JP2016132183A - Composite preform, manufacturing method of composite container, composite container, plastic member and inner label member - Google Patents

Composite preform, manufacturing method of composite container, composite container, plastic member and inner label member Download PDF

Info

Publication number
JP2016132183A
JP2016132183A JP2015008706A JP2015008706A JP2016132183A JP 2016132183 A JP2016132183 A JP 2016132183A JP 2015008706 A JP2015008706 A JP 2015008706A JP 2015008706 A JP2015008706 A JP 2015008706A JP 2016132183 A JP2016132183 A JP 2016132183A
Authority
JP
Japan
Prior art keywords
preform
plastic member
composite
plastic
bottom portion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2015008706A
Other languages
Japanese (ja)
Other versions
JP6516142B2 (en
Inventor
賀 勇 介 須
Yusuke Suga
賀 勇 介 須
脇 琢 磨 宮
Takuma Miyawaki
脇 琢 磨 宮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dai Nippon Printing Co Ltd
Original Assignee
Dai Nippon Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dai Nippon Printing Co Ltd filed Critical Dai Nippon Printing Co Ltd
Priority to JP2015008706A priority Critical patent/JP6516142B2/en
Publication of JP2016132183A publication Critical patent/JP2016132183A/en
Application granted granted Critical
Publication of JP6516142B2 publication Critical patent/JP6516142B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

PROBLEM TO BE SOLVED: To provide a composite preform capable of manufacturing a composite container with high quality, to which various functions and characteristics such as gas barrier properties are imparted, and also to provide a manufacturing method of a composite container, a composite container, a plastic member and an inner label member.SOLUTION: A composite preform 70 includes: a preform 10a made of a plastic material having a mouth part 11a, a trunk part 20a and a bottom part 30a, with a gate mark projection 34a formed on the bottom part 30a; and a plastic member 40a formed so as to surround the outer side of the preform 10a. The plastic member 40a includes: a cylindrical trunk part 41; and a bottom part 42 with an accommodation recess 49 for accommodating the gate mark projection 34a of the preform 10a. The plastic member 40a is closely adhered on the outer side of the preform 10a.SELECTED DRAWING: Figure 3

Description

本発明は、複合プリフォーム、複合容器の製造方法、複合容器、プラスチック製部材、および内側ラベル部材に関する。   The present invention relates to a composite preform, a method for manufacturing a composite container, a composite container, a plastic member, and an inner label member.

近時、飲食品等の内容液を収容するボトルとして、プラスチック製のものが一般化してきており、このようなプラスチックボトルには内容液が収容される。   Recently, plastic bottles for storing content liquids such as foods and drinks have become common, and such plastic bottles store content liquids.

このような内容液を収容するプラスチックボトルは、金型内にプリフォームを挿入し、2軸延伸ブロー成形することにより製造される。   A plastic bottle containing such a content liquid is manufactured by inserting a preform into a mold and biaxially stretch-blow molding.

ところで、従来の2軸延伸ブロー成形法では、例えばPETやPP等の単層材料、多層材料又はブレンド材料等を含むプリフォームを用いて容器形状に成形している。しかしながら、従来の2軸延伸ブロー成形法においては、単にプリフォームを容器形状に成形するだけであるのが一般的である。このため、容器に対して様々な機能や特性(バリア性や保温性等)を持たせる場合、例えばプリフォームを構成する材料を変更する等、その手段は限定されてしまう。   By the way, in the conventional biaxial stretch blow molding method, for example, a preform including a single layer material such as PET or PP, a multilayer material, a blend material, or the like is used to form a container shape. However, in the conventional biaxial stretch blow molding method, the preform is generally simply formed into a container shape. For this reason, when various functions and characteristics (barrier property, heat retaining property, etc.) are given to the container, the means is limited, for example, by changing the material constituting the preform.

特開2009−241526号公報JP 2009-241526 A

本発明はこのような点を考慮してなされたものであり、ガスバリア性等の様々な機能や特性が付与された複合容器を高い品質で製造することが可能な、複合プリフォーム、複合容器の製造方法、複合容器、プラスチック製部材、および内側ラベル部材を提供することを目的とする。   The present invention has been made in consideration of such points, and it is possible to produce a composite container having various functions and characteristics such as gas barrier properties with high quality. An object is to provide a manufacturing method, a composite container, a plastic member, and an inner label member.

本発明は、複合プリフォームにおいて、口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームと、前記プリフォームの外側を取り囲むように設けられ、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有するプラスチック製部材とを備え、前記プラスチック製部材は、前記プリフォームの外側に密着されていることを特徴とする複合プリフォームである。   The present invention provides a composite preform having a mouth portion, a body portion, and a bottom portion, and a plastic material preform having a gate mark protrusion formed on the bottom portion and surrounding the outside of the preform. A plastic member having a cylindrical body portion and a bottom portion in which a receiving recess for receiving the gate trace protrusion of the preform is formed, and the plastic member is in close contact with the outside of the preform It is a composite preform characterized by the above.

本発明は、前記収容凹部は、非貫通孔からなることを特徴とする複合プリフォームである。   The present invention is the composite preform characterized in that the accommodation recess is formed of a non-through hole.

本発明は、前記収容凹部は、前記プラスチック製部材の前記底部を貫通する貫通孔からなることを特徴とする複合プリフォームである。   The present invention is the composite preform, wherein the housing recess is formed of a through hole that penetrates the bottom of the plastic member.

