JP2017170854A - Production method of decorative article - Google Patents

Production method of decorative article Download PDF

Info

Publication number
JP2017170854A
JP2017170854A JP2016062409A JP2016062409A JP2017170854A JP 2017170854 A JP2017170854 A JP 2017170854A JP 2016062409 A JP2016062409 A JP 2016062409A JP 2016062409 A JP2016062409 A JP 2016062409A JP 2017170854 A JP2017170854 A JP 2017170854A
Authority
JP
Japan
Prior art keywords
decorative
sheet
mold
decorative sheet
resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2016062409A
Other languages
Japanese (ja)
Inventor
俊次 藤村
Shunji Fujimura
俊次 藤村
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nissha Printing Co Ltd
Original Assignee
Nissha Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nissha Printing Co Ltd filed Critical Nissha Printing Co Ltd
Priority to JP2016062409A priority Critical patent/JP2017170854A/en
Publication of JP2017170854A publication Critical patent/JP2017170854A/en
Pending legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To provide a production method of a decorative article in which the shape of a seam-like part is not deformed.SOLUTION: A production method of a decorative article is constituted as follows. A decorative sheet having a plurality of holes formed thereon is arranged on either or both molding surfaces of a pair of molds, the molds are closed, and a molten resin is injected into a cavity of the molds, to thereby mold the molten resin integrally with the decorative sheet so that a plurality of seam-like parts blocking the plurality of holes are aligned on the decorative surface side, and the molds are opened, to thereby take out the decorative article on which the plurality of seam-like parts exposed to the surface of the decorative sheet are formed.SELECTED DRAWING: Figure 1

Description

本発明は、加飾品の製造方法に関する。   The present invention relates to a method for manufacturing a decorative product.

自動車などにおいて、インストルメントパネルやフロアコンソールなどの車両内装部材は、本革または本革に似せて成形された樹脂シートからなる複数の表皮片を糸で縫合した表皮材を基材の表面に設置することで、デザイン面での質感向上を図ったものがある。近年では、表皮片を縫合することは手間やコストがかかることから、縫目を樹脂成形により再現した車両内装部材が提案されている。たとえば特許文献1には、まず、凸形状の縫目状部を含む第一部材を第一樹脂で成形し、次に、第一部材の縫目状部以外を覆うように第二部材を第二樹脂で成形し、縫目状部を有する成形品を製造するものである。   In automobiles, vehicle interior parts such as instrument panels and floor consoles are installed on the surface of the base material by stitching multiple pieces of skin made of genuine leather or resin sheets molded to resemble genuine leather with thread. By doing so, there is something that has improved the texture in design. In recent years, since it takes time and cost to sew skin pieces, a vehicle interior member in which a seam is reproduced by resin molding has been proposed. For example, in Patent Document 1, first, a first member including a convex seam-shaped portion is formed with a first resin, and then a second member is formed so as to cover other than the seam-shaped portion of the first member. A molded product having a seam-like portion is produced by molding with two resins.

特開2013−086369号公報JP 2013-086369 A

しかし、上記の製造方法においては、第二樹脂の射出圧力および熱によって、先に成形した凸形状の縫目状部が変形してしまうという問題がある。   However, in the above manufacturing method, there is a problem that the convex seam-shaped portion that has been formed is deformed by the injection pressure and heat of the second resin.

本発明は上記のような課題を解決するためになされたものであり、製造時に縫目状部の形状が変形しない加飾品の製造方法を提供することを目的とする。   The present invention has been made to solve the above-described problems, and an object of the present invention is to provide a method for manufacturing a decorative product in which the shape of the stitch-like portion is not deformed during manufacturing.

以下に、課題を解決するための手段として複数の態様を説明する。これら態様は必要に応じて任意に組み合わせることができる。   Hereinafter, a plurality of modes will be described as means for solving the problems. These embodiments can be arbitrarily combined as necessary.

本発明の加飾品の製造方法は、
複数の穴が形成された加飾シートを一対の金型の一方または両方の成形面に配置し、
金型を型閉じし、
金型のキャビティ内に溶融樹脂を射出して加飾シートの複数の穴をふさいでなる複数の縫目状部が加飾面側に並ぶように溶融樹脂を加飾シートと一体成形し、金型を型開きし、
加飾シートの表面に露出する複数の縫目状部が形成された加飾品を取り出すことを特徴とするものである。
The method for producing a decorative product of the present invention is as follows:
A decorative sheet in which a plurality of holes are formed is arranged on one or both molding surfaces of a pair of molds,
Close the mold,
The molten resin is injected into the cavity of the mold and the molten resin is integrally formed with the decorative sheet so that a plurality of stitched portions covering the multiple holes of the decorative sheet are arranged on the decorative surface side. Open the mold,
A decorative product in which a plurality of seam-shaped portions exposed on the surface of the decorative sheet is formed is taken out.

また、本発明の加飾品の製造方法は、
加飾シートと成形樹脂からなり複数の穴が形成された成形品を一対の金型の一方または両方の成形面に配置し、金型を型閉じし、
金型のキャビティ内に溶融樹脂を射出して成形品の複数の穴をふさいでなる複数の縫目状部が加飾面側に並ぶように溶融樹脂を成形品と一体成形し、
金型を型開きし、
成形品の表面に露出する複数の縫目状部が形成された加飾品を取り出すことを特徴とするものである。
Moreover, the manufacturing method of the decorative product of the present invention includes:
Place a molded product consisting of a decorative sheet and molding resin with multiple holes on one or both molding surfaces of a pair of molds, close the molds,
Injecting molten resin into the cavity of the mold and integrally molding the molten resin with the molded product so that the plurality of seams formed by blocking the plurality of holes of the molded product are arranged on the decorative surface side,
Open the mold,
The decorative product in which a plurality of stitch-like portions exposed on the surface of the molded product is formed is taken out.

好ましくは、加飾シートまたは成形品が配置された成形面における加飾シートまたは成形品に形成された複数の穴が位置する箇所に凹部が形成されているものである。   Preferably, a recess is formed at a position where a plurality of holes formed in the decorative sheet or the molded product on the molding surface on which the decorative sheet or the molded product is arranged.

さらに好ましくは、加飾シートは基材シートを含み、基材シートが加飾品の最表面にあるものである   More preferably, the decorative sheet includes a base sheet, and the base sheet is on the outermost surface of the decorative product.

