, upper surface and combustion bowl of the upper annular groove are coated. In some piston structures, the combustion bowl has a concave bowl structure so that the combustion bowl undercuts the upper lip of the outer periphery of the bowl, so conventional plating bath equipment will plate these areas. Is particularly difficult. The present invention, in the case of the upper annular groove, extends a portion of the anode into the annular groove so that the anode crosses the top surface and enters the combustion bowl and, if necessary, includes a concave configuration of the combustion bowl. It is possible to cope with such a difficult contour by forming the material into a shape. Therefore, as the piston rotates relative to the anode about the longitudinal axis of the piston to deposit the plating material uniformly in the desired area associated with the molded anode, the desired amount of coating is as desired during the plating process. Applied to the surface.

発明のさらなる特定の特徴によれば、当該装置および方法は、めっきされる物品に対して静止し、かつ第1のアノードに対して移動可能な少なくとも第2のアノードを任意に含み得る。好ましい一配置では、この第2のアノードは、第1の固定アノードによって接近不可能なまたは接近しにくい物品の他の領域を同時にめっきするために第1のアノードに対して物品とともに回転するように設計される。たとえば物品は、物品の外側から接近不可能な内部構成または通路(たとえば、通路もしくはボアまたは非円形特徴)を有し得る。ピストンの場合、たとえばめっき槽からピンボアをめっきすることが望ましい場合がある。ピン成形アノードがピンボア内に位置決めされ、ピストンの長手軸を中心にピストンとともに回転するように支持され、関連する整流器に連結されて、制御されためっきをピンボアの表面に与え得る。これは、回転するように固定された第1のアノードに対して回転するにつれてピストンの外側面がめっきされるのと同時に行われ得る。この装置および方法によれば、1つの処理工程ですべての所望の表面において所望の軟度および均一性のめっきを実現するように、第1のアノードによってピストンのピストンスカート、上部環状溝および燃焼ボウルをコーティングしつつ、同じめっき槽において同時に第2のアノードによってピンボアもめっきすることが可能となる。   According to further particular features of the invention, the apparatus and method may optionally include at least a second anode that is stationary relative to the article to be plated and movable relative to the first anode. In a preferred arrangement, the second anode rotates with the article relative to the first anode to simultaneously plate other areas of the article that are inaccessible or inaccessible by the first stationary anode. Designed. For example, the article may have an internal configuration or passage (eg, a passage or bore or non-circular feature) that is inaccessible from the outside of the article. In the case of a piston, it may be desirable to plate the pin bore from a plating bath, for example. A pin-formed anode may be positioned within the pin bore, supported to rotate with the piston about the longitudinal axis of the piston, and coupled to an associated rectifier to provide controlled plating to the surface of the pin bore. This can be done at the same time as the outer surface of the piston is plated as it rotates relative to the first anode fixed for rotation. According to this apparatus and method, the piston skirt, upper annular groove and combustion bowl of the piston are provided by the first anode so as to achieve the desired softness and uniformity plating on all desired surfaces in one processing step. It is possible to plate the pin bore by the second anode at the same time in the same plating tank.

図面の簡単な説明
本発明のこれらおよび他の特徴および利点は、以下の詳細な実施形態の説明および最良の形態、添付の請求項ならびに添付の図面を参照して考慮すると、より容易に理解されるであろう。
BRIEF DESCRIPTION OF THE DRAWINGS These and other features and advantages of the present invention will be more readily understood upon consideration of the following detailed description of the embodiments and best mode, the appended claims and the accompanying drawings. It will be.

本方法によってめっきされた物品の斜視図である。1 is a perspective view of an article plated by the method. めっき装置に関連付けて示された物品の概略断面図である。It is a schematic sectional drawing of the articles | goods shown in relation with the plating apparatus. 物品の中心軸を中心に90°回転させた、図2と同様の図である。FIG. 3 is a view similar to FIG. 2, rotated 90 ° around the central axis of the article.