本発明は、複合プリフォームにおいて、口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームと、前記プリフォームの外側を取り囲むように密着して設けられ、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有する内側ラベル部材と、前記内側ラベル部材の外側を取り囲むように設けられたプラスチック製部材とを備え、前記プラスチック製部材は、前記プリフォームおよび前記内側ラベル部材の外側に密着されていることを特徴とする複合プリフォームである。   The present invention provides a composite preform having a mouth portion, a body portion, and a bottom portion, and a plastic material preform having a gate mark protrusion formed on the bottom portion, and is closely attached so as to surround the outside of the preform. An inner label member having a cylindrical body portion and a bottom portion in which an accommodating recess for accommodating the gate mark protrusion of the preform is formed, and provided so as to surround the outer side of the inner label member. And a plastic member, wherein the plastic member is in close contact with the outside of the preform and the inner label member.

本発明は、複合容器の製造方法において、口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームを準備する工程と、前記プリフォームの外側に、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有するプラスチック製部材を設ける工程と、前記プリフォームおよび前記プラスチック製部材に対してブロー成形を施すことにより、前記プリフォームおよび前記プラスチック製部材を一体として膨張させる工程とを備えたことを特徴とする複合容器の製造方法である。   The present invention relates to a method of manufacturing a composite container, the step of preparing a preform made of a plastic material having a mouth portion, a trunk portion, and a bottom portion, and having a gate trace protrusion formed on the bottom portion, and an outer side of the preform Providing a plastic member having a cylindrical body portion and a bottom portion in which an accommodating recess for accommodating the gate mark protrusion of the preform is formed, and blowing the preform and the plastic member. And a step of expanding the preform and the plastic member as a single body by performing molding.

本発明は、前記収容凹部は、非貫通孔からなることを特徴とする複合容器の製造方法である。   The present invention is the method of manufacturing a composite container, wherein the housing recess is a non-through hole.

本発明は、前記収容凹部は、前記プラスチック製部材の前記底部を貫通する貫通孔からなることを特徴とする複合容器の製造方法である。   The present invention is the method for manufacturing a composite container, wherein the housing recess is a through-hole penetrating the bottom of the plastic member.

本発明は、複合容器の製造方法において、口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームを準備する工程と、前記プリフォームの外側に、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有する内側ラベル部材を設ける工程と、前記内側ラベル部材の外側に、プラスチック製部材を設ける工程と、前記プリフォーム、前記内側ラベル部材および前記プラスチック製部材に対してブロー成形を施すことにより、前記プリフォーム、前記内側ラベル部材および前記プラスチック製部材を一体として膨張させる工程とを備えたことを特徴とする複合容器の製造方法である。   The present invention relates to a method of manufacturing a composite container, the step of preparing a preform made of a plastic material having a mouth portion, a trunk portion, and a bottom portion, and having a gate trace protrusion formed on the bottom portion, and an outer side of the preform A step of providing an inner label member having a cylindrical body portion and a bottom portion in which an accommodating recess for accommodating the gate mark protrusion of the preform is formed, and a plastic member on the outer side of the inner label member. And a step of inflating the preform, the inner label member, and the plastic member together by performing blow molding on the preform, the inner label member, and the plastic member. This is a method for manufacturing a composite container.

本発明は、前記複合容器の製造方法によって作製されたことを特徴とする複合容器である。   The present invention is a composite container produced by the method for manufacturing a composite container.

本発明は、口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームの外側を取り囲むように装着されるプラスチック製部材であって、前記プリフォームの胴部を覆う筒状の胴部と、前記プリフォームの底部を覆うとともに、前記プリフォームの前記ゲート跡突起を収容可能な収容凹部が形成された底部とを有することを特徴とするプラスチック製部材である。   The present invention is a plastic member that has a mouth portion, a body portion, and a bottom portion, and that is mounted so as to surround the outside of a preform made of plastic material in which a gate mark protrusion is formed on the bottom portion. A plastic having a cylindrical body portion that covers the body portion of the reform, and a bottom portion that covers the bottom portion of the preform and that is formed with an accommodation recess capable of accommodating the gate trace protrusion of the preform. It is a member made.

本発明は、口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームの外側を取り囲むように装着されるとともに、プラスチック製部材の内側に装着される内側ラベル部材であって、前記プリフォームの胴部を覆う筒状の胴部と、前記プリフォームの底部を覆うとともに、前記プリフォームの前記ゲート跡突起を収容可能な収容凹部が形成された底部とを有することを特徴とする内側ラベル部材である。   The present invention has a mouth portion, a body portion, and a bottom portion, and is mounted so as to surround an outer side of a plastic material preform having a gate mark protrusion formed on the bottom portion, and is mounted on the inner side of the plastic member. The inner label member is formed with a cylindrical body portion that covers the body portion of the preform, and an accommodation recess that covers the bottom portion of the preform and that can accommodate the gate mark protrusion of the preform. And an inner label member.

