JP3087484U - Adhesive moldings and hooks - Google Patents

Adhesive moldings and hooks

Info

Publication number
JP3087484U
JP3087484U JP2002000270U JP2002000270U JP3087484U JP 3087484 U JP3087484 U JP 3087484U JP 2002000270 U JP2002000270 U JP 2002000270U JP 2002000270 U JP2002000270 U JP 2002000270U JP 3087484 U JP3087484 U JP 3087484U
Authority
JP
Japan
Prior art keywords
mating surface
hook
adhesive
molded body
adhesive molded
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP2002000270U
Other languages
Japanese (ja)
Inventor
由紀子 高橋
Original Assignee
大一鋼業株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 大一鋼業株式会社 filed Critical 大一鋼業株式会社
Priority to JP2002000270U priority Critical patent/JP3087484U/en
Application granted granted Critical
Publication of JP3087484U publication Critical patent/JP3087484U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

(57)【要約】 【課題】 アプリケーターなどの塗布機を用いず、熟練
を要することなく、容易かつ短時間のうちに掛止具本体
に保持させることのできるホットメルトタイプの接着剤
成形体を提供する。そのような接着剤成形体を備えた掛
止具を提供する。 【解決手段】 接着剤成形体4は、フック体3と被着体
に対する合せ面2Bとを備えた掛止具本体2の合せ面2
Bに加熱溶融状態で接合されて接合後に硬化されるホッ
トメルト接着剤を、合せ面2Bの大きさよりも小さい板
片状に成形してなる。掛止具1は、掛止具本体2と接着
剤成形体4との組み合わせでなる。合せ面2Bに凹凸面
領域2Aが形成する。
(57) [Problem] To provide a hot-melt type adhesive molded body that can be easily and quickly held on a latch body without using a coating machine such as an applicator and without skill. provide. A hook provided with such an adhesive molded body is provided. SOLUTION: An adhesive molded body 4 has a mating surface 2 of a hook body 2 having a hook body 3 and a mating surface 2B for an adherend.
A hot-melt adhesive that is joined to B in a heat-melted state and cured after joining is formed into a plate piece smaller than the size of the mating surface 2B. The latch 1 is a combination of a latch main body 2 and an adhesive molded body 4. An uneven surface area 2A is formed on the mating surface 2B.

Description

【考案の詳細な説明】[Detailed description of the invention]

【0001】[0001]

【考案の属する技術分野】[Technical field to which the invention belongs]

本考案は、例えば壁面、柱、天井等の被着体に貼着して額ぶちやカレンダー等 を掛けるための掛止具に用いる接着剤成形体及びその接着剤成形体を用いた上記 掛止具に関する。 The present invention relates to an adhesive molded article used as a fastener for attaching a frame, a calendar, or the like by being attached to an adherend such as a wall surface, a pillar, or a ceiling, and the above-described latch using the adhesive molded article. About.

【0002】[0002]

【従来の技術】[Prior art]

実願2000−001773号(先行例)によってホットメルト接着剤を用い た掛止具についての記載がある。この掛止具は、物を掛止するフック体を形成し た掛止具本体の裏面にホットメルト接着剤層を接合しておき、該ホットメルト接 着剤層を溶融させて壁面や柱等の被着体に接着して取付けるものである。また、 この掛止具では、工場で出荷前に、摂氏120〜160度の温度で溶融させたホ ットメルト接着剤を、アプリケーター(塗付機)で掛止具本体の裏面に円形板状 に象って塗布した後に、そのホットメルト接着剤を硬化させている。 Japanese Utility Model Application No. 2000-001773 (prior example) describes a fastener using a hot melt adhesive. In this hook, a hot-melt adhesive layer is bonded to the back surface of a hook body having a hook body for hooking an object, and the hot-melt adhesive layer is melted to form a wall surface or a pillar. To be adhered to the adherend. In addition, in this hanging tool, a hot melt adhesive melted at a temperature of 120 to 160 degrees Celsius before being shipped from a factory is applied to the back surface of the hanging tool body by an applicator (coating machine) in a circular plate shape. Then, the hot melt adhesive is cured.