好ましい実施形態の詳細な説明
本発明は、適合可能なアノードをめっき処理において利用して、めっき材料を物品に塗布する方法および装置を提供する。アノードに適切なワイヤまたは他の材料が、物品のコーティングされる領域のおおよその形状に適合するように成形される。アノードは、電源、たとえば整流器によって駆動され、物品はカソードとして機能し、アノードおよび物品が両方ともめっき槽に浸漬される。浸漬されている間、アノードと物品との間に相対的な移動が与えられる。ここで好ましい1つの実施形態では、物品は、物品の中心軸を中心にアノードに対して回転され、アノードは中心軸を中心に回転しないように固定され得る。アノードと物品との間の相対的な移動の結果、アノードの傍を通過する物品の領域に均一なめっきが塗布され、それによって、所望であれば物品の360°めっきが行われる。
Detailed Description of the Preferred Embodiments The present invention provides a method and apparatus for applying a plating material to an article utilizing a compatible anode in a plating process. A wire or other material suitable for the anode is shaped to conform to the approximate shape of the coated area of the article. The anode is driven by a power source, such as a rectifier, the article functions as a cathode, and both the anode and article are immersed in the plating bath. While immersed, a relative movement is provided between the anode and the article. In one preferred embodiment herein, the article can be rotated relative to the anode about the central axis of the article, and the anode can be fixed so as not to rotate about the central axis. As a result of the relative movement between the anode and the article, a uniform plating is applied to the area of the article that passes by the anode, thereby providing a 360 ° plating of the article if desired.

当該方法および装置は、物品に対して位置が固定され(したがって、他の形状のアノードに対して相対的に移動可能であって、他の形状のアノードによって接近不可能な、または従来コーティングしにくかった物品の他の領域をめっきし)得る1つ以上の追加的なアノードも含み得る。たとえば、物品の回転軸を横切って設けられたボアを物品が有する場合、当該装置および方法は、対応する形状のアノードをボアに挿入することを意図する。アノードは、成形アノードに関連して他の面がめっきされるのと同じ槽において同時にボアの表面がめっきされるように、物品とともに回転することができる。   The method and apparatus are fixed in position relative to the article (and are therefore movable relative to other shaped anodes and are not accessible by other shaped anodes or are conventionally difficult to coat). It may also include one or more additional anodes that may be plated on other areas of the article. For example, if the article has a bore provided across the axis of rotation of the article, the apparatus and method intends to insert a correspondingly shaped anode into the bore. The anode can be rotated with the article so that the surface of the bore is simultaneously plated in the same bath where the other surface is plated in connection with the shaped anode.

図面を参照し、例として、限定はしないが、図1から図3は、めっきされる物品として以下にピストンと称するピストン物品10を示す。ピストン10は、燃焼ボウル16が形成される中心軸22に対してほぼ垂直に延在する上側面14を有するピストンヘッド12を含む。燃焼ボウル16は、エッジまたはリップ18と、リップ18から径方向外方に延在するアンダーカット領域20とを有し得る。ピストン10は中心長手軸22を有し、ピストンのさまざまな外側面が長手軸を中心に少なくとも部分的に対称的に延在する。ピストン10は、1対の水平方向に離間されたピンボス24も含み、そこに、共通ピンボア軸28を有する整列されたピンボア26が形成される。ピンボア軸28は中心軸22を横切って延在し、中心軸22に対して垂直であり得る。ピストン10は、ピンボス24と一体として形成され、外側面32を有する1対の対向するピストンスカート部分30をさらに含み得る。ピストンヘッド12は複数の環状溝を伴って形成され、ピストン物品10の上側面14に最も近い上側環状溝34を含む。   Referring to the drawings, by way of example and not limitation, FIGS. 1-3 show a piston article 10, hereinafter referred to as a piston, as the article to be plated. The piston 10 includes a piston head 12 having an upper side 14 that extends substantially perpendicular to a central axis 22 in which a combustion bowl 16 is formed. The combustion bowl 16 may have an edge or lip 18 and an undercut region 20 that extends radially outward from the lip 18. The piston 10 has a central longitudinal axis 22 and the various outer surfaces of the piston extend at least partially symmetrically about the longitudinal axis. The piston 10 also includes a pair of horizontally spaced pin bosses 24 in which an aligned pin bore 26 having a common pin bore shaft 28 is formed. The pin bore axis 28 extends across the central axis 22 and may be perpendicular to the central axis 22. The piston 10 may further include a pair of opposing piston skirt portions 30 formed integrally with the pin boss 24 and having an outer surface 32. The piston head 12 is formed with a plurality of annular grooves and includes an upper annular groove 34 that is closest to the upper side 14 of the piston article 10.