本発明によれば、プラスチック製部材の底部に、プリフォームのゲート跡突起を収容する収容凹部が形成されているので、プラスチック製部材をプリフォームに対して密着して取り付けることができる。これにより、プラスチック製部材とプリフォームとの間に空気が残存することが防止され、ガスバリア性等の様々な機能や特性が付与された複合容器を高い品質で製造することができる。   According to the present invention, since the housing recess for housing the gate trace of the preform is formed at the bottom of the plastic member, the plastic member can be attached in close contact with the preform. Thereby, it is possible to prevent air from remaining between the plastic member and the preform, and to manufacture a composite container having various functions and characteristics such as gas barrier properties with high quality.

図1は、本発明の第1の実施の形態による複合容器を示す部分垂直断面図。FIG. 1 is a partial vertical sectional view showing a composite container according to a first embodiment of the present invention. 図2は、本発明の第1の実施の形態による複合容器を示す水平断面図(図1のII−II線断面図)。FIG. 2 is a horizontal sectional view showing the composite container according to the first embodiment of the present invention (sectional view taken along the line II-II in FIG. 1). 図3は、本発明の第1の実施の形態による複合プリフォームを示す部分垂直断面図。FIG. 3 is a partial vertical sectional view showing the composite preform according to the first embodiment of the present invention. 図4(a)〜(b)は、本発明の第1の実施の形態による複合プリフォームの変形例を示す部分拡大断面図。4A and 4B are partially enlarged cross-sectional views showing modifications of the composite preform according to the first embodiment of the present invention. 図5(a)〜(f)は、本発明の第1の実施の形態による複合容器の製造方法を示す概略図。FIGS. 5A to 5F are schematic views showing a method of manufacturing the composite container according to the first embodiment of the present invention. 図6は、本発明の第2の実施の形態による複合容器を示す部分垂直断面図。FIG. 6 is a partial vertical sectional view showing a composite container according to a second embodiment of the present invention. 図7は、本発明の第2の実施の形態による複合容器を示す水平断面図(図6のVII−VII線断面図)。FIG. 7 is a horizontal sectional view (sectional view taken along line VII-VII in FIG. 6) showing the composite container according to the second embodiment of the present invention. 図8は、本発明の第2の実施の形態による複合プリフォームを示す部分垂直断面図。FIG. 8 is a partial vertical sectional view showing a composite preform according to the second embodiment of the present invention. 図9(a)〜(b)は、本発明の第2の実施の形態による複合プリフォームの変形例を示す部分拡大断面図。FIGS. 9A and 9B are partially enlarged cross-sectional views showing modifications of the composite preform according to the second embodiment of the present invention. 図10(a)〜(f)は、本発明の第2の実施の形態による複合容器の製造方法を示す概略図。10 (a) to 10 (f) are schematic views showing a method for manufacturing a composite container according to the second embodiment of the present invention.

第1の実施の形態
以下、図面を参照して本発明の第1の実施の形態について説明する。図1乃至図5は本発明の第1の実施の形態を示す図である。
First Embodiment Hereinafter, a first embodiment of the present invention will be described with reference to the drawings. 1 to 5 are views showing a first embodiment of the present invention.

まず、図1および図2により、本実施の形態による複合容器の製造方法(ブロー成形方法)によって作製される複合容器の概要について説明する。なお、本明細書中、「上」および「下」とは、それぞれ複合容器10Aを正立させた状態(図1)における上方および下方のことをいう。   First, an outline of a composite container produced by the composite container manufacturing method (blow molding method) according to the present embodiment will be described with reference to FIGS. 1 and 2. In the present specification, “upper” and “lower” refer to the upper side and the lower side in a state where the composite container 10A is erected (FIG. 1), respectively.

図1および図2に示す複合容器10Aは、後述するように、ブロー成形金型50を用いてプリフォーム10aおよびプラスチック製部材40aを含む複合プリフォーム70(図3参照)に対して2軸延伸ブロー成形を施すことにより、複合プリフォーム70のプリフォーム10aおよびプラスチック製部材40aを一体として膨張させて得られたものである。   A composite container 10A shown in FIGS. 1 and 2 is biaxially stretched with respect to a composite preform 70 (see FIG. 3) including a preform 10a and a plastic member 40a using a blow molding die 50, as will be described later. By performing blow molding, the preform 10a of the composite preform 70 and the plastic member 40a are integrally expanded.

このような複合容器10Aは、内側に位置するプラスチック材料製の容器本体10と、容器本体10の外側に密着して設けられたプラスチック製部材40とを備えている。   Such a composite container 10 </ b> A includes a container body 10 made of a plastic material located inside and a plastic member 40 provided in close contact with the outside of the container body 10.

このうち容器本体10は、口部11と、口部11下方に設けられた首部13と、首部13下方に設けられた肩部12と、肩部12下方に設けられた胴部20と、胴部20下方に設けられた底部30とを備えている。   Among these, the container body 10 includes a mouth portion 11, a neck portion 13 provided below the mouth portion 11, a shoulder portion 12 provided below the neck portion 13, a trunk portion 20 provided below the shoulder portion 12, And a bottom portion 30 provided below the portion 20.

他方、プラスチック製部材40は、容器本体10の外面に薄く延ばされた状態で密着されており、容器本体10に対して容易に移動又は回転しない状態で取付けられている。   On the other hand, the plastic member 40 is in close contact with the outer surface of the container main body 10 in a thinly extended state, and is attached to the container main body 10 without being easily moved or rotated.

