JP4421591B2 - Molding simultaneous double-sided decorative mold and molding simultaneous double-sided decorative product manufacturing method - Google Patents

Molding simultaneous double-sided decorative mold and molding simultaneous double-sided decorative product manufacturing method Download PDF

Info

Publication number
JP4421591B2
JP4421591B2 JP2006300999A JP2006300999A JP4421591B2 JP 4421591 B2 JP4421591 B2 JP 4421591B2 JP 2006300999 A JP2006300999 A JP 2006300999A JP 2006300999 A JP2006300999 A JP 2006300999A JP 4421591 B2 JP4421591 B2 JP 4421591B2
Authority
JP
Japan
Prior art keywords
mold
decorative film
decorative
molding
resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP2006300999A
Other languages
Japanese (ja)
Other versions
JP2007022096A (en
Inventor
俊次 藤村
尚登 豊岡
富士男 森
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nissha Printing Co Ltd
Original Assignee
Nissha Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nissha Printing Co Ltd filed Critical Nissha Printing Co Ltd
Priority to JP2006300999A priority Critical patent/JP4421591B2/en
Publication of JP2007022096A publication Critical patent/JP2007022096A/en
Application granted granted Critical
Publication of JP4421591B2 publication Critical patent/JP4421591B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

この発明は、携帯通信機器や電子応用玩具の一部品や、炊飯器入力部、食器容器として使用される板状体等の樹脂成形品からなる加飾品であって、その樹脂成形品の表裏両面に加飾シートが接着した加飾品を製造するための成形同時両面加飾金型と成形同時両面加飾品の製造方法に関するものである。   The present invention is a decorative article made of a resin molded product such as a part of a portable communication device or an electronic application toy, a rice cooker input unit, a plate-like body used as a tableware container, and both front and back surfaces of the resin molded product It is related with the manufacturing method of the simultaneous molding double-sided decoration metal mold | die for manufacturing the decorative product which the decorating sheet adhere | attached on and the simultaneous molding double-sided decorative product.

従来、第1型の射出口を覆わない部分に第1加飾フィルムを沿わせ、第1型の射出口および第1加飾フィルムに対応した部分を覆う部分の第2型に第2加飾フィルムを沿わせて、第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から透光性を有する成形樹脂を射出して樹脂成形品を成形すると同時に、該樹脂成形品の表裏両面に加飾フィルムを接着させる成形同時加飾法としては、特開平6−99457号に記載されたものが公知である。   Conventionally, the first decorative film is placed along the portion that does not cover the first type injection port, and the second decoration is applied to the second type of the portion that covers the portion corresponding to the first type injection port and the first decorative film. Along with the film, the first mold and the second mold are closed, and a molding resin having translucency is injected between the first decorative film and the second decorative film from the first mold injection port. As a molding simultaneous decorating method in which a decorative film is adhered to both the front and back surfaces of a resin molded product at the same time as molding a resin molded product, a method described in JP-A-6-99457 is known.

この技術は、第1型に沿わせた第1加飾フィルムの射出口側端部を吸着により第1型に固定することによって、射出された成形樹脂が第1加飾フィルムの射出口側端部に衝突しないようにして、第1加飾フィルムの射出口側端部の浮きやめくれ上りなどを防止しようとする技術である。   In this technique, the injection port side end of the first decorative film is fixed to the first mold by suction to fix the injection port side end of the first decorative film along the first mold. This is a technique for preventing the end of the first decorative film from rising or turning up so as not to collide with the part.

特開平6−99457号公報JP-A-6-99457

しかし、上記従来の技術は、次のような課題があった。第1型側の加飾フィルムを吸着によって第1型に固定するため、固定力が弱く不安定であり、射出された成形樹脂の流動力によって、加飾フィルムの射出口側端部の浮きやめくれ上がりを完全には防止できず、第1型と加飾フィルムとの間に成形樹脂が潜り込みやすかった。加飾フィルムの膜厚が大きいのものは吸着が弱くなりやすく、加飾フィルムの射出口側端部に成形樹脂がひっかかりやすいので、特に不向きであった。   However, the conventional technique has the following problems. Since the decorative film on the first mold side is fixed to the first mold by adsorption, the fixing force is weak and unstable, and the floating force of the injection molding resin stops the floating end of the decorative film on the injection port side. It was not possible to completely prevent the bulging up, and the molding resin could easily sink between the first mold and the decorative film. A film with a large decorative film thickness is particularly unsuitable because the adsorption tends to be weak and the molding resin tends to get caught at the injection port side end of the decorative film.

この発明は、上記課題を解決するためにつぎのようにした。請求項1に記載されているように、この発明の成形同時両面加飾金型は、射出口を有する第1型の射出口を覆わない部分の型底に第1加飾フィルムを沿わせるとともに第2型の型底に第2加飾フィルムを沿わせた後に第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させる成形同時加飾法に用いる成形同時両面加飾金型であって、第1加飾フィルムの射出口側端部を挟み込むことにより射出した成形樹脂が第1加飾フィルムの前記射出口側端部に衝突しないようにする挟み込み部材と、第1加飾フィルムの射出口側端部とは反対側の端部を挟み込む後方挟み込み部材とを第1型に有することを特徴とする。 In order to solve the above-mentioned problems, the present invention is as follows. As described in claim 1, the simultaneous double-sided decorative mold of the present invention has the first decorative film along the mold bottom of the portion that does not cover the injection port of the first mold having the injection port. After placing the second decorative film on the mold bottom of the second mold, the first mold and the second mold are closed, and the first mold is shot between the first decorative film and the second decorative film. A molding simultaneous double-sided decorative mold for use in a simultaneous molding decoration method in which a molded resin is injected from an outlet to mold a resin molded product and at the same time, a decorative film is adhered to both the front and back surfaces of the resin molded product. A sandwiching member that prevents the molding resin injected by sandwiching the injection port side end of the decorative film from colliding with the injection port side end of the first decorative film, and the injection port side end of the first decorative film JP that has a rear gripping members sandwich the end opposite to the first type and To.

