JP2018118509A - Door for opening and shutting outlet of rubber kneader - Google Patents
Door for opening and shutting outlet of rubber kneader Download PDFInfo
- Publication number
- JP2018118509A JP2018118509A JP2018004769A JP2018004769A JP2018118509A JP 2018118509 A JP2018118509 A JP 2018118509A JP 2018004769 A JP2018004769 A JP 2018004769A JP 2018004769 A JP2018004769 A JP 2018004769A JP 2018118509 A JP2018118509 A JP 2018118509A
- Authority
- JP
- Japan
- Prior art keywords
- door
- rubber
- passing
- rubber kneader
- straight line
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
本発明は、ゴム混練機のチャンバの底部に形成された排出口に設けられ、当該排出口を開閉するドアに関する。 The present invention relates to a door that is provided at a discharge port formed at the bottom of a chamber of a rubber kneader and opens and closes the discharge port.
この種のドアとして、例えば特許文献1,2に記載のものがある。
Examples of this type of door include those described in
特許文献1に記載のドア(排出ドア)は、次のようにして特定される形状を有する。密閉混合室の排出口と排出ドアとの接点(D),(E)と、混練用ロータの回転中心(A),(B)とを結ぶ線上(L1 ),(L2)上に、半径(S)の中心(Q)を夫々設ける。この中心(Q)を支点として、接点(D),(E)を通る円弧を夫々描く。この円弧の交点を排出ドアの先端(P)とする。排出ドアの旋回中心(O)を支点として半径(R)の円弧を描いた時、先端(P)が、前記接点(D)及び回転する混練用ロータの先端と干渉せず、かつ前記中心(Q)ができるだけ混練用ロータの回転中心(A),(B)に近づくように排出ドアの先端形状を形成する。
The door (discharge door) described in
上記形状の排出ドアにより、密閉混合室内でコンパウンドの混練を効率良く行うことが出来ると共に、密着し易いコンパウンドを混練しても、コンパウンドの放出時に全部が排出されずに排出口の周縁部と排出ドアとの間に挟まったり、排出口の周縁部と排出ドアとの隙間に付着することがなく、コンパウンドの排出を簡単に、しかも効率良く行うことが出来る、と特許文献1に記載されている。
With the discharge door of the above shape, the compound can be efficiently kneaded in the hermetic mixing chamber, and even if the compound that is easy to adhere is kneaded, the whole is not discharged when the compound is discharged, and the periphery of the discharge port is discharged.
特許文献2に記載のドア(ドロップドア)は、次のようにして特定される形状を有する。ドロップドアの高さhとチャンバの半径Rとの比α(=h/R)が、0.6≦α≦0.8とされる。 The door (drop door) described in Patent Document 2 has a shape specified as follows. The ratio α (= h / R) between the height h of the drop door and the radius R of the chamber is set to 0.6 ≦ α ≦ 0.8.
上記形状のドロップドアにより、混練室内での混合・分散作用が向上し、均一な混練物を短時間で得ることが可能になる。また、ドロップドア上部とロータとで形成される空間も少なくなるため、配合剤や被混練物の滞留、固着等も減少する、と特許文献2に記載されている。 The drop door having the above shape improves the mixing and dispersing action in the kneading chamber and makes it possible to obtain a uniform kneaded material in a short time. Further, Patent Document 2 describes that since the space formed by the upper portion of the drop door and the rotor is reduced, the retention of the compounding agent and the material to be kneaded and the sticking are also reduced.
被混練材料としてシート状のゴム(ゴムシート)が、ゴム混練機に投入されて混練される場合がある。ゴムシートは、チャンバへの投入初期の固体状態のとき(シート状のとき)に、ロータ(混練ロータ)に巻き込まれて巻き付いてしまうことがある。 A sheet-like rubber (rubber sheet) may be put into a rubber kneader and kneaded as a material to be kneaded. The rubber sheet may be wound around the rotor (kneading rotor) when the rubber sheet is in a solid state (in the form of a sheet) at the beginning of charging into the chamber.
特許文献1,2に記載のドアは、いずれのドアにおいても、ゴムと接する混練室側の斜面の全てが滑らかな連続する曲面とされている。なお、特許文献2に記載のドアについては、その頂部の僅かな部分は水平方向に延びる直線とされている。このような形状のドアの場合、当該ドアへのゴムの付着は抑制される。しかしながら、被混練材料がゴムシートの場合、ドア部分でゴムが滞留しにくい。そのため、ロータへのゴムシートの巻き込みが、発生しやすい。
In any of the doors described in
本発明は、上記実情に鑑みてなされたものであり、その目的は、混練対象であるゴムが、ロータに巻き込まれることを抑制することができる、ゴム混練機の排出口を開閉するドアを提供することである。 The present invention has been made in view of the above circumstances, and an object of the present invention is to provide a door that opens and closes a discharge port of a rubber kneader, which can suppress the rubber to be kneaded from being caught in the rotor. It is to be.
本発明は、ゴム混練機のチャンバの底部に形成された排出口を開閉する、前記チャンバに挿入される側が左右対称の山形状とされたドアである。このドアは、長手方向に直交する断面視において、前記山形状の外形が、前記排出口の内方側開口端と接するドア下端角部と、鉛直方向に最も高いドア頂部との間において、相互に異なる角度で水平方向に対して傾斜した複数の直線で構成されている。 The present invention is a door that opens and closes a discharge port formed at the bottom of a chamber of a rubber kneader and that has a symmetrical mountain shape on the side inserted into the chamber. This door has a cross-sectional view perpendicular to the longitudinal direction in which the mountain-shaped outer shape is between the door lower end corner portion that is in contact with the inner opening end of the discharge port and the highest door top portion in the vertical direction. Are composed of a plurality of straight lines inclined at different angles with respect to the horizontal direction.