次に容器本体10について詳述する。容器本体10は、上述したように口部11と、首部13と、肩部12と、胴部20と、底部30とを有している。   Next, the container body 10 will be described in detail. As described above, the container body 10 includes the mouth portion 11, the neck portion 13, the shoulder portion 12, the trunk portion 20, and the bottom portion 30.

このうち口部11は、図示しないキャップに螺着されるねじ部14と、ねじ部14下方に設けられたフランジ部17とを有している。なお、口部11の形状は、従来公知の形状であっても良い。   Of these, the mouth portion 11 includes a screw portion 14 screwed into a cap (not shown) and a flange portion 17 provided below the screw portion 14. The shape of the mouth portion 11 may be a conventionally known shape.

首部13は、フランジ部17と肩部12との間に位置しており、略均一な径をもつ略円筒形状を有している。また、肩部12は、首部13と胴部20との間に位置しており、首部13側から胴部20側に向けて徐々に径が拡大する形状を有している。   The neck portion 13 is located between the flange portion 17 and the shoulder portion 12 and has a substantially cylindrical shape having a substantially uniform diameter. The shoulder 12 is located between the neck 13 and the trunk 20 and has a shape whose diameter gradually increases from the neck 13 toward the trunk 20.

さらに、胴部20は、全体として略均一な径をもつ円筒形状を有している。しかしながら、これに限られるものではなく、胴部20が四角形筒形状や八角形筒形状等の多角形筒形状を有していても良い。あるいは、胴部20が上方から下方に向けて均一でない水平断面をもつ筒形状を有していても良い。また、本実施の形態において、胴部20は、凹凸が形成されておらず、略平坦な表面を有しているが、これに限られるものではない。例えば、胴部20にパネル又は溝等の凹凸が形成されていても良い。   Furthermore, the trunk | drum 20 has a cylindrical shape with a substantially uniform diameter as a whole. However, the present invention is not limited to this, and the body portion 20 may have a polygonal cylindrical shape such as a rectangular cylindrical shape or an octagonal cylindrical shape. Or the trunk | drum 20 may have a cylinder shape with a horizontal cross section which is not uniform toward upper direction from the downward direction. Moreover, in this Embodiment, although the unevenness | corrugation is not formed in the trunk | drum 20, and has a substantially flat surface, it is not restricted to this. For example, unevenness such as a panel or a groove may be formed on the body portion 20.

一方、底部30は、中央に位置する凹部31と、この凹部31周囲に設けられた接地部32とを有している。なお、底部30の形状についても特に限定されるものではなく、従来公知の底部形状(例えばペタロイド底形状や丸底形状等)を有していても良い。   On the other hand, the bottom portion 30 has a concave portion 31 located in the center and a grounding portion 32 provided around the concave portion 31. The shape of the bottom 30 is not particularly limited, and may have a conventionally known bottom shape (for example, a petaloid bottom shape or a round bottom shape).

また胴部20における容器本体10の厚みは、これに限定されるものではないが、例えば50μm〜250μm(50μm以上かつ250μm以下をいう。以下同様)程度に薄くすることができる。さらに、容器本体10の重量についても、これに限定されるものではないが、10g〜20gとすることができる。このように容器本体10の肉厚を薄くすることにより、容器本体10の軽量化を図ることができる。   Moreover, although the thickness of the container main body 10 in the trunk | drum 20 is not limited to this, For example, it can be made thin about 50 micrometers-250 micrometers (50 micrometers or more and 250 micrometers or less. The same applies hereafter). Further, the weight of the container body 10 is not limited to this, but can be 10 g to 20 g. Thus, by reducing the thickness of the container main body 10, the weight of the container main body 10 can be reduced.

このような容器本体10は、合成樹脂材料を射出成形して製作したプリフォーム10a(後述)を二軸延伸ブロー成形することにより作製することができる。なおプリフォーム10a、すなわち容器本体10の材料としては熱可塑性樹脂、特にPE(ポリエチレン)、PP(ポリプロピレン)、PET(ポリエチレンテレフタレート)、PEN(ポリエチレンナフタレート)、PC(ポリカーボネート)を使用することが好ましい。容器本体10は、赤色、青色、黄色、緑色、茶色、黒色、白色等の色に着色されていても良いが、リサイクルのしやすさを考慮した場合、無色透明であることが好ましい。また、上述した各種樹脂をブレンドして用いても良い。さらに、容器本体10の内面に、容器のバリア性を高めるために、例えばダイヤモンド状炭素膜や酸化珪素薄膜等の蒸着膜を形成しても良い。   Such a container main body 10 can be manufactured by biaxially stretching blow-molding a preform 10a (described later) manufactured by injection molding a synthetic resin material. As the material of the preform 10a, that is, the container body 10, a thermoplastic resin, particularly PE (polyethylene), PP (polypropylene), PET (polyethylene terephthalate), PEN (polyethylene naphthalate), or PC (polycarbonate) may be used. preferable. The container body 10 may be colored in colors such as red, blue, yellow, green, brown, black, and white, but is preferably colorless and transparent in consideration of ease of recycling. Moreover, you may blend and use the various resin mentioned above. Further, a vapor deposition film such as a diamond-like carbon film or a silicon oxide thin film may be formed on the inner surface of the container body 10 in order to enhance the barrier property of the container.