また、請求項2に記載されているように、この発明の成形同時両面加飾金型は、射出口を有する第1型の射出口を覆わない部分の型底に第1加飾フィルムを沿わせるとともに第2型の型底に第2加飾フィルムを沿わせた後に第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させる成形同時加飾法に用いる成形同時両面加飾金型であって、第1加飾フィルムの射出口側端部を挟み込むことにより射出した成形樹脂が第1加飾フィルムの前記射出口側端部に衝突しないようにする第1挟み込み部材と、第1加飾フィルムの射出口側端部とは反対側の端部を挟み込む後方挟み込み部材とを第1型に有するとともに、第2加飾フィルムの射出口側端部を挟み込むことにより射出した成形樹脂が第2加飾フィルムの前記射出口側端部に衝突しないようにする第2挟み込み部材を第2型に有することを特徴とする。 In addition, as described in claim 2, the simultaneous molding double-sided decorative mold of the present invention has the first decorative film along the mold bottom of the portion that does not cover the injection port of the first mold having the injection port. And the first mold and the second mold are closed after placing the second decorative film on the mold bottom of the second mold, and the first mold is placed between the first decorative film and the second decorative film. A molding simultaneous double-sided decoration mold used in a simultaneous molding method for molding a resin molded product by injecting a molding resin from the injection port and simultaneously adhering a decorative film to both front and back surfaces of the resin molded product, A first sandwiching member that prevents the molded resin injected by sandwiching the injection opening side end of the first decorative film from colliding with the injection opening side end of the first decorative film, and the first decorative film irradiation having a a rear sandwiching member to sandwich the end opposite to the first type and the outlet end In addition, the second mold has a second sandwiching member that prevents the molded resin injected by sandwiching the injection opening side end of the second decorative film from colliding with the injection opening side end of the second decorative film. It is characterized by that.

また、請求項3に記載されているように、この発明の成形同時両面加飾品の製造方法は、前記請求項1に記載の成形同時両面加飾金型を用いて、第1型の型底に第1加飾フィルムを沿わせるとともに第1加飾フィルムの射出口側端部を挟み込み部材で挟み込み、第1加飾フィルムの射出口側端部とは反対側の端部を後方挟み込み部材で挟み込み、他方で第2型の型底に第2加飾フィルムを沿わせ、第1型と第2型とを型閉めし、次に第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得ることを特徴とする。 In addition, as described in claim 3, the method for producing a simultaneous molding double-sided decorative product according to the present invention uses the mold simultaneous double-sided decorative mold according to claim 1, and uses the mold bottom of the first mold. The end of the first decorative film is sandwiched by the sandwiching member and the end opposite to the end of the first decorative film is sandwiched by the rear sandwiching member. pinching the other hand placed along a second decorative film into a mold bottom of the second type, the first type and the second type and closed type, then the first decorative film between the second decorative film A molding resin is injected from the injection port of the first mold to mold a resin molded product, and at the same time, a decorative film is adhered to both the front and back surfaces of the resin molded product to obtain a molded simultaneous double-sided decorative product.

また、請求項4に記載されているように、この発明の成形同時両面加飾品の製造方法は、前記請求項2に記載の成形同時両面加飾金型を用いて、第1型の型底に第1加飾フィルムを沿わせるとともに第1加飾フィルムの射出口側端部を第1挟み込み部材で挟み込み、第1加飾フィルムの射出口側端部とは反対側の端部を後方挟み込み部材で挟み込み、他方で第2型の型底に第2加飾フィルムを沿わせるとともに第2加飾フィルムの射出口側端部を第2挟み込み部材で挟み込み、第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得ることを特徴とする。 According to a fourth aspect of the present invention, there is provided a method for producing a simultaneous molding double-sided decorative product according to the present invention, wherein the mold bottom of the first mold is formed using the simultaneous molding double-sided decorative mold according to the second aspect. The end of the first decorative film is sandwiched between the first decorative film and the end of the first decorative film is sandwiched by the first sandwiching member, and the end opposite to the end of the first decorative film is sandwiched rearward sandwiched between members, sandwiched by second gripping members to exit end of the second decorative film causes the other hand along the second decorative film into a mold bottom of the second type, the first type and the second type The mold is closed and a molding resin is injected between the first decorative film and the second decorative film from the injection port of the first mold to form a resin molded product. At the same time, the decorative film is formed on both the front and back surfaces of the resin molded product. Are bonded to form a double-sided decorative article.

この発明では、射出口を有する第1型の射出口を覆わない部分の型底に沿わされた第1加飾フィルムの射出口側端部に射出された成形樹脂が衝突しないようにするために、加飾フィルムの射出口側端部を第1型に挟み込むための挟み込み部材を成形同時両面加飾金型が有する。   In this invention, in order to prevent the molding resin injected to the injection port side end portion of the first decorative film along the mold bottom of the portion not covering the injection port of the first mold having the injection port from colliding. The molding simultaneous double-sided decorating mold has a sandwiching member for sandwiching the exit side end of the decorative film in the first mold.

したがって、つぎのような効果を奏する。第1型側の加飾フィルムの射出口側端部を挟み込み部材によって固定するため、固定力が強く安定しており、射出された成形樹脂の流動力によって、加飾フィルムの射出口側端部の浮きやめくれ上がりを完全に防止でき、第1型と加飾フィルムとの間に成形樹脂が潜り込むこともない。加飾フィルムの膜厚が大きいものでも同様の効果を得ることができる。   Therefore, the following effects are produced. Since the injection port side end of the decorative film on the first mold side is fixed by the sandwiching member, the fixing force is strong and stable, and the injection film side end of the decorative film is caused by the flow force of the injected molding resin. Can be prevented completely, and the molding resin does not sink between the first mold and the decorative film. The same effect can be obtained even when the decorative film has a large thickness.

この発明の成形同時両面加飾金型の説明をする。   The molding simultaneous double-sided decorative mold of this invention will be described.

この発明の成形同時両面加飾金型は、射出口を有する第1型の射出口を覆わない部分の型底に第1加飾フィルムを沿わせるとともに第2型の型底に第2加飾フィルムを沿わせた後に第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させる成形同時加飾法に用いる成形同時両面加飾金型であって、第1型に沿わせた第1加飾フィルムの射出口側端部を挟み込むことにより射出した成形樹脂が第1加飾フィルムの射出口側端部に衝突しないようにする挟み込み部材を第1型に有することを特徴とするものである。   The molding simultaneous double-sided decorative mold of this invention has a first decorative film along the bottom of the mold that does not cover the injection port of the first mold having the injection port and a second decoration on the bottom of the second mold. After aligning the film, the first mold and the second mold are closed, and a molded resin is injected between the first decorative film and the second decorative film through the injection port of the first mold, and the resin molded product. Is a molding simultaneous double-sided decoration mold used in the simultaneous molding and decorating method in which a decorative film is adhered to both the front and back surfaces of the resin molded product, and the first decorative film is shot along the first mold. The first mold has a sandwiching member that prevents the molded resin injected by sandwiching the outlet side end portion from colliding with the injection port side end portion of the first decorative film.

さらに具体的には、図1〜3に記載のように、第1型と第2型とからなり、第1型は射出口、型底にフィルム挟み込み用斜面を持つ嵌合凹部および第1加飾フィルムを介して嵌合凹部に嵌合可能な形状を呈する挟み込み部材を有し、挟み込み部材はロッドを介してエアシリンダーにより嵌合凹部への嵌合・嵌合凹部からの離脱が可能であることを特徴とするものがある。   More specifically, as shown in FIGS. 1 to 3, the mold includes a first mold and a second mold. The first mold has an injection port, a fitting recess having a slope for sandwiching a film at the mold bottom, and a first process. It has a pinching member that has a shape that can be fitted into the fitting recess via a decorative film, and the pinching member can be fitted into the fitting recess and detached from the fitting recess via an air cylinder via a rod. There are things that are characterized by that.