また、好ましくは、キャビティ内に射出される溶融樹脂は、熱可塑性エラストマーである。   Preferably, the molten resin injected into the cavity is a thermoplastic elastomer.

また、好ましくは、キャビティ内に射出される溶融樹脂は、熱可塑性透光性樹脂である。   Preferably, the molten resin injected into the cavity is a thermoplastic translucent resin.

さらに好ましくは、加飾シートまたは成形樹脂の少なくとも一方が着色されているものである。   More preferably, at least one of the decorative sheet or the molded resin is colored.

また、好ましくは、加飾シートは図柄層を含み、図柄層には、加飾シートに形成された複数の穴によって区分された2以上の領域において、互いに異なる図柄が形成されているものである。   Preferably, the decorative sheet includes a design layer, and the design layer has different designs formed in two or more regions divided by a plurality of holes formed in the decorating sheet. .

さらに好ましくは、加飾シートまたは成形品を配置した金型の成形面には、加飾シートまたは成形品に形成された複数の穴が位置する箇所を境に、互いに異なる凹凸形状が形成されているものである。   More preferably, on the molding surface of the mold on which the decorative sheet or molded product is arranged, different concave and convex shapes are formed on the boundary where a plurality of holes formed in the decorative sheet or molded product are located. It is what.

本発明の加飾品の製造方法は、複数の穴が形成された加飾シートを一対の金型の一方または両方の成形面に配置し、金型を型閉じし、金型のキャビティ内に溶融樹脂を射出して加飾シートの複数の穴をふさいでなる複数の縫目状部が加飾面側に並ぶように溶融樹脂を加飾シートと一体成形し、金型を型開きし、加飾シートの表面に露出する複数の縫目状部が形成された加飾品を取り出すように構成した。   In the method for producing a decorative product according to the present invention, a decorative sheet in which a plurality of holes are formed is arranged on one or both molding surfaces of a pair of molds, the molds are closed, and the molds are melted in the mold cavities. The molten resin is integrally formed with the decorative sheet so that the seams formed by injecting the resin and blocking the holes of the decorative sheet are aligned on the decorative surface side, and the mold is opened and the mold is opened. The decorative article formed with a plurality of stitch-like portions exposed on the surface of the decorative sheet was taken out.

また、本発明の加飾品の製造方法は、加飾シートと成形樹脂からなり複数の穴が形成された成形品を一対の金型の一方または両方の成形面に配置し、金型を型閉じし、金型のキャビティ内に溶融樹脂を射出して成形品の複数の穴をふさいでなる複数の縫目状部が加飾面側に並ぶように溶融樹脂を成形品と一体成形し、金型を型開きし、成形品の表面に露出する複数の縫目状部が形成された加飾品を取り出すように構成した。   In addition, the method for producing a decorative product according to the present invention includes disposing a molded product made of a decorative sheet and a molding resin and having a plurality of holes on one or both molding surfaces of a pair of molds, and closing the mold. Then, the molten resin is injected into the mold cavity, and the molten resin is integrally formed with the molded product so that the plurality of stitched portions covering the plurality of holes of the molded product are arranged on the decorative surface side. The mold was opened, and a decorative product in which a plurality of stitch-like portions exposed on the surface of the molded product was formed was taken out.

したがって、本発明によれば、製造時に縫目状部の形状が変形しない加飾品を得ることができる。   Therefore, according to the present invention, it is possible to obtain a decorative product in which the shape of the stitch-like portion is not deformed at the time of manufacture.

本発明の第一実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 1st embodiment of this invention. 本発明の第一実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 1st embodiment of this invention. 本発明の第一実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 1st embodiment of this invention. 本発明の第一実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 1st embodiment of this invention. 本発明に係る第一実施形態の加飾品を示す斜視図である。It is a perspective view which shows the decorating goods of 1st embodiment which concerns on this invention. 図6のA−A断面図である。It is AA sectional drawing of FIG. 本発明に係る金型の一例を示す断面図である。It is sectional drawing which shows an example of the metal mold | die which concerns on this invention. 本発明に係る金型の一例を示す断面図である。It is sectional drawing which shows an example of the metal mold | die which concerns on this invention. 加飾シートの一例を示す平面図および断面図である。It is the top view and sectional drawing which show an example of a decorating sheet. 金型の成形面の形状の一例を示す平面図および断面図である。It is the top view and sectional drawing which show an example of the shape of the molding surface of a metal mold | die. 縫目状部の変形例を示す斜視図である。It is a perspective view which shows the modification of a stitch-like part. 本発明の第二実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 2nd embodiment of this invention. 本発明の第二実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 2nd embodiment of this invention. 本発明の第二実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 2nd embodiment of this invention. 本発明の第二実施形態における加飾品の製造工程を示す断面図である。It is sectional drawing which shows the manufacturing process of the decorating goods in 2nd embodiment of this invention. 本発明に係る第二実施形態の加飾品を示す斜視図である。It is a perspective view which shows the decorating product of 2nd embodiment which concerns on this invention. 図17のB−B断面図である。It is BB sectional drawing of FIG. 本発明の第二実施形態の加飾品の変形例を示す断面図である。It is sectional drawing which shows the modification of the decorating product of 2nd embodiment of this invention. 本発明に係る金型の一例を示す断面図である。It is sectional drawing which shows an example of the metal mold | die which concerns on this invention.

以下、本発明の加飾品の製造方法について、実施形態の一例を説明する。   Hereinafter, an example of an embodiment is explained about a manufacturing method of a decoration article of the present invention.

<第一実施形態>
本発明の加飾品の製造方法は、複数の穴が形成された加飾シートを一対の金型の一方または両方の成形面に配置し、金型を型閉じし、金型のキャビティ内に溶融樹脂を射出して加飾シートの複数の穴をふさいでなる複数の縫目状部が加飾面側に並ぶように溶融樹脂を加飾シートと一体成形し、金型を型開きし、加飾シートの表面に露出する複数の縫目状部が形成された加飾品を取り出すことを特徴とするものである。
<First embodiment>
In the method for producing a decorative product according to the present invention, a decorative sheet in which a plurality of holes are formed is arranged on one or both molding surfaces of a pair of molds, the molds are closed, and the molds are melted in the mold cavities. The molten resin is integrally formed with the decorative sheet so that the seams formed by injecting the resin and blocking the holes of the decorative sheet are aligned on the decorative surface side, and the mold is opened and the mold is opened. A decorative product in which a plurality of stitch-like portions exposed on the surface of the decorative sheet is formed is taken out.