上記構成のドアによれば、チャンバ内のドア近傍においてゴムをある程度滞留させることができ、これにより、ロータへのゴムの巻き込みを抑制することができる。 According to the door configured as described above, the rubber can be retained to some extent in the vicinity of the door in the chamber, thereby suppressing the rubber from being caught in the rotor.
以下、本発明を実施するための形態について図面を参照しつつ説明する。 Hereinafter, embodiments for carrying out the present invention will be described with reference to the drawings.
(ゴム混練機の構成)
図1を参照しつつ、本発明の一実施形態に係るドア32を備えるゴム混練機100の構成について説明する。なお、本発明のドアを備えるゴム混練機の混練対象であるゴムは、形状がシート状のゴム(ゴムシート)に限定されることはない。
(Configuration of rubber kneader)
A configuration of a
ゴム混練機100は、被混練材料であるゴムの混練を行う装置であって、供給部20と、混練部30とを備える。供給部20は、混練部30に被混練材料を供給する部分であり、ホッパ21と、材料供給筒22と、シリンダ装置23とを備える。
The
ホッパ21には、ゴム混練機100の外部から混練対象のゴム(被混練材料)が投入される。材料供給筒22は、被混練材料が通ることが可能な筒である。材料供給筒22の上部は、ホッパ21に連通する。
The
シリンダ装置23は、材料供給筒22から混練部30(後述する混練室33)に被混練材料を押し込む装置である。シリンダ装置23は、例えば空圧式のアクチュエータである。シリンダ装置23は、シリンダ24と、ピストン25と、ピストンロッド26と、フローティングウェイト27とを備える。
The
ピストンロッド26の下端部に連結されたフローティングウェイト27は、ホッパ21から投入された被混練材料を混練室33に押し込む部材である。
The floating
混練部30は、被混練材料を混練する部分であり、チャンバ31と、チャンバ31の底部に形成された排出口37を開閉(開放および閉止)するドア32と、一対のロータ34・35(混練ロータ)とを備える。
The kneading
チャンバ31は、内部に混練室33を形成する部分であり、その上部に被混練材料の供給口36が設けられている。この供給口36部分にめがけて、その上方から、フローティングウェイト27が降下させられる。
The
混練室33は、被混練材料が混練される空間である。混練室33の縦断面形状は、まゆ型である。この縦断面形状は、ロータ34・35の軸方向から見たときの混練室33の断面形状である。
The
ドア32は、アクチュエータにより駆動されることで、チャンバ31の排出口37を開閉する。チャンバ31の排出口37は、被混練材料の混練中はドア32により閉止され、混練が終了したゴム(混練物)をチャンバ31から出すときに開放される。ドア32を駆動するアクチュエータは、例えば回転式アクチュエータ(ロータリアクチュエータ)である。ドア32(ドアの形状)は、チャンバ31内(混練室33内)でロータ34・35によって混練されるゴムの混練度におよぼす影響が大きい。
The
ロータ34・35は、被混練材料を混練する部材であり、チャンバ31内(混練室33内)に配置される。ロータ34・35は、その中心軸まわりに回転する。ロータ34・35の回転中心Cを、図1に示している。ロータ34・35は、対向する部分が下方に移動するように、互いに異なる方向に回転する。
The
(ドアの形状)
ドア32について詳述する。ドア32は、チャンバ31に挿入される側が山形状とされている。なお、この山形状は、当該ドア32の長手方向に直交する断面視において、左右対称の形状である。
(Door shape)
The
例えば図1中のドア32部分、および図2中の外形4を参照されたい。本発明の実施形態に係るドア32は、長手方向に直交する断面視において、上記山形状の外形4が、排出口37の内方側開口端と接するドア下端角部32aと、鉛直方向に最も高いドア頂部32bとの間において、相互に異なる角度で水平方向に対して傾斜した3つの直線4a〜4cで構成されている。なお、図2は、長手方向に直交するドアの断面視において、当該ドアの山形状部分の外形(主に片側のみ)を示す図である。また、図2中の一点鎖線は、中心線である。
See, for example, the
図2には、本発明の実施形態に係る、外形1から外形9まで計9つのドアの形状を示している。図2に示すように、外形1〜9は、ドア下端角部32aとドア頂部との間が、ドア下端角部32aからドア頂部へ向けて、順に、直線1a〜9a、直線1b〜9b、および直線1c〜9cという、相互に異なる角度で水平方向に対して傾斜した3つの直線でそれぞれ構成されている。なお、図2中において「従来技術」と付記した点線で示すドア(エキセントリックドア)の外形は、ドア頂部を除いて全て滑らかな連続する曲面である。なお、この従来技術のドア頂部の僅かな部分は、水平方向に延びる直線とされている。
In FIG. 2, the shape of nine doors from the
本発明者らは、図2に示す外形1〜9の計9つのドア、図2に示す従来技術形状のドア、について、ロータ34・35へのゴムの巻き込み、ゴムの混練度への影響、およびドアへのゴムの付着性、について評価した。評価結果を表1に示す。なお、被混練材料としてのゴムは、初期形態(投入時の形態)がシート状のゴム(ゴムシート)とした。
The present inventors made a total of nine
[表1の説明]
巻き込み ○:巻き込み抑制効果有り
×:巻き込み抑制効果無し
混練度 ◎:非常に良い
○:良い
×:悪い
付着 ○:付着無し
△:配合によっては付着有り
[Explanation of Table 1]
Entrainment ○: Effective in inhibiting entrainment
X: Kneading degree without entrainment inhibiting effect ◎: Very good
○: Good
×: Bad adhesion ○: No adhesion
Δ: Adhesion depending on the formulation
[ゴムの巻き込みについて]
従来技術では、ゴムと接する混練室33側の斜面の全てが滑らかな連続する曲面とされている。これに対して、本発明のドアでは、図2に示す外形1〜9のように、ゴムと接する混練室33側の斜面が、ドア下端角部32aからドア頂部へ向けて、順に、直線1a〜9a、直線1b〜9b、および直線1c〜9cという、相互に異なる角度で水平方向に対して傾斜した3つの直線のみで構成される。これにより、チャンバ31内(混練室33内)のドア近傍においてゴムをある程度滞留させることができ、ロータ34・35へのゴムの巻き込みを抑制することができる。外形1〜9の計9つのドアは、全て、ゴムの巻き込み抑制効果を有し、これに対して、従来技術形状のドアは、ゴムの巻き込み抑制効果を有さない。この評価を、○、×で表1に示している。
[About rubber entrainment]
In the prior art, all of the slopes on the kneading