図2および図3は、めっき装置36と併せてピストン10を示す。装置36は好ましくは、ピストン10が浸漬され得る選択的めっき溶液のめっき槽38(たとえばクロミウムベースのコーティングを生成するもの等)を含む。装置36は第1の成形アノード40を含み、アノードとして機能し得るワイヤまたは他の適切な材料の形態であり得る。アノード40はピストン10の外側に沿って設けられ、ピストン10の外側面の全領域よりも領域が小さい。アノード40は、めっきされる表面についてアノード40に与えられるピストンの長手方向断面に関するピストンの外側面の概略形状に対応する形状を有するように形成される。したがって、軸方向断面において幾何学的に不連続な形状を有する領域、たとえば直線的な表面から非直線的および/または曲線をなす表面に移行する表面上でも、アノード40は当該表面の起伏に従うように適合する。これは、さまざまな環状溝およびアンダーカット領域20にわたって均一なコーティングを塗布できるようにするために特に重要である。   2 and 3 show the piston 10 together with the plating device 36. The apparatus 36 preferably includes a plating bath 38 of a selective plating solution in which the piston 10 can be immersed (such as one that produces a chromium-based coating). Device 36 includes a first shaped anode 40 and may be in the form of a wire or other suitable material that can function as the anode. The anode 40 is provided along the outside of the piston 10 and has a smaller area than the entire area of the outer surface of the piston 10. The anode 40 is formed to have a shape that corresponds to the approximate shape of the outer surface of the piston with respect to the longitudinal cross-section of the piston provided to the anode 40 for the surface to be plated. Thus, even on regions having geometrically discontinuous shapes in the axial cross-section, such as surfaces that transition from a linear surface to a non-linear and / or curved surface, the anode 40 will follow the undulations of that surface. Fits. This is particularly important so that a uniform coating can be applied across the various annular grooves and undercut regions 20.

たとえば、図1から図3に示すピストン10の例に関して、成形アノード40は、スカート部分30の外側面32と、上側環状溝34と、好ましくは燃焼ボウル16の全面とにおいてめっきを発現させるために、ピストン10の形状に相関して構成される。このため、成形アノード40は、中心軸22に対して概ね平行な長手方向に、かつピストン12のヘッドに沿ったスカート部分30の外側面32に隣接するピストン10の外側面に沿って、少なくとも部分的に延在する。アノード40は、中心軸22に対して概ね垂直な上側環状溝34内に延在する部分42を有するものとして示され、ピストン10の上側面14を包囲し、燃焼ボウル16内に下降する部分も有する。アノード40の燃焼ボウル内の部分はアンダーカット領域20の輪郭に従い、中心長手軸22において終端し得る。したがって、アンダーカット領域20を、所望通り均一な厚さのコーティング材料でめっきすることができる。隣接する表面からアノード40が離間される距離は、高精度で制御できることが望ましい。したがって、ピストン物品10をアノード40に対して(またはその逆に)回転させると、相対的な移動によって、コーティングしたいピストン10の領域の外側面全体が、成形アノードに対して露出する。換言すれば、各回転ごとに、固定された成形アノード40の傍を外側面が通過する。   For example, with respect to the piston 10 example shown in FIGS. 1-3, the molded anode 40 is used to develop plating on the outer surface 32 of the skirt portion 30, the upper annular groove 34, and preferably the entire surface of the combustion bowl 16. , In relation to the shape of the piston 10. Thus, the molded anode 40 is at least partially along the outer surface of the piston 10 adjacent to the outer surface 32 of the skirt portion 30 along a longitudinal direction generally parallel to the central axis 22 and along the head of the piston 12. Extended. The anode 40 is shown as having a portion 42 that extends into an upper annular groove 34 that is generally perpendicular to the central axis 22, and also surrounds the upper side 14 of the piston 10 and also descends into the combustion bowl 16. Have. The portion of the anode 40 in the combustion bowl may follow the contour of the undercut region 20 and terminate at the central longitudinal axis 22. Thus, the undercut region 20 can be plated with a coating material having a uniform thickness as desired. It is desirable that the distance at which the anode 40 is separated from the adjacent surface can be controlled with high accuracy. Thus, when the piston article 10 is rotated relative to the anode 40 (or vice versa), the relative movement exposes the entire outer surface of the area of the piston 10 that is to be coated to the molded anode. In other words, the outer surface passes by the fixed shaped anode 40 for each rotation.

めっき処理において、成形アノード40は、対応する電源、たとえば整流器44に連結され、ピストン10は、アノード40に関連してカソードとなるように電気的に連結される。成形アノード40とともにめっき槽38に浸漬されたピストン10は、成形アノード40に対して回転され、上述のように、ピストン10の目的の領域上に、制御された厚さのめっき46を発現させる。もちろん、他の領域もコーティングされ得るが、成形アノードによって、これらの目的の領域が注意して制御されることが確実となる。   In the plating process, the molded anode 40 is connected to a corresponding power source, such as a rectifier 44, and the piston 10 is electrically connected to be a cathode relative to the anode 40. The piston 10 immersed in the plating bath 38 with the molded anode 40 is rotated relative to the molded anode 40 to develop a controlled thickness of plating 46 on the target area of the piston 10 as described above. Of course, other areas can be coated, but the shaped anode ensures that these areas of interest are carefully controlled.