まず、複数の穴5が形成された加飾シート2を、金型3の可動型30の成形面に配置する(図1参照)。加飾シート2は、基体シート20上に、保護層、図柄層、接着層などを含む加飾層21を積層したものを用いることができる。加飾シート2は、基体シート20と加飾層21の両方を貫通する複数の穴5が形成されたものを用いる。   First, the decorative sheet 2 in which the plurality of holes 5 are formed is disposed on the molding surface of the movable mold 30 of the mold 3 (see FIG. 1). The decorative sheet 2 may be a laminate obtained by laminating a decorative layer 21 including a protective layer, a design layer, an adhesive layer and the like on the base sheet 20. As the decorative sheet 2, a sheet in which a plurality of holes 5 penetrating both the base sheet 20 and the decorative layer 21 is formed is used.

基体シート20の材質は特に限定されず、たとえば、ポリプロピレン系樹脂、ポリエチレン系樹脂、ポリアミド系樹脂、アクリル系樹脂、オレフィン系樹脂、ポリエステル系樹脂、塩ビ系樹脂、ポリカーボネート系樹脂、ABS系樹脂などの熱可塑性樹脂およびこれらの積層品を挙げることができる。基体シート20の厚みは、20μm〜600μmとすることができる。   The material of the base sheet 20 is not particularly limited, and examples thereof include a polypropylene resin, a polyethylene resin, a polyamide resin, an acrylic resin, an olefin resin, a polyester resin, a vinyl resin, a polycarbonate resin, and an ABS resin. A thermoplastic resin and these laminated products can be mentioned. The thickness of the base sheet 20 can be 20 μm to 600 μm.

保護層、図柄層、接着層の形成方法としては、グラビア印刷法、スクリーン印刷法、オフセット印刷法などの通常の印刷法や、グラビアコート法、ロールコート法、ダイコート法などのコート法を用いるとよい。   As a method for forming the protective layer, the design layer, and the adhesive layer, a normal printing method such as a gravure printing method, a screen printing method, an offset printing method, or a coating method such as a gravure coating method, a roll coating method, or a die coating method is used. Good.

なお、基体シート20を加飾品から剥離しない場合において、保護層、図柄層、接着層は基体シート20の表裏に振り分けて形成してもよい。たとえば、保護層のみを基体シートの一方の面に電離放射線硬化型樹脂を用いて形成し、図柄層と接着層を基体シートの他方の面に形成してもよい。このようにすると、基体シートよりも硬度の高い保護層が加飾品の表面となるため、加飾品の摩耗や傷付きなどをより有効に防止することができる。また、保護層に表皮に似た柔らかい触感層を形成することや、防指紋性や反射防止性を付与することもできる。   In the case where the base sheet 20 is not peeled from the decorative article, the protective layer, the design layer, and the adhesive layer may be formed separately on the front and back of the base sheet 20. For example, only the protective layer may be formed on one side of the base sheet using an ionizing radiation curable resin, and the design layer and the adhesive layer may be formed on the other side of the base sheet. If it does in this way, since the protective layer whose hardness is higher than a base sheet will be the surface of a decorative article, abrasion, damage, etc. of a decorative article can be prevented more effectively. In addition, a soft tactile layer similar to the epidermis can be formed on the protective layer, and fingerprint resistance and antireflection can be imparted.

なお、上記の各層を形成する際の乾燥温度は、たとえば、50℃〜200℃にすることができる。   In addition, the drying temperature at the time of forming each said layer can be 50 degreeC-200 degreeC, for example.

上記の加飾シート2を、可動型30の成形面に配置する(図1参照)。可動型30の成形面には、吸引孔を設けるとよい(図示せず)。このようにすると、可動型30と加飾シート2との間の空気を吸引孔から吸引でき、加飾シート2を可動型30の成形面に密着することができる。加飾シート2は枚葉で供給する。なお、加飾シート2は、たとえば、加飾シート2を長尺で成形面に送り込む装置を用いて金型内に供給することもできる。上記した内容は、加飾シート2を固定型31の成形面に配置する場合も適用できる。吸引孔は、加飾シート2に跡が残らないように成形面外周にスリット状に形成してもよい。   The decorative sheet 2 is placed on the molding surface of the movable mold 30 (see FIG. 1). A suction hole may be provided on the molding surface of the movable mold 30 (not shown). If it does in this way, the air between the movable mold | type 30 and the decorating sheet 2 can be attracted | sucked from a suction hole, and the decorating sheet 2 can be closely_contact | adhered to the molding surface of the movable mold | type 30. The decorative sheet 2 is supplied as a single sheet. In addition, the decorating sheet 2 can also be supplied in a metal mold | die using the apparatus which sends the decorating sheet 2 to a molding surface by elongate, for example. The contents described above can also be applied when the decorative sheet 2 is arranged on the molding surface of the fixed mold 31. The suction hole may be formed in a slit shape on the outer periphery of the molding surface so that no trace remains on the decorative sheet 2.

なお、加飾シート2は金型外で予備賦形してから金型内に配置してもよく、金型内に供給した後に加飾シート2を加熱し賦形することで配置してもよい。   The decorative sheet 2 may be preliminarily shaped outside the mold and then placed in the mold, or may be arranged by heating and shaping the decorative sheet 2 after being supplied into the mold. Good.

また、加飾シート2を可動型30と固定型31の両方の成形面に長尺で供給する場合は、それぞれの加飾シートを送り込む方向を90度ずらすとよい。つまり、可動型30側の加飾シートは図1の上から下へ送り込まれ、固定型31側の加飾シートは図1の奥から手前(または手前から奥)へ送り込まれるよう配置する。   Moreover, when supplying the decorating sheet 2 to the molding surfaces of both the movable mold 30 and the fixed mold 31 in a long length, the direction of feeding the decorating sheets may be shifted by 90 degrees. That is, the decorative sheet on the movable mold 30 side is sent from the top to the bottom of FIG. 1, and the decorative sheet on the fixed mold 31 side is sent from the back of FIG. 1 to the front (or the front to the back).

次に、可動型30と固定型31とを型閉じする(図2参照)。このとき、可動型30と固定型31との間には、キャビティ4が形成される。   Next, the movable mold 30 and the fixed mold 31 are closed (see FIG. 2). At this time, the cavity 4 is formed between the movable mold 30 and the fixed mold 31.