[混練度への影響について]
図3は、図2に示す従来形状のドアに対する、図2に示す本発明の実施形態の外形1〜9のドアのCV値比を示すグラフである。ここで、CV値は、値が小さい程、ゴムの分配混合が進んでいると判断できる指標である。また、CV値比は、図2に示す従来技術形状のドアのCV値を1としたときの各ドアのCV値(CV値の比)のことである。CV値比は、その値が小さい程、ゴムの分配混合がより改善していることを示す。従来技術を含む計10のドアについて流動解析を行った時の、ロータ34・35が10回転した後のCV値比を図3のグラフに示している。
[Influence on kneading degree]
FIG. 3 is a graph showing the CV value ratio of the doors of the
図3からわかるように、従来技術形状のドア(エキセントリックドア)よりもCV値が10%以上改善したドアは、外形3、外形4、外形5、および外形6の4つのドアであった。また、CV値が10%未満の改善となったドアは、外形2、外形8、および外形9の3つのドアであった。なお、外形1、および外形7の2つのドアは、従来技術形状のドアよりも若干ではあるがCV値が悪化した。これらの結果を、◎、○、×で表1に示している。
As can be seen from FIG. 3, the doors having CV values improved by 10% or more than the doors of the prior art shape (eccentric doors) were four doors of the outer shape 3, the outer shape 4, the outer shape 5, and the outer shape 6. Further, the doors whose CV value was improved by less than 10% were the three doors of the outer shape 2, the outer shape 8, and the outer shape 9. In addition, the CV value of the two doors of the
[ゴムの付着性について]
従来技術を含む計10のドアについて流動解析を行うことにより、各ドアへのゴムの付着性について評価した。表1に示すように、従来技術形状のドア、本発明の実施形態の外形2〜6、8、9の各ドアについては、ゴムの付着が認められなかったが、本発明の実施形態の外形1、7の各ドアについては、ゴムの配合によってはゴムの付着が認められた。
[Rubber adhesion]
By performing flow analysis on a total of 10 doors including the prior art, rubber adhesion to each door was evaluated. As shown in Table 1, the adhesion of rubber was not recognized for the doors of the prior art shape and the outer shapes 2 to 6, 8, and 9 of the embodiment of the present invention, but the outer shape of the embodiment of the present invention. About each door of 1 and 7, adhesion of rubber | gum was recognized depending on the mixing | blending of rubber | gum.
[より好ましいドア形状について]
ドアの形状に関し、前記したように、長手方向に直交する断面視において、山形状の外形1が、ドア下端角部32aと、鉛直方向に最も高いドア頂部との間において、相互に異なる角度で水平方向に対して傾斜した3つの直線で構成されていることで、チャンバ31内(混練室33内)のドア近傍においてゴムをある程度滞留させることができ、これにより、ロータ34・35へのゴムの巻き込みを抑制することができる。
[About more preferable door shape]
Regarding the shape of the door, as described above, in the cross-sectional view orthogonal to the longitudinal direction, the mountain-shaped
<1.ゴムの巻き込み抑制に加えて、ドアへのゴム付着を抑制しつつ、且つゴムの分配混合を向上させることができるドア形状>
図2、4、5を参照しつつ、より好ましいドア形状について説明する。ここで、長手方向に直交する断面視において、ドア下端角部32aを原点O、水平方向をx軸(図4,5参照)、水平方向におけるドア下端角部32aからドア頂部への方向をx軸の正(図4,5中のx軸の矢印参照)とする。また、鉛直方向をy軸(図4,5参照)、鉛直方向におけるドア下端角部32aからドア頂部への方向をy軸の正(図4,5中のy軸の矢印参照)、原点Oとドア頂部との間の水平方向の距離をLとする。外形1〜9は、それぞれ、0≦x≦0.5Lの範囲が直線1a〜9aとされ、0.5L≦x≦0.75Lの範囲が直線1b〜9bとされ、且つ0.75L≦x≦Lの範囲が直線1c〜9cとされている。
<1. In addition to suppressing rubber entrainment, door shape that can suppress rubber adhesion to the door and improve rubber distribution and mixing>
A more preferable door shape will be described with reference to FIGS. Here, in a cross-sectional view orthogonal to the longitudinal direction, the door
ドアへのゴムの付着に関し、ドア下端角部32aから水平方向に0.75L(0≦x≦0.75L)の範囲は、ドア頂部側に比べてゴムが付着しやすい領域である。
Regarding the adhesion of rubber to the door, the range of 0.75 L (0 ≦ x ≦ 0.75 L) in the horizontal direction from the door lower
表1に示す評価結果より、ドアの0≦x≦0.5Lの範囲における、ドアへのゴム付着を抑制することができるドアの外形は、次の式(1)を満たす領域を通過する、水平方向に対して傾斜する直線とされていることである。 From the evaluation results shown in Table 1, in the range of 0 ≦ x ≦ 0.5 L of the door, the outer shape of the door that can suppress rubber adhesion to the door passes through a region that satisfies the following expression (1). The straight line is inclined with respect to the horizontal direction.
