JP4892916B2 - Thin glass folding device and folding method - Google Patents

Thin glass folding device and folding method Download PDF

Info

Publication number
JP4892916B2
JP4892916B2 JP2005291624A JP2005291624A JP4892916B2 JP 4892916 B2 JP4892916 B2 JP 4892916B2 JP 2005291624 A JP2005291624 A JP 2005291624A JP 2005291624 A JP2005291624 A JP 2005291624A JP 4892916 B2 JP4892916 B2 JP 4892916B2
Authority
JP
Japan
Prior art keywords
thin glass
line
glass plate
bar
folding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP2005291624A
Other languages
Japanese (ja)
Other versions
JP2007099563A (en
Inventor
和彦 真鍋
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Central Glass Co Ltd
Original Assignee
Central Glass Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Central Glass Co Ltd filed Critical Central Glass Co Ltd
Priority to JP2005291624A priority Critical patent/JP4892916B2/en
Priority to KR1020060096846A priority patent/KR101129830B1/en
Publication of JP2007099563A publication Critical patent/JP2007099563A/en
Application granted granted Critical
Publication of JP4892916B2 publication Critical patent/JP4892916B2/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、フラットパネルディスプレイ等で使用する薄板ガラスの折割装置および折割方法であって、特に幅狭な耳部をクリーンでキズをつけない折割装置および折割方法に関する。   The present invention relates to a folding device and a folding method for thin glass used in a flat panel display or the like, and more particularly to a folding device and a folding method in which a narrow ear portion is clean and not scratched.

ガラス板を切筋線に沿って折割する方法や装置は、従来より知られている。特に、液晶ディスプレイ、プラズマディスプレイ、有機ELディスプレイ等のフラットパネルディスプレイで使用するガラス板については、折り口の端面をクリーンとし、また端縁部にキズを発生させないようにして折り割る必要がある。   A method and an apparatus for breaking a glass plate along a score line are conventionally known. In particular, for glass plates used in flat panel displays such as liquid crystal displays, plasma displays, and organic EL displays, it is necessary to fold them so that the end surfaces of the folds are clean and scratches are not generated at the edges.

例えば特開昭53−88817号の公報には、板ガラスにダイヤモンドあるいは超硬合金製チップで切筋線を付与した短冊材の四隅を押え片で押さえると共に、その一対の押え片に押え角を与えて前記短冊材を押えこみ、ベンデングを起こさせると共に前記押え片の近傍に浮上する浮上棒を配設して、クラックを起生促進せしめるクラック促進の方法が開示されている(特許文献1)。   For example, in Japanese Patent Application Laid-Open No. 53-88817, the four corners of a strip material in which a cut line is given to a plate glass with a diamond or cemented carbide tip are pressed with a presser piece, and a presser angle is given to the pair of presser pieces. A method of promoting cracks is disclosed in which the strip material is pressed down to cause bending and a floating bar that floats in the vicinity of the presser piece is disposed to promote the initiation of cracks (Patent Document 1).

また、特開平5−132328号公報には、ガラス板の切筋線を上流側搬送ベルトと下流側搬送ベルト間の所定位置に位置決めして、各々の挟持部がガラス板の切筋線の両側を挟持し、一方の挟持部が上流または下流の搬送ベルトの回動に追従し回動し、回動と同時に上流または下流の搬送ベルトが互いに引き離されるガラス板の切断方法とその装置が開示されている(特許文献2)。   Japanese Patent Laid-Open No. 5-132328 discloses that the scoring line of the glass plate is positioned at a predetermined position between the upstream conveying belt and the downstream conveying belt, and each sandwiching portion is on both sides of the scoring line of the glass plate. Disclosed is a method and apparatus for cutting a glass plate in which one clamping part rotates following and follows the rotation of an upstream or downstream conveyor belt, and at the same time the upstream or downstream conveyor belt is separated from each other. (Patent Document 2).

また、特開平7−237929公報には、薄板ガラスの上面に切筋線を付与した端縁をテーブルの端縁より突出し、該切筋線の両脇を挟持して曲げモーメントを付与する薄板ガラスの折割方法において、前記テーブル上で前記薄板ガラスを前記切筋線に平行に押圧固定し、該切筋線と一致しかつ反テーブル側の突出した前記薄板ガラスの下面端縁を前記テーブル上より上昇せしめ、該薄板ガラスの前記切筋線からの端縁を挟持圧接するようにした薄板ガラスの折割方法が開示されている(特許文献3)。   Japanese Patent Laid-Open No. 7-237929 discloses a thin glass plate in which an edge having a score line provided on the upper surface of a thin glass plate protrudes from an edge of the table and a bending moment is applied by sandwiching both sides of the score line. The sheet glass is pressed and fixed on the table in parallel with the score line, and the lower edge of the sheet glass that is aligned with the score line and protrudes on the opposite side of the table is formed on the table. There is disclosed a method of folding a thin glass, which is further raised and the end edge of the thin glass from the score line is sandwiched and pressed (Patent Document 3).

また、特開平8−253336号公報には、薄板ガラスの上面に切筋線を付与した端縁を搬送コンベアの端部より突出させ、該切筋線に沿って薄板ガラスを折割切断する方法において、薄板ガラスの切筋線の斜め下方に位置し、下部昇降機構により切筋線に平行かつ、該切筋線より反端縁側を下部押圧部材により押圧支持と同時または時間遅れを持たせて、薄板ガラス端縁に付与した切筋線に平行で、かつ該切筋線の斜め上方より上部昇降機構により上部押圧部材を円弧状に下降させ、下降するに従って上部押圧部材が薄板ガラスの切筋線より端縁側を押圧するとともに端縁方向にモーメントを付加することで折割切断することを特徴とする薄板ガラスの折割方法が開示されている(特許文献4)。
特開昭53−88817号公報 特開平5−132328号公報 特開平7−237929公報 特開平8−253336公報
Japanese Patent Application Laid-Open No. 8-253336 discloses a method in which an edge having a score line provided on the upper surface of a thin glass plate is protruded from an end of a conveyor, and the thin glass is cut along the score line. In the sheet glass, it is located obliquely below the scoring line of the thin glass, parallel to the scoring line by the lower elevating mechanism, and at the same time as the pressing support by the lower pressing member on the opposite end side from the scoring line or with a time delay. The upper pressing member is lowered in an arc shape by the upper lifting mechanism parallel to the cutting line applied to the edge of the thin glass glass and obliquely above the cutting line, and the upper pressing member becomes the cutting line of the thin glass as it goes down. There is disclosed a method of folding a thin glass, characterized in that the glass sheet is cut by pressing the edge side from the wire and applying a moment in the edge direction (Patent Document 4).
JP-A-53-88817 JP-A-5-132328 JP-A-7-237929 JP-A-8-253336

前記特許文献1に記載されたベンディングを付与するものは、薄板ガラスにおいてはベンディング手段を手作業に因るところが多く、昨今の省力化には追従することができないという問題点がある。   The thing which gives the bending described in the said patent document 1 has a problem that there are many places which depend on a manual work for a bending means in thin glass, and cannot follow the labor saving of these days.

また、前記特許文献2に記載のものは、機械化されたものであるが、上下流側の搬送ベルト上にガラス板が位置するため、搬送ベルトの回動時に挟持部も同じように回動するが、回動力を付与するだけの大きな板幅を必要とし、耳部等の小幅な折割切断においては適さないものであった。   Moreover, although the thing of the said patent document 2 is mechanized, since a glass plate is located on the conveyance belt of an upstream / downstream side, when a conveyance belt rotates, a clamping part will also rotate similarly. However, it requires a large plate width for imparting a rotational force, and is not suitable for cutting a narrow fold such as an ear portion.

さらに、前記特許文献3に記載のものは、ガラス板の上面に設けた切筋線側の端部を固定具と昇降具間に挿入し、昇降具を切筋線の一端側から他端側にかけて順次上昇させるようにしたものであるが、ガラス板の耳部を固定具と昇降具の各板状部で挟んだ状態で折り割るのでせん断力が発生しクリーンにカットされない恐れがある。   Furthermore, the thing of the said patent document 3 inserts the edge part by the side of a cut line provided in the upper surface of the glass plate between a fixing tool and a lifting tool, and the lifting tool is inserted into the other end side from the one end side of a cutting line. However, since the glass plate is folded in a state where the ear portion of the glass plate is sandwiched between the plate-like portions of the fixture and the lifting tool, a shearing force may be generated and the glass plate may not be cut cleanly.

