JP3040433U - Parts for welded joints - Google Patents
Parts for welded jointsInfo
- Publication number
- JP3040433U JP3040433U JP1997000550U JP55097U JP3040433U JP 3040433 U JP3040433 U JP 3040433U JP 1997000550 U JP1997000550 U JP 1997000550U JP 55097 U JP55097 U JP 55097U JP 3040433 U JP3040433 U JP 3040433U
- Authority
- JP
- Japan
- Prior art keywords
- welding
- joint member
- reinforcing bar
- welded
- interval
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
(57)【要約】
【課題】 鉄筋を突き合わせて溶接する際のルート間隔
を簡単に決める。
【解決する手段】 2本の鉄筋5、5を突き合わせて溶
接する際に、突合わせ部の外側に被せ、鉄筋5、5と一
緒に溶接する継手用部材1であって、該継手用部材1は
鉄筋の外周を略半周する円弧状に形成され、鉄筋の方向
に沿う側縁の略中央部にルート間隔に対応する幅にて切
欠3が形成されている。
(57) [Abstract] [Problem] To easily determine a route interval when butt-welding reinforcing bars. SOLUTION: When joining two welded bars 5 and 5 to each other for welding, the joint member 1 is put on the outer side of the butted portion and welded together with the rebars 5, 5. Is formed in an arc shape that makes a substantially half circumference of the outer periphery of the reinforcing bar, and a notch 3 is formed in a substantially central portion of a side edge along the direction of the reinforcing bar with a width corresponding to the root interval.
Description
【0001】[0001]
本考案は、鉄筋を突合わせ溶接する際に、定められたルート間隔を存して鉄筋 を対向させることが出来、又、溶接時の溶接金属の溶け落ちを防止してルート間 隔に確実に溶接金属を充満させ、強度的に信頼性の高い溶接継手を構成できる溶 接継手用部材に関するものである。 The present invention enables the reinforcing bars to face each other at a predetermined route interval when butt-welding the reinforcing bars, and also prevents burn-through of the weld metal during welding to ensure reliable spacing between the routes. The present invention relates to a welding joint member that can be filled with weld metal and can form a welded joint having high strength reliability.
【0002】[0002]
従来、筒体の周面の略中央部に溶接用の開口部を開設し、ルート間隔を決める ためのストッパを内面に突設した溶接継手用筒体が案出されている(特開昭62 −4906号)。 これは、筒体の両端から鉄筋を挿入し、鉄筋の先端をストッパに当ててルート 間隔を確保し、開口部から溶接ワイヤーを挿入して、炭酸ガスシールド溶接によ りルート間隔を溶接金属によって埋めて、鉄筋を強固に接続するものである。 BACKGROUND ART Conventionally, a welding joint cylinder has been devised in which an opening for welding is opened in a substantially central portion of a peripheral surface of a cylinder, and a stopper for determining a route interval is projected on an inner surface (JP-A-62-62). -4906). This is done by inserting the rebar from both ends of the cylinder, applying the tip of the rebar to the stopper to secure the route interval, inserting the welding wire from the opening, and using carbon dioxide shield welding to set the route interval by welding metal. It is buried and connects the reinforcing bars firmly.
【0003】 上記溶接用筒体のルート間隔を決めるためのストッパは、溶接時に根元が溶断 され、ストッパ自体が完全に溶融しないまま溶接金属の表面に浮き上がり、この 状態で固化すれば、溶接検査の際に問題となる。 本考案は、上記問題を解決できる溶接継手用部材を明らかにするものである。The stopper for determining the root interval of the welding cylinder is melted at the root at the time of welding, and the stopper itself floats on the surface of the weld metal without being completely melted, and if solidified in this state, it can be used for welding inspection. It becomes a problem. The present invention discloses a member for a welded joint that can solve the above problems.
【0004】[0004]
本考案の請求項1の溶接継手用部材(1)は、鉄筋(5)(5)の外周を略半周する 円弧状に形成され、鉄筋の方向に沿う側縁の略中央部にルート間隔に対応する幅 にて切欠(3)が開設されている。 The member (1) for welded joints according to claim 1 of the present invention is formed in an arc shape which substantially circumscribes the outer circumference of the reinforcing bars (5) (5), and has a root interval at a substantially central portion of a side edge along the direction of the reinforcing bars. A notch (3) is opened in the corresponding width.