第1型1と第2型2とは、第1加飾フィルム4と第2加飾フィルム5とを挟み込んで型閉めされることにより、第1加飾フィルム4と第2加飾フィルム5との間にできた空間に第1型1の射出口3から成形樹脂を射出して樹脂成形品を成形し、樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得る金型である。第1型1と第2型2とからなる金型としては、射出成形用金型などがある。   The 1st type | mold 1 and the 2nd type | mold 2 are the 1st decorating film 4 and the 2nd decorating film 5 by sandwiching the 1st decorating film 4 and the 2nd decorating film 5, and closing the type | mold. A molded resin is injected into the space formed between the injection port 3 of the first mold 1 to form a resin molded product, and a decorative film is adhered to both the front and back surfaces of the resin molded product to obtain a molded simultaneous double-sided decorative product. It is a mold. Examples of the mold including the first mold 1 and the second mold 2 include an injection mold.

第1型1は、射出口3を有する金型であって、射出口3を覆わない部分の型底には第1加飾フィルム4が沿わせられる。射出口3は、第1加飾フィルム4と第2加飾フィルム5との間に溶融した成形樹脂を射出するための開口である。射出口3は、第1加飾フィルム4の射出口側端部6によって覆われない位置に形成される。成形樹脂を射出する際に第1加飾フィルム4が射出口を塞いでしまわないようにするためである。第1型1の第1加飾フィルム4を沿わせる型底の面は、平面であってもよいし、凹面であってもよい。要求される樹脂成形品の立体形状に応じて適宜設計される。具体的な第1型1としては、型底にフィルム挟み込み用斜面を持つ嵌合凹部14を有するものがある(図2参照)。   The 1st type | mold 1 is a metal mold | die which has the injection port 3, Comprising: The 1st decorating film 4 is put along the type | mold bottom of the part which does not cover the injection port 3. FIG. The injection port 3 is an opening for injecting molten molding resin between the first decorative film 4 and the second decorative film 5. The injection port 3 is formed at a position that is not covered by the injection port side end 6 of the first decorative film 4. This is to prevent the first decorative film 4 from blocking the injection port when the molding resin is injected. The surface of the mold bottom along which the first decorative film 4 of the first mold 1 is aligned may be a flat surface or a concave surface. It is designed appropriately according to the required three-dimensional shape of the resin molded product. As a concrete 1st type | mold 1, there exists what has the fitting recessed part 14 which has the slope for film clamping on the type | mold bottom (refer FIG. 2).

第1型1には、第1加飾フィルム4の射出口側端部6を挟み込んで、射出された成形樹脂が射出口側端部6に衝突しないようにする挟み込み部材7を有する(図8参照)。具体的な挟み込み部材7としては、第1加飾フィルム4を介して嵌合凹部14に嵌合可能な形状を呈するものであり、挟み込み部材7はロッド11を介してエアシリンダー10により嵌合凹部への嵌合・嵌合凹部からの離脱が可能であるものがある(図2参照)。   The first mold 1 has a sandwiching member 7 that sandwiches the injection port side end portion 6 of the first decorative film 4 so that the injected molding resin does not collide with the injection port side end portion 6 (FIG. 8). reference). The specific sandwiching member 7 has a shape that can be fitted into the fitting recess 14 via the first decorative film 4, and the sandwiching member 7 is fitted into the fitting recess by the air cylinder 10 via the rod 11. There are some which can be fitted and detached from the fitting recess (see FIG. 2).

挟み込み部材7の形状としては、断面略台形形状がある(図1〜図4、図7〜8参照)。挟み込み部材7の長さは、例えば、得ようとする樹脂成形品の幅が50mmである場合は、70mmとするとよい。加飾フィルムの長手方向の張力に対抗するためである。挟み込み部材7の形状を上記の通りとする理由は、加飾フィルムの張力に抗して無理なく加飾フィルムを挟み込むことができ、皺の発生を抑えることもできるからである。挟み込み部材7の形状は、加飾フィルムを挟み込むことにより、挟み込み部材7の表面と第1型1の面とが面一になるような形状とすることができる(図1、図2、図4参照)。挟み込み部材7のうち、フィルム挟み込み用斜面13に対応する斜面の幅は、3〜5mmとするのが好ましい(図2参照)。3mm未満であると挟み込み力が弱くなり浮きやめくれ上りが発生しやすくなるからであり、5mmを越えると加飾フィルムの表面積をその分大きくする必要があり経済的でなく、また、挟み込み時に加飾フィルムのずれ込みが大きくなるからである。フィルム挟み込み用斜面13の角度は、10〜45°とすることができる。特に25°が好ましい。10°未満であると、挟み込み部材7の強度が弱くなり先端が折れて破損しやすくなり、45°を超えると、加飾フィルムを大きな角度で折曲げる必要があるため、加飾フィルムが剪断されやすくなり、特に剛性があって変形しにくい加飾フィルムに適用しにくくなるからである。挟み込み部材7の強度を強くするために、挟み込み部材7を肉厚のものにすることができる(図3参照)。なお、この場合、成形樹脂が射出される空間12自体が変形することになるが、このようにしても構わないのは、成形樹脂が射出される空間12のうち、挟み込み部材7が存在する部分は、成形同時両面加飾品が得られた後、切除される部分だからである(図6参照)。図6における成形同時両面加飾品は、第1加飾フィルム4による加飾(文字及び枠状淡色部)と第2加飾フィルム5による加飾(枠状濃色部)とが複合し、第1加飾フィルム4による加飾(文字及び枠状淡色部)が第2加飾フィルム5の透光部を通して観察される態様の成形同時両面加飾品である。   The sandwiching member 7 has a substantially trapezoidal cross section (see FIGS. 1 to 4 and FIGS. 7 to 8). For example, when the width of the resin molded product to be obtained is 50 mm, the length of the sandwiching member 7 is preferably 70 mm. This is to counter the tension in the longitudinal direction of the decorative film. The reason why the shape of the sandwiching member 7 is as described above is that the decorative film can be easily sandwiched against the tension of the decorative film, and the generation of wrinkles can be suppressed. The sandwiching member 7 can be shaped so that the surface of the sandwiching member 7 is flush with the surface of the first mold 1 by sandwiching a decorative film (FIGS. 1, 2, and 4). reference). Of the sandwiching member 7, the width of the slope corresponding to the slope 13 for film sandwiching is preferably 3 to 5 mm (see FIG. 2). If it is less than 3 mm, the pinching force will be weak, and it will be easy for floating and turning up. If it exceeds 5 mm, the surface area of the decorative film will need to be increased by that amount, which is not economical. This is because the displacement of the decorative film increases. The angle of the film sandwiching slope 13 can be 10 to 45 °. In particular, 25 ° is preferable. If the angle is less than 10 °, the strength of the sandwiching member 7 is weakened and the tip is easily broken and easily damaged. If the angle exceeds 45 °, the decorative film needs to be bent at a large angle. This is because it becomes easy to apply to a decorative film that is particularly rigid and difficult to deform. In order to increase the strength of the sandwiching member 7, the sandwiching member 7 can be made thick (see FIG. 3). In this case, the space 12 itself into which the molding resin is injected is deformed. However, this may be done in a portion where the sandwiching member 7 is present in the space 12 in which the molding resin is injected. This is because it is the part that is cut out after the molded double-sided decorative product is obtained (see FIG. 6). The molding simultaneous double-sided decorative product in FIG. 6 is a combination of decoration (characters and frame-shaped light colored portion) by the first decorative film 4 and decoration (frame-shaped dark colored portion) by the second decorative film 5. It is a simultaneous molding double-sided decorative product in which the decoration (characters and frame-like light colored part) by the 1 decorative film 4 is observed through the translucent part of the second decorative film 5.