また、切筋線部分の停止位置がオーバーランして、固定具と昇降具間で停止した場合には、切筋線部分で折割ができなくなるという問題点があった。   In addition, when the stop position of the cut line portion is overrun and stopped between the fixture and the lifting tool, there is a problem that it is not possible to split the cut line portion.

さらにまた、前記特許文献4に記載のものは、下部押圧部材を切筋線の斜め下方より水平に一斉に上昇させるようにしたものであって、切筋線の一端から他端にかけてニューと呼ばれる割れ目を発生させるものではないため、上部押圧部材が切筋線の端縁寄りを下降させてガラス板を折り割ると、切り筋線全体に亘って一斉にニューが発生して、ガラス板の端面同士の接触によりクリーンカットできない恐れがあった。   Furthermore, the thing of the said patent document 4 is made to raise a lower press member all at once from diagonally downward of a score line, and is called new from one end of a score line to the other end. Because it does not generate a crack, when the upper pressing member lowers the edge of the scoring line and breaks the glass plate, a new material is generated all at once across the scoring line, and the end surface of the glass plate There was a possibility that clean cut could not be done due to contact between each other.

また、ガラス板の折割後、下部押圧部材の上面に付着した切り粉を回転ブラシで除去する手段が設けられているが、除去ブラシはガラス板の上部側にあって、下部押圧部材はガラス板の下部にあるので、除去作業が終わらないとガラス板を搬送させることができず、処理タクトが遅くなるという問題点があった。   Further, after the glass plate is broken, there is provided means for removing the chips adhering to the upper surface of the lower pressing member with a rotating brush. The removing brush is on the upper side of the glass plate, and the lower pressing member is made of glass. Since it is in the lower part of the plate, the glass plate cannot be transported unless the removal operation is finished, and there is a problem that the processing tact time is delayed.

本発明はこのような点に鑑みてなされたものであり、簡易な構成で互いの折割端面同士が衝突するように当接することなく確実な折割とクリーンカットを目的とし、さらには、ガラス板の折割後に下部押圧バーの上面に切り粉が付着しても、簡単に除去できて、次のガラス板の折割時に悪影響を与えないようにするものである。   The present invention has been made in view of the above points, and aims at reliable folding and clean cutting without contact so that the folded end faces collide with each other with a simple configuration. Even if chips adhere to the upper surface of the lower pressing bar after the plate is broken, it can be easily removed so that no adverse effects are caused when the next glass plate is folded.

すなわち、本発明は、薄板ガラスの端縁に付与した切筋線に沿って薄板ガラスを折割切断する装置において、薄板ガラスの搬送停止を自在とする搬送コンベアからなる搬送手段と、
搬送コンベアの搬送方向先端部より突出した薄板ガラスの端縁の上面に付与した切筋線に平行、かつ上方にガラス板の全幅に亘って上部押圧バーを設け、該上部押圧バーを昇降させて切筋線より端縁側を下方に押圧させる上部押圧手段と、
前記薄板ガラスの切筋線の真下位置にガラス板の全幅に亘る長さの昇降自在な下部折割バーを設け、下部折割バーの上端部に断面円形状のベルトを張設し、下部折割バーの両端を別々の昇降手段で昇降自在に軸着させた下部押圧手段と、からなることを特徴とする薄板ガラスの折割装置である。
That is, the present invention is a device that breaks and cuts a thin glass sheet along a scoring line applied to an edge of the thin glass sheet.
An upper pressing bar is provided over the entire width of the glass plate in parallel with the scoring line provided on the upper surface of the edge of the thin glass protruding from the front end of the conveying conveyor, and the upper pressing bar is moved up and down. Upper pressing means for pressing the edge side downward from the score line;
A lower folding bar that can be raised and lowered over the entire width of the glass plate is provided at a position directly below the scoring line of the thin glass plate, and a belt having a circular cross section is stretched on the upper end of the lower folding bar. A sheet glass folding device comprising: a lower pressing means in which both ends of a split bar are pivotally attached to each other by separate lifting means.

あるいはまた、本発明は、前記の下部折割バーの上端面の中心線に沿って設けた断面円形の断面円形状のベルトをプーリーの回転により回転移動自在な無限ループとし、折割時にベルト上に付着した切粉を除去可能とするブラシをベルトの下部位置に配設したことを特徴とする上述の薄板ガラスの折割装置である。   Alternatively, in the present invention, a belt having a circular cross-section with a circular cross section provided along the center line of the upper end surface of the lower split bar is formed into an infinite loop that can be rotated and moved by rotation of a pulley. The above-described sheet glass folding device is characterized in that a brush capable of removing chips adhering to the belt is disposed at a lower position of the belt.

あるいはまた、本発明は、前記上部押圧バーの下面にゴムシートを貼着したことを特徴とする上述の薄板ガラスの折割装置である。   Alternatively, the present invention is the above-described sheet glass splitting device, wherein a rubber sheet is attached to the lower surface of the upper pressing bar.

あるいはまた、本発明は、搬送コンベア間に設けた前記下部押圧手段を挟むようにその上流側と下流側に合わせて2セットの上部押圧手段を前後対称位置に配設し、下流側の上部押圧手段と下部押圧手段でガラス板の先端側の切筋線を折割し、上流側の上部押圧手段と下部押圧手段でガラス板の後端側の切筋線を折割するようにしたことを特徴とする上述のいずれかに記載の薄板ガラスの折割装置である。   Alternatively, in the present invention, two sets of upper pressing means are arranged in the front-rear symmetrical position so as to sandwich the lower pressing means provided between the conveyors, on the upstream side and the downstream side. The cutting line on the tip side of the glass plate is broken by the means and the lower pressing means, and the cutting line on the rear end side of the glass plate is broken by the upper pressing means and the lower pressing means on the upstream side. A thin glass folding apparatus according to any one of the above-mentioned features.

あるいはまた、本発明は、搬送コンベア間に設けた前記上部押圧手段をガラス板の搬送方向に走行移動自在とする走行手段を設け、ガラス板の先端側の切筋線を折割する場合と、ガラス板の後端側の切筋線を折割する場合の上部押圧手段の位置を前記走行手段によって切り替えるようにしたことを特徴とする上述のいずれかに記載の薄板ガラスの折割装置である。   Alternatively, in the present invention, when the upper pressing means provided between the conveyors is provided with traveling means for allowing the upper pressing means to travel and move in the conveying direction of the glass plate, the cutting line on the tip side of the glass plate is broken, The sheet glass splitting device according to any one of the above, wherein the position of the upper pressing means when the scoring line on the rear end side of the glass plate is split is switched by the traveling means. .

あるいはまた、本発明は、前記のいずれかに記載の薄板ガラスの折割装置を用いたガラス板の折割方法において、端縁の上面、かつ平行に付与した切筋線を設けた薄板ガラスの端縁部を搬送コンベアの搬送方向先端部より突出させ、端縁側上方よりガラス板の端縁の全幅にわたる上部押圧バーを下降させて切筋線より端縁側の全幅に当接させ、
前記切筋線の真下位置に設けたガラス板の全幅に亘る長さの下部折割バーの上面中心に張設した断面円形状のベルトを前記切筋線に沿って、該切筋線の一端側から他端側に当接するように、下部折割バーの両端の昇降手を時間差を設けて順次上昇させるようにしてガラス板を切筋線に沿って折割るようにしたことを特徴とする薄板ガラスの折割方法である。
Alternatively, the present invention relates to a method for splitting a glass plate using the thin glass splitting device according to any one of the above, wherein the top surface of the edge and the thin glass plate provided with the parallel cut lines are provided. The end edge part protrudes from the conveyance direction front end part of the conveyer, the upper pressing bar over the entire width of the edge of the glass plate is lowered from the upper side of the edge side, and is brought into contact with the entire width on the edge side from the score line,
A belt having a circular cross-section stretched around the center of the upper surface of the lower folding bar having a length over the entire width of the glass plate provided immediately below the score line, along the score line, one end of the score line The glass plate is folded along the score line so that the raising and lowering hands at both ends of the lower folding bar are sequentially raised with a time difference so as to contact the other end side from the side. This is a method of folding thin glass.