【0003】[0003]

【考案が解決しようとする課題】[Problems to be solved by the invention]

しかし、先行例では、ホットメルト接着剤を掛止具本体の裏面に保持させると きにアプリケーター(塗付機)を用いる必要があるので作業が比較的大掛かりに なり、しかも、アプリケーターで掛止具本体の裏面に円形板状に象って塗布する 必要があるので作業に熟練が必要であり、さらに、その塗布後にホットメルト接 着剤を硬化させる必要があるので、掛止具本体の裏面にホットメルト接着剤を保 持させる作業を完了させるまでに比較的時間がかかるという問題があった。 However, in the prior example, since the hot melt adhesive is required to be held on the back surface of the hook body by using an applicator (coating machine), the work becomes relatively large, and furthermore, the applicator uses the hook. It is necessary to apply it in the shape of a circular plate on the back of the main body, so it requires skill in the work, and it is necessary to cure the hot melt adhesive after the application. There has been a problem that it takes a relatively long time to complete the operation of holding the hot melt adhesive.

【0004】 本考案は以上の問題に鑑みてなされたものであり、アプリケーターなどの塗布 機を用いず、熟練を要することなく、容易かつ短時間のうちに掛止具本体に保持 させることのできるホットメルトタイプの接着剤成形体を提供することを目的と する。[0004] The present invention has been made in view of the above problems, and can be easily and quickly held on a latch body without using an applicator such as an applicator and without any skill. An object of the present invention is to provide a hot melt type adhesive molded article.

【0005】 また、本考案は、そのような接着剤成形体を備えた掛止具を提供することを目 的とする。Another object of the present invention is to provide a hook provided with such an adhesive molded body.

【0006】[0006]

【課題を解決するための手段】[Means for Solving the Problems]

本考案に係る接着剤成形体は、フック体と被着体に対する合せ面とを備えた掛 止具本体の上記合せ面に加熱溶融状態で接合されて接合後に硬化されるホットメ ルト接着剤を、上記合せ面の大きさよりも小さい板片状に成形してなるものであ る。 The adhesive molded product according to the present invention comprises a hot-melt adhesive which is joined in a heated and melted state to the above-mentioned mating surface of a hook body having a hook body and a mating surface with an adherend, and then cured after joining. It is formed into a plate piece smaller than the size of the mating surface.

【0007】 この接着剤成形体は、手で持って片面側を加熱溶融させた後、その溶融面を掛 止具本体の合せ面に押し付けるだけで掛止具本体に接合でき、しかも、接着剤成 形体が板片状であるために、溶融面は掛止具本体の合せ面に押し付けた後、短時 間で硬化して強固に合せ面に接合される。さらに、掛止具本体の合せ面の大きさ よりも小さい板片状に成形されているために熟練を要することなく、その合せ面 の所定箇所に誰でもが容易にかつ短時間で接合することが可能である。その上、 この接着剤成形体は、シート状に成形したホットメルト接着剤のシートから打抜 き型を用いて打ち抜くという方法で一度に多数を安価に製作することが可能であ るという利点を持っている。この接着剤成形体は、以上のような作用を発揮する ため、工場の作業員が掛止具本体の合せ面に保持させる場合でも、ユーザが掛止 具本体の合せ面に保持させる場合でも、その作業を容易に行うことができる。The adhesive molded body can be joined to the main body of the hook by simply holding the hand and melting one side by heating and then pressing the melted surface against the mating surface of the main body of the hook. Since the molded body is in the shape of a plate, the molten surface is pressed against the mating surface of the latch body, then hardens in a short time and is firmly joined to the mating surface. Furthermore, since it is formed into a plate piece smaller than the size of the mating surface of the latch body, anyone can easily and quickly join the specified location on the mating surface without skill. Is possible. In addition, this adhesive molded article has the advantage that a large number can be manufactured at a time at low cost by punching out a hot melt adhesive sheet formed into a sheet shape using a punching die. have. Since this adhesive molded body exerts the above-described effects, it can be used regardless of whether the worker at the factory holds it on the mating surface of the main body of the hook or the user holds it on the mating surface of the main body of the hook. The work can be easily performed.

【0008】 本考案に係る掛止具は、物を掛止するためのフック体と被着体に対する合せ面 とを備えた掛止具本体と、その掛止具本体の上記合せ面に加熱溶融状態で接合さ れて接合後に硬化されるホットメルト接着剤を上記合せ面の大きさよりも小さい 板片状に成形してなる接着剤成形体との組み合わせでなる。この掛止具は、接着 剤成形体の片面側を加熱溶融させて掛止具本体の合せ面に押し付けるだけで掛止 具本体の合せ面に保持させることができ、そのように掛止具本体の合せ面に保持 させた接着剤成形体を加熱溶融させて被着面に押し付けるだけで、掛止具を被着 面に貼着することが可能である。[0008] A latch according to the present invention includes a latch main body having a hook body for latching an object and a mating surface for an adherend, and heat-melting on the mating surface of the latch main body. It is a combination with a hot melt adhesive that is joined in a state and cured after joining into a plate shape smaller than the size of the mating surface. This latch can be held on the mating surface of the latch body only by heating and melting one side of the adhesive molded body and pressing against the mating surface of the latch body. By simply heating and melting the adhesive molded body held on the mating surface and pressing it against the surface to be adhered, it is possible to attach the hook to the surface to be adhered.