また、容器本体10は、2層以上の多層成形ボトルとして形成することもできる。すなわち押し出し成形または射出成形により、例えば、中間層をMXD6、MXD6+脂肪酸塩、PGA(ポリグリコール酸)、EVOH(エチレンビニルアルコール共重合体)又はPEN(ポリエチレンナフタレート)等のガスバリア性及び遮光性を有する樹脂(中間層)として3層以上からなるプリフォーム10aを成形した後、ブロー成形することによりガスバリア性及び遮光性を有する多層ボトルとして形成しても良い。なお、中間層としては、上述した各種樹脂をブレンドした樹脂を用いても良い。   The container body 10 can also be formed as a multilayer molded bottle having two or more layers. That is, by extrusion molding or injection molding, for example, the intermediate layer has gas barrier properties and light shielding properties such as MXD6, MXD6 + fatty acid salt, PGA (polyglycolic acid), EVOH (ethylene vinyl alcohol copolymer) or PEN (polyethylene naphthalate). You may form as a multilayer bottle which has gas barrier property and light-shielding property by shape | molding the preform 10a which consists of 3 or more layers as resin which has (intermediate layer), and carrying out blow molding. As the intermediate layer, a resin obtained by blending the above-described various resins may be used.

また、熱可塑性樹脂の溶融物に不活性ガス(窒素ガス、アルゴンガス)を混ぜることで、0.5〜100μmの発泡セル径を持つ発泡プリフォームを成形し、この発泡プリフォームをブロー成形することによって、容器本体10を作製しても良い。このような容器本体10は、発泡セルを内蔵しているため、容器本体10全体の遮光性を高めることができる。   Further, by mixing an inert gas (nitrogen gas, argon gas) with the thermoplastic resin melt, a foam preform having a foam cell diameter of 0.5 to 100 μm is formed, and this foam preform is blow-molded. Thus, the container body 10 may be manufactured. Since such a container main body 10 contains the foam cell, the light shielding property of the container main body 10 whole can be improved.

このような容器本体10は、例えば満注容量が100ml〜2000mlのボトルからなっていても良い。あるいは、容器本体10は、満注容量が例えば10L〜60Lの大型のボトルであっても良い。   Such a container main body 10 may consist of a bottle with a full capacity of 100 ml to 2000 ml, for example. Alternatively, the container main body 10 may be a large bottle having a full capacity of, for example, 10L to 60L.

次にプラスチック製部材40について説明する。プラスチック製部材40(40a)は後述するようにプリフォーム10aの外側を取り囲むように設けられ、プリフォーム10aの外側に密着された後、プリフォーム10aとともに2軸延伸ブロー成形されることにより得られたものである。このプラスチック製部材40は、後述するように、プラスチック製部材40aをプリフォーム10aとともに一体として延伸することにより作製されたものである。   Next, the plastic member 40 will be described. As will be described later, the plastic member 40 (40a) is provided so as to surround the outer side of the preform 10a. It is a thing. As will be described later, the plastic member 40 is produced by stretching a plastic member 40a together with the preform 10a.

プラスチック製部材40は容器本体10の外面に接着されることなく取付けられており、容器本体10に対して移動又は回転しないほどに密着されている。このプラスチック製部材40は、容器本体10の外面において薄く引き延ばされて容器本体10を覆っている。また、図2に示すように、プラスチック製部材40は、容器本体10を取り囲むようにその周方向全域にわたって設けられており、略円形状の水平断面を有している。   The plastic member 40 is attached to the outer surface of the container body 10 without being bonded, and is in close contact with the container body 10 so as not to move or rotate. The plastic member 40 is thinly extended on the outer surface of the container body 10 to cover the container body 10. As shown in FIG. 2, the plastic member 40 is provided over the entire circumferential direction so as to surround the container body 10, and has a substantially circular horizontal cross section.

この場合、プラスチック製部材40は、容器本体10のうち、口部11および首部13を除く、肩部12、胴部20および底部30を覆うように設けられている。これにより、容器本体10の肩部12、胴部20および底部30に対して所望の機能や特性を付与することができる。   In this case, the plastic member 40 is provided so as to cover the shoulder portion 12, the trunk portion 20, and the bottom portion 30 of the container body 10 except for the mouth portion 11 and the neck portion 13. Thereby, desired functions and characteristics can be imparted to the shoulder portion 12, the trunk portion 20, and the bottom portion 30 of the container body 10.

なお、プラスチック製部材40は、容器本体10のうち口部11以外の全域又は一部領域に設けられていても良い。例えば、プラスチック製部材40は、容器本体10のうち、口部11を除く、首部13、肩部12、胴部20および底部30の全体を覆うように設けられていても良い。さらに、プラスチック製部材40は1つに限らず、複数設けても良い。例えば、2つのプラスチック製部材40を肩部12の外面および底部30の外面にそれぞれ設けても良い。   The plastic member 40 may be provided in the entire region or a partial region other than the mouth portion 11 of the container body 10. For example, the plastic member 40 may be provided so as to cover the neck portion 13, the shoulder portion 12, the trunk portion 20, and the bottom portion 30 of the container body 10 except for the mouth portion 11. Further, the number of plastic members 40 is not limited to one, and a plurality of plastic members 40 may be provided. For example, you may provide the two plastic members 40 in the outer surface of the shoulder part 12, and the outer surface of the bottom part 30, respectively.