tan(θ+10)×x≦y≦tan(θ+31)×x ・・・・・式(1)
θ:ゴム混練機100のロータの回転中心Cを中心とする原点Oを通る半径Rの円の原点Oにおける接線の水平方向に対する傾斜角(図4,5参照)
tan (θ + 10) × x ≦ y ≦ tan (θ + 31) × x Expression (1)
θ: Inclination angle with respect to the horizontal direction of the tangent line at the origin O of a circle of radius R passing through the origin O centered on the rotation center C of the rubber kneader 100 (see FIGS. 4 and 5)
なお、半径Rは、チャンバ31の内壁面の円形状部の半径(図1参照)である。また、式(1)の中の左側の直線式は、外形9の直線9a(図2参照)を示し、式(1)の中の右側の直線式は、外形6,8の直線6a,8a(図2参照)を示す。 The radius R is the radius of the circular portion of the inner wall surface of the chamber 31 (see FIG. 1). Further, the left-side linear expression in the equation (1) indicates a straight line 9a (see FIG. 2) of the outer shape 9, and the right-side linear equation in the expression (1) indicates the straight lines 6a and 8a of the outer shapes 6 and 8. (See FIG. 2).
次に、ドアの0.5L≦x≦0.75Lの範囲における、ドアへのゴム付着を抑制することができるドアの外形は、次の式(2)を満たす領域を通過する、水平方向に対して傾斜する直線とされていることである。 Next, in the range of 0.5L ≦ x ≦ 0.75L of the door, the outer shape of the door that can suppress the rubber adhesion to the door passes through a region that satisfies the following expression (2) in the horizontal direction. In other words, it is a straight line that is inclined with respect to.
・・・・・式(2)
θ:ゴム混練機100のロータの回転中心Cを中心とする原点Oを通る半径Rの円の原点Oにおける接線の水平方向に対する傾斜角(図4,5参照)
・ ・ ・ ・ ・ Formula (2)
θ: Inclination angle with respect to the horizontal direction of the tangent line at the origin O of a circle of radius R passing through the origin O centered on the rotation center C of the rubber kneader 100 (see FIGS. 4 and 5)
なお、半径Rは、チャンバ31の内壁面の円形状部の半径(図1参照)である。また、式(2)の中の左側の直線式は、外形9の直線9b(図2参照)を示し、式(2)の中の右側の直線式は、外形6,8の直線6b,8b(図2参照)を示す。 The radius R is the radius of the circular portion of the inner wall surface of the chamber 31 (see FIG. 1). Further, the left-side linear expression in the equation (2) indicates the straight line 9b (see FIG. 2) of the outer shape 9, and the right-side linear equation in the expression (2) indicates the straight lines 6b and 8b of the outer shapes 6 and 8. (See FIG. 2).
ゴムの分配混合(混練)においては、ドアのドア頂部側の形状の影響が大きい。そのため、ドアの0.75L≦x≦Lの範囲の山形状領域は、ゴムの分配混合が向上する領域である。 In the distribution mixing (kneading) of rubber, the influence of the shape of the door top portion side is large. Therefore, the mountain-shaped region in the range of 0.75 L ≦ x ≦ L of the door is a region where rubber distribution and mixing is improved.
ドアの0.75L≦x≦Lの範囲における、ゴムの分配混合を従来よりも向上させることができるドアの外形は、次の式(3)を満たす領域を通過する、水平方向に対して傾斜する直線とされていることである。 In the range of 0.75L ≦ x ≦ L of the door, the outer shape of the door capable of improving the distribution and mixing of the rubber as compared with the conventional one is inclined with respect to the horizontal direction passing through the region satisfying the following expression (3). Is a straight line.
tan(θ+41)×x+b2≦y≦tan(θ+45)×x+b1 ・・・・式(3)
θ:ゴム混練機100のロータの回転中心Cを中心とする原点Oを通る半径Rの円の原点Oにおける接線の水平方向に対する傾斜角(図4,5参照)
b1:ロータの回転中心Cを中心とする半径R1が0.97Rの円と、ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点P1を通る傾きがtan(θ+45)の直線の切片(切片のy座標)(図4参照)
b2:ロータの回転中心Cを中心とする半径R2が1.05Rの円と、ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点P2を通る傾きがtan(θ+41)の直線の切片(切片のy座標)(図4参照)
tan (θ + 41) × x + b2 ≦ y ≦ tan (θ + 45) × x + b1 (3)
θ: Inclination angle with respect to the horizontal direction of the tangent line at the origin O of a circle of radius R passing through the origin O centered on the rotation center C of the rubber kneader 100 (see FIGS. 4 and 5)
b1: An inclination passing through a lower point P1 of two intersections of a circle having a radius R1 of 0.97R centering on the rotation center C of the rotor and a straight line x = L passing through the top of the door is tan (θ + 45). Straight section (section y coordinate) (see Fig. 4)
b2: The inclination passing through the lower point P2 of the two intersections of the circle having the radius R2 of 1.05R centered on the rotation center C of the rotor and the straight line x = L passing through the top of the door is tan (θ + 41). Straight section (section y coordinate) (see Fig. 4)
なお、半径Rは、チャンバ31の内壁面の円形状部の半径(図1参照)である。また、上記したドア頂部を通る直線x=Lは、2つのロータ34・35の中心を結ぶ線分の垂直二等分線でもある。また、式(3)の中の左側の直線式は、外形9の直線9c(図2参照)を示し、式(3)の中の右側の直線式(式(3)の中の右式)は、外形8の直線8c(図2参照)を示す。
The radius R is the radius of the circular portion of the inner wall surface of the chamber 31 (see FIG. 1). The straight line x = L passing through the top of the door is also a perpendicular bisector that connects the centers of the two
ロータ34・35へのゴムの巻き込み抑制に加えて、ドアへのゴム付着を抑制しつつ、且つゴムの分配混合を向上させることができるドア形状について、前記記載をまとめると、ドアの形状は、当該ドアの山形状部分に関し、0≦x≦0.5Lの範囲の外形が、上記式(1)を満たす領域を通過する水平方向に対して傾斜する直線とされ、0.5L≦x≦0.75Lの範囲の外形が、上記式(2)を満たす領域を通過する水平方向に対して傾斜する直線とされ、且つ、0.75L≦x≦Lの範囲の外形が、上記式(3)を満たす領域を通過する水平方向に対して傾斜する直線とされていることである。但し、これらの3つの直線の水平方向に対する傾斜角度は、相互に異なる。
Summarizing the above description of the door shape that can improve rubber distribution and mixing while suppressing rubber adhesion to the
<2.前記したドアよりも、ゴムの分配混合をさらに向上させることができるドア形状>
表1に示す評価結果より、ゴムの巻き込み抑制に加えて、ドアへのゴム付着を抑制しつつ、且つゴムの分配混合をさらに向上させることができる(CV値が10%以上改善)ドアの山形状部分の外形は、0≦x≦0.5Lの範囲の前記外形が、さらに次の式(4)を満たす領域を通過する、水平方向に対して傾斜する直線とされていることである。
<2. Door shape that can further improve rubber distribution and mixing than the door described above>
From the evaluation results shown in Table 1, in addition to suppressing rubber entrainment, it is possible to further improve the distribution and mixing of rubber while suppressing rubber adhesion to the door (CV value is improved by 10% or more). The external shape of the shape part is that the external shape in the range of 0 ≦ x ≦ 0.5L is a straight line that passes through a region satisfying the following expression (4) and is inclined with respect to the horizontal direction.