あるいはまた、本発明は、前記下部折割バーの上端面に設けた無端の断面円形状のベルトを、ガラス板の折割直後毎に少なくとも1回転以上回転させ、該ベルトの下部位置に配設したブラシによって該ベルト上に付着した切粉を除去して、下部折割バーをガラス板面に押圧時にキズをつけないようにしたことを特徴とする上述の薄板ガラスの折割方法である。   Alternatively, according to the present invention, an endless cross-sectional belt provided on the upper end surface of the lower folding bar is rotated at least once or more immediately after the glass plate is broken, and disposed at a lower position of the belt. The above-mentioned method for folding thin glass is characterized in that chips adhering to the belt are removed by a brush and the lower folding bar is not scratched when pressed against the glass plate surface.

本発明は、薄板ガラスの折割装置および折割方法にあたり、簡易な構成で互いの折割端面が衝突するように当接することなく確実な折割とクリーンカットができ、さらには、ガラス板下面に当接する断面円形状のベルトを回転させながらブラシ等による切粉除去手段を設けたことで、ガラス板の折割後に該ベルトの上面に切り粉が付着しても、簡単に迅速に除去できて、次の薄板ガラスの折割時に薄板ガラスへのスリ傷等を与えないようにすることができ、生産歩留の向上を図ることができるものである。   The present invention relates to a sheet glass folding apparatus and method, and can be reliably broken and clean cut with a simple configuration without abutment so that each other's edge faces collide with each other. By providing a chip removal means with a brush or the like while rotating a belt with a circular cross section in contact with the belt, even if chips adhere to the upper surface of the belt after breaking the glass plate, it can be removed easily and quickly. As a result, it is possible to prevent the thin glass from being scratched when the next thin glass is folded, and to improve the production yield.

図3に示すように、本発明は、長方形状の薄板ガラス1の一辺または対向するニ辺の近傍で、該辺に平行に付与した切筋線2に沿って薄板ガラス1を折割る装置および方法であり、折割時の折割端面同士の接触によるキズや欠け等を発生させないクリーンな切断面を得られるようにした折割装置および方法である。   As shown in FIG. 3, the present invention is an apparatus that breaks the thin glass plate 1 along one of the sides of the rectangular thin glass plate 1 or in the vicinity of the opposite two sides, along the scoring line 2 provided in parallel with the side. This is a folding apparatus and method that can obtain a clean cut surface that does not cause scratches or chipping due to contact between the split end faces during splitting.

本発明の折割装置の構成は、図1に示すように、薄板ガラス1の搬送停止を自在とする搬送コンベア6からなる搬送手段5と、搬送コンベア6の搬送方向先端部より突出した薄板ガラス1の端縁の上面に付与した切筋線2に平行、かつ切筋線2より端縁側の上方に薄板ガラスの全幅にわたって当接可能な長尺の上部押圧バー12を設け、該上部押圧バー12を下降させて切筋線2より端縁側部分を下方に押圧させる上部押圧手段10と、前記薄板ガラス1の切筋線2の真下位置に薄板ガラス1の全幅に亘る長さの昇降自在な長尺の下部折割バー22を設け、下部折割バー22の上端部に前記切筋線2に当接する断面円形状のベルト31を張設し、下部折割バー22の両端の昇降高さに差を設けることを可能とするために両端を別々の昇降手段で昇降自在に軸着させた下部押圧手段20とからなる。   As shown in FIG. 1, the folding apparatus of the present invention is composed of a conveying means 5 including a conveying conveyor 6 that can freely stop the conveyance of the thin glass 1, and a thin glass that protrudes from the leading end of the conveying conveyor 6 in the conveying direction. A long upper pressing bar 12 that is parallel to the cut line 2 provided on the upper surface of one edge and that can be contacted over the entire width of the thin glass is provided above the cut line 2 and on the upper edge side. The upper pressing means 10 that lowers the edge 12 and presses the edge side portion downward from the score line 2 and the length of the entire sheet glass 1 can be raised and lowered directly below the score line 2 of the thin glass plate 1. A long lower split bar 22 is provided, and a belt 31 having a circular cross section that is in contact with the scoring line 2 is stretched at the upper end of the lower split bar 22, and the elevation height of both ends of the lower split bar 22 is extended. Separate lifting means at both ends to make it possible to make a difference in Liftably made from the lower pressing means 20. which is pivotally attached.

図1に示すように、前記の下部折割バー22の上端面の中心線に沿って設けたベルト31は断面円形状のゴム製であり、図2に示すように、下部折割バー22の長手方向の両外側に設けたプーリー32、32により回転移動自在な無限ループとなっており、片側のプーリー32の下部には前記ベルト31に当接する位置にブラシ33を設けて、折割時にベルト31上に付着した切粉を除去できる。   As shown in FIG. 1, the belt 31 provided along the center line of the upper end surface of the lower split bar 22 is made of rubber having a circular cross section, and as shown in FIG. It is an infinite loop that can be rotated and moved by pulleys 32, 32 provided on both outer sides in the longitudinal direction, and a brush 33 is provided at a position in contact with the belt 31 below the pulley 32 on one side, Chips adhering to 31 can be removed.

また、図1に示すように、薄板ガラス1の端面に上部押圧バー12を迅速に押圧した場合でも端面およびその近傍に無理な衝撃を与えないように、前記上部押圧バー12の下面にゴムシートを貼着し、クッションを持たせて薄板ガラス1の端面を押圧するようにした。   Further, as shown in FIG. 1, even when the upper pressing bar 12 is quickly pressed against the end surface of the thin glass plate 1, a rubber sheet is formed on the lower surface of the upper pressing bar 12 so as not to give an excessive impact to the end surface and the vicinity thereof. Was attached and a cushion was provided to press the end face of the thin glass plate 1.

前記薄板ガラス1は、フラットパネルディスプレイ等で使用する場合には、矩形状で通常、四辺の各辺に平行な切筋線2を設け、該切筋線2より端縁側部分(通称、耳部と呼ぶ)を順次折割して、切筋線2の内部だけを使用し、該耳部はガラス屑としてカレット化される。   When the thin glass 1 is used in a flat panel display or the like, it is rectangular and usually has cut lines 2 parallel to each side of the four sides, and an edge side portion (common name, ear part) from the cut lines 2. Are called in order, and only the inside of the cut line 2 is used, and the ears are culleted as glass waste.

本発明の折割装置は、薄板ガラス1の搬送方向の前端辺、又は後端辺の1辺だけ、または対向する前後の2辺を折り割ることができ、4辺の耳部を折り割る場合には、まず搬送方向の前後の2辺の耳部を折り割った後、90度方向変換して残りの2辺の耳部を折り割れば良い。   The folding device of the present invention can fold only one side of the front edge or the rear edge in the conveying direction of the thin glass plate 1 or two opposite front and back sides, and folds four ears. First, the two ears on the front and rear sides in the transport direction are folded, and then the direction is changed by 90 degrees and the remaining two ears are folded.

前記搬送手段5は、搬送ベルト式、あるいはローラー式の搬送コンベア6上に、予め位置決めされた薄板ガラス1を水平姿勢で載置し、搬送コンベア6上で蛇行やスリップ等を発生させずに位置決めされた姿勢を保ちながら前記薄板ガラス1が搬送できるものが望ましい。   The conveying means 5 places a thin glass plate 1 positioned in advance on a conveying belt 6 or roller-type conveying conveyor 6 in a horizontal position, and positions on the conveying conveyor 6 without causing meandering or slipping. What can convey the said sheet glass 1 is preferable, maintaining the attitude | position made.

また、薄板ガラス1の先端側の耳部を折り割る場合には、搬送コンベア6上には図示しない位置検出センサーが薄板ガラス1の先端位置を検出することにより薄板ガラス1の先端辺側の耳部(端縁側部分)が搬送コンベア6よりはみ出した状態で、切筋線2が下部折割バー22の断面円形状のベルト31の上部側位置で停止可能なものとする。   When the edge portion on the front end side of the thin glass 1 is folded, a position detection sensor (not shown) detects the front end position of the thin glass glass 1 on the conveyor 6 so that the ear on the front side of the thin glass glass 1 is detected. It is assumed that the scoring line 2 can be stopped at the upper side position of the belt 31 having a circular cross section of the lower folding bar 22 in a state where the portion (edge side portion) protrudes from the conveyor 6.