一方、プラスチック製部材40は、容器本体10に対して溶着ないし接着されていないため、容器本体10から剥離して除去することができる。具体的には、例えば刃物等を用いてプラスチック製部材40を切除したり、プラスチック製部材40に予め図示しない切断線を設け、この切断線に沿ってプラスチック製部材40を剥離したりすることができる。これにより、プラスチック製部材40を容器本体10から分離除去することができる。   On the other hand, since the plastic member 40 is not welded or bonded to the container body 10, it can be peeled off from the container body 10 and removed. Specifically, for example, the plastic member 40 may be cut using a blade or the like, or a cutting line (not shown) may be provided in advance on the plastic member 40, and the plastic member 40 may be peeled along the cutting line. it can. Thereby, the plastic member 40 can be separated and removed from the container body 10.

またプラスチック製部材40の厚みは、これに限定されるものではないが、容器本体10に取り付けられた状態で例えば5μm〜500μm程度とすることができる。   The thickness of the plastic member 40 is not limited to this, but can be set to, for example, about 5 μm to 500 μm in a state of being attached to the container body 10.

本実施の形態において、プラスチック製部材40は、赤色、青色、黄色、緑色、茶色、黒色、白色等の可視光色に着色されていても良い。また、プラスチック製部材40は、(半)透明であっても良く、不透明であっても良い。この場合、例えばプラスチック製部材40を可視光色に着色するとともに、容器本体10を無色透明にしても良い。あるいは、容器本体10およびプラスチック製部材40の両方を可視光色に着色しても良い。なお、可視光色に着色されたプラスチック製部材40を作製する場合、ブロー成形前のプラスチック製部材40aを射出成形等により作製する工程で、成形材料に可視光色の顔料を添加しても良い。   In the present embodiment, the plastic member 40 may be colored in a visible light color such as red, blue, yellow, green, brown, black, and white. The plastic member 40 may be (semi) transparent or opaque. In this case, for example, the plastic member 40 may be colored with visible light and the container body 10 may be colorless and transparent. Alternatively, both the container body 10 and the plastic member 40 may be colored in a visible light color. When producing the plastic member 40 colored in visible light color, a visible light color pigment may be added to the molding material in the step of producing the plastic member 40a before blow molding by injection molding or the like. .

次に図3により、本実施の形態による複合プリフォームの構成について説明する。   Next, the structure of the composite preform according to this embodiment will be described with reference to FIG.

図3に示すように、複合プリフォーム70は、プラスチック材料製のプリフォーム10aと、プリフォーム10aの外側に設けられた有底円筒状のプラスチック製部材40aとを備えている。   As shown in FIG. 3, the composite preform 70 includes a preform 10a made of a plastic material, and a bottomed cylindrical plastic member 40a provided outside the preform 10a.

プリフォーム10aは、口部11aと、口部11aに連結された胴部20aと、胴部20aに連結された底部30aとを備えている。このうち口部11aは、上述した容器本体10の口部11に対応するものであり、口部11と略同一の形状を有している。また、胴部20aは、上述した容器本体10の首部13、肩部12および胴部20に対応するものであり、略円筒形状を有している。底部30aは、上述した容器本体10の底部30に対応するものであり、略半球形状を有している。   The preform 10a includes a mouth portion 11a, a body portion 20a connected to the mouth portion 11a, and a bottom portion 30a connected to the body portion 20a. Of these, the mouth portion 11 a corresponds to the mouth portion 11 of the container body 10 described above, and has substantially the same shape as the mouth portion 11. Moreover, the trunk | drum 20a respond | corresponds to the neck part 13, the shoulder part 12, and the trunk | drum 20 of the container main body 10 mentioned above, and has a substantially cylindrical shape. The bottom 30a corresponds to the bottom 30 of the container body 10 described above, and has a substantially hemispherical shape.

底部30aの中央部(下端部)には、略円柱状のゲート跡突起34aが形成されている。このゲート跡突起34aは、例えば射出成形法によりプリフォーム10aを作製した際、底部30aに残存する不要部分であり、射出成形金型のゲート部内の樹脂に対応している。ゲート跡突起34aの突出高さは、例えば0.1mm〜5mm程度であり、ゲート跡突起34aの幅(直径)は例えば3mm〜12mm程度である。   A substantially cylindrical gate mark protrusion 34a is formed at the center (lower end) of the bottom 30a. This gate mark protrusion 34a is an unnecessary portion remaining on the bottom 30a when the preform 10a is produced by, for example, injection molding, and corresponds to the resin in the gate portion of the injection mold. The protruding height of the gate trace protrusion 34a is, for example, about 0.1 mm to 5 mm, and the width (diameter) of the gate trace protrusion 34a is, for example, about 3 mm to 12 mm.

プラスチック製部材40aは、プリフォーム10aの外面に接着されることなく取付けられており、プリフォーム10aに対して移動又は回転しないほどに密着されているか、又は自重で落下しない程度に密着されている。プラスチック製部材40aは、プリフォーム10aを取り囲むようにその周方向全域にわたって設けられており、円形状の水平断面を有している。   The plastic member 40a is attached to the outer surface of the preform 10a without being bonded, and is in close contact with the preform 10a so as not to move or rotate, or in close contact with the preform 10a so as not to fall by its own weight. . The plastic member 40a is provided over the entire circumferential direction so as to surround the preform 10a, and has a circular horizontal cross section.