【0005】 本考案の請求項2の溶接継手用部材(1)は、鉄筋(5)(5)の外周を略半周する 円弧状に形成され、鉄筋の方向に沿う側縁の略中央部に隣合わせに2つの切欠( 3)(3)が開設されている。The member (1) for a welded joint according to claim 2 of the present invention is formed in an arc shape which substantially circumscribes the outer circumference of the reinforcing bar (5) (5), and is formed at a substantially central portion of the side edge along the direction of the reinforcing bar. Two notches (3) (3) are opened next to each other.
【0006】[0006]
本考案の溶接継手用部材(1)は、鉄筋(5)(5)の外周を半周する円弧状に形成 されているため、鉄筋の突合わせ部に跨がって、外側から被せることができ、作 業性がよい。 Since the member (1) for welded joints of the present invention is formed in an arc shape that half-circulates the outer circumference of the reinforcing bars (5), (5), it can be covered from the outside by straddling the abutting portion of the reinforcing bars. , Workability is good.
【0007】 又、請求項1の考案では、溶接継手用部材(1)の切欠(3)の幅に対応して、ル ート間隔を決定することができ、作業者の感に頼ることなく、適正なルート間隔 を設定できる。 従来の溶接用筒体におけるルート間隔用ストッパの様に、継手用部材(1)の内 側への突出物は存在しないため、溶接時にストッパの根元が溶断され、ストッパ 自体が完全に溶融しない状態で溶接金属の表面に浮き上がった状態で固化する不 都合は生じない。Further, in the invention of claim 1, the root interval can be determined in accordance with the width of the notch (3) of the member (1) for welded joints, without depending on the feeling of the operator. , You can set the proper route interval. Unlike the stopper for the root gap in the conventional welding cylinder, there is no protrusion to the inside of the joint member (1), so the root of the stopper is melted during welding and the stopper itself does not completely melt. Therefore, there is no inconvenience of solidifying while being floated on the surface of the weld metal.
【0008】 請求項2の考案では、切欠(3)(3)間の幅及び切欠自体の幅に対応して複数種 類のルート間隔を設定できる利点がある。According to the second aspect of the invention, there is an advantage that a plurality of types of route intervals can be set in accordance with the width between the notches (3) and (3) and the width of the notch itself.
【0009】[0009]
以下、図面に示す実施例に基づき、本考案を説明するが、実施例は本考案を説 明するためのものであって、実用新案登録請求の範囲を限定し、或は減縮する様 に解すべきではない。 BEST MODE FOR CARRYING OUT THE INVENTION Hereinafter, the present invention will be described based on the embodiments shown in the drawings, but the embodiments are for explaining the present invention, and are understood so as to limit or reduce the scope of utility model registration claims. Should not be.
【0010】 本考案で使用する溶接継手用部材(1)は、厚み3.2〜6mm、長さ25〜60mmの略長 方形の板を、幅方向を略1/2円弧に湾曲して形成されており、曲率半径は溶接 すべき鉄筋の呼び径の1/2よりも少し大である。 図3に2点鎖線で示す如く、溶接継手用部材(1)の幅方向の両端は、該部材( 1)の直径線を越えて、少し平行に延ばしてもよい。The member (1) for welded joints used in the present invention is formed by bending a substantially rectangular plate having a thickness of 3.2 to 6 mm and a length of 25 to 60 mm into a substantially half arc in the width direction. The radius of curvature is slightly larger than 1/2 of the nominal diameter of the reinforcing bar to be welded. As shown by the chain double-dashed line in FIG. 3, both ends in the width direction of the welded joint member (1) may extend slightly parallel to each other beyond the diameter line of the member (1).