さらに、薄板ガラス1の後端側の耳部を折り割る場合には、下部折割バー22の下流側に配置された搬送コンベア6上の図示しない位置検出センサーが薄板ガラス1の後端位置を検出することにより薄板ガラス1の後端辺側の耳部(端縁側部分)が搬送コンベア6よりはみ出した状態で切筋線2が下部折割バー22の断面円形状のベルト31の上部側位置で停止可能なものとする。   Further, when the rear edge of the thin glass 1 is to be folded, a position detection sensor (not shown) on the transport conveyor 6 arranged downstream of the lower folding bar 22 determines the rear end position of the thin glass 1. By detecting, the upper side position of the belt 31 having a circular cross section of the lower folding bar 22 in which the scoring line 2 is in a state where the ear portion (end edge side portion) on the rear end side of the thin glass 1 protrudes from the conveyor 6. It can be stopped by.

また、前記上部押圧手段10は、薄板ガラス1の端縁の上面に付与した切筋線2に平行で、かつ切筋線2より端縁側である耳部の上方位置で薄板ガラス1の全幅にわたって当接可能な長さの長尺の上部押圧バー12を水平方向に設けたものである。   Further, the upper pressing means 10 extends over the entire width of the thin glass plate 1 at a position above the ear portion that is parallel to the cut line 2 provided on the upper surface of the edge of the thin glass plate 1 and on the edge side of the cut line 2. A long upper pressing bar 12 having a length capable of contacting is provided in the horizontal direction.

該上部押圧バー12は、その両端部分を上部昇降シリンダ11、11のシリンダロッドの先端と連結させ、前記左右の上部昇降シリンダ11、11を同期させて作動させることにより、上部押圧バー12を昇降自在とするが、上部昇降シリンダ11、11の作動により上部押圧バー12を下降させた時、上部押圧バー12の下面が前記切筋線2より端縁側の耳部部分と当接し、押圧した状態となるようにした。   The upper pressing bar 12 is connected to the tip of the cylinder rod of the upper elevating cylinders 11 and 11 at both ends, and the upper and lower upper elevating cylinders 11 and 11 are operated in synchronization to move the upper pressing bar 12 up and down. Although it is free, when the upper pressing bar 12 is lowered by the operation of the upper elevating cylinders 11, 11, the lower surface of the upper pressing bar 12 is in contact with and pressed against the ear portion on the edge side from the cut line 2. It was made to become.

また、前記下部折割バー22は、搬送コンベア6間に配置するが、図4に示すように、該空間内に配置する下部折割バー22を挟んでその上流側と下流側に合わせて2セットの上部押圧手段10を前後対称位置に配設するようにしても良い。この場合には、下流側に配置した上部押圧手段10と下部押圧手段20で薄板ガラス1の先端側の切筋線2を折割し、上流側に配置した上部押圧手段10’と下部押圧手段20で薄板ガラス1の後端側の切筋線2を折割する。   Further, the lower folding bar 22 is arranged between the conveyors 6, but as shown in FIG. 4, the lower folding bar 22 sandwiches the lower folding bar 22 arranged in the space and has 2 on the upstream side and the downstream side. You may make it arrange | position the upper press means 10 of a set in the back-and-front symmetrical position. In this case, an upper pressing means 10 'and a lower pressing means arranged on the upstream side are broken by the upper pressing means 10 and the lower pressing means 20 arranged on the downstream side, and the scoring line 2 on the tip side of the thin glass 1 is broken. At 20, the scoring line 2 on the rear end side of the thin glass plate 1 is broken.

また、前記上部押圧手段10は、下部折割バー22を挟んでその上流側と下流側に合わせて2セット設ける代わりに、図5に示すように、1つの上部押圧手段10を薄板ガラス1の搬送方向に走行移動自在とする走行手段を設け、薄板ガラス1の先端側の切筋線2を折割する場合は、上部押圧手段10を前端側の切筋線2の位置より下流側位置(図5の実線で示した上部押圧手段10参照)に移動させ、薄板ガラス1の後端側の切筋線2を折割する場合は後端側の切筋線2の上流側位置(図5の点線で示した上部押圧手段10参照)に移動させる等、上部押圧手段10の位置を図示しない走行手段によって切り替えるようにしても良い。   Further, instead of providing two sets of the upper pressing means 10 on the upstream side and the downstream side with respect to the lower folding bar 22, as shown in FIG. In the case where traveling means that can move and move in the conveying direction is provided and the scoring line 2 on the front end side of the thin glass plate 1 is to be broken, the upper pressing means 10 is positioned downstream from the position of the scoring line 2 on the front end side ( When moving to the upper pressing means 10 indicated by the solid line in FIG. 5 and breaking the cut line 2 on the rear end side of the thin glass 1, the upstream position of the cut line 2 on the rear end side (FIG. 5). The position of the upper pressing means 10 may be switched by a traveling means (not shown), for example, by moving to the upper pressing means 10 indicated by the dotted line.

また、前記下部押圧手段20は、前記薄板ガラス1の切筋線2の真下位置に昇降自在な長尺の下部折割バー22が配置されるように設け、該下部折割バー22は、薄板ガラス1の全幅に亘る長さを有し、下部折割バー22の上端面部の中心線上には前記切筋線2の下面真下部に当接可能な断面円形状のベルト31を1本張設した。   The lower pressing means 20 is provided so that a long lower folding bar 22 that can be moved up and down is disposed immediately below the score line 2 of the thin glass plate 1, and the lower folding bar 22 is a thin plate. One belt 31 having a circular cross section that has a length over the entire width of the glass 1 and that can be brought into contact with the lower part of the lower surface of the kerf line 2 on the center line of the upper end surface portion of the lower folding bar 22 is stretched. did.

前記断面円形状のベルト31は、市販品の弾性材を使用することができ、その形状は、断面が円形状に留まらず、略円形状とすることができ、ガラス板との当接時に極力細幅で線条で当接可能なものが好都合である。   A commercially available elastic material can be used for the belt 31 having a circular cross section, and the shape of the belt 31 is not limited to a circular shape, and can be a substantially circular shape. It is advantageous to have a narrow width that can be contacted by a line.

前記下部折割バー22は、その長手方向の両端を下部昇降シリンダ21、21のシリンダロッドの先端とそれぞれ取付部材23、23を介してリンク状に連結し、下部昇降シリンダ21、21はそれぞれ別々に独立して動作可能である。   The lower folding bar 22 has both ends in the longitudinal direction connected to the tip ends of the cylinder rods of the lower elevating cylinders 21 and 21 via attachment members 23 and 23, respectively, and the lower elevating cylinders 21 and 21 are separately provided. Can operate independently.

また、本発明の折割方法は、上述の薄板ガラス1の折割装置を用いて、端縁の上面、かつ平行に付与した切筋線2を設けた薄板ガラス1の端縁部を搬送コンベア6の搬送方向先端部より突出させ、図6(a)、(b)に示すように、端縁側上方より薄板ガラス1の端縁の全幅にわたる上部押圧バー12を下降させて切筋線2より端縁側の全幅に当接させ、前記切筋線2の真下位置に設けた薄板ガラス1の全幅に亘る長さの下部折割バー22の上面中心に張設した断面円形状のベルト31を前記切筋線2に沿って、該切筋線2の一端側から他端側に当接するように、下部折割バー22の両端の昇降手段の上昇開始時間に時間差を設けて順次上昇させるようにして薄板ガラス1を切筋線2に沿って折割るようにした。   Moreover, the folding method of this invention uses the above-mentioned folding apparatus of the thin glass 1, and conveys the edge part of the thin glass 1 which provided the upper surface of an edge, and the cut line 2 provided in parallel with a conveyor. 6 projecting from the front end in the conveying direction, and as shown in FIGS. 6A and 6B, the upper pressing bar 12 is lowered from the upper end side over the entire width of the end edge of the thin glass plate 1 and then cut from the scoring line 2. A belt 31 having a circular cross section, which is in contact with the entire width on the edge side and stretched around the center of the upper surface of the lower folding bar 22 having a length over the entire width of the thin glass plate 1 provided at a position directly below the cut line 2. Along the incision line 2, the ascending start times of the lifting means at both ends of the lower folding bar 22 are sequentially raised with a time difference so as to come into contact with the other end side from the one end side of the incision line 2. Then, the thin glass plate 1 was broken along the score line 2.