この場合、プラスチック製部材40aは、胴部20aのうち容器本体10の首部13に対応する部分13aを除く全域と、底部30aの全域とを覆うように設けられている。また、プラスチック製部材40aは、赤色、青色、黄色、緑色、茶色、黒色、白色等の可視光色に着色されていても良い。   In this case, the plastic member 40a is provided so as to cover the entire region of the body portion 20a excluding the portion 13a corresponding to the neck portion 13 of the container body 10 and the entire region of the bottom portion 30a. Moreover, the plastic member 40a may be colored in visible light colors such as red, blue, yellow, green, brown, black, and white.

なお、プラスチック製部材40aは、口部11a以外の全域又は一部領域に設けられていても良い。例えば、プラスチック製部材40aは、口部11aを除く、首部13a、胴部20aおよび底部30aの全体を覆うように設けられていても良い。さらに、プラスチック製部材40aは1つに限らず、複数設けても良い。例えば、2つのプラスチック製部材40aを胴部20aの外側2箇所にそれぞれ設けても良い。   The plastic member 40a may be provided in the entire region or a partial region other than the mouth portion 11a. For example, the plastic member 40a may be provided so as to cover the neck portion 13a, the trunk portion 20a, and the bottom portion 30a except for the mouth portion 11a. Furthermore, the number of plastic members 40a is not limited to one, and a plurality of plastic members 40a may be provided. For example, two plastic members 40a may be provided at two locations outside the trunk portion 20a.

図3に示すように、プラスチック製部材40aは、全体として有底円筒形状からなり、円筒状の胴部41と、胴部41に連結された半球状の底部42とを有している。この場合、プラスチック製部材40aの底部42がプリフォーム10aの底部30a全域を覆うので、複合容器10Aの胴部20に加え、底部30に対しても、ガスバリア性等の様々な機能や特性を付与することができる。   As shown in FIG. 3, the plastic member 40 a has a bottomed cylindrical shape as a whole, and includes a cylindrical barrel portion 41 and a hemispherical bottom portion 42 connected to the barrel portion 41. In this case, since the bottom portion 42 of the plastic member 40a covers the entire bottom portion 30a of the preform 10a, various functions and characteristics such as gas barrier properties are imparted to the bottom portion 30 in addition to the trunk portion 20 of the composite container 10A. can do.

プラスチック製部材40aの底部42には、プリフォーム10aのゲート跡突起34aを収容する収容凹部49が設けられている。この収容凹部49は、プラスチック製部材40aをプリフォーム10aに装着した際、ゲート跡突起34aに対応する位置に設けられている。本実施の形態において、収容凹部49は、底部42の中央1箇所に設けられているが、その位置や個数はこれに限定されるものではない。   An accommodation recess 49 for accommodating the gate mark protrusion 34a of the preform 10a is provided at the bottom 42 of the plastic member 40a. The housing recess 49 is provided at a position corresponding to the gate mark protrusion 34a when the plastic member 40a is mounted on the preform 10a. In the present embodiment, the accommodation recess 49 is provided at one central portion of the bottom 42, but the position and number thereof are not limited to this.

また、収容凹部49の形状は、底面方向(図3の下方)から見て円形状となっているが、これに限らず、長方形状、楕円形状、角丸長方形状、菱形形状、三角形状、五角形状、矢羽根形状、六角形状等としても良い。また、収容凹部49の深さおよび幅(径)を、それぞれゲート跡突起34aの突出高さおよび幅(径)よりも大きくすることにより、ゲート跡突起34a全体を収容凹部49に収容可能とすることが好ましい。具体的には、収容凹部49の深さは、例えば0.5mm〜5mmであり、収容凹部49の幅(径)は、例えば3mm〜12mmである。本明細書において、収容凹部49の幅とは、底面方向から収容凹部49を見たとき、収容凹部49のうち最も長くなる部分の長さをいう(後述する内側ラベル部材60aの収容凹部66についても同様)。   In addition, the shape of the housing recess 49 is circular when viewed from the bottom surface direction (lower side in FIG. 3), but is not limited to this, rectangular shape, elliptical shape, rounded rectangular shape, rhombus shape, triangular shape, It is good also as a pentagon shape, an arrow feather shape, a hexagon shape, etc. Further, by making the depth and width (diameter) of the accommodating recess 49 larger than the protruding height and width (diameter) of the gate trace protrusion 34a, the entire gate trace protrusion 34a can be accommodated in the accommodation recess 49. It is preferable. Specifically, the depth of the housing recess 49 is, for example, 0.5 mm to 5 mm, and the width (diameter) of the housing recess 49 is, for example, 3 mm to 12 mm. In this specification, the width of the housing recess 49 refers to the length of the longest portion of the housing recess 49 when the housing recess 49 is viewed from the bottom surface direction (for the housing recess 66 of the inner label member 60a described later). The same).