挟み込み部材としては、第1加飾フィルム4の射出口側端部6ではなく、反対側の端部を挟み込む後方挟み込み部材73を有していてもよい(図7参照)。加飾フィルムのうち射出口側端部6だけでなく、反対側の端部をも同時または非同時に挟み込むことによって、加飾フィルムを第1型により強固に固定することができるので、加飾フィルムのしわ発生やバタつきを防止したり、射出された成形樹脂が第1加飾フィルム4と第1型との間に潜り込まないようにすることができる。   As a pinching member, you may have the back pinching member 73 which pinches | interposes the edge part on the opposite side instead of the injection port side edge part 6 of the 1st decorating film 4 (refer FIG. 7). Since the decorative film can be firmly fixed by the first mold by sandwiching not only the injection port side end portion 6 but also the opposite end portion of the decorative film simultaneously or non-simultaneously, the decorative film It is possible to prevent the generation of wrinkles and fluttering, and to prevent the injected molding resin from entering between the first decorative film 4 and the first mold.

挟み込み部材7の駆動機構としては、エアシリンダー方式、カム方式、型閉め力利用方式などがある。図1〜図5は、エアシリンダー方式が例示されており、固定型1に内蔵されたエアシリンダー10とロッド11とからなり、ロッド11の先端に挟み込み部材7が固定されている。エアシリンダー10内の圧縮空気によりロッド11が押し上げられる機構である。加飾フィルムに傷がより付きにくくするためにはカム方式を採用するのが有効である。挟み込み部材7の移動の程度を微調整できるからである。特に、剛性があって変形しにくい基体シートを用いた加飾フィルムを軟らかく挟み込む場合などに好適である。また、第1型1と第2型2との型開き状態ではエアシリンダー方式によって加飾フィルムを挟み込み、型閉め時には、金型の型閉め力によりカム構造が寄与して、加飾フィルムの挟み込みをより強固にする構造にすることも可能である。特に剛性があって変形しにくい基体シートを用いた加飾フィルムでは、挟み込み力不足による加飾フィルムの浮きを防止するとともに、ポリカーボネート樹脂のような流動性の低い成形樹脂の通路をより広く確保することができるので好適である。   As a driving mechanism of the sandwiching member 7, there are an air cylinder system, a cam system, a mold closing force utilization system, and the like. 1 to 5 illustrate an air cylinder system, which includes an air cylinder 10 and a rod 11 incorporated in a fixed mold 1, and a sandwiching member 7 is fixed to the tip of the rod 11. This is a mechanism in which the rod 11 is pushed up by the compressed air in the air cylinder 10. In order to make the decorative film less likely to be scratched, it is effective to adopt a cam system. This is because the degree of movement of the sandwiching member 7 can be finely adjusted. In particular, it is suitable when a decorative film using a base sheet that is rigid and hardly deforms is softly sandwiched. In addition, the decorative film is sandwiched by the air cylinder method when the first mold 1 and the second mold 2 are opened. When the mold is closed, the cam structure contributes to the mold closing force of the mold, and the decorative film is sandwiched. It is also possible to make the structure stronger. In particular, a decorative film using a base sheet that is rigid and difficult to deform prevents the decorative film from floating due to insufficient pinching force and secures a wider passage for molding resin such as polycarbonate resin with low fluidity. This is preferable.

第2型2は、第2加飾フィルム5を沿わせる金型である。第2型2の第2加飾フィルム5を沿わせる面は、平面であってもよいし、凹面であってもよい。要求される樹脂成形品の立体形状に応じて適宜設計される。   The second mold 2 is a mold that allows the second decorative film 5 to follow. The surface along which the second decorative film 5 of the second mold 2 is aligned may be a flat surface or a concave surface. It is designed appropriately according to the required three-dimensional shape of the resin molded product.

第1型1と第2型2の両方に、前記挟み込み部材7を有してもよい。つまり、この態様では、射出口3を有する第1型1の射出口3を覆わない部分の型底に第1加飾フィルム4を沿わせるとともに第2型2の型底に第2加飾フィルム5を沿わせた後に第1型1と第2型2とを型閉めし、第1加飾フィルム4と第2加飾フィルム5との間に第1型の射出口3から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させる成形同時加飾法に用いる成形同時両面加飾金型であって、第1加飾フィルム4の射出口側端部6を挟み込むことにより射出した成形樹脂が第1加飾フィルム4の前記射出口側端部6に衝突しないようにする第1挟み込み部材71を第1型に有するとともに、第2加飾フィルムの前記射出口側端部6を挟み込むことにより射出した成形樹脂が第2加飾フィルム5の前記射出口側端部6に衝突しないようにする第2挟み込み部材72を第2型2に有する。第1挟み込み部材71と第2挟み込み部材72の形状や駆動機構は、前記した挟み込み部材7と同様にすることができる。第1挟み込み部材71と第2挟み込み部材72の形成位置は、真正面に対向するような位置に形成してもよいし(図4参照)、対向しない位置に形成してもよい。   You may have the said pinching member 7 in both the 1st type | mold 1 and the 2nd type | mold 2. In other words, in this aspect, the first decorative film 4 is placed along the mold bottom of the portion that does not cover the injection port 3 of the first mold 1 having the injection port 3 and the second decorative film is formed on the mold bottom of the second mold 2. 5, the first mold 1 and the second mold 2 are closed, and a molding resin is injected from the first mold injection port 3 between the first decorative film 4 and the second decorative film 5. And a molding simultaneous double-sided decorative mold used in a simultaneous molding method for molding a resin molded product and simultaneously adhering a decorative film to both the front and back surfaces of the resin molded product, the injection port of the first decorative film 4 The first mold has a first sandwiching member 71 that prevents the molded resin injected by sandwiching the side end portion 6 from colliding with the injection port side end portion 6 of the first decorative film 4, and the second decoration. The molded resin injected by sandwiching the injection port side end 6 of the film is the second decoration. The second gripping members 72 so as not to impinge on the exit-side end portion 6 of Irumu 5 having the second type 2. The shape and driving mechanism of the first sandwiching member 71 and the second sandwiching member 72 can be the same as those of the sandwiching member 7 described above. The formation positions of the first sandwiching member 71 and the second sandwiching member 72 may be formed at positions facing directly in front (see FIG. 4) or at positions not facing each other.