図7(a)、(b)に示すように、2つの下部昇降シリンダ21、21を若干時間差を設けて作動させ、下部折割バー22を僅かに傾斜させた姿勢で上昇させ、下部折割バー22の一端側が上昇して薄板ガラス1の切筋下面に当接後、さらに僅かに上昇させて切筋線2の一端側から折割分離を開始すると、該切筋線2の端部近傍を支点にして折割バー22の他端側を上昇させ、折割バーを傾斜姿勢から水平姿勢に徐々に変化させて切筋線2の一端側の分離部分を徐々に切り筋線の他端側に進行させて、薄板ガラス1の端面同士が接触しないようにして折り割る方法である。   As shown in FIGS. 7 (a) and 7 (b), the two lower elevating cylinders 21 and 21 are operated with a slight time difference, and the lower folding bar 22 is lifted in a slightly tilted posture, When one end side of the bar 22 rises and abuts against the lower surface of the cut glass 1, the bar 22 is further raised slightly and when split separation is started from one end side of the cut line 2, the vicinity of the end of the cut line 2 The other end of the split bar 22 is raised with the fulcrum as a fulcrum, and the split bar is gradually changed from the inclined posture to the horizontal posture, so that the separation portion on one end side of the cut line 2 is gradually changed to the other end of the cut line. It is the method of making it progress to the side and folding it so that the end surfaces of the sheet glass 1 may not contact.

すなわち、下部折割バー22の一方側の端部を上昇端まで上昇させると、下部折割バー22の上面の断面円形状のベルト31が薄板ガラス1の下面で切筋線2の真下部分に接触し、切筋線2の一端側から他端側に向けて直線状に接触部分が伸びて薄板ガラス1同士の接触がなく、クリーンに折り割ることができる。   That is, when the one end portion of the lower folding bar 22 is raised to the rising end, the belt 31 having a circular cross section on the upper surface of the lower folding bar 22 is placed on the lower surface of the thin glass plate 1 directly below the score line 2. They contact each other, and the contact portion extends linearly from one end side to the other end side of the scoring line 2 so that there is no contact between the thin glass plates 1 and can be folded cleanly.

薄板ガラス1を切筋線2に沿って折割ると、切粉が落下して下部折割バー22と断面円形状のベルト31上に付着する可能性があるが、薄板ガラス1の折割時に薄板ガラス1の下面と該ベルト31が当接するため、図2の切粉除去手段30に示したように、薄板ガラス1を1枚折割する毎に無端の該ベルト31を少なくとも一周回転させて、プーリー32に係止する該ベルト31の下部位置に配設したブラシ33によって該ベルト31上に付着した切粉を除去して、折割後の次に搬入された薄板ガラス1に対して下部折割バー22を薄板ガラス1面に押圧する時に、切筋線2の下面にキズをつけないようにすることができる。   When the thin glass 1 is broken along the cutting line 2, chips may fall and adhere to the lower folding bar 22 and the belt 31 having a circular cross section. Since the belt 31 comes into contact with the lower surface of the thin glass plate 1, the endless belt 31 is rotated at least once every time the thin glass plate 1 is broken as shown in the chip removing means 30 in FIG. 2. The chips 33 attached to the belt 31 are removed by a brush 33 disposed at a lower position of the belt 31 to be engaged with the pulley 32, and the lower portion of the thin glass 1 carried next after the folding is removed. When the folding bar 22 is pressed against the surface of the thin glass sheet 1, it is possible to prevent the lower surface of the score line 2 from being scratched.

下部押圧手段20の前記ベルト31は断面が円形状で、薄板ガラス1の切筋線2の下面に線接触させるため、ウレタン樹脂等の弾性材とし、薄板ガラス1の下面を押圧時、滑りもなく密着性を高めて薄板ガラス1の切筋線2の下面側を押圧でき、擦り傷等を防止できるものである。   The belt 31 of the lower pressing means 20 has a circular cross section, and is made of an elastic material such as urethane resin so as to be in line contact with the lower surface of the scoring line 2 of the thin glass plate 1, and slips when the lower surface of the thin glass plate 1 is pressed. Therefore, the adhesiveness can be improved and the lower surface side of the scoring line 2 of the thin glass plate 1 can be pressed, and scratches can be prevented.

また、前記の上部押圧バー12の底面部には薄板ガラス1の耳部と面接触する部分に上部押圧ゴムを設けた。   Further, an upper pressing rubber was provided on the bottom portion of the upper pressing bar 12 at a portion in surface contact with the ear portion of the thin glass plate 1.

尚、薄板ガラス1の端縁3の四辺に切筋線2が付与された場合であっても、本装置を2台用意し、本装置間で薄板ガラス1を方向変換させれば、薄板ガラス1の四辺の耳部折割の自動化を図ることができることは言うまでもない。   Even when the scoring lines 2 are provided on the four sides of the edge 3 of the thin glass 1, if the two devices are prepared and the direction of the thin glass 1 is changed between the devices, the thin glass is obtained. Needless to say, it is possible to automate the folding of the four sides of the ear.

前記薄板ガラス1は、フラットパネルディスプレイ等で使用する薄板ガラスを対象としたものであるため、その板厚が概ね1mm以上、3mm以下の薄板を対象としたものであるが、この板厚範囲内のガラス板に限定するものではなく、若干の増減も含むことができる。   Since the thin glass 1 is intended for a thin glass used in a flat panel display or the like, it is intended for a thin plate having a thickness of approximately 1 mm or more and 3 mm or less. It is not limited to the glass plate, and a slight increase / decrease can be included.

例えば、板厚が1mmを若干下回る板厚、あるいは3mmを若干上回る板厚であってももちろん本発明の方法および装置を使用することは可能である。   For example, it is of course possible to use the method and apparatus of the present invention even if the plate thickness is slightly less than 1 mm, or slightly greater than 3 mm.

次に、本発明の作用について説明する。   Next, the operation of the present invention will be described.

本発明は、端縁の上面、かつ平行に付与した切筋線2を設けた薄板ガラス1の端縁部を搬送コンベア6の搬送方向先端部より突出させ、端縁側上方より薄板ガラス1の端縁の全幅にわたる上部押圧バー12を下降させて切筋線2より端縁側の全幅に当接させ、
前記切筋線2の真下位置に設けた薄板ガラス1の全幅に亘る長さの下部折割バー22の上面中心に張設した断面円形状のベルト31を前記切筋線2に沿って、該切筋線2の一端側から他端側に当接するように、下部折割バー22の両端の昇降手を時間差を設けて順次上昇させるようにして薄板ガラス1を切筋線2に沿って折割るようにしたものである。
In the present invention, the edge of the thin glass sheet 1 provided with the upper surface of the edge and the cut lines 2 provided in parallel is projected from the front end of the conveyance conveyor 6 in the conveyance direction, and the edge of the thin glass glass 1 from above the edge side. The upper pressing bar 12 over the entire width of the edge is lowered and brought into contact with the entire width on the edge side from the scoring line 2,
A belt 31 having a circular cross-section stretched around the center of the upper surface of the lower split bar 22 having a length extending over the entire width of the thin glass plate 1 provided just below the score line 2 along the score line 2, The sheet glass 1 is folded along the score line 2 so that the raising and lowering hands at both ends of the lower folding bar 22 are sequentially raised with a time difference so as to come into contact with one end side from the one end side of the score line 2. It is something to be divided.