次に、キャビティ4内に溶融樹脂を射出する(図3参照)。樹脂としては、たとえば、ポリスチレン系樹脂、ポリオレフィン系樹脂、ABS樹脂、AS樹脂、AN樹脂などの汎用樹脂を挙げることができる。また、ポリフェニレンオキシド・ポリスチレン系樹脂、ポリカーボネート系樹脂、ポリアセタール系樹脂、アクリル系樹脂、ポリカーボネート変性ポリフェニレンエーテル樹脂、ポリブチレンテレフタレート樹脂、超高分子量ポリエチレン樹脂などの汎用エンジニアリング樹脂や、ポリスルホン樹脂、ポリフェニレンサルファイド系樹脂、ポリフェニレンオキシド系樹脂、ポリアリレート樹脂、ポリエーテルイミド樹脂、ポリイミド樹脂、液晶ポリエステル樹脂、ポリアリル系耐熱樹脂などのスーパーエンジニアリング樹脂を使用することもできる。さらに、ガラス繊維や無機フィラーなどの補強材を添加した複合樹脂も使用できる。   Next, molten resin is injected into the cavity 4 (see FIG. 3). Examples of the resin include general-purpose resins such as polystyrene resin, polyolefin resin, ABS resin, AS resin, and AN resin. Also, general engineering resins such as polyphenylene oxide / polystyrene resins, polycarbonate resins, polyacetal resins, acrylic resins, polycarbonate-modified polyphenylene ether resins, polybutylene terephthalate resins, ultrahigh molecular weight polyethylene resins, polysulfone resins, polyphenylene sulfide Super engineering resins such as resins, polyphenylene oxide resins, polyarylate resins, polyetherimide resins, polyimide resins, liquid crystal polyester resins, and polyallyl heat-resistant resins can also be used. Furthermore, composite resins to which reinforcing materials such as glass fibers and inorganic fillers are added can also be used.

射出した溶融樹脂は、加飾シート2に形成された複数の穴5を通って、可動型30の成形面に到達する。つまり溶融樹脂は、複数の穴5をふさぎ、加飾層21の側に複数の縫目状部11が並ぶように加飾シート2と一体成形される(図3、図6参照)。   The injected molten resin passes through the plurality of holes 5 formed in the decorative sheet 2 and reaches the molding surface of the movable mold 30. That is, the molten resin closes the plurality of holes 5 and is integrally formed with the decorating sheet 2 so that the plurality of stitch portions 11 are arranged on the decorating layer 21 side (see FIGS. 3 and 6).

次いで、金型を型開きする(図4参照)。固定型31には、溶融樹脂が加飾シート2と一体成形された加飾品1が残る。加飾品1の加飾面側には、加飾シート2の複数の穴5によって形成された複数の縫目状部11が並んでいる(図6参照)。   Next, the mold is opened (see FIG. 4). On the fixed mold 31, the decorative product 1 in which the molten resin is integrally formed with the decorative sheet 2 remains. A plurality of seam-like portions 11 formed by the plurality of holes 5 of the decorative sheet 2 are arranged on the decorative surface side of the decorative article 1 (see FIG. 6).

最後に、加飾品1を金型から取り出す(図5参照)。本実施形態では、加飾シート2の基体シート20は加飾層21から剥離しない。そのため、基体シート20が加飾品1の最表面となる。また、図示したように、複数の縫目状部11は加飾シート2の表面から飛び出さないため、加飾品1の表面は平滑となる。なお、後述する第二実施形態などにおいて、基体シート20が加飾層21から剥離されている場合は、基体シート20の厚み分だけ加飾層21から複数の縫目状部11が飛び出した加飾品1を得ることができる。   Finally, the decorative article 1 is taken out from the mold (see FIG. 5). In this embodiment, the base sheet 20 of the decorative sheet 2 does not peel from the decorative layer 21. Therefore, the base sheet 20 becomes the outermost surface of the decorative article 1. Moreover, since the some stitch-shaped part 11 does not jump out from the surface of the decorating sheet 2 as shown in figure, the surface of the decorating goods 1 becomes smooth. In addition, in 2nd embodiment etc. which are mentioned later, when the base sheet 20 is peeled from the decorating layer 21, the several stitch-like part 11 protruded from the decorating layer 21 by the thickness of the base sheet 20. The ornament 1 can be obtained.

また、本発明の加飾品の製造方法の変形例としては、加飾シート2が配置された成形面における加飾シート2に形成された複数の穴5が位置する箇所に凹部30aが形成されているものである(図7、図8参照)。さらに、キャビティ4内に射出される溶融樹脂は、熱可塑性エラストマーである。   Moreover, as a modification of the method for manufacturing a decorative product according to the present invention, the concave portion 30a is formed at a position where the plurality of holes 5 formed in the decorative sheet 2 on the molding surface on which the decorative sheet 2 is arranged. (See FIGS. 7 and 8). Furthermore, the molten resin injected into the cavity 4 is a thermoplastic elastomer.

加飾シート2は上記実施形態と同様のものを用い、可動型30の成形面に配置する。このとき、加飾シート2が配置された成形面には、加飾シート2に形成された複数の穴5が位置する箇所に凹部30aを形成する。次に、型締めを行い、熱可塑性エラストマー樹脂をキャビティ4内に射出する。図7の態様においては、可動型30の成形面に凹部30aが形成されているため、得られる加飾品1の表面からは、凹部30aの深さ分だけ複数の縫目状部11が突出する。柔軟な熱可塑性エラストマーを成形して縫目状部11を形成しているため、縫目状部が糸で形成された従来の加飾品よりも、縫目状部11の触感が柔らかい加飾品1を得ることができる。図8の態様においては、加飾品1の表面と同じかそれよりも低い位置に縫目状部11の頭頂部分が形成された加飾品1を得ることができる。このようにすると、表皮を糸できつく縫合したとき縫目が表皮に食い込んだような形状の縫目状部を形成することができる。つまり、糸で形成した縫目により近い縫目状部を形成することができる。   The decorative sheet 2 is the same as that in the above embodiment, and is arranged on the molding surface of the movable mold 30. At this time, the recessed part 30a is formed in the location in which the some hole 5 formed in the decorating sheet 2 is located in the molding surface where the decorating sheet 2 is arrange | positioned. Next, mold clamping is performed, and a thermoplastic elastomer resin is injected into the cavity 4. In the aspect of FIG. 7, since the recessed part 30a is formed in the shaping | molding surface of the movable mold | type 30, from the surface of the decoration 1 obtained, the some stitch-like part 11 protrudes by the depth of the recessed part 30a. . Since the stitched portion 11 is formed by molding a flexible thermoplastic elastomer, the stitched portion 1 has a softer tactile feel than the conventional decorated product in which the stitched portion is formed of a thread. Can be obtained. In the aspect of FIG. 8, it is possible to obtain the decorative product 1 in which the top portion of the stitch portion 11 is formed at the same position as or lower than the surface of the decorative product 1. In this way, it is possible to form a seam-like portion having a shape in which the seam bites into the skin when the skin is tightly stitched. That is, it is possible to form a seam-like portion that is closer to the seam formed by the thread.