【0011】 溶接継手用部材(1)は、長手方向の略中央部内面に、周方向の全長に延びる溝 条(2)を形成し、溝条(2)の一端に切欠(3)を開設している。 又、溝条(2)の長さ方向の中央部及び両端側に溶接検査用の貫通孔(4)を開設 している。貫通孔(4)は、直径が2〜3mmであって、溶接時の溶接金属は流れ出 ない程の小径である。The welded joint member (1) is provided with a groove (2) extending along the entire length in the circumferential direction on the inner surface of the substantially central portion in the longitudinal direction, and a notch (3) is formed at one end of the groove (2). doing. In addition, a through hole (4) for welding inspection is provided at the center and both ends of the groove (2) in the longitudinal direction. The through hole (4) has a diameter of 2 to 3 mm and is small enough to prevent the weld metal from flowing out during welding.
【0012】 上記、溝条(2)、切欠(3)、貫通孔(4)は、溶接継手用部材(1)がフラットな 板体の時に、プレス装置によって加工され、その後、曲げ加工して図1に示す溶 接継手用部材(1)が完成する。The groove (2), the notch (3), and the through hole (4) are processed by a press machine when the welding joint member (1) is a flat plate, and then bent. The welding joint member (1) shown in FIG. 1 is completed.
【0013】 然して、図2の如く、溶接継手用部材(1)の内面上にて溶接すべき2本の鉄筋 を対向させる。この時、鉄筋間の間隔を切欠(3)の幅に合わせて設定し、溶接継 手用部材(1)を溶接により鉄筋に仮付けする。However, as shown in FIG. 2, the two reinforcing bars to be welded are opposed to each other on the inner surface of the welded joint member (1). At this time, the interval between the reinforcing bars is set according to the width of the notch (3), and the welding joint member (1) is temporarily attached to the reinforcing bar by welding.
【0014】 次に、鉄筋間の間隔、即ち、ルート間隔に炭酸ガスシールド半自動溶接を施し 、ルート間隔を溶接金属で充満させる。 溶接は、溶接継手用部材(1)の底側から溶接金属を多層に盛って行なうが、最 下層に生じ易い溶接欠陥は、溶接継手用部材(1)の溝条(2)内に位置するため、 鉄筋の端面が対向する領域は全体に良好な溶接部分となり、溶接強度及び信頼性 が向上する。Next, carbon dioxide shield semi-automatic welding is performed on the interval between the reinforcing bars, that is, the root interval, and the root interval is filled with weld metal. Welding is performed by stacking multiple layers of weld metal from the bottom side of the member for welded joint (1), but the welding defect that is likely to occur in the lowermost layer is located in the groove (2) of the member for welded joint (1). Therefore, the region where the end faces of the reinforcing bars face each other becomes a good welded part as a whole, and the welding strength and reliability are improved.
【0015】 溶接完了後、貫通孔(4)からルート間隔の底側の溶接金属の埋まり状態が目視 でき、非破壊検査の様に大掛かりな装置や、手間を必要とせず、簡単に溶接継手 の検査を行なうことができる。After the welding is completed, the filling state of the weld metal on the bottom side of the route interval can be visually observed from the through hole (4), and it does not require a large-scale device such as nondestructive inspection or labor, and the welded joint can be easily welded. An inspection can be performed.
【0016】 図5は、溶接継手用部材(1)の他の実施例を示しており、一方の側縁の中央部 寄りに、隣り合わせに2箇所に切欠(3)(3)を開設している。 切欠(3)(3)間の幅は、ルート間隔に対応しており、又、両切欠(3)の幅は、 該ルート間隔と同じ或いは、それよりも広く、又は狭く開設されている。 溝条(2)の幅は、両切欠(3)の外端間に対応している。FIG. 5 shows another embodiment of the welded joint member (1), in which two notches (3) and (3) are formed adjacent to each other near the center of one side edge. There is. The width between the notches (3) and (3) corresponds to the root interval, and the width of both notches (3) is the same as, wider than, or narrower than the root interval. The width of the groove (2) corresponds between the outer ends of the notches (3).
【0017】 図5の場合、鉄筋間の間隔を切欠(3)(3)間の幅に対応させるか、或いは切欠 (3)自体の幅に対応させるかによって、2種類のルート間隔を選択できる。 2つの切欠(3)(3)の幅長さを互いに違えれば、3種類のルート間隔を選択で きる。In the case of FIG. 5, two types of route intervals can be selected depending on whether the distance between the reinforcing bars corresponds to the width between the notches (3) and (3) or the width of the notch (3) itself. . If the widths of the two notches (3) and (3) are different from each other, three types of route intervals can be selected.