この発明の成形同時両面加飾品の製造方法を説明する。   The manufacturing method of the simultaneous molding double-sided decorative article of this invention is demonstrated.

第1型1にのみ挟み込み部材7を有する金型を用いた場合の製造方法を説明する。まず、第1型の型底に第1加飾フィルムを沿わせるとともに第1加飾フィルムの射出口側端部6を挟み込み部材で挟み込み、他方で第2型の型底に第2加飾フィルム5を沿わせる。第1型1の射出口3を覆わない部分に第1加飾フィルム4を沿わせる。成形樹脂を射出する際に第1加飾フィルム4が射出口3を塞いでしまわないようにするためである。また、第1加飾フィルム4に対応した部分及び、第1型1の射出口3に対応した部分をも覆うように第2型2に第2加飾フィルム5を沿わせる。第1加飾フィルム4に対応した部分を覆うようにするのは、樹脂成形品の表裏両面に加飾フィルムを形成するためである。第1型1の射出口3に対応した部分をも覆うようにするのは、第2加飾フィルム5の射出口側端部が成形樹脂によって浮いたりめくれたりして第2型2と第2加飾フィルム5との間に成形樹脂が潜り込まないようにするためである。さらに具体的には、第1型1の型底に第1加飾フィルム4を沿わせるとともに嵌合凹部から離脱した挟み込み部材をロッド11を介してエアシリンダー10を作動させることにより、第1加飾フィルム4の射出口側端部6を嵌合凹部と挟み込み部材7との間に挟み込ませる。   A manufacturing method in the case of using a mold having the sandwiching member 7 only in the first mold 1 will be described. First, the first decorative film is placed along the bottom of the first mold, and the injection opening side end 6 of the first decorative film is sandwiched by the sandwiching member, while the second decorative film is placed on the bottom of the second mold. 5 along. The first decorative film 4 is placed along a portion that does not cover the injection port 3 of the first mold 1. This is to prevent the first decorative film 4 from blocking the injection port 3 when the molding resin is injected. Further, the second decorative film 5 is placed along the second mold 2 so as to cover the part corresponding to the first decorative film 4 and the part corresponding to the injection port 3 of the first mold 1. The reason for covering the portion corresponding to the first decorative film 4 is to form the decorative film on both the front and back surfaces of the resin molded product. The part corresponding to the injection port 3 of the first mold 1 is also covered by the second mold 2 and the second mold 2 because the injection port side end of the second decorative film 5 is floated or turned up by the molding resin. This is to prevent the molding resin from entering between the decorative film 5. More specifically, the first decorative film 4 is placed along the mold bottom of the first mold 1 and the sandwiching member released from the fitting recess is operated by operating the air cylinder 10 via the rod 11 to thereby perform the first processing. The injection port side end portion 6 of the decorative film 4 is sandwiched between the fitting recess and the sandwiching member 7.

第1加飾フィルム4および第2加飾フィルム5を第1型1および第2型2にセットするには、加飾フィルム送り装置で長尺状の加飾フィルムを連続的に送るようにしてもよいし、トムソン型などにより所定形状にカットされた加飾フィルムを一枚一枚セットしてもよい。第1型1の嵌合凹部14の第1フィルム挟み込み用斜面13などに真空吸引孔(図示せず)を形成して第1加飾フィルム4の射出口端部6を第1型1に補助的に吸引密着させてもよい。また、クランプ部材(図示せず)で第1加飾フィルム4を第1型1に固定してもよい。また、加熱手段(図示せず)により第1加飾フィルム4を加熱してもよい。   In order to set the first decorative film 4 and the second decorative film 5 to the first mold 1 and the second mold 2, the long decorative film is continuously fed by the decorative film feeder. Alternatively, decorative films cut into a predetermined shape by a Thomson mold or the like may be set one by one. A vacuum suction hole (not shown) is formed on the slope 13 for sandwiching the first film of the fitting recess 14 of the first mold 1 to assist the first mold 1 with the injection port end 6 of the first decorative film 4. Alternatively, suction adhesion may be performed. Further, the first decorative film 4 may be fixed to the first mold 1 with a clamp member (not shown). Moreover, you may heat the 1st decorating film 4 with a heating means (not shown).

第2加飾フィルム5を第2型2に沿わせる位置は、前記したとおりである。   The position where the second decorative film 5 is placed along the second mold 2 is as described above.

第1加飾フィルム4と第2加飾フィルム5との加飾部分の相対的な配置は、第1加飾フィルム4の透光性を有する部分に、第2加飾フィルム5の文字や図柄などが配置されるようにするとよい。こうすることで、第1加飾フィルム4側から見ると、第1加飾フィルム4の図柄(例えば、黒枠)と第2加飾フィルム5の図柄(例えば、白枠と文字)とが複合して観察できるため、あたかも、第1加飾フィルム4の図柄(例えば、黒枠)と第2加飾フィルム5の図柄(例えば、白枠と文字)とが同一平面上に形成されているように見えるからである。   The relative arrangement of the decorative portions of the first decorative film 4 and the second decorative film 5 is the character or design of the second decorative film 5 on the portion having the translucency of the first decorative film 4. Etc. should be arranged. By doing so, when viewed from the first decorative film 4 side, the design of the first decorative film 4 (for example, a black frame) and the design of the second decorative film 5 (for example, a white frame and characters) are combined. Therefore, it looks as if the design of the first decorative film 4 (for example, a black frame) and the design of the second decorative film 5 (for example, a white frame and characters) are formed on the same plane. Because.

次に、第1型と第2型とを型閉めし、次に第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得る。射出口3から成形樹脂を射出すると、第1加飾フィルム4の射出口側端部6は挟み込み部材によって第1型1の型底に挟み込まれているので、第1加飾フィルム4の射出口側端部の浮きやめくれ上り、成形樹脂の潜り込みは発生しない。第1加飾フィルム4が基体シートを剥離して用いるタイプである場合は、第1型1と第2型2とを型開きする際、または、型開きした後に、基体シートを剥がす。成形樹脂としては、アクリル樹脂、ABS樹脂、ポリカーボネイト樹脂、ポリプロピレン樹脂、ポリ乳酸樹脂などがある。成形樹脂は透光性を有していてもよい。その理由は、第2加飾フィルム5の図柄を第1加飾フィルム4側から透視でき、かつ、第1加飾フィルム4の図柄を第2加飾フィルム5側から透視できるようにするためである。   Next, the first mold and the second mold are closed, and then a molded resin is injected between the first decorative film and the second decorative film from the injection port of the first mold to obtain a resin molded product. At the same time as molding, a decorative film is adhered to both the front and back surfaces of the resin molded product to obtain a molded simultaneous double-sided decorative product. When the molding resin is injected from the injection port 3, the injection port side end portion 6 of the first decorative film 4 is sandwiched between the mold bottoms of the first mold 1 by the sandwiching member. The side end does not float or turn up, and molding resin does not sink. When the first decorative film 4 is a type that is used by peeling the base sheet, the base sheet is peeled off when the first mold 1 and the second mold 2 are opened or after the mold is opened. Examples of the molding resin include acrylic resin, ABS resin, polycarbonate resin, polypropylene resin, and polylactic acid resin. Molding resin may have translucency. The reason is that the design of the second decorative film 5 can be seen through from the first decorative film 4 side, and the design of the first decorative film 4 can be seen through from the second decorative film 5 side. is there.