また、透光性を有する熱可塑性エラストマーを用いれば、加飾品1の加飾面側とは反対側に光源を含む電子部品などを配置することで、複数の縫目状部11を発光させることができる。たとえば、複数のLEDを含む電子部品を加飾品1と組み合せてオーディオパネルとして用いれば、オーディオの使用者はそのときの気分によって任意に縫目状部の色を変えることができる。また、複数のLEDと温度センサを含む電子部品を加飾品1と組み合せて自動車の内装部材として用いれば、車内の温度の変化に応じて縫目状部の色を変化させることができる。透光性を有する熱可塑性エラストマーを用いる場合、加飾シート2は着色されていることが好ましい。着色された基体シート20を用いてもよいし、着色樹脂によって加飾層21を形成してもよい。このようにすると、光源からの光が加飾品1から漏れることを抑制することができる。   Moreover, if the thermoplastic elastomer which has translucency is used, the several stitch-shaped part 11 will be light-emitted by arrange | positioning the electronic component etc. which contain a light source on the opposite side to the decorating surface side of the decorating goods 1. FIG. Can do. For example, if an electronic component including a plurality of LEDs is combined with the decorative article 1 and used as an audio panel, the audio user can arbitrarily change the color of the stitch-like portion depending on the mood at that time. Moreover, if the electronic component containing several LED and a temperature sensor is combined with the decorating goods 1, and it uses as an interior member of a motor vehicle, the color of a stitch-like part can be changed according to the change of the temperature in a vehicle. When using the thermoplastic elastomer which has translucency, it is preferable that the decorating sheet 2 is colored. The colored base sheet 20 may be used, or the decorative layer 21 may be formed of a colored resin. If it does in this way, it can control that the light from a light source leaks from decoration 1.

本実施形態で用いる加飾シート2の変形例としては、複数の穴5によって区分された2以上の領域において、互いに異なる図柄が形成されているものである(図9参照)。図9(a)においては、複数の穴5によって囲まれているほぼ長方形の領域内には図柄21bを形成し、領域外には図柄21cを形成する。この態様では、異なる図柄21b、21cを縫い合わせたような加飾シート2を得ることができる。なお、図柄21bの領域は、複数の穴5によって形成される領域よりも大きくてもよいし、小さくてもよい。このようにすると、複数の図柄を組み合わせられるため、多様な表現が可能となる。   As a modification of the decorative sheet 2 used in the present embodiment, different symbols are formed in two or more regions divided by a plurality of holes 5 (see FIG. 9). In FIG. 9A, a symbol 21b is formed in a substantially rectangular region surrounded by the plurality of holes 5, and a symbol 21c is formed outside the region. In this aspect, it is possible to obtain a decorative sheet 2 in which different symbols 21b and 21c are stitched together. In addition, the area | region of the pattern 21b may be larger than the area | region formed by the several hole 5, and may be small. In this way, since a plurality of symbols can be combined, various expressions are possible.

また、本実施形態で用いる金型の変形例としては、可動型30の成形面には、加飾シート2に形成された複数の穴5が位置する箇所を境に、互いに異なる凹凸形状が形成されているものである(図9、図10参照)。成形面における加飾シート2に形成された複数の穴5が位置する箇所には、凹部30aが形成されている。凹部30aによって形成される領域内には凹凸形状30bを形成し、領域外には凹凸形状30cを形成する(図10(a)、(b)、(c)参照)。凹凸形状30bと凹凸形状30cは互いに異なる形状である。なお、本明細書においては、凹凸がない平滑な面も凹凸形状に含むものとする。図10(a)に示す可動型30の成形面に、たとえば、図9(a)に示す加飾シート2を配置すると、加飾シート2に形成された複数の穴5が可動型30の成形面に形成された凹部30aに位置する。このとき、凹凸形状30bが形成された成形面には図柄21bが配置され、凹凸形状30cが形成された成形面には図柄21cが配置される。たとえば、図柄21bが皮革調で凹凸形状30bがシボ加工による形状であり、図柄21cが金属調で凹凸形状30cが平滑面である場合、皮革調の部材と金属調の部材とを縫合したような意外性のある加飾品1を得ることができる。上記のように、成形面の凹凸形状と加飾シートの図柄とを同期することによって、より質感の高い加飾品を得ることができる。   Further, as a modification of the mold used in the present embodiment, different concave and convex shapes are formed on the molding surface of the movable mold 30 on the boundary where the plurality of holes 5 formed in the decorative sheet 2 are located. (See FIGS. 9 and 10). Concave portions 30a are formed at locations where the plurality of holes 5 formed in the decorative sheet 2 on the molding surface are located. An uneven shape 30b is formed in the region formed by the recess 30a, and an uneven shape 30c is formed outside the region (see FIGS. 10A, 10B, and 10C). The uneven shape 30b and the uneven shape 30c are different from each other. In the present specification, a smooth surface without unevenness is also included in the uneven shape. When, for example, the decorative sheet 2 shown in FIG. 9A is arranged on the molding surface of the movable mold 30 shown in FIG. 10A, a plurality of holes 5 formed in the decorative sheet 2 are formed into the movable mold 30. Located in the recess 30a formed on the surface. At this time, the pattern 21b is arranged on the molding surface on which the concavo-convex shape 30b is formed, and the design 21c is arranged on the molding surface on which the concavo-convex shape 30c is formed. For example, when the pattern 21b is leather-like and the concavo-convex shape 30b is a textured shape, and the pattern 21c is metallic and the concavo-convex shape 30c is a smooth surface, the leather-like member and the metal-like member are stitched together. An unexpected decorative item 1 can be obtained. As described above, by synchronizing the uneven shape of the molding surface with the design of the decorative sheet, a decorative product with higher texture can be obtained.