【0009】 本考案に係る掛止具は、上記合せ面が凹凸面であることが望ましい。これによ れば、接着剤成形体と合せ面との接合面積が大きく確保されるため、接着剤成形 体を強固に合せ面に接合しておくことが可能である。[0009] In the latch according to the present invention, it is preferable that the mating surface is an uneven surface. According to this, a large bonding area between the adhesive molded body and the mating surface is secured, so that the adhesive molded body can be firmly joined to the mating surface.

【0010】[0010]

【考案の実施の形態】[Embodiment of the invention]

図1において(A)はこの考案にかかる接着剤成形体4と、その接着剤成形体 4を用いて被着面に貼着される掛止具本体の裏面側を示した斜視図、(B)は接 着剤成形体の製作方法説明図、(C)は接着剤成形体の他の製作方法説明図であ る。また、図2は掛止具本体の正面側を示す斜視図である。 In FIG. 1, (A) is a perspective view showing an adhesive molded body 4 according to the present invention, and a back surface side of a hook body adhered to an adherend using the adhesive molded body 4, () Is an explanatory view of a method of manufacturing an adhesive molded article, and (C) is an explanatory view of another method of manufacturing an adhesive molded article. FIG. 2 is a perspective view showing the front side of the hook body.

【0011】 図1又は図2において、1は掛止具で、この掛止具1は、掛止具本体2、フッ ク体3、ホットメルトタイプの接着剤成形体4とを備えている。In FIG. 1 or FIG. 2, reference numeral 1 denotes a hook, and the hook 1 includes a hook body 2, a hook body 3, and a hot melt type adhesive molded body 4.

【0012】 掛止具本体2は、合成樹脂により方形平板状に形成され、その裏面が壁面、柱 、天井等の被着体に対する合せ面2Bとして形成されていて、その合せ面2Bに は、接着剤成形体4の接合領域としての微細な凹凸を有する矩形の凹凸面領域2 Aが備わっている。凹凸面領域2Aの微細な凹凸は、掛止具本体2の成型金型に 加工を施し、掛止具本体2の成型の際に同時に形成されるものである。2Cは掛 止具本体2の表面に形成された装飾面で、両側方向に湾曲面を連続して形成され 、かつその両側方向中央部の上端から下端にかけてフック体3が嵌合するための 嵌合溝2Dが形成されている。The main body 2 of the hook is formed of a synthetic resin in the shape of a rectangular flat plate, and its back surface is formed as a mating surface 2B for an adherend such as a wall surface, a pillar, a ceiling, and the like. A rectangular uneven surface area 2A having fine unevenness as a bonding area of the adhesive molded body 4 is provided. The fine unevenness of the uneven surface area 2A is formed at the same time as the processing of the molding die of the hook body 2 and the molding of the hook body 2. Reference numeral 2C denotes a decorative surface formed on the surface of the hook body 2, having a curved surface continuously formed in both sides, and a fitting for fitting the hook body 3 from the upper end to the lower end of the center part in the both sides. A mating groove 2D is formed.

【0013】 フック体3は、長尺の金属平板で形成され、先端部を厚み方向一方へ略U字状 に折返し形成し、後端を厚み方向他方へL字状に折り曲げて形成し、全体が略釣 針状に形成されている。このフック体3は、フック体3のU字形の湾曲部の付け 根部分を嵌合溝2Dの上端に嵌合させた後、後端のL字状の部分が掛止具本体2 の上端部に引掛かるまで、フック体3を下方へスライドさせながら掛止具本体2 に嵌合する。尚、フック体3と掛止具本体2の表面が面一となるように掛止具本 体2の上端部に切込部2Eが設けられている。[0013] The hook body 3 is formed of a long metal flat plate, and is formed by bending a front end portion in a U-shape in one direction in the thickness direction and bending a rear end in an L-shape in the other direction in the thickness direction. Is formed in a substantially hook shape. The hook body 3 is formed such that the base of the U-shaped curved portion of the hook body 3 is fitted to the upper end of the fitting groove 2D, and the L-shaped portion at the rear end is the upper end of the hook body 2. The hook body 3 is fitted to the hook body 2 while sliding the hook body 3 downward until the hook body 3 is hooked. A notch 2E is provided at the upper end of the hook body 2 so that the surfaces of the hook body 3 and the hook body 2 are flush with each other.