このような切筋線2の真下方向から下部折割バー22の上面に配設した線条の断面円形状のベルト31で、切筋線2の片側より線接触するように持上げた状態で折割るため、薄板ガラス1を折割り分離直後において製品となる薄板ガラス1の端面と耳部の端面の各端面が少しづつ開いていく状態となり、互いの薄板ガラス1の端面同士が接触することがなく、また順次切筋線2に沿って折り割られた部分が進行していく過程においても、既に折割分離した端面部分同士が接触しないので、クリーンな切断面が得られる。   A belt 31 having a circular cross-section of a line disposed on the upper surface of the lower folding bar 22 from directly below the cut line 2 is folded in a state of being lifted so as to be in line contact from one side of the cut line 2. In order to divide, the end face of the thin glass 1 used as a product and the end face of an ear | edge part will be in the state opened little by little immediately after splitting the thin glass 1, and the end faces of each thin glass 1 may contact. In addition, even in the process in which the portions that are sequentially broken along the score line 2 proceed, the end face portions that have already been split and separated do not come into contact with each other, so that a clean cut surface can be obtained.

下部押圧バーの上面に設けた断面円形状のベルト31を合成樹脂の弾性ゴムとしたので、下部押圧バーの上昇により薄板ガラス1の切筋線2の下面側にキズをつけないようにすることができる、
上部より耳部をピンポイント的に押圧する手段に比べて、上部押圧バー12を薄板ガラス1の切筋線2より端縁側の全幅にわたって設け、該上部押圧バー12の下面で耳部を全幅にわたって面で当接させるようにしたので、切筋線2の真下より切筋線2の片側から他端に向けて持上げる部分が進行するときに、薄板ガラス1の切筋線2の切断されようとしている部分に加わる力は一定となる。
Since the belt 31 having a circular cross section provided on the upper surface of the lower pressing bar is made of an elastic rubber made of a synthetic resin, the lower surface of the scoring line 2 of the thin glass plate 1 is not damaged by the rising of the lower pressing bar. Can
Compared with the means for pinpointly pressing the ear part from the upper part, the upper pressing bar 12 is provided over the entire width on the edge side from the score line 2 of the thin glass plate 1, and the ear part is extended over the entire width on the lower surface of the upper pressing bar 12. Since the surface is brought into contact with the surface, when the portion to be lifted from one side of the scoring line 2 toward the other end proceeds from directly below the scoring line 2, the scoring line 2 of the thin glass plate 1 will be cut. The force applied to the part is fixed.

また、前記下部折割バー22の上端面に設けた無端の断面円形状のベルト31を、薄板ガラス1の折割直後毎に少なくとも1回転以上回転させるとしたのは、1回転すれば、該ベルト31の下部位置に配設したブラシ33によって該ベルト31上に付着した切粉を除去し、該ベルト31が再び回転前の位置に戻った時に該ベルト31全周の切粉が除去できるためである。   Further, the endless cross-sectional belt 31 provided on the upper end surface of the lower split bar 22 is rotated at least once or more immediately after the thin glass plate 1 is split. Since the chips attached on the belt 31 are removed by the brush 33 disposed at the lower position of the belt 31 and the belt 31 returns to the position before the rotation again, the chips on the entire circumference of the belt 31 can be removed. It is.

前記の上部押圧バー12の底面部には薄板ガラス1の耳部と面接触させるため水平面となるようにして、上部押圧バー12の下面にウレタン樹脂等の上部押圧ゴムを貼着したことにより滑りもなく密着性を高めて薄板ガラス1の耳部を押圧できる。   The bottom surface of the upper pressing bar 12 is slipped by sticking an upper pressing rubber such as urethane resin on the lower surface of the upper pressing bar 12 so as to be in a horizontal plane so as to make surface contact with the ears of the thin glass plate 1. It is possible to improve the adhesion and press the ear portion of the thin glass plate 1.

また、 前記の下部折割バー22の上面部には薄板ガラス1の切筋線2の下面と接触させるため、ウレタン樹脂等の断面円形状のベルト31を無限ループにして張設したことにより、切筋線2の下面から滑りもなく密着性を高めて薄板ガラス1の切筋線2を下方から持上げて折割ることができ、また、ウレタン樹脂等の弾性材からなるため、擦り傷等を防止できるものである。   Moreover, in order to make it contact with the lower surface of the scoring line | wire 2 of the sheet glass 1 in the upper surface part of the said lower folding bar 22, by extending the belt 31 of circular cross-sections, such as urethane resin, as an infinite loop, The lower surface of the scoring line 2 is slippery without slipping and can be broken by lifting the scoring line 2 of the thin glass 1 from below, and it is made of an elastic material such as urethane resin, thus preventing scratches, etc. It can be done.

以下、本発明の動作を説明する。
[実施例1]
搬送コンベア6内に搬入され、前もって切筋線2を付与された薄板ガラス1は搬送コンベア6上の図示しない位置決め装置により位置決めされ、搬送コンベア6内に設けた位置検出センサーにより、薄板ガラス1の切筋線2より先端部側が搬送コンベア6の先端より突出する位置で薄板ガラス1を停止させる。薄板ガラス1の停止位置は、下部折割バー22の断面円形状のベルト31の中心線と切筋線2とが一致する位置とする。
The operation of the present invention will be described below.
[Example 1]
The thin glass sheet 1 loaded into the transport conveyor 6 and previously provided with the scoring line 2 is positioned by a positioning device (not shown) on the transport conveyor 6, and the position detection sensor provided in the transport conveyor 6 is used to detect the thin glass sheet 1. The thin glass sheet 1 is stopped at a position where the tip end side protrudes from the tip of the conveyor 6 from the scoring line 2. The stop position of the thin glass plate 1 is a position where the center line of the belt 31 having a circular cross section of the lower folding bar 22 and the cut line 2 coincide.

次に、図6(a)、(b)に示すように、上部押圧シリンダ11、11を作動させて、上部押圧バー12を水平姿勢のまま下降させ、薄板ガラス1の端面の耳部を押圧する。詳細な押圧位置は切筋線2に平行で、かつ切筋線2よりも端面側位置を押圧する。上部押圧バー12は薄板ガラス1と当接する位置で停止するように調整し、薄板ガラス1を無理に下方に押し下げないようにする。   Next, as shown in FIGS. 6A and 6B, the upper pressing cylinders 11 and 11 are actuated to lower the upper pressing bar 12 in a horizontal posture and press the ears on the end surface of the thin glass plate 1. To do. The detailed pressing position is parallel to the scoring line 2 and presses the end surface side position from the scoring line 2. The upper pressing bar 12 is adjusted so as to stop at a position where it comes into contact with the thin glass plate 1 so that the thin glass plate 1 is not pushed down by force.

続いて、下部折割バー22はその上面に無限ループ状に配設した断面円形状のベルト31を持上げて、該ベルト31を薄板ガラス1の切筋線2の下面側に当接させるが、下部折割バー22を昇降させる下部昇降シリンダ21を下部折割バー22の両端部に設け、2つの下部昇降シリンダ21、21を若干時間差を設けて作動させる。   Subsequently, the lower folding bar 22 lifts a belt 31 having a circular cross section disposed in an infinite loop shape on the upper surface thereof, and abuts the belt 31 on the lower surface side of the cut line 2 of the thin glass 1. Lower elevating cylinders 21 for elevating the lower folding bar 22 are provided at both ends of the lower folding bar 22, and the two lower elevating cylinders 21, 21 are operated with a slight time difference.

図7(a)、(b)に示すように、下部昇降シリンダ21、21を若干時間差を設けて作動させると、下部折割バー22は僅かに傾斜させた姿勢で上昇し、下部折割バー22の一端が薄板ガラス1の切筋線2の下面に当接後も、さらに僅かに上昇させて切筋線2の一端側から折割分離を開始する。   As shown in FIGS. 7 (a) and 7 (b), when the lower elevating cylinders 21 and 21 are operated with a slight time difference, the lower folding bar 22 rises in a slightly inclined posture, and the lower folding bar Even after one end of 22 comes into contact with the lower surface of the cut line 2 of the thin glass plate 1, the separation is started from one end side of the cut line 2 by slightly raising it.