なお、凹凸形状30bが形成された成形面と、凹凸形状30cが形成された成形面とは、必ずしも同一平面状に形成しなくてもよい。たとえば、図10(b)を参照して、凹凸形状30bが形成された成形面を、凹凸形状30cが形成された成形面よりも全体的に深く形成してもよい。このようにすると、凹凸形状30bが形成された成形面が凸形状となり、立体感のある加飾品を得ることができる。   Note that the molding surface on which the concavo-convex shape 30b is formed and the molding surface on which the concavo-convex shape 30c are formed do not necessarily have to be formed in the same plane. For example, referring to FIG. 10B, the molding surface on which the concavo-convex shape 30b is formed may be formed deeper overall than the molding surface on which the concavo-convex shape 30c is formed. If it does in this way, the molding surface in which the uneven | corrugated shape 30b was formed will become a convex shape, and a decorative article with a three-dimensional effect can be obtained.

なお、加飾シート2に形成された複数の穴5は必ずしも環状になっていなくてもよい。このような加飾シート2を用いれば、たとえば、図11に示すような加飾品1を得ることができる。図11(a)の加飾品1は、直線状の1つの縫目状部11によって区分された領域にそれぞれ図柄21b、21cを有している。図11(b)の加飾品1は、斜め状の2つの縫目状部11によって区分された3つの領域にそれぞれ図柄21b、21cを有している。図11(c)の加飾品1は、直線状の交差する縫目状部11によって区分された4つの領域に、それぞれ図柄21b、21c、21d、21eを有している。   In addition, the some hole 5 formed in the decorating sheet 2 does not necessarily need to be cyclic | annular. If such a decorating sheet 2 is used, for example, a decorating product 1 as shown in FIG. 11 can be obtained. The decorative article 1 in FIG. 11A has symbols 21b and 21c in regions divided by one linear stitch portion 11, respectively. The decorative article 1 in FIG. 11B has symbols 21b and 21c in three regions divided by two oblique seam-like portions 11, respectively. The decorative article 1 in FIG. 11 (c) has symbols 21b, 21c, 21d, and 21e in four regions divided by straight intersecting stitch portions 11, respectively.

本実施形態は、基体シート20と加飾層21の両方を貫通する複数の穴5を有する加飾シート2を可動型30の成形面に配置した後、溶融樹脂によって縫目状部11を形成するものである。したがって、従来の製造方法のような2色成形法を用いるものではないため、本実施形態の製造方法では縫目状部11が変形しにくい。   In the present embodiment, the decorative sheet 2 having a plurality of holes 5 penetrating both the base sheet 20 and the decorative layer 21 is arranged on the molding surface of the movable mold 30, and then the stitch-like portion 11 is formed by molten resin. To do. Therefore, since the two-color molding method as in the conventional manufacturing method is not used, the stitch-like portion 11 is not easily deformed in the manufacturing method of the present embodiment.

<第二実施形態>
次に、本発明の第二実施形態について説明する。本発明の加飾品の製造方法は、加飾シートと成形樹脂からなり複数の穴が形成された成形品を一対の金型の一方または両方の成形面に配置し、金型を型閉じし、金型のキャビティ内に溶融樹脂を射出して成形品の複数の穴をふさいでなる複数の縫目状部が加飾面側に並ぶように溶融樹脂を成形品と一体成形し、金型を型開きし、成形品の表面に露出する複数の縫目状部が形成された加飾品を取り出すことを特徴とするものである。
<Second embodiment>
Next, a second embodiment of the present invention will be described. The method for producing a decorative product of the present invention is a method of arranging a molded product formed of a decorative sheet and a molding resin and having a plurality of holes formed on one or both molding surfaces of a pair of molds, and closing the mold. The molten resin is injected into the mold cavity, and the molten resin is integrally molded with the molded product so that the seams formed by blocking the holes in the molded product are lined up on the decorative surface. The mold is opened, and a decorative product in which a plurality of stitch-like portions exposed on the surface of the molded product is formed is taken out.

まず、加飾シート2Aと成形樹脂10Aからなり複数の穴5Aが形成された成形品6を、可動型30Aの成形面に配置する(図12参照)。加飾シート2Aは第一実施形態と同様のものを用いることができる。成形品6は加飾シート2Aと成形樹脂10Aとを一体成形したものを用いる。成形品6には、加飾シート2Aと成形樹脂10Aの両方に貫通する複数の穴5Aを形成する。成形品6は、可動型30Aの成形面に設けた吸引孔を介して、または固定用治具などを用いて、可動型30Aの成形面に固定することができる。なお、成形品6は、成形品6を成形した後に加飾シート2Aの基体シートを剥離したものを用いてもよい。   First, the molded product 6 made of the decorative sheet 2A and the molded resin 10A and having a plurality of holes 5A is arranged on the molding surface of the movable mold 30A (see FIG. 12). The same decorative sheet 2A as in the first embodiment can be used. As the molded product 6, a product obtained by integrally molding the decorative sheet 2A and the molded resin 10A is used. In the molded product 6, a plurality of holes 5A penetrating both the decorative sheet 2A and the molded resin 10A are formed. The molded product 6 can be fixed to the molding surface of the movable mold 30A through a suction hole provided on the molding surface of the movable mold 30A or using a fixing jig or the like. In addition, after shape | molding the molded product 6, you may use the molded product 6 which peeled the base sheet of the decorating sheet 2A.

次に、可動型30Aと固定型31Aとを型閉じする(図13参照)。このとき、可動型30Aと固定型31Aとの間には、キャビティ4Aが形成される。   Next, the movable mold 30A and the fixed mold 31A are closed (see FIG. 13). At this time, a cavity 4A is formed between the movable mold 30A and the fixed mold 31A.