【0014】 図1(A)に示してある接着剤成形体4は、ホットメルト接着剤を、上記掛止 具本体2の合せ面2Bの大きさよりも小さい円形の板片状に成形してなる。接着 剤成形体4を構成するホットメルト接着剤には、ポリアミド系、ポリエステル系 、合成ゴム系等種々のものを用い得るが、中でも、ポリオレフィン系のEVA( エチレン・酢酸ビニル共重合体)は、製本や電気機器自動車等の製造過程で主に 使用されている接着強度に優れたものであり、掛止具の分野ではそれほどは用い られていない。この実施形態では、接着強度に優れているポリオレフィン系のE VAをホットメルト接着剤として用いていて、このものは、摂氏120〜160 度の温度で溶融する。The adhesive molded body 4 shown in FIG. 1A is formed by molding a hot melt adhesive into a circular plate piece smaller than the size of the mating surface 2 B of the latch body 2. . Various hot melt adhesives such as polyamide-based, polyester-based, and synthetic rubber-based adhesives can be used as the hot-melt adhesive that forms the adhesive molded body 4. Among them, polyolefin-based EVA (ethylene / vinyl acetate copolymer) is used. It has excellent adhesive strength, which is mainly used in the manufacturing process of bookbinding and electric equipment cars, and is not used so much in the field of fasteners. In this embodiment, a polyolefin-based EVA having excellent adhesive strength is used as a hot melt adhesive, which melts at a temperature of 120 to 160 degrees Celsius.

【0015】 上記した円形の板片状の接着剤成形体4は、図1(B)のように、シート状に 成形したホットメルト接着剤のシートSから打抜き型を用いて打ち抜くという方 法で一度に多数を安価に製作することが可能である。打抜き型には手の平に納ま る程度の大きさの円筒体を好適に用いることが可能である。また、図1(C)の ように、浅底の円形凹所12を有する成形型13の上記凹所12に溶融状態のホ ットメルト接着剤を流し込んで円形に成形し、硬化後に接着剤成形体4を離型す ることによっても容易かつ安価に製作することができる。As shown in FIG. 1 (B), the above-mentioned circular plate-shaped adhesive molded body 4 is punched out from a sheet S of hot melt adhesive formed into a sheet using a punching die. Many can be manufactured at a low cost at one time. For the punching die, it is possible to suitably use a cylinder having a size that fits in the palm of the hand. As shown in FIG. 1 (C), a hot melt adhesive in a molten state is poured into the recess 12 of a mold 13 having a circular recess 12 having a shallow bottom to form a circular shape. 4 can be easily and inexpensively manufactured by releasing the mold.

【0016】 この接着剤成形体4は、手で持って片面側をライターやマッチ、あるいは専用 加熱具を用いて加熱溶融させた後、その溶融面を掛止具本体2の合せ面2Bに押 し付けるだけで掛止具本体2に接合でき、しかも、接着剤成形体4が板片状であ るために、溶融面は掛止具本体2の合せ面2Bに押し付けた後、短時間で硬化し て強固に合せ面に接合される。この場合、接着剤成形体4が掛止具本体2の合せ 面2Bの大きさよりも小さい板片状に成形されているために熟練を要することな く、その合せ面2Bの所定箇所に誰でもが容易にかつ短時間で接合することがで きる。そして、図例のように合せ面2Bに凹凸面領域2Aを形成しておき、その 凹凸面領域2Aに接着剤成形体4の溶融面を押し付けて硬化させるようにすると 、接着剤成形体4と合せ面2Bとの接合面積が大きく確保されるため、接着剤成 形体4を強固に合せ面2Bに接合することができる。接着剤成形体4を合せ面2 Bに接合する作業は、工場の作業員が出荷前に行っておいても、ユーザが使用時 に行うようにしてもよい。The adhesive molded body 4 is heated and melted on one side by using a lighter, a match, or a special heating tool, and then the melted surface is pressed against the mating surface 2 B of the hook body 2. Since the adhesive molded body 4 can be joined to the hook body 2 by simply attaching it, and the adhesive molded body 4 is in the form of a plate, the molten surface is pressed against the mating surface 2B of the hook body 2 in a short time. It hardens and is firmly joined to the mating surface. In this case, since the adhesive molded body 4 is formed in a plate-like shape smaller than the size of the mating surface 2B of the hook body 2, no skill is required, and anyone can set a predetermined position on the mating surface 2B. Can be easily and quickly joined. Then, as shown in the example of the drawing, the uneven surface area 2A is formed on the mating surface 2B, and the molten surface of the adhesive molded body 4 is pressed against the uneven surface area 2A to be cured. Since a large bonding area with the mating surface 2B is ensured, the adhesive molded body 4 can be firmly joined to the mating surface 2B. The operation of joining the adhesive molded body 4 to the mating surface 2B may be performed by a factory worker before shipment, or may be performed by a user at the time of use.