tan(θ+16)×x≦y≦tan(θ+26)×x ・・・・・式(4)
θ:ゴム混練機100のロータの回転中心Cを中心とする原点Oを通る半径Rの円の原点Oにおける接線の水平方向に対する傾斜角(図4,5参照)
tan (θ + 16) × x ≦ y ≦ tan (θ + 26) × x Equation (4)
θ: Inclination angle with respect to the horizontal direction of the tangent line at the origin O of a circle of radius R passing through the origin O centered on the rotation center C of the rubber kneader 100 (see FIGS. 4 and 5)
なお、半径Rは、チャンバ31の内壁面の円形状部の半径(図1参照)である。また、式(4)の中の左側の直線式は、外形3の直線3a(図2参照)を示し、式(4)の中の右側の直線式は、外形5の直線5a(図2参照)を示す。 The radius R is the radius of the circular portion of the inner wall surface of the chamber 31 (see FIG. 1). Further, the left-side linear expression in the equation (4) indicates the straight line 3a (see FIG. 2) of the outer shape 3, and the right-side linear equation in the equation (4) is the straight line 5a of the outer shape 5 (see FIG. 2). ).
次に、ゴムの巻き込み抑制に加えて、ドアへのゴム付着を抑制しつつ、且つゴムの分配混合をさらに向上させることができる(CV値が10%以上改善)ドアの山形状部分の外形は、0.5L≦x≦0.75Lの範囲の前記外形が、さらに次の式(5)を満たす領域を通過する、水平方向に対して傾斜する直線とされていることである。 Next, in addition to suppressing rubber entrainment, it is possible to further improve the distribution and mixing of rubber while suppressing rubber adhesion to the door (CV value is improved by 10% or more). The outer shape in the range of 0.5L ≦ x ≦ 0.75L is a straight line that passes through a region satisfying the following expression (5) and is inclined with respect to the horizontal direction.
・・・・・式(5)
θ:ゴム混練機100のロータの回転中心Cを中心とする原点Oを通る半径Rの円の原点Oにおける接線の水平方向に対する傾斜角(図4,5参照)
..... Formula (5)
θ: Inclination angle with respect to the horizontal direction of the tangent line at the origin O of a circle of radius R passing through the origin O centered on the rotation center C of the rubber kneader 100 (see FIGS. 4 and 5)
なお、半径Rは、チャンバ31の内壁面の円形状部の半径(図1参照)である。また、式(5)の中の左側の直線式は、外形3の直線3b(図2参照)を示し、式(5)の中の右側の直線式は、外形5の直線5b(図2参照)を示す。 The radius R is the radius of the circular portion of the inner wall surface of the chamber 31 (see FIG. 1). Further, the left-side linear equation in the equation (5) indicates the straight line 3b (see FIG. 2) of the outer shape 3, and the right-side linear equation in the equation (5) is the straight line 5b of the outer shape 5 (see FIG. 2). ).
また、ゴムの巻き込み抑制に加えて、ドアへのゴム付着を抑制しつつ、且つゴムの分配混合をさらに向上させることができる(CV値が10%以上改善)ドアの山形状部分の外形は、0.75L≦x≦Lの範囲の前記外形が、さらに次の式(6)を満たす領域を通過する、水平方向に対して傾斜する直線とされていることである。 In addition to suppressing rubber entrainment, rubber adhesion to the door can be suppressed, and rubber distribution and mixing can be further improved (CV value is improved by 10% or more). The outer shape in the range of 0.75L ≦ x ≦ L is a straight line that passes through a region satisfying the following expression (6) and is inclined with respect to the horizontal direction.