次に、キャビティ4A内に溶融樹脂を射出する(図14参照)。樹脂としては、第一実施形態と同様のものを使用することができる。射出した溶融樹脂は、成形品6に形成された複数の穴5Aを通って、可動型30Aの成形面に到達する。つまり溶融樹脂は、複数の穴5Aをふさぎ、加飾シート2Aの側に複数の縫目状部11Aが並ぶように成形品6と一体成形される(図14、図17参照)。   Next, molten resin is injected into the cavity 4A (see FIG. 14). As the resin, the same resin as in the first embodiment can be used. The injected molten resin passes through the plurality of holes 5A formed in the molded product 6 and reaches the molding surface of the movable mold 30A. That is, the molten resin is integrally formed with the molded product 6 so as to close the plurality of holes 5A and to arrange the plurality of stitch-like portions 11A on the decorative sheet 2A side (see FIGS. 14 and 17).

本実施形態において、可動型30Aの成形面には、成形品6に形成された複数の穴5が位置する箇所に凹部30a´を形成することが好ましい(図19(a)、(b)参照)。図19(a)の態様においては、加飾シート2Aの表面と同じかそれよりも低い位置に縫目状部11Aの頭頂部分が形成された加飾品1Aを得ることができる。このようにすると、表皮片を糸できつく縫合したとき縫目が表皮に食い込んだような形状の縫目状部を形成することができる。つまり、糸で形成した縫目により近い縫目状部を形成することができる。また、図19(a)においては、穴5Aに対応する位置に可動型30Aの成形面から突出した部分があり、その端面に凹部30a´が形成されているということもできる。したがって、凹部30a´を含む突出部を穴5Aの位置決め手段として用い、成形品6を可動型30Aの成形面に配置することができる。図19(b)の態様においては、凹部30a´の深さ分だけ縫目状部が突出した加飾品1Aを得ることができる。いずれの態様においても、表皮片に糸で縫目を形成したような、高級感のある加飾品を得ることができる。   In the present embodiment, it is preferable to form a recess 30a ′ on the molding surface of the movable mold 30A at a position where the plurality of holes 5 formed in the molded product 6 are located (see FIGS. 19A and 19B). ). In the aspect of Fig.19 (a), the decoration 1A in which the top part of the stitch-like part 11A was formed in the same position as the surface of the decoration sheet 2A or lower than that can be obtained. In this way, it is possible to form a seam-like portion having a shape in which the seam bites into the epidermis when the epidermis piece is sewn tightly. That is, it is possible to form a seam-like portion that is closer to the seam formed by the thread. In FIG. 19A, it can also be said that there is a portion protruding from the molding surface of the movable mold 30A at a position corresponding to the hole 5A, and a recess 30a ′ is formed on the end surface. Therefore, it is possible to arrange the molded product 6 on the molding surface of the movable mold 30A by using the protruding portion including the recess 30a ′ as the positioning means for the hole 5A. In the embodiment of FIG. 19 (b), it is possible to obtain a decorative product 1A in which the seam-like portion protrudes by the depth of the recess 30a ′. In any embodiment, it is possible to obtain a high-quality decorative product in which a stitch is formed with a thread on the skin piece.

次いで、金型を型開きする(図15参照)。固定型31Aには、成形樹脂10Bが成形品6と一体成形された加飾品1Aが残る。加飾面側には、複数の穴5Aによって形成された複数の縫目状部11Aが並んでいる(図17参照)。   Next, the mold is opened (see FIG. 15). In the fixed mold 31A, the decorative product 1A in which the molded resin 10B is integrally formed with the molded product 6 remains. On the decorative surface side, a plurality of seam-like portions 11A formed by a plurality of holes 5A are arranged (see FIG. 17).

最後に、加飾品1Aを金型から取り出す(図16参照)。   Finally, the decorative article 1A is taken out from the mold (see FIG. 16).

また、本発明の加飾品の製造方法の変形例として、キャビティ4A内に射出する溶融樹脂は、熱可塑性エラストマーである。特に加飾品が車載用途である場合には、100℃以上の耐熱使用温度を有するポリエステル系またはポリアミド系エラストマーが有効である。従来の製造方法は、複数の縫目状部を一次樹脂で成形し、その後に二次樹脂で成形を行うものであった。したがって、従来の製造方法において熱可塑性エラストマーを一次樹脂に使用した場合は、二次成形における樹脂圧や樹脂熱により、熱可塑性エラストマーが変形する。これに対して本発明の製造方法では、成形品6に複数の貫通穴を形成した後、熱可塑性エラストマーを二次樹脂として使用し、複数の縫目状部11Aを形成する。したがって、熱可塑性エラストマーで形成される複数の縫目状部11Aが変形しにくい。   As a modification of the method for manufacturing a decorative product of the present invention, the molten resin injected into the cavity 4A is a thermoplastic elastomer. In particular, when the decorative product is used in a vehicle, a polyester-based or polyamide-based elastomer having a heat resistant use temperature of 100 ° C. or higher is effective. In the conventional manufacturing method, a plurality of seam-shaped portions are formed with a primary resin, and then formed with a secondary resin. Therefore, when the thermoplastic elastomer is used as the primary resin in the conventional manufacturing method, the thermoplastic elastomer is deformed by the resin pressure or the resin heat in the secondary molding. On the other hand, in the manufacturing method of the present invention, after forming a plurality of through holes in the molded article 6, a thermoplastic elastomer is used as a secondary resin to form a plurality of stitched portions 11A. Accordingly, the plurality of seam-like portions 11A formed of the thermoplastic elastomer are not easily deformed.

また、透光性を有する熱可塑性エラストマーを用いる場合、加飾シート2Aまたは成形樹脂10Aの少なくとも一方は着色されていることが好ましい。加飾シート2Aが基体シートを含む場合は、着色された基体シートを用いるとよい。加飾シート2Aが基体シートを含まない場合は、着色樹脂によって加飾層を形成してもよい。また、着色された成形樹脂10Aを用いてもよい。着色された加飾シート2Aと、着色された成形樹脂10Aとを用いてもよい。このようにすると、光源からの光が加飾品1Aから漏れることを抑制することができる。   Moreover, when using the thermoplastic elastomer which has translucency, it is preferable that at least one of the decorating sheet 2A or the molding resin 10A is colored. When the decorative sheet 2A includes a base sheet, a colored base sheet may be used. When 2 A of decorating sheets do not contain a base sheet, you may form a decorating layer with colored resin. Alternatively, a colored molding resin 10A may be used. Colored decorative sheet 2A and colored molding resin 10A may be used. If it does in this way, it can control that the light from a light source leaks from decoration 1A.