【0017】 次に掛止具本体2の合せ面2Bに接着剤成形体4を接合してなる掛止具1の取 付方法を説明する。Next, a description will be given of a method of attaching the hook 1 formed by bonding the adhesive molded body 4 to the mating surface 2B of the hook body 2.

【0018】 まず、図3のように接着剤成形体4にライター5やマッチなどの炎を当てがい 、その接着剤成形体4を加熱溶融させ、溶融状態の接着剤成形体4を壁面や柱等 の被着体6(図4参照)に押し付ける。このようにすると、接着剤成形体4が合 せ面2Bの凹凸面領域2Aと被着体6との間に薄く拡がり、その溶融部分が急速 に冷却されて硬化し、掛止具1が被着体6に貼着される。こうして被着体6に貼 着して取付けられた掛止具1のフック体3に直接、額縁等を掛止して使用しても よいし、図4のように棚8を掛止具1に掛止し、この棚8に物を乗せるようにし て使用してもよい。First, as shown in FIG. 3, a flame such as a lighter 5 or a match is applied to the adhesive molded body 4 and the adhesive molded body 4 is heated and melted. Etc. to the adherend 6 (see FIG. 4). In this way, the adhesive molded body 4 spreads thinly between the uneven surface area 2A of the joining surface 2B and the adherend 6, the molten portion thereof is rapidly cooled and hardened, and the hook 1 is covered. Affixed to the body 6. A frame or the like may be directly hooked on the hook body 3 of the hook 1 attached and attached to the adherend 6 in this manner, or the shelf 8 may be attached to the hook 1 as shown in FIG. The shelf 8 may be used by placing an object on it.

【0019】 加熱溶融した接着剤成形体4はドロドロした状態でほぼ液状になっている。し かし、接着剤成形体4がホットメルト接着剤であり、そのホットメルト接着剤は 粘度を有しているため、接着剤成形体4が凹凸面領域2Aから落下することはな い。尚、接着剤成形体4を強く押圧して薄く拡がらせた方が早く温度が下がるの で、短時間に接着が必要な時は接着剤成形体4を強く押圧することが望ましい。The adhesive molded body 4 that has been heated and melted is almost in a liquid state in a slime state. However, since the adhesive molded product 4 is a hot melt adhesive and the hot melt adhesive has a viscosity, the adhesive molded product 4 does not fall from the uneven surface area 2A. In addition, it is desirable to strongly press the adhesive molded body 4 when bonding is required in a short time because the temperature decreases more quickly when the adhesive molded body 4 is strongly pressed and spread thinly.

【0020】 被着体6に貼着した掛止具1が何かの拍子に剥がれてしまった場合、或いは、 掛止具1の位置を付け代えたい場合などは、掛止具本体2と被着体6との隙間に マイナスドライバーを差し込んで両者を離間させるように動かすと、被着体6か ら接着剤成形体4が剥れる。そのため、再び、上記の手順を繰り返せば、掛止具 1を被着体6に取付けることができる。When the hook 1 stuck to the adherend 6 has been peeled off in some way, or when it is desired to change the position of the hook 1, the hook body 2 and the hook When a flathead screwdriver is inserted into the gap with the adherend 6 and moved so as to separate them, the adhesive molded body 4 is peeled from the adherend 6. Therefore, by repeating the above procedure again, the hook 1 can be attached to the adherend 6.