図3において、収容凹部49は非貫通孔からなっている。すなわち、収容凹部49は、プラスチック製部材40aの内面側に開口する一方、プラスチック製部材40aの外面側には開口されていない。この場合、ブロー成形後に、容器本体10の底部30がプラスチック製部材40によって完全に覆われるので、底部30の機能や特性(バリア性や保温性等)が損なわれるおそれがない。なお、プラスチック製部材40aの外面のうち収容凹部49に対応する領域が、外方に向けて突出することにより、外面突起49cが形成されている。外面突起49cは、例えばダイレクトブロー成形によってプラスチック製部材40aを作製する際、金型によって賦形されたものであり、外面突起49cが形成されることに伴って、底部42が厚み方向に変形され、外面突起49cと同時に収容凹部49も形成される。   In FIG. 3, the housing recess 49 is a non-through hole. That is, the housing recess 49 opens on the inner surface side of the plastic member 40a, but does not open on the outer surface side of the plastic member 40a. In this case, since the bottom 30 of the container body 10 is completely covered with the plastic member 40 after blow molding, the function and characteristics (barrier property, heat retaining property, etc.) of the bottom 30 are not likely to be impaired. In addition, the outer surface protrusion 49c is formed when the area | region corresponding to the accommodation recessed part 49 protrudes outward among the outer surfaces of the plastic members 40a. The outer protrusion 49c is formed by a mold when the plastic member 40a is produced by, for example, direct blow molding, and the bottom 42 is deformed in the thickness direction as the outer protrusion 49c is formed. A housing recess 49 is also formed at the same time as the outer projection 49c.

このように、プラスチック製部材40aの底部42に収容凹部49を設けたことにより、有底のプラスチック製部材40aをプリフォーム10aに嵌め込む際(図5(b)参照)、プリフォーム10aのゲート跡突起34aが収容凹部49に収容される。この結果、プラスチック製部材40aの底部42とプリフォーム10aの底部30aとの間に隙間が生じない。これにより、ブロー成形後に容器本体10とプラスチック製部材40との間に空気が残存することによってガスバリア性等の機能が損なわれる不具合を防止することができる。   Thus, by providing the accommodating recess 49 in the bottom portion 42 of the plastic member 40a, when the bottomed plastic member 40a is fitted into the preform 10a (see FIG. 5B), the gate of the preform 10a. The trace protrusion 34 a is accommodated in the accommodating recess 49. As a result, no gap is generated between the bottom 42 of the plastic member 40a and the bottom 30a of the preform 10a. Thereby, the malfunction which functions, such as gas barrier property, are impaired by air remaining between the container main body 10 and the plastic members 40 after blow molding can be prevented.

このようなプラスチック製部材40aは、例えばダイレクトブロー成形法によって作製されたダイレクトブロー成形品(ダイレクトブロー成形チューブ)、シート成形法によって作製されたシート成形品(シート成形チューブ)又は射出成形法によって作製された射出成形品(射出成形チューブ)であっても良い。   Such a plastic member 40a is produced by, for example, a direct blow molded product (direct blow molded tube) produced by a direct blow molding method, a sheet molded product (sheet molded tube) produced by a sheet molding method, or an injection molding method. It may be an injection molded product (injection molded tube).

プラスチック製部材40aとしては、例えば、ポリエチレン、ポリプロピレン、ポリエチレンテレフタレート、ポリエチレンナフタレート、ポリ−4−メチルペンテン−1、ポリスチレン、AS樹脂、ABS樹旨、ポリ塩化ビニル、ポリ塩化ビニリデン、ポリ酢酸ビニル、ポリビニルアルコール、ポリビニルアセタール、ポリビニルブチラール、フタル酸ジアリル樹脂、フッ素系樹脂、ポリメタクリル酸メチル、ポリアクリル酸、ポリアクリル酸メチル、ポリアクリロニトリル、ポリアクリルアミド、ポリブタジエン、ポリブテン−1、ポリイソプレン、ポリクロロプレン、エチレンプロピレンゴム、ブチルゴム、ニトリルゴム、アクリルゴム、シリコーンゴム、フッ素ゴム、ナイロン6、ナイロン6,6、ナイロンMXD6、芳香族ポリアミド、ポリカーボネート、ポリテレフタル酸エチレン、ポリテレフタル酸ブチレン、ポリナフタレン酸エチレン、Uポリマー、液晶ポリマー、変性ポリフェニレンエーテル、ポリエーテルケトン、ポリエーテルエーテルケトン、不飽和ポリエステル、アルキド樹脂、ポリイミド、ポリスルホン、ポリフェニレンスルフィド、ポリエーテルスルホン、シリコーン樹脂、ポリウレタン、フェノール樹脂、尿素樹脂、ポリエチレンオキシド、ポリプロピレンオキシド、ポリアセタール、エポキシ樹脂等を挙げることができる。このうちポリエチレン(PE)、ポリプロピレン(PP)、ポリエチレンテレフタレート(PET)、ポリエチレンナフタレート(PEN)等の熱可塑性非弾性樹脂を用いることが好ましい。またそれらのブレンド材料や多層構造、部分的多層構造のものであってもよい。さらに、プラスチック製部材40aの材料には、その特性が損なわれない範囲において、主成分の樹脂以外にも、各種の添加剤を添加してもよい。添加剤としては、例えば、可塑剤、紫外線安定化剤、着色防止剤、艶消し剤、消臭剤、難燃剤、耐候剤、帯電防止剤、糸摩擦低減剤、スリップ剤、離型剤、抗酸化剤、イオン交換剤、および着色顔料等を添加することができる。また、熱可塑性樹脂の溶融物に不活性