ピンボア26の内径面48を槽38のめっき材料でコーティングすることがさらに望ましい場合がある。これは、以下でピンボアアノード50と称する別のアノードをピンボア26内に位置決めし、ピストン10に対してピンボアアノード50を相対的に固定して支持する一方、めっき処理中に長手中心軸22を中心に、したがって成形アノード40に対して、ピストン10と同時にピンボアアノード50を回転できるようにすることによって、外側面がコーティングされるのと同時に行なうことができる。ピンボアアノード50は、関連付けられた整流器52に連結され、その結果、めっき材料がピンボア面48に堆積される。他の整流器44とは別個のそれ自身の整流器52にピンボアアノード50を連結することにより、成形アノード40とは独立したピンボアアノード50の独立制御および対応するピンボア面48のめっきと、所望であれば上側面14、燃焼ボウル16、スカート部分30、1本以上の環状溝を含む他の表面の対応するめっきとが可能になる。   It may be further desirable to coat the inner diameter surface 48 of the pin bore 26 with the plating material of the bath 38. This positions another anode, hereinafter referred to as pin bore anode 50, within pin bore 26 and supports pin bore anode 50 relative to piston 10 relative to piston 10 while supporting longitudinal central axis 22 during the plating process. At the same time as the outer surface is coated by allowing the pin bore anode 50 to rotate simultaneously with the piston 10 relative to the molded anode 40. The pin bore anode 50 is coupled to an associated rectifier 52 so that plating material is deposited on the pin bore surface 48. By connecting the pin bore anode 50 to its own rectifier 52 separate from the other rectifiers 44, independent control of the pin bore anode 50 independent of the molded anode 40 and plating of the corresponding pin bore surface 48, as desired. If present, the upper side 14, combustion bowl 16, skirt portion 30, and corresponding plating of other surfaces including one or more annular grooves are possible.

したがって、本発明の一局面は、めっき処理、たとえば高強度(HD)鋼ピストンをコーティングするのに用いられるめっき処理でめっきされる表面の変動する幾何学的形状に適合可能なアノードの使用をもたらす。40で示すようなワイヤ、またはピストン上のめっきされる表面(スカート領域30からスカート領域上の環状領域から上側ボウル領域14まで)のおおよその形状に適合する他の予備成形アノード部材を利用して、注目する領域にコーティングを堆積させることができる。これは、整流器44などのめっき用電源によって駆動される。適合可能なアノード40を通過して回転し、その結果目的の領域上にコーティングを堆積させるように、ピストンアセンブリ全体がめっき槽38内で回転される。また、共通カソード接続が同じ鋼ピストン10である第2のアノード50が利用され、この第2の適合可能なアノード50がピンボア26内に配置され、その結果ピンボア26の内径面48上にコーティングを堆積させる。これは、上述のように整流器44とは別個の整流器52によって駆動される。   Accordingly, one aspect of the present invention results in the use of an anode that is adaptable to the varying geometry of the surface being plated in a plating process, such as the plating process used to coat a high strength (HD) steel piston. . Utilizing a wire as shown at 40 or other preformed anode member that conforms to the approximate shape of the surface to be plated on the piston (from the skirt region 30 to the annular region on the skirt region to the upper bowl region 14). , A coating can be deposited in the area of interest. This is driven by a plating power source such as a rectifier 44. The entire piston assembly is rotated in the plating bath 38 to rotate past the adaptable anode 40, thereby depositing the coating on the area of interest. Also, a second anode 50 is utilized in which the common cathode connection is the same steel piston 10 and this second adaptable anode 50 is disposed in the pin bore 26 so that a coating on the inner diameter surface 48 of the pin bore 26 is achieved. Deposit. This is driven by a rectifier 52 separate from the rectifier 44 as described above.

ピストン10の表面をめっきするために、適合可能なアノード40,50を使用することによって、所望の厚さでのコーティングが望まれる領域においてコーティングを堆積させることができる。ピストン10を回転させることによって、ピストン10の外周全体の周囲に均一に堆積させることができる。2つの別個の整流器44、52およびアノード40、50の使用によって(共通カソードはここではピストン10で示される)、1つの整流器/アノード構成ではコーティングすることができない領域に互いに別個にコーティングを堆積させることが可能となり、所望の厚さのめっき材料を必要な箇所に塗布することが可能となる。   By using compatible anodes 40, 50 to plate the surface of the piston 10, the coating can be deposited in areas where coating at the desired thickness is desired. By rotating the piston 10, it can be uniformly deposited around the entire outer periphery of the piston 10. By using two separate rectifiers 44, 52 and anodes 40, 50 (the common cathode is shown here as piston 10), coatings are deposited separately from each other in areas that cannot be coated with a single rectifier / anode configuration. It becomes possible, and it becomes possible to apply | coat the plating material of desired thickness to a required location.