【0021】 本考案の掛止具1は、物を掛止するフック体を形成した掛止具本体2の裏面に 接着剤成形体4を接合し、その接着剤成形体4を溶融させて被着体6に貼着する ものであることから、被着体6側に多少の凹凸が存在していても強固に掛止具1 を被着体6に取付けることができる。すなわち、溶融状態の接着剤成形体4を被 着体6に貼着するから、接着剤成形体4の溶融部分が被着体6の凹凸に入り込み 確実に被着体6の凹凸をとらえることができて、かえって、被着体6に多小の凹 凸が有る方が望ましいといえる。In the hook 1 of the present invention, an adhesive molded body 4 is joined to the back surface of a hook body 2 having a hook body for hooking an object, and the adhesive molded body 4 is melted to be covered. Since it is to be adhered to the body 6, the hook 1 can be firmly attached to the body 6 even if there is some unevenness on the body 6 side. In other words, since the adhesive molded body 4 in a molten state is adhered to the adherend 6, the molten portion of the adhesive molded body 4 enters the irregularities of the adherend 6 to reliably capture the irregularities of the adherend 6. It can be said that it is more desirable that the adherend 6 has many concaves and convexes.

【0022】[0022]

【考案の効果】[Effect of the invention]

以上のように、本考案によれば、アプリケーターなどの塗布機を用いず、熟練 を要することなく、容易かつ短時間のうちに掛止具本体に保持させることのでき るホットメルトタイプの接着剤成形体を提供することが可能になる。また、本考 案は、そのような接着剤成形体を備えた掛止具を提供することが可能になる。 As described above, according to the present invention, a hot-melt type adhesive that can be easily and quickly held on a latch body without using a coating machine such as an applicator and without any skill is required. It becomes possible to provide a molded article. Further, the present invention can provide a hook having such an adhesive molded body.

【図面の簡単な説明】[Brief description of the drawings]

【図1】(A)はこの考案にかかる接着剤成形体や掛止
具本体などを示した斜視図、(B)は接着剤成形体の製
作方法説明図、(C)は接着剤成形体の他の製作方法説
明図である。
1 (A) is a perspective view showing an adhesive molded body and a latch body according to the present invention, FIG. 1 (B) is an explanatory view of a method of manufacturing the adhesive molded body, and FIG. 1 (C) is an adhesive molded body. It is another manufacturing method explanatory drawing.

【図2】掛止具本体の正面側を示す斜視図である。FIG. 2 is a perspective view showing a front side of a hook body.

【図3】掛止具の取付方法を示す要領図である。FIG. 3 is a schematic view showing a method of attaching a hook.

【図4】掛止具の使用状態を例示した斜視図である。FIG. 4 is a perspective view illustrating a use state of the hook.

【符号の説明】[Explanation of symbols]

2 掛止具本体 2A 凹凸面領域 2B 合せ面 3 フック体 4 接着剤成形体 6 被着体 2 Hook main body 2A Uneven surface area 2B Mating surface 3 Hook body 4 Adhesive molded body 6 Adherend

Claims (3)

【実用新案登録請求の範囲】[Utility model registration claims] 【請求項1】 フック体と被着体に対する合せ面とを備
えた掛止具本体の上記合せ面に加熱溶融状態で接合され
て接合後に硬化されるホットメルト接着剤を、上記合せ
面の大きさよりも小さい板片状に成形してなることを特
徴とする接着剤成形体。
1. A hot-melt adhesive which is joined in a heat-melted state to the above-mentioned mating surface of a hook body having a hook body and a mating surface with an adherend, and which is cured after joining, is made to have a size of the mating surface. An adhesive molded article formed by molding into a smaller piece.
【請求項2】 物を掛止するためのフック体と被着体に
対する合せ面とを備えた掛止具本体と、その掛止具本体
の上記合せ面に加熱溶融状態で接合されて接合後に硬化
されるホットメルト接着剤を成形型を用いて上記合せ面
の大きさよりも小さい板片状に成形してなる接着剤成形
体との組み合わせでなる掛止具。
2. A hooking tool main body having a hook body for hooking an object and a mating surface to an adherend, and being joined to the mating surface of the hooking tool body in a heated and molten state, and after joining. A latch comprising a combination of a hot melt adhesive to be cured and an adhesive molded product formed by using a molding die into a plate piece smaller than the size of the mating surface.
【請求項3】 上記合せ面に凹凸面領域が形成されてい
る請求項2に記載した掛止具。
3. The latch according to claim 2, wherein an uneven surface area is formed on the mating surface.
JP2002000270U 2002-01-24 2002-01-24 Adhesive moldings and hooks Expired - Lifetime JP3087484U (en)