tan(θ+48)×x+b4≦y≦tan(θ+39)×x+b3 ・・・・式(6)
θ:ゴム混練機100のロータの回転中心Cを中心とする原点Oを通る半径Rの円の原点Oにおける接線の水平方向に対する傾斜角(図4,5参照)
b3:ロータの回転中心Cを中心とする半径R3が1.01Rの円と、ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点P3を通る傾きがtan(θ+39)の直線の切片(切片のy座標)(図5参照)
b4:ロータの回転中心Cを中心とする半径R3が1.01Rの円と、ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点P3を通る傾きがtan(θ+48)の直線の切片(切片のy座標)(図5参照)
tan (θ + 48) × x + b4 ≦ y ≦ tan (θ + 39) × x + b3 (6)
θ: Inclination angle with respect to the horizontal direction of the tangent line at the origin O of a circle of radius R passing through the origin O centered on the rotation center C of the rubber kneader 100 (see FIGS. 4 and 5)
b3: The inclination passing through the lower point P3 of the two intersections of the circle with the radius R3 of 1.01R centered on the rotation center C of the rotor and the straight line x = L passing through the top of the door is tan (θ + 39). Straight section (y-coordinate of section) (see Fig. 5)
b4: The inclination passing through the lower point P3 of the two intersections of the circle having the radius R3 of 1.01R centered on the rotation center C of the rotor and the straight line x = L passing through the top of the door is tan (θ + 48). Straight section (y-coordinate of section) (see Fig. 5)
なお、半径Rは、チャンバ31の内壁面の円形状部の半径(図1参照)である。また、上記したドア頂部を通る直線x=Lは、2つのロータ34・35の中心を結ぶ線分の垂直二等分線でもある。また、式(6)の中の左側の直線式は、外形3の直線3c(図2参照)を示し、式(6)の中の右側の直線式は、外形5の直線5c(図2参照)を示す。
The radius R is the radius of the circular portion of the inner wall surface of the chamber 31 (see FIG. 1). The straight line x = L passing through the top of the door is also a perpendicular bisector that connects the centers of the two
(ドアへの温度計取り付けについて)
図6,7を参照しつつ、ドア32への温度計40取り付けについて説明する。図6,7に示すように、ドア頂部32bの長手方向の中央部は凹部38とされている。この凹部38部分には孔39があけられており、当該孔39に温度計40が挿入されて固定されている(設置されている)。この凹部38部分は、図6に示すように、曲面とされている。
(Attaching a thermometer to the door)
The attachment of the
長手方向に直交する断面視において、凹部38を除く部分の、ドア32の山形状の外形4が、ドア32の長手方向の全長にわたって、左右対称の3つの直線3a。3b、3cで形成されている。温度計40は、ドア頂部32bよりも上方に突出しないように設置される。この構成によると、ドア32の温度計40設置付近でのゴムの付着を防止することができる。
In a cross-sectional view orthogonal to the longitudinal direction, the mountain-shaped outer shape 4 of the
図6に示すように、上記の凹部38は、ドア32の長手方向に直交する断面視において左右対称の山形状とされている。ここで、凹部38を除く部分のドア頂部32bの高さ(高さ寸法)をT1とし、凹部38の山形状の頂部38bの高さ(高さ寸法)をT2としたとき、0.71T1≦T2≦0.96T1を満たし、且つ、前記した式(3)の中の右式(tan(θ+45)×x+b1)で特定される、凹部38を除く部分のドア頂部32bの高さ(高さ寸法)をTxとしたとき、0.79Tx≦T2も満たし、ドア32の長手方向から視たときに、温度計40の先端部が、ドア頂部32bと、凹部38の山形状の頂部38bとの間に配置されていることが好ましい。この構成によると、温度計40の摩耗や折損を防止することができるとともに、チャンバ31内を流動するゴムの温度をより正確に測定することができる。
As shown in FIG. 6, the
また、図7に示すように、凹部38の山形状の頂部38bの長手方向の長さD2が、温度計40の直径Dtよりも長く、且つ、ドア32の長手方向の長さD1の1/2未満の長さとされていることが好ましい。なお、凹部38の山形状の頂部38bの長手方向の長さD2が、ドア32の長手方向の長さD1の1/2未満の長さとされているというのは、凹部38の山形状の頂部38bの長手方向の長さD2が、当該凹部38以外の部分の、ドア32の長手方向の長さ(=D1−D2)未満の長さとされているということである。この構成によると、チャンバ31内を流動するゴムの温度計40設置部への付着を抑制することができるとともに、ゴムの温度をより正確に測定することができる。また、シート状のゴムの巻きつきを抑制することもできる。なお、凹部38の山形状の頂部38bの長手方向の長さD2は、頂部38bの長手方向における一端から他端までの長さ、すなわち、温度計40が挿入されて固定される孔39部分を含む長さである。
Further, as shown in FIG. 7, the length D2 of the crest-shaped
(変形例)
前記した実施形態のドアは、その山形状部分の外形が、ドア下端角部32aと、ドア頂部との間において、相互に異なる角度で水平方向に対して傾斜した3つの直線とされているが、相互に異なる角度で水平方向に対して傾斜した2つの直線とされてもよい。さらには、相互に異なる角度で水平方向に対して傾斜した4つ以上の直線とされてもよい。すなわち、ドアの山形状部分の外形が、ドア下端角部32aと、ドア頂部との間において、円弧などの曲線、および水平方向に延びる直線を含まない、相互に異なる角度で水平方向に対して傾斜した複数の直線のみで構成されていれば、斜面の全てが滑らかな連続する曲面とされている従来形状のドアに比べて、チャンバ31内(混練室33内)のドア近傍においてゴムをある程度滞留させることができ、これによりロータ34・35へのゴムの巻き込みを抑制することができる。
(Modification)
In the door of the embodiment described above, the outer shape of the mountain-shaped portion is three straight lines inclined with respect to the horizontal direction at mutually different angles between the door lower
図2からわかるように、前記した実施形態のドアでは、水平方向におけるドア下端角部32aからドア頂部への0.5Lの位置、および0.75Lの位置で、その外形の直線の傾きが変化しているが、直線の傾きが変化する位置は、0.5Lの位置、および0.75Lの位置に限られることはない。0.5Lの位置よりも、ドア下端角部32a側で直線の傾きが変化してもよいし、ドア頂部側で直線の傾きが変化してもよい。同様に、0.75Lの位置よりも、ドア下端角部32a側で直線の傾きが変化してもよいし、ドア頂部側で直線の傾きが変化してもよい。
As can be seen from FIG. 2, in the door of the embodiment described above, the inclination of the straight line of the outer shape changes at the position of 0.5 L from the door lower
1〜9:外形
1a〜9a:直線
1b〜9b:直線
1c〜9c:直線
31:チャンバ
32:ドア
32a:ドア下端角部
32b:ドア頂部
37:排出口
38:凹部
40:温度計
100:ゴム混練機
1 to 9: Outlines 1a to 9a: Straight lines 1b to 9b: Straight lines 1c to 9c: Straight line 31: Chamber 32:
Claims (11)
長手方向に直交する断面視において、前記山形状の外形が、前記排出口の内方側開口端と接するドア下端角部と、鉛直方向に最も高いドア頂部との間において、相互に異なる角度で水平方向に対して傾斜した複数の直線で構成されている、
ゴム混練機の排出口を開閉するドア。 A door that opens and closes a discharge port formed at the bottom of the chamber of the rubber kneader, the side to be inserted into the chamber is a symmetrical mountain shape,
In a cross-sectional view perpendicular to the longitudinal direction, the mountain-shaped outer shape is different from each other between the door lower end corner portion in contact with the inner opening end of the discharge port and the highest door top portion in the vertical direction. Consists of a plurality of straight lines inclined with respect to the horizontal direction,
A door that opens and closes the outlet of a rubber kneader.