なお、この発明において用いる第1加飾フィルム4及び第2加飾フィルム5の基本的な層構成の具体例としては、基体シート、離型層、剥離層、図柄層、接着層が順次積層されたものがある。なお、基体シートを剥離せずに用いる場合は、離型層、剥離層は不要である。基体シートの材質としては、アクリル系樹脂、ポリカーボネート系樹脂、ポリオレフィン系樹脂、ポリエステル系樹脂、ABS樹脂などの樹脂シートがある。あるいは以上の各シートをラミネート加工した複合体などがある。基体シートの膜厚としては、10μm〜200μmのものを使用することができる。さらに具体的には、膜厚38μmまたは70μm、あるいは188μmの二軸延伸ポリエステルフィルムや膜厚100μmの二軸延伸ポリ乳酸フィルムがある。離型層の材質としては、メラミン樹脂系離型剤、シリコーン樹脂系離型剤などがある。剥離層の材質としては、アクリル系樹脂、ポリエステル系樹脂、ポリ塩化ビニル系樹脂などがある。剥離層としては、ウレタンアクリレート系樹脂を用いてハードコート機能を付与したものがある。図柄層は、通常は印刷層として形成する。印刷層の材質としては、アクリル系樹脂、ポリビニル系樹脂、ポリアミド系樹脂、ポリエステル系樹脂などの樹脂をバインダーとし、適切な色の顔料または染料を着色剤として含有する着色インキを用いるとよい。印刷層の乾燥膜厚は、1μm〜50μmとするのが一般的である。図柄層は、金属薄膜層からなるもの、あるいは印刷層と金属薄膜層との組み合わせからなるものでもよい。金属薄膜層は、真空蒸着法、スパッターリング法、イオンプレーティング法などで形成したものである。接着層の材質は、アクリル系樹脂やビニル系樹脂がある。成形樹脂に適した感熱性あるいは感圧性の樹脂を適宜使用する。たとえば、成形樹脂の材質がポリアクリル系樹脂の場合はポリアクリル系樹脂を用いるとよい。また、成形樹脂の材質がポリフェニレンオキシド・ポリスチレン系樹脂、ポリカーボネート系樹脂、スチレン共重合体系樹脂、ポリスチレン系ブレンド樹脂の場合は、これらの樹脂と親和性のあるポリアクリル系樹脂、ポリスチレン系樹脂、ポリアミド系樹脂などを使用すればよい。接着層の乾燥膜厚は、1
μm〜10μmとするのが一般的である。接着層は、透光性を有するものである。第2加飾フィルム5の図柄を第1加飾フィルム4側から透視でき、かつ、第1加飾フィルム4の図柄を第2加飾フィルム5側から透視できるようにするためである。
In addition, as a specific example of the basic layer structure of the first decorative film 4 and the second decorative film 5 used in the present invention, a base sheet, a release layer, a release layer, a design layer, and an adhesive layer are sequentially laminated. There is something. Note that when the base sheet is used without being peeled, the release layer and the release layer are unnecessary. Examples of the material for the base sheet include resin sheets such as acrylic resin, polycarbonate resin, polyolefin resin, polyester resin, and ABS resin. Alternatively, there are composites obtained by laminating each of the above sheets. As the film thickness of the substrate sheet, a film having a thickness of 10 μm to 200 μm can be used. More specifically, a biaxially stretched polyester film having a film thickness of 38 μm, 70 μm, or 188 μm and a biaxially stretched polylactic acid film having a film thickness of 100 μm are available. Examples of the material of the release layer include melamine resin release agents and silicone resin release agents. Examples of the material for the release layer include acrylic resins, polyester resins, and polyvinyl chloride resins. As a peeling layer, there exists what provided the hard-coat function using the urethane acrylate resin. The design layer is usually formed as a printing layer. As a material of the printing layer, it is preferable to use a colored ink containing a resin such as an acrylic resin, a polyvinyl resin, a polyamide resin, or a polyester resin as a binder and a pigment or dye of an appropriate color as a colorant. The dry film thickness of the printed layer is generally 1 μm to 50 μm. The pattern layer may be a metal thin film layer or a combination of a printed layer and a metal thin film layer. The metal thin film layer is formed by a vacuum deposition method, a sputtering method, an ion plating method, or the like. The material of the adhesive layer includes acrylic resin and vinyl resin. A heat-sensitive or pressure-sensitive resin suitable for the molding resin is appropriately used. For example, when the material of the molding resin is a polyacrylic resin, a polyacrylic resin may be used. In addition, when the molding resin material is polyphenylene oxide / polystyrene resin, polycarbonate resin, styrene copolymer resin, or polystyrene blend resin, polyacrylic resin, polystyrene resin, polyamide having affinity with these resins A series resin or the like may be used. The dry film thickness of the adhesive layer is 1
Generally, it is set to μm to 10 μm. The adhesive layer has translucency. This is because the design of the second decorative film 5 can be seen through from the first decorative film 4 side, and the design of the first decorative film 4 can be seen through from the second decorative film 5 side.

第1型1と第2型2の両方に挟み込み部材を有する場合の製造方法を説明する。つまり、前記した第1型1と第2型2の両方に挟み込み部材を有する成形同時両面加飾金型を用いて、第1型1の型底に第1加飾フィルム4を沿わせるとともに第1加飾フィルム4の射出口側端部6を第1挟み込み部材71で挟み込み、他方で第2型2の型底に第2加飾フィルム5を沿わせるとともに第2加飾フィルム5の射出口側端部6を第2挟み込み部材72で挟み込み、第1型1と第2型2とを型閉めし、第1加飾フィルム4と第2加飾フィルム5との間に第1型1の射出口3から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得るものである。   A manufacturing method in the case where both the first mold 1 and the second mold 2 have sandwiching members will be described. That is, the first decorative film 4 is placed along the mold bottom of the first mold 1 using the molding simultaneous double-sided decorative mold having the sandwiching member between both the first mold 1 and the second mold 2 described above. The injection port side end 6 of the first decorative film 4 is sandwiched by the first sandwiching member 71, and the second decorative film 5 is placed along the mold bottom of the second mold 2 and the injection port of the second decorative film 5. The side end 6 is sandwiched by the second sandwiching member 72, the first mold 1 and the second mold 2 are closed, and the first mold 1 is sandwiched between the first decorative film 4 and the second decorative film 5. A molded resin is injected from the injection port 3 to mold a resin molded product, and at the same time, a decorative film is adhered to both the front and back surfaces of the resin molded product to obtain a molded simultaneous double-sided decorative product.