一端側が折割開始できる高さで、該部分を昇降させる下部昇降シリンダ21、21を停止できるように設定し、先に上昇し、折割の開始点近傍を支点にして折割バー22の他端側を上昇させるようにすると、折割バーは傾斜姿勢から水平姿勢に徐々に変化していくが、切筋線2の折割り側の端部側の切断分離部分を徐々に切筋線2の他端側に進行させて、薄板ガラス1の端面同士が接触しないようにして折り割る。   It is set so that the lower lifting cylinders 21 and 21 for raising and lowering the part can be stopped at a height at which one end side can start splitting. When the end side is raised, the folding bar gradually changes from the inclined posture to the horizontal posture, but the cutting separation portion on the end side of the cutting line 2 on the folding side is gradually changed. The other end side of the glass sheet 1 is folded so that the end faces of the thin glass plate 1 do not contact each other.

薄板ガラス1の折割が完了すると、上部押圧バー12を上昇させると同時に、下部折割バー22を下降させ、薄板ガラス1を搬出させ、次の薄板ガラス1の搬入に備える。   When the folding of the thin glass 1 is completed, the upper pressing bar 12 is raised and the lower folding bar 22 is lowered at the same time to carry out the thin glass 1 to prepare for the next loading of the thin glass 1.

次の薄板ガラス1が搬入される前に、図2に示すように。断面円形状のベルト31を少なくとも1周させ、該ベルト31を支持するプーリー32の下部に設けたブラシ33に接触させて、該ベルト31の表面に付着した切粉を除去し、次の薄板ガラス1の下面側からの押圧時に薄板ガラス1下面に切粉を押し付けて薄板ガラス1にキズをつけないようにさせた。
[実施例2]
図4に示すように、切筋線2が薄板ガラス1の前端辺側と後端辺側の両側にある場合には、前記下部折割バー22は、搬送コンベア6間の空間に配置するが、該空間内下部に配置する下部折割バー22を挟んでその上流側と下流側に合わせて2セットの上部押圧手段10を前後対称位置に配設する。
Before the next thin glass plate 1 is carried in, as shown in FIG. A belt 31 having a circular cross section is rotated at least once and brought into contact with a brush 33 provided at a lower portion of a pulley 32 that supports the belt 31 to remove chips adhering to the surface of the belt 31. At the time of pressing from the lower surface side of 1, chips were pressed against the lower surface of the thin glass 1 so that the thin glass 1 was not damaged.
[Example 2]
As shown in FIG. 4, when the scoring line 2 is on both the front end side and the rear end side of the thin glass plate 1, the lower folding bar 22 is arranged in the space between the conveyors 6. The two sets of upper pressing means 10 are arranged at symmetrical positions on the upstream and downstream sides of the lower folding bar 22 arranged in the lower part of the space.

搬送コンベア6によって薄板ガラス1を搬送するときに、薄板ガラス1の先端部が搬送コンベア6の先端から突出した状態で、薄板ガラス1の先端側の切筋線2が下部押圧手段20の断面円形状のベルト31と一致する位置で、前述した実施例1と同様な折割装置と折割方法で、薄板ガラス1を下流側に配置した上部押圧手段10と下部押圧手段20で薄板ガラス1の先端側の切筋線2に沿って前端側の耳部を折割するとともに、該ベルト31に付着した切粉を除去する。   When the thin glass 1 is transported by the transport conveyor 6, the scoring line 2 on the front end side of the thin glass 1 is a cross-sectional circle of the lower pressing means 20 with the front end of the thin glass 1 protruding from the front end of the transport conveyor 6. The sheet glass 1 is formed by the upper pressing means 10 and the lower pressing means 20 in which the thin glass 1 is arranged on the downstream side by the same folding device and the same folding method as in the first embodiment, at a position corresponding to the belt 31 having the shape. The ear part on the front end side is broken along the cutting line 2 on the front end side, and the chips adhering to the belt 31 are removed.

続いて、薄板ガラス1をさらに搬送させ、搬送コンベア6の後端から突出した状態で、薄板ガラス1の後端側の切筋線2が下部押圧手段20の断面円形状のベルト31と一致する位置で、上流側に配置した上部押圧手段10と下部押圧手段20で薄板ガラス1の後端側の切筋線2に沿って後端側の耳部を折割するとともに、該ベルト31に付着した切粉を除去する。
[実施例3]
図5に示すように、1つの上部押圧手段10を薄板ガラス1の搬送方向に走行手段によって走行移動自在とし、上部押圧手段10の位置を切り替え可能としても良い。
Subsequently, the sheet glass 1 is further conveyed, and the scoring line 2 on the rear end side of the sheet glass 1 coincides with the belt 31 having a circular cross section of the lower pressing means 20 in a state of protruding from the rear end of the conveyor 6. At the position, the upper pressing means 10 and the lower pressing means 20 disposed on the upstream side fold the rear end side ears along the cut line 2 on the rear end side of the thin glass 1 and adhere to the belt 31. Remove the cut chips.
[Example 3]
As shown in FIG. 5, one upper pressing means 10 may be movable by the traveling means in the conveying direction of the thin glass 1 and the position of the upper pressing means 10 may be switched.

搬送コンベア6によって薄板ガラス1を搬送するときに、薄板ガラス1の先端部が搬送コンベア6の先端から突出した状態で、薄板ガラス1の先端側の切筋線2が下部押圧手段20の断面円形状のベルト31と一致する位置で、上部押圧手段10を前端側の切筋線2の位置より下流側の所定位置に走行手段によって移動させ、前述した実施例1と同様な折割装置と折割方法で、薄板ガラス1を下流側に配置した上部押圧手段10と下部押圧手段20で薄板ガラス1の先端側の切筋線2に沿って前端側の耳部を折割するとともに、前記ベルト31に付着した切粉を除去する。   When the thin glass 1 is transported by the transport conveyor 6, the scoring line 2 on the front end side of the thin glass 1 is a cross-sectional circle of the lower pressing means 20 with the front end of the thin glass 1 protruding from the front end of the transport conveyor 6. The upper pressing means 10 is moved to a predetermined position on the downstream side from the position of the scoring line 2 on the front end side by a traveling means at a position coinciding with the belt 31 in the shape, and the same folding device and folding as in the first embodiment described above. In the splitting method, the upper pressing means 10 and the lower pressing means 20 in which the thin glass 1 is arranged on the downstream side is used to fold the front end side ear along the cutting line 2 on the leading end side of the thin glass 1 and the belt The chips adhering to 31 are removed.

続いて、薄板ガラス1をさらに搬送させ、搬送コンベア6の後端から突出した状態で、薄板ガラス1の後端側の切筋線2が下部押圧手段20の断面円形状のベルト31と一致する位置で、上部押圧手段10を後端側の切筋線2の位置より上流側の所定位置に走行手段によって移動させ、上流側に配置した上部押圧手段10と下部押圧手段20で薄板ガラス1の後端側の切筋線2に沿って後端側の耳部を折割するとともに、該ベルト31に付着した切粉を除去する。   Subsequently, the sheet glass 1 is further conveyed, and the scoring line 2 on the rear end side of the sheet glass 1 coincides with the belt 31 having a circular cross section of the lower pressing means 20 in a state of protruding from the rear end of the conveyor 6. At the position, the upper pressing means 10 is moved by the traveling means to a predetermined position on the upstream side from the position of the cut line 2 on the rear end side, and the upper pressing means 10 and the lower pressing means 20 arranged on the upstream side of the thin glass 1 The ear part on the rear end side is broken along the rear cut line 2 and the chips adhering to the belt 31 are removed.

本発明の実施例1を説明する薄板ガラスの折割装置の一部を切欠、省略した概略側面図。BRIEF DESCRIPTION OF THE DRAWINGS The schematic side view which notched and abbreviate | omitted a part of thin glass glass splitting apparatus explaining Example 1 of this invention. 本発明の実施例1を説明するガラス板の端面側からみた正面図。The front view seen from the end surface side of the glass plate explaining Example 1 of this invention. 本発明の実施例1を説明する一部を切欠、省略した斜視図。The perspective view which abbreviate | omitted and abbreviate | omitted one part explaining Example 1 of this invention. 上部押圧バーを2箇所設けた実施例2を説明する側面図。The side view explaining Example 2 which provided two upper pressing bars. 上部押圧バーを走行移動可能にした実施例3を説明する側面図。The side view explaining Example 3 which enabled the traveling movement of the upper press bar. 本発明の折割方法を説明する図で、下部折割バーの上昇前の状態を示す正面図、および側面図。It is a figure explaining the folding method of this invention, and the front view and side view which show the state before the raise of a lower folding bar. 本発明の折割方法を説明する図で、下部折割バーの一端を上昇させた状態を示す正面図、および側面図。It is a figure explaining the splitting method of this invention, and the front view and side view which show the state which raised the end of the lower split bar.