前記外形が、相互に異なる角度で水平方向に対して傾斜した3つの直線で構成されている、
ゴム混練機の排出口を開閉するドア。 The door according to claim 1,
The outer shape is composed of three straight lines inclined with respect to the horizontal direction at different angles.
A door that opens and closes the outlet of a rubber kneader.
長手方向に直交する断面視において、前記ドア下端角部を原点、水平方向をx軸、水平方向における前記ドア下端角部から前記ドア頂部への方向をx軸の正、鉛直方向をy軸、鉛直方向における前記ドア下端角部から前記ドア頂部への方向をy軸の正、前記原点と前記ドア頂部との間の水平方向の距離をLとしたとき、0≦x≦0.5Lの範囲の前記外形が、式(1)を満たす領域を通過する直線とされている、
ゴム混練機の排出口を開閉するドア。
tan(θ+10)×x≦y≦tan(θ+31)×x ・・・・・式(1)
θ:ゴム混練機のロータの回転中心を中心とする前記原点を通る円の前記原点における接線の水平方向に対する傾斜角 The door according to claim 2,
In a cross-sectional view orthogonal to the longitudinal direction, the lower end corner of the door is the origin, the horizontal direction is the x axis, the direction from the lower end corner of the door in the horizontal direction to the top of the door is the positive x axis, the vertical direction is the y axis, The range from 0 ≦ x ≦ 0.5L, where the direction from the lower corner of the door in the vertical direction to the top of the door is positive on the y-axis and the horizontal distance between the origin and the top of the door is L. The outer shape is a straight line passing through a region satisfying the formula (1),
A door that opens and closes the outlet of a rubber kneader.
tan (θ + 10) × x ≦ y ≦ tan (θ + 31) × x Expression (1)
θ: Inclination angle with respect to the horizontal direction of the tangent at the origin of a circle passing through the origin with the rotation center of the rotor of the rubber kneader as the center
0.5L≦x≦0.75Lの範囲の前記外形が、式(2)を満たす領域を通過する直線とされている、
ゴム混練機の排出口を開閉するドア。
・・・・・式(2)
θ:ゴム混練機のロータの回転中心を中心とする前記原点を通る円の前記原点における接線の水平方向に対する傾斜角 The door according to claim 3,
The outer shape in the range of 0.5 L ≦ x ≦ 0.75 L is a straight line passing through a region satisfying the formula (2).
A door that opens and closes the outlet of a rubber kneader.
・ ・ ・ ・ ・ Formula (2)
θ: Inclination angle with respect to the horizontal direction of the tangent at the origin of a circle passing through the origin with the rotation center of the rotor of the rubber kneader as the center
0.75L≦x≦Lの範囲の前記外形が、式(3)を満たす領域を通過する直線とされている、
ゴム混練機の排出口を開閉するドア。
tan(θ+41)×x+b2≦y≦tan(θ+45)×x+b1 ・・・・式(3)
θ:ゴム混練機のロータの回転中心を中心とする前記原点を通る円の前記原点における接線の水平方向に対する傾斜角
b1:前記円の半径をRとしたとき、前記ロータの回転中心を中心とする半径が0.97Rの円と、前記ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点を通る傾きがtan(θ+45)の直線の切片
b2:前記円の半径をRとしたとき、前記ロータの回転中心を中心とする半径が1.05Rの円と、前記ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点を通る傾きがtan(θ+41)の直線の切片
なお、前記半径Rは、前記チャンバの内壁面の円形状部の半径である。 The door according to claim 3 or 4,
The outer shape in the range of 0.75 L ≦ x ≦ L is a straight line that passes through a region that satisfies Equation (3).
A door that opens and closes the outlet of a rubber kneader.
tan (θ + 41) × x + b2 ≦ y ≦ tan (θ + 45) × x + b1 (3)
θ: Inclination angle of the circle passing through the origin centered on the rotation center of the rotor of the rubber kneader with respect to the horizontal direction of the tangent line at the origin, b1: When the radius of the circle is R, the rotation center of the rotor is the center The intercept of the straight line whose slope is tan (θ + 45) passing through the lower point of two intersections of the circle having a radius of 0.97R and the straight line x = L passing through the top of the door b2: The radius of the circle is R The inclination passing through the lower point of the two intersections of the circle having a radius around the rotation center of the rotor of 1.05R and the straight line x = L passing through the top of the door is tan (θ + 41) The radius R is the radius of the circular portion of the inner wall surface of the chamber.