さらに具体的には、図4に示すように、第1型1と第2型2とからなり、第1型1は射出口3、型底に第1フィルム挟み込み用斜面13を持つ第1嵌合凹部14および第1加飾フィルム4を介して第1嵌合凹部14に嵌合可能な形状を呈する第1挟み込み部材71を有し、第1挟み込み部材71はロッド11を介してエアシリンダー10により第1嵌合凹部14への嵌合・嵌合凹部からの離脱が可能であり、第2型2は型底に第2フィルム挟み込み用斜面15を有する第2嵌合凹部16および第2加飾フィルム5を介して第2嵌合凹部16に嵌合可能な形状を呈する第2挟み込み部材72を有し、第2挟み込み部材72はロッド11を介してエアシリンダー10により第2嵌合凹部16への嵌合・嵌合凹部からの離脱が可能である成形同時両面加飾金型を用いた製造方法であって、第1型1の型底に第1加飾フィルム4を沿わせるとともに第1嵌合凹部14から離脱した第1挟み込み部材71をロッド11を介してエアシリンダー10により作動させることにより第1加飾フィルム4の射出口側端部6を第1嵌合凹部と第1挟み込み部材との間に挟み込み、他方で第2型の型底に第2加飾フィルムを沿わせるとともに第2嵌合凹部から離脱した第2挟み込み部材をロッド11を介してエアシリンダー10により作動させることにより第2加飾フィルムの射出口側端部6を第2嵌合凹部と第2挟み込み部材との間に挟み込み、第1型1と第2型2とを型閉めし、次に、第1加飾フィルム4と第2加飾フィルム5との間に第1型1の射出口3から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得るものである。   More specifically, as shown in FIG. 4, the first mold 1 comprises a first mold 1 and a second mold 2, and the first mold 1 has a first fitting having an injection port 3 and a slope 13 for sandwiching the first film at the mold bottom. It has the 1st pinching member 71 which exhibits the shape which can be fitted to the 1st fitting recessed part 14 via the joint recessed part 14 and the 1st decoration film 4, and the 1st pinching member 71 is the air cylinder 10 via the rod 11. The second mold 2 can be fitted to the first fitting recess 14 and can be detached from the fitting recess, and the second mold 2 has a second fitting recess 16 having a second film sandwiching inclined surface 15 on the mold bottom and a second process. It has the 2nd pinching member 72 which exhibits the shape which can be fitted to the 2nd fitting recessed part 16 via the decoration film 5, and the 2nd pinching member 72 is 2nd fitting recessed part 16 by the air cylinder 10 via the rod 11. Simultaneous molding and removal from the fitting recess In the manufacturing method using the decorative mold, the first sandwiching member 71 separated from the first fitting recess 14 and the first sandwiching film 4 along the first decorative film 4 is placed on the bottom of the first mold 1 via the rod 11. By operating the air cylinder 10, the end 6 on the injection port side of the first decorative film 4 is sandwiched between the first fitting recess and the first sandwiching member, and on the other hand, the second mold is fixed to the mold bottom of the second mold. A second fitting member is placed on the injection opening side end 6 of the second decorative film by operating the second sandwiching member along the decorative film and being released from the second fitting recess by the air cylinder 10 via the rod 11. The first mold 1 and the second mold 2 are clamped between the recess and the second clamping member, and then the first mold is interposed between the first decorative film 4 and the second decorative film 5. 1 Molding resin is injected from the injection port 3 to mold a resin molded product At the same time it is intended to obtain a molded simultaneous double-side decorating articles by adhering a decorative film on both sides of the resin molded article.

この場合、使用する加飾フィルムの構成や、第1型1の第1挟み込み部材71の動作は、前記と同様であり、第2型2の第2挟み込み部材の動作は、前記したように第1型1にのみ挟み込み部材7を有する場合と同様である。   In this case, the configuration of the decorative film to be used and the operation of the first sandwiching member 71 of the first mold 1 are the same as described above, and the operation of the second sandwiching member of the second mold 2 is the same as described above. This is similar to the case where the sandwiching member 7 is provided only in the type 1.

この発明の成形同時両面加飾金型の一例と成形同時両面加飾品の製造方法の一工程を示す断面図である。It is sectional drawing which shows one process of the manufacturing method of an example of the simultaneous molding double-sided decoration metal mold | die of this invention, and a simultaneous molding double-sided decorative product. この発明の成形同時両面加飾金型の一例と成形同時両面加飾品の製造方法の一工程を示す断面図である。It is sectional drawing which shows one process of the manufacturing method of an example of the simultaneous molding double-sided decoration metal mold | die of this invention, and a simultaneous molding double-sided decorative product. この発明の成形同時両面加飾金型の一例と成形同時両面加飾品の製造方法の一工程を示す断面図である。It is sectional drawing which shows one process of the manufacturing method of an example of the simultaneous molding double-sided decoration metal mold | die of this invention, and a simultaneous molding double-sided decorative product. この発明の成形同時両面加飾金型の一例と成形同時両面加飾品の製造方法の一工程を示す断面図である。It is sectional drawing which shows one process of the manufacturing method of an example of the simultaneous molding double-sided decoration metal mold | die of this invention, and a simultaneous molding double-sided decorative product. この発明の成形同時両面加飾金型の第1型の一例を示す平面図であって、加飾フィルムと挟み込み部材との位置関係を示す図である。It is a top view which shows an example of the 1st type | mold of the shaping | molding simultaneous double-sided decorating metal mold | die of this invention, Comprising: It is a figure which shows the positional relationship of a decorating film and a clamping member. この発明の成形同時両面加飾品の製造方法によって得られる成形同時両面加飾品の一例を示す平面図である。It is a top view which shows an example of the simultaneous molding double-sided decorative article obtained by the manufacturing method of the simultaneous simultaneous double-sided decorative article of this invention. この発明の成形同時両面加飾金型の一例と成形同時両面加飾品の製造方法の一工程を示す断面図である。It is sectional drawing which shows one process of the manufacturing method of an example of the simultaneous molding double-sided decoration metal mold | die of this invention, and a simultaneous molding double-sided decorative product. この発明の成形同時両面加飾金型の一部品であるフィルム挟み込み部材の一例を示す斜視図である。It is a perspective view which shows an example of the film pinching member which is one part of the simultaneous mold | die double-sided decoration metal mold | die of this invention.