符号の説明Explanation of symbols

1 薄板ガラス
2 切筋線
3 端縁(耳部)
5 搬送手段
6 搬送コンベア
10 上部押圧手段
11 上部昇降シリンダ
12 上部押圧バー
13 上部押圧ゴム
20 下部押圧手段
21 下部昇降シリンダ
22 下部折割バー
23 取付部材
30 切粉除去手段
31 断面円形状のベルト
32 プーリー
33 ブラシ
1 thin glass 2 scoring line 3 edge (ear)
DESCRIPTION OF SYMBOLS 5 Conveying means 6 Conveying conveyor 10 Upper pressing means 11 Upper raising / lowering cylinder 12 Upper pressing bar 13 Upper pressing rubber 20 Lower pressing means 21 Lower raising cylinder 22 Lower folding bar 23 Mounting member 30 Chip removal means 31 Belt 32 having a circular cross section Pulley 33 brush

Claims (8)

薄板ガラスの端縁に付与した切筋線に沿って薄板ガラスを折割切断する装置において、薄板ガラスの搬送停止を自在とする搬送コンベアからなる搬送手段と、
搬送コンベアの搬送方向先端部より突出した薄板ガラスの端縁の上面に付与した切筋線に平行、かつ上方にガラス板の全幅に亘って上部押圧バーを設け、該上部押圧バーを昇降させて切筋線より端縁側を下方に押圧させる上部押圧手段と、
前記薄板ガラスの切筋線の真下位置にガラス板の全幅に亘る長さの昇降自在な下部折割バーを設け、下部折割バーの上端部に断面円形状のベルトを張設し、下部折割バーの両端を別々の昇降手段で昇降自在に軸着させた下部押圧手段と、からなることを特徴とする薄板ガラスの折割装置。
In the apparatus for breaking and cutting the thin glass along the scoring line given to the edge of the thin glass, a transport means comprising a transport conveyor that can freely stop the transport of the thin glass,
An upper pressing bar is provided over the entire width of the glass plate in parallel with the scoring line provided on the upper surface of the edge of the thin glass protruding from the front end of the conveying conveyor, and the upper pressing bar is moved up and down. Upper pressing means for pressing the edge side downward from the score line;
A lower folding bar that can be raised and lowered over the entire width of the glass plate is provided at a position directly below the scoring line of the thin glass plate, and a belt having a circular cross section is stretched on the upper end of the lower folding bar. A sheet glass folding device, comprising: a lower pressing means in which both ends of the split bar are pivotally attached to each other by separate lifting means.
前記の下部折割バーの上端面の中心線に沿って設けた断面円形状のベルトをプーリーの回転により回転移動自在な無限ループとしたことを特徴とする請求項1記載の薄板ガラスの折割装置。   2. A thin glass break according to claim 1, wherein a belt having a circular cross section provided along the center line of the upper end surface of the lower break bar is an infinite loop which can be rotated and rotated by rotation of a pulley. apparatus. 前記上部押圧バーの下面にゴムシートを貼着したことを特徴とする請求項1または2に記載の薄板ガラスの折割装置。   The sheet glass folding apparatus according to claim 1 or 2, wherein a rubber sheet is attached to the lower surface of the upper pressing bar. 搬送コンベア間に設けた前記上部押圧手段をガラス板の搬送方向に走行移動自在とする走行手段を設け、ガラス板の先端側の切筋線を折割する場合と、ガラス板の後端側の切筋線を折割する場合の上部押圧手段の位置を前記走行手段によって切り替えるようにしたことを特徴とする請求項1乃至3のいずれかに記載の薄板ガラスの折割装置。   When the upper pressing means provided between the conveyors is provided with traveling means for allowing the upper plate to travel in the conveying direction of the glass plate, and when the scoring line on the tip side of the glass plate is broken, 4. The sheet glass folding device according to claim 1, wherein the position of the upper pressing means when the scoring line is broken is switched by the traveling means. 搬送コンベア間に設けた前記下部押圧手段を挟むようにその上流側と下流側に合わせて2セットの上部押圧手段を前後対称位置に配設し、下流側の上部押圧手段と下部押圧手段でガラス板の先端側の切筋線を折割し、上流側の上部押圧手段と下部押圧手段でガラス板の後端側の切筋線を折割するようにしたことを特徴とする請求項1乃至3のいずれかに記載の薄板ガラスの折割装置。   Two sets of upper pressing means are arranged in the front-rear symmetrical position so as to sandwich the lower pressing means provided between the conveyors on the upstream side and the downstream side, and the upper and lower pressing means on the downstream side are made of glass. The scoring line on the front end side of the plate is broken, and the scoring line on the rear end side of the glass plate is broken by the upper and lower pressing means on the upstream side. 4. A thin glass folding apparatus according to any one of 3 above. 前記請求項1乃至5のいずれかに記載の薄板ガラスの折割装置を用いたガラス板の折割方法において、端縁の上面に付与した切筋線を設けた薄板ガラスの端縁部を搬送コンベアの搬送方向先端部より突出させ、端縁側上方よりガラス板の端縁の全幅にわたる上部押圧バーを下降させて切筋線より端縁側の全幅に当接させ、
前記切筋線の真下位置に設けたガラス板の全幅に亘る長さの下部折割バーの上面中心に張設した断面円形状のベルトを前記切筋線に沿って、該切筋線の一端側から他端側に当接するように、下部折割バーの両端を時間差を設けて上昇させ、ガラス板を切筋線の一端側より他端側に順次折割るようにしたことを特徴とする薄板ガラスの折割方法。
In the glass plate folding method using the thin glass folding device according to any one of claims 1 to 5, the edge portion of the thin glass provided with the scoring line provided on the upper surface of the edge is conveyed. Protruding from the front end of the conveyor in the transport direction, lowering the upper pressing bar across the entire width of the edge of the glass plate from above the edge side and bringing it into contact with the entire width on the edge side from the score line,
A belt having a circular cross-section stretched around the center of the upper surface of the lower folding bar having a length over the entire width of the glass plate provided immediately below the score line, along the score line, one end of the score line The both ends of the lower folding bar are raised with a time difference so as to come into contact with the other end side from the side, and the glass plate is sequentially broken from the one end side to the other end side of the score line. Folding method for thin glass.
前記下部折割バーの一端側を上昇させてガラス板の切筋下面に断面円形状のベルトを当接させ切筋線の一端側から折割分離を開始後、該切筋線の端部近傍を支点にして折割バーの他端側を上昇させ、折割バーを傾斜姿勢から水平姿勢に変化させることによって切筋線の分離部分を徐々に他端側に進行させて、ガラス板を折り割るようにしたことを特徴とする請求項6記載の薄板ガラスの折割方法。   After raising one end side of the lower split bar and contacting a belt with a circular cross section on the lower surface of the cut line of the glass plate and starting split separation from one end side of the cut line, near the end of the cut line Fold the glass plate by raising the other end side of the folding bar with the fulcrum as the fulcrum, and changing the folding bar from the inclined position to the horizontal position so that the separation part of the scissor line gradually advances to the other end side. The method for breaking a thin glass sheet according to claim 6, characterized in that it is broken. 前記下部折割バーの上端面に設けた無端の断面円形状のベルトを、ガラス板の折割直後毎に少なくとも1回転以上回転させ、該ベルトの下部位置に配設したブラシによってベルト上に付着した切粉を除去して、下部折割バーをガラス板面に押圧時にキズをつけないようにしたことを特徴とする請求項6または7記載の薄板ガラスの折割方法。   The endless circular belt provided on the upper end surface of the lower split bar is rotated at least once or more immediately after the glass plate is split, and is attached onto the belt by a brush disposed at the lower position of the belt. The method of breaking a thin glass according to claim 6 or 7, wherein the cut chips are removed so that the lower folding bar is not scratched when pressed against the glass plate surface.
JP2005291624A 2005-10-04 2005-10-04 Thin glass folding device and folding method Expired - Fee Related JP4892916B2 (en)