0≦x≦0.5Lの範囲の前記外形が、式(4)を満たす領域を通過する直線とされている、
ゴム混練機の排出口を開閉するドア。
tan(θ+16)×x≦y≦tan(θ+26)×x ・・・・・式(4)
θ:ゴム混練機のロータの回転中心を中心とする前記原点を通る円の前記原点における接線の水平方向に対する傾斜角 In the door in any one of Claims 3-5,
The outer shape in the range of 0 ≦ x ≦ 0.5L is a straight line that passes through a region that satisfies Equation (4).
A door that opens and closes the outlet of a rubber kneader.
tan (θ + 16) × x ≦ y ≦ tan (θ + 26) × x Equation (4)
θ: Inclination angle with respect to the horizontal direction of the tangent at the origin of a circle passing through the origin with the rotation center of the rotor of the rubber kneader as the center
0.5L≦x≦0.75Lの範囲の前記外形が、式(5)を満たす領域を通過する直線とされている、
ゴム混練機の排出口を開閉するドア。
・・・・・式(5)
θ:ゴム混練機のロータの回転中心を中心とする前記原点を通る円の前記原点における接線の水平方向に対する傾斜角 In the door in any one of Claims 3-6,
The outer shape in the range of 0.5 L ≦ x ≦ 0.75 L is a straight line that passes through a region that satisfies Equation (5).
A door that opens and closes the outlet of a rubber kneader.
..... Formula (5)
θ: Inclination angle with respect to the horizontal direction of the tangent at the origin of a circle passing through the origin with the rotation center of the rotor of the rubber kneader as the center
0.75L≦x≦Lの範囲の前記外形が、式(6)を満たす領域を通過する直線とされている、
ゴム混練機の排出口を開閉するドア。
tan(θ+48)×x+b4≦y≦tan(θ+39)×x+b3 ・・・・式(6)
θ:ゴム混練機のロータの回転中心を中心とする前記原点を通る円の前記原点における接線の水平方向に対する傾斜角
b3:前記円の半径をRとしたとき、前記ロータの回転中心を中心とする半径が1.01Rの円と、前記ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点を通る傾きがtan(θ+39)の直線の切片
b4:前記円の半径をRとしたとき、前記ロータの回転中心を中心とする半径が1.01Rの円と、前記ドア頂部を通る直線x=Lとの2つの交点のうちの下方の点を通る傾きがtan(θ+48)の直線の切片
なお、前記半径Rは、前記チャンバの内壁面の円形状部の半径である。 In the door in any one of Claims 3-7,
The outer shape in the range of 0.75 L ≦ x ≦ L is a straight line that passes through a region that satisfies Equation (6).
A door that opens and closes the outlet of a rubber kneader.
tan (θ + 48) × x + b4 ≦ y ≦ tan (θ + 39) × x + b3 (6)
θ: Inclination angle with respect to the horizontal direction of the tangent line at the origin centered on the rotation center of the rotor of the rubber kneader b3: When the radius of the circle is R, the rotation center of the rotor is the center. The intercept of the straight line whose slope is tan (θ + 39) passing through the lower point of the two intersections of the circle having a radius of 1.01R and the straight line x = L passing through the top of the door b4: The radius of the circle is R , The inclination passing through the lower point of the two intersections of the circle having a radius of 1.01R centered on the rotation center of the rotor and the straight line x = L passing through the top of the door is tan (θ + 48). The radius R is the radius of the circular portion of the inner wall surface of the chamber.
前記ドア頂部の長手方向の中央部は凹部とされており、
前記凹部に温度計が設置され、
長手方向に直交する断面視において、前記凹部を除く部分の、前記山形状の外形が、前記複数の直線で構成されている、
ゴム混練機の排出口を開閉するドア。 The door according to claim 5,
The central part in the longitudinal direction of the door top is a recess,
A thermometer is installed in the recess,
In the cross-sectional view orthogonal to the longitudinal direction, the mountain-shaped outer shape of the portion excluding the concave portion is composed of the plurality of straight lines.
A door that opens and closes the outlet of a rubber kneader.
前記凹部は、当該ドアの長手方向に直交する断面視において左右対称の山形状とされており、
前記凹部を除く部分の前記ドア頂部の高さをT1とし、前記凹部の山形状の頂部の高さをT2としたとき、
0.71T1≦T2≦0.96T1を満たし、
且つ、前記式(3)の中の右式で特定される、前記凹部を除く部分の前記ドア頂部の高さをTxとしたとき、
0.79Tx≦T2も満たし、
当該ドアの長手方向から視たときに、前記温度計の先端部が、前記ドア頂部と、前記凹部の山形状の頂部との間に配置されている、
ゴム混練機の排出口を開閉するドア。 The door according to claim 9,
The concave portion has a bilaterally symmetrical mountain shape in a cross-sectional view orthogonal to the longitudinal direction of the door,
When the height of the top portion of the door excluding the concave portion is T1, and the height of the mountain-shaped top portion of the concave portion is T2,
0.71T1 ≦ T2 ≦ 0.96T1 is satisfied,
And when the height of the door top portion of the portion excluding the concave portion specified by the right formula in the formula (3) is Tx,
0.79Tx ≦ T2 is also satisfied,
When viewed from the longitudinal direction of the door, the tip of the thermometer is disposed between the door top and the mountain-shaped top of the recess,
A door that opens and closes the outlet of a rubber kneader.
前記凹部は、当該ドアの長手方向に直交する断面視において左右対称の山形状とされており、
前記凹部の山形状の頂部の長手方向の長さが、前記温度計の直径よりも長く、且つ、当該ドアの長手方向の長さの1/2未満の長さとされている、
ゴム混練機の排出口を開閉するドア。 The door according to claim 9 or 10,
The concave portion has a bilaterally symmetrical mountain shape in a cross-sectional view orthogonal to the longitudinal direction of the door,
The length in the longitudinal direction of the crest-shaped top of the recess is longer than the diameter of the thermometer and less than half the length in the longitudinal direction of the door.
A door that opens and closes the outlet of a rubber kneader.