【0018】 図6、図7は溝条(2)を省略した溶接継手用部材(1)の他の実施例を示してい る。6 and 7 show another embodiment of the welded joint member (1) in which the groove (2) is omitted.
【0019】 上記の如く本考案の溶接継手用部材(1)は、鉄筋の外周を略1/2周する円弧 状に形成されているため、突合わせ状態の鉄筋の突合わせ部に跨がって、外側か ら被せることができ、作業性がよい。As described above, since the welded joint member (1) of the present invention is formed in the shape of an arc that makes about 1/2 circumference of the outer circumference of the reinforcing bar, it does not straddle the butt portion of the reinforced reinforcing bars. Therefore, it can be covered from the outside and workability is good.
【0020】 又、溶接継手用部材(1)の切欠(3)の幅或いは切欠(3)間の幅に対応して、ル ート間隔を決定することができ、作業者の感に頼ることなく、適正なルート間隔 を確保できる。Further, the root interval can be determined in accordance with the width of the notch (3) of the welded joint member (1) or the width between the notches (3), depending on the feeling of the operator. It is possible to secure proper route intervals.
【図1】第1実施例の溶接継手用部材の斜面図である。FIG. 1 is a perspective view of a welded joint member of a first embodiment.
【図2】ルート間隔を決める説明図である。FIG. 2 is an explanatory diagram for determining a route interval.
【図3】図2のA−A線に沿う断面図である。FIG. 3 is a sectional view taken along line AA of FIG. 2;
【図4】溶接継手部の断面図である。FIG. 4 is a sectional view of a welded joint portion.
【図5】第2実施例の斜面図である。FIG. 5 is a perspective view of the second embodiment.
【図6】第1実施例において、溝条と孔を省略した他の
実施例の斜面図である。FIG. 6 is a perspective view of another embodiment in which grooves and holes are omitted in the first embodiment.
【図7】第2実施例において、溝条と孔を省略した他の
実施例の斜面図である。FIG. 7 is a perspective view of another embodiment in which grooves and holes are omitted in the second embodiment.
(1) 溶接継手用部材 (2) 溝条 (3) 切欠 (4) 孔 (1) Welded joint members (2) Grooves (3) Notches (4) Holes
Claims (3)
する際に、突合わせ部の外側に被せ、鉄筋(5)(5)と一
緒に溶接する継手用部材(1)であって、該継手用部材
(1)は鉄筋の外周を略半周する円弧状に形成され、鉄筋
の方向に沿う側縁の略中央部にルート間隔に対応する幅
にて切欠(3)が形成されている溶接継手用部材。1. A joint member (1) for covering two outer reinforcing bars (5), (5) on the outer side of the butted portion and welding together with the reinforcing bars (5), (5) when welding them together. Yes, the joint member
(1) is a member for a welded joint, which is formed in an arc shape that substantially circumscribes the outer circumference of a reinforcing bar and has a notch (3) formed in a substantially central portion of a side edge along the direction of the reinforcing bar with a width corresponding to a root interval. .
する際に、突合わせ部の外側に被せ、鉄筋(5)(5)と一
緒に溶接する継手用部材(1)であって、該継手用部材
(1)は鉄筋の外周を略半周する円弧状に形成され、鉄筋
の方向に沿う側縁の略中央部に2つの切欠(3)(3)が隣
り合わせに開設されている溶接継手用部材。2. A joint member (1) for welding two rebars (5) (5) together by butt welding, covering the outer side of the butted portion and welding together with the rebars (5) (5). Yes, the joint member
(1) is a member for welded joints, which is formed in an arc shape that substantially circumscribes the outer circumference of a reinforcing bar, and two notches (3) and (3) are opened side by side at the substantially central portion of the side edge along the direction of the reinforcing bar.
接時の溶接金属は流れ出ない程の小径の貫通孔(4)が開
設されている請求項1又は2の溶接継手用部材。3. The welded joint according to claim 1 or 2, wherein a through hole (4) having a small diameter is formed in the groove-corresponding portion of the joint member (1) so that the weld metal does not flow out during welding. Element.