なお、第二実施形態においては、成形樹脂10Bを、成形樹脂10Aの裏側全面に筐体状で形成した。成形樹脂10Bの形状はこれに限定されず、図18に示すように、成形品6の裏側の一部に成形樹脂10Bを形成することもできる。   In the second embodiment, the molding resin 10B is formed in a casing shape on the entire back surface of the molding resin 10A. The shape of the molded resin 10B is not limited to this, and the molded resin 10B can be formed on a part of the back side of the molded product 6 as shown in FIG.

なお、成形樹脂10Bの成形において、圧縮成形を組み合わせて低圧成形にすることで、射出時に発生する成形品6の変形をより有効に抑制することができる。   In the molding of the molded resin 10B, the deformation of the molded product 6 occurring at the time of injection can be more effectively suppressed by combining the compression molding with the low pressure molding.

以上のようにして、本発明の加飾品を得ることができる。   As described above, the decorative product of the present invention can be obtained.

1、1A :加飾品
10、10A、10B:成形樹脂
11、11A :縫目状部
2、2A :加飾シート
20 :基体シート
21 :加飾層
22 :保護層
23 :接着層
3、3A :金型
30、30A :可動型
31、31A :固定型
30a、30a´ :凹部
4、4A :キャビティ
5、5A :穴
6 :成形品
1, 1A: Decorative product 10, 10A, 10B: Molded resin 11, 11A: Stitched portion 2, 2A: Decorative sheet 20: Base sheet 21: Decorative layer 22: Protective layer 23: Adhesive layer 3, 3A: Mold 30, 30A: Movable mold 31, 31A: Fixed mold 30a, 30a ': Recess 4, 4, A: Cavity 5, 5A: Hole 6: Molded product

Claims (9)

複数の穴が形成された加飾シートを一対の金型の一方または両方の成形面に配置し、
前記金型を型閉じし、
前記金型のキャビティ内に溶融樹脂を射出して前記加飾シートの複数の前記穴をふさいでなる複数の縫目状部が加飾面側に並ぶように前記溶融樹脂を前記加飾シートと一体成形し、前記金型を型開きし、
前記加飾シートの表面に露出する複数の前記縫目状部が形成された加飾品を取り出すことを特徴とする加飾品の製造方法。
A decorative sheet in which a plurality of holes are formed is arranged on one or both molding surfaces of a pair of molds,
Close the mold,
The molten resin is injected into the cavity of the mold, and the molten resin and the decorative sheet are arranged so that a plurality of stitch-like portions formed by blocking the plurality of holes of the decorative sheet are arranged on the decorative surface side. Integrally molding, opening the mold,
A method for producing a decorative product, comprising: taking out a decorative product in which a plurality of the stitch-like portions exposed on the surface of the decorative sheet are formed.
加飾シートと成形樹脂からなり複数の穴が形成された成形品を一対の金型の一方または両方の成形面に配置し、前記金型を型閉じし、
前記金型のキャビティ内に溶融樹脂を射出して前記成形品の複数の前記穴をふさいでなる複数の縫目状部が加飾面側に並ぶように前記溶融樹脂を前記成形品と一体成形し、
前記金型を型開きし、
前記成形品の表面に露出する複数の前記縫目状部が形成された加飾品を取り出すことを特徴とする加飾品の製造方法。
A molded product made of a decorative sheet and a molding resin and formed with a plurality of holes is disposed on one or both molding surfaces of a pair of molds, and the mold is closed.
The molten resin is injected into the cavity of the mold, and the molten resin is integrally formed with the molded product so that a plurality of seam-like portions formed by blocking the plurality of holes of the molded product are arranged on the decorative surface side. And
Open the mold,
A method for producing a decorative product, comprising: taking out a decorative product in which a plurality of the stitch-like portions exposed on the surface of the molded product is formed.
前記加飾シートまたは前記成形品が配置された前記成形面における前記加飾シートまたは前記成形品に形成された複数の前記穴が位置する箇所に凹部が形成されているものである請求項1または2に記載の加飾品の製造方法。   The concave portion is formed at a position where the plurality of holes formed in the decorative sheet or the molded product on the molding surface on which the decorative sheet or the molded product is arranged. The manufacturing method of the decorative article of 2. 前記加飾シートは基材シートを含み、前記基材シートが前記加飾品の最表面にあるものである請求項1〜3のいずれか一項に記載の加飾品の製造方法。   The said decorating sheet contains a base material sheet, The said base material sheet exists in the outermost surface of the said decorating goods, The manufacturing method of the decorating goods as described in any one of Claims 1-3. 前記キャビティ内に射出される溶融樹脂は、熱可塑性エラストマーである請求項1〜4のいずれか一項に記載の加飾品の製造方法。   The method for producing a decorative article according to any one of claims 1 to 4, wherein the molten resin injected into the cavity is a thermoplastic elastomer. 前記キャビティ内に射出される溶融樹脂は、熱可塑性透光性樹脂である請求項1〜5のいずれか一項に記載の加飾品の製造方法。   The method for producing a decorative article according to any one of claims 1 to 5, wherein the molten resin injected into the cavity is a thermoplastic translucent resin. 前記加飾シートまたは前記成形樹脂の少なくとも一方が着色されているものである請求項6に記載の加飾品の製造方法。   The method for producing a decorative product according to claim 6, wherein at least one of the decorative sheet or the molded resin is colored. 前記加飾シートは図柄層を含み、前記図柄層には、前記加飾シートに形成された複数の前記穴によって区分された2以上の領域において、互いに異なる図柄が形成されているものである請求項1〜7のいずれか一項に記載の加飾品の製造方法。   The decorative sheet includes a design layer, and in the design layer, different designs are formed in two or more regions divided by the plurality of holes formed in the decorative sheet. The manufacturing method of the decoration article as described in any one of claim | item 1 -7. 前記加飾シートまたは前記成形品を配置した前記金型の前記成形面には、前記加飾シートまたは前記成形品に形成された複数の前記穴が位置する箇所を境に、互いに異なる凹凸形状が形成されているものである請求項8に記載の加飾品の製造方法。   The molding surface of the mold on which the decorative sheet or the molded product is arranged has different concave and convex shapes on the boundary where the plurality of holes formed in the decorative sheet or the molded product are located. The method for producing a decorative article according to claim 8, which is formed.
JP2016062409A 2016-03-25 2016-03-25 Production method of decorative article Pending JP2017170854A (en)