符号の説明Explanation of symbols

1 第1型
2 第2型
3 射出口
4 第1加飾フィルム
5 第2加飾フィルム
6 射出口側端部
7 挟み込み部材
71 第1挟み込み部材
72 第2挟み込み部材
73 後方挟み込み部材
10 エアシリンダー
11 ロッド
12 成形樹脂が射出される空間
13 第1フィルム挟み込み斜面
14 第1勘合凹部
15 第2フィルム挟み込み斜面
16 第2嵌合凹部
DESCRIPTION OF SYMBOLS 1 1st type | mold 2 2nd type | mold 3 Injection port 4 1st decorative film 5 2nd decorative film 6 Injection port side edge part 7 Clamping member 71 1st clamping member 72 2nd clamping member 73 Back clamping member 10 Air cylinder 11 Rod 12 Space in which molding resin is injected 13 First film sandwich slope 14 First fitting recess 15 Second film sandwich slope 16 Second fitting recess

Claims (4)

射出口を有する第1型の射出口を覆わない部分の型底に第1加飾フィルムを沿わせるとともに第2型の型底に第2加飾フィルムを沿わせた後に第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させる成形同時加飾法に用いる成形同時両面加飾金型であって、第1加飾フィルムの射出口側端部を挟み込むことにより射出した成形樹脂が第1加飾フィルムの前記射出口側端部に衝突しないようにする挟み込み部材と、第1加飾フィルムの射出口側端部とは反対側の端部を挟み込む後方挟み込み部材とを第1型に有することを特徴とする成形同時両面加飾金型。 After the first decorative film is placed along the mold bottom of the portion of the first mold having the injection opening that does not cover the first mold, and after the second decorative film is placed along the bottom of the second mold, the first mold and the second mold The mold is closed, and a molding resin is injected from the injection port of the first mold between the first decorative film and the second decorative film to form a resin molded product, and at the same time on both front and back surfaces of the resin molded product The molding simultaneous double-sided decoration mold used in the simultaneous molding and decorating method for adhering the decorative film, wherein the molding resin injected by sandwiching the injection port side end of the first decorative film is the first decorative film. The first mold has a sandwiching member that prevents collision with the exit side end, and a rear sandwiching member that sandwiches an end opposite to the exit side end of the first decorative film. Double-sided decorative mold for simultaneous molding. 射出口を有する第1型の射出口を覆わない部分の型底に第1加飾フィルムを沿わせるとともに第2型の型底に第2加飾フィルムを沿わせた後に第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させる成形同時加飾法に用いる成形同時両面加飾金型であって、第1加飾フィルムの射出口側端部を挟み込むことにより射出した成形樹脂が第1加飾フィルムの前記射出口側端部に衝突しないようにする第1挟み込み部材と、第1加飾フィルムの射出口側端部とは反対側の端部を挟み込む後方挟み込み部材とを第1型に有するとともに、第2加飾フィルムの射出口側端部を挟み込むことにより射出した成形樹脂が第2加飾フィルムの前記射出口側端部に衝突しないようにする第2挟み込み部材を第2型に有することを特徴とする成形同時両面加飾金型。 After the first decorative film is placed along the mold bottom of the portion of the first mold having the injection opening that does not cover the first mold, and after the second decorative film is placed along the bottom of the second mold, the first mold and the second mold The mold is closed, and a molding resin is injected from the injection port of the first mold between the first decorative film and the second decorative film to form a resin molded product, and at the same time on both front and back surfaces of the resin molded product The molding simultaneous double-sided decoration mold used in the simultaneous molding and decorating method for adhering the decorative film, wherein the molding resin injected by sandwiching the injection port side end of the first decorative film is the first decorative film. The first mold has a first sandwiching member that does not collide with the exit side end, and a rear sandwiching member that sandwiches the end opposite to the exit side end of the first decorative film, in the first mold, The injection is performed by sandwiching the end of the second decorative film on the injection port side. Resin the injection port side molding simultaneous double-side pressure Kazarikin type, characterized in that it comprises a second gripping members so as not to collide with the second type to the end of the second decoration film. 請求項1に記載の成形同時両面加飾金型を用いて、第1型の型底に第1加飾フィルムを沿わせるとともに第1加飾フィルムの射出口側端部を挟み込み部材で挟み込み、第1加飾フィルムの射出口側端部とは反対側の端部を後方挟み込み部材で挟み込み、他方で第2型の型底に第2加飾フィルムを沿わせ、第1型と第2型とを型閉めし、次に第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得ることを特徴とする成形同時両面加飾品の製造方法。 Using the molding simultaneous double-sided decorative mold according to claim 1, the first decorative film is placed along the mold bottom of the first mold, and the injection opening side end of the first decorative film is sandwiched between the sandwiching members, The end of the first decorative film opposite to the end on the injection port side is sandwiched by the rear sandwiching member, and on the other hand, the second decorative film is placed along the bottom of the second mold, and the first mold and the second mold The mold is then closed, and then a molding resin is injected from the injection port of the first mold between the first decorative film and the second decorative film to form a resin molded product, and at the same time both front and back surfaces of the resin molded product A method for producing a simultaneously molded double-sided decorative product, comprising: adhering a decorative film to a molded simultaneous double-sided decorative product. 請求項2に記載の成形同時両面加飾金型を用いて、第1型の型底に第1加飾フィルムを沿わせるとともに第1加飾フィルムの射出口側端部を第1挟み込み部材で挟み込み、第1加飾フィルムの射出口側端部とは反対側の端部を後方挟み込み部材で挟み込み、他方で第2型の型底に第2加飾フィルムを沿わせるとともに第2加飾フィルムの射出口側端部を第2挟み込み部材で挟み込み、第1型と第2型とを型閉めし、第1加飾フィルムと第2加飾フィルムとの間に第1型の射出口から成形樹脂を射出して樹脂成形品を成形すると同時に該樹脂成形品の表裏両面に加飾フィルムを接着させて成形同時両面加飾品を得ることを特徴とする成形同時両面加飾品の製造方法。 Using the molding simultaneous double-sided decorative mold according to claim 2, the first decorative film is placed along the mold bottom of the first mold, and the outlet side end of the first decorative film is a first sandwiching member. The end of the first decorative film opposite to the injection opening side end is sandwiched by the rear sandwiching member, and on the other hand, the second decorative film is placed along the mold bottom of the second mold and the second decorative film. The injection port side end of the first mold is sandwiched by the second sandwiching member, the first mold and the second mold are closed, and molding is performed from the first mold injection port between the first decorative film and the second decorative film. A method for producing a simultaneous molding double-sided decorative product, comprising: injecting a resin to form a resin molded product and simultaneously attaching a decorative film to both front and back surfaces of the resin molded product to obtain a simultaneous molding double-sided decorative product.
JP2006300999A 2006-11-06 2006-11-06 Molding simultaneous double-sided decorative mold and molding simultaneous double-sided decorative product manufacturing method Expired - Lifetime JP4421591B2 (en)