ピストン10は、ホルダに嵌合するか、またはピストン10に対して共通カソード接続をなす部材によって他の方法で支持される適合可能なアノード40を通過して回転することができるように中心軸22を中心にピストン10を回転させるための機構としても機能する。ピンボア26は、ピンボア領域内に配置された円柱状アノード50によってめっきされ、上述のとおり第2の整流器52によって駆動される。これにより、めっきされる2つの別個の領域の各々について、適切なめっき密度および厚さの塗布が可能となる。したがって、1回のめっき処理において、別個のアノード40、50によってめっきされるピストン領域は、異なるめっき密度および厚さを有し得る。   The piston 10 can be rotated through the adaptable anode 40 that fits in the holder or otherwise supported by a member that makes a common cathode connection to the piston 10. It also functions as a mechanism for rotating the piston 10 around the center. The pin bore 26 is plated by a cylindrical anode 50 located in the pin bore region and is driven by the second rectifier 52 as described above. This allows application of the appropriate plating density and thickness for each of the two separate areas to be plated. Thus, in a single plating process, the piston areas plated by the separate anodes 40, 50 can have different plating densities and thicknesses.

明らかに、上記の教示に鑑みて、本発明の多くの修正および変更が可能である。したがって、添付の請求項の範囲内において具体的に記載した以外の方法で本発明を実施し得ると理解される。   Obviously, many modifications and variations of the present invention are possible in light of the above teachings. It is therefore to be understood that the invention may be practiced otherwise than as specifically described within the scope of the appended claims.

Claims (6)

カソードとして機能するピストンの表面をめっきするための装置であって、前記表面は前記ピストンの中心軸を中心に少なくとも部分的に対称的に延在し、かつ軸方向断面において起伏を有する部分を含み、
めっき材料を内部に有するめっき槽と、
電源と、
前記電源と電気的に連通する第1のアノードとを備え、前記第1のアノードは、前記ピストンの一部分の前記起伏にほぼ適合する形状を有し、
前記第1のアノードによってめっきされる部分とは別の部分をめっきするための第2のアノードをさらに備え、
前記第1のアノードは前記めっき槽に対して静止したままであり、前記第2のアノードは、前記ピストンの中心軸に対する動きのために回転可能に支持される、装置。
An apparatus for plating a surface of a piston that functions as a cathode, the surface including a portion extending at least partially symmetrically about a central axis of the piston and having undulations in an axial cross section ,
A plating tank having a plating material therein;
Power supply,
A first anode in electrical communication with the power source, the first anode having a shape that substantially conforms to the relief of a portion of the piston;
A second anode for plating a portion different from the portion to be plated by the first anode;
The apparatus wherein the first anode remains stationary with respect to the plating bath and the second anode is rotatably supported for movement relative to the central axis of the piston.
前記第1のアノードは、前記ピストンの燃焼ボウルをめっきするように設けられ、前記第2のアノードは、前記ピストンの1対のピンボアを同時にめっきするように設けられる、請求項1に記載の装置。   The apparatus of claim 1, wherein the first anode is provided to plate a combustion bowl of the piston and the second anode is provided to plate a pair of pin bores of the piston simultaneously. . 前記第1のアノードは、前記中心軸に対して部分的に概ね平行に延在し、前記第2のアノードは、中心軸に対して概ね垂直に延在する、請求項1に記載の装置。   The apparatus of claim 1, wherein the first anode extends partially generally parallel to the central axis, and the second anode extends generally perpendicular to the central axis. 前記第1のアノードの少なくとも一部分は、前記中心軸に対して概ね垂直に延在する、請求項3に記載の装置。   The apparatus of claim 3, wherein at least a portion of the first anode extends generally perpendicular to the central axis. 前記第1のアノードはワイヤである、請求項1に記載の装置。   The apparatus of claim 1, wherein the first anode is a wire. 前記第1のアノードとは別個の前記第2のアノードと電気的に連通する別の電源をさらに備える、請求項1に記載の装置。   The apparatus of claim 1, further comprising another power source in electrical communication with the second anode separate from the first anode.
JP2012202956A 2012-09-14 2012-09-14 Equipment for plating articles Expired - Fee Related JP5695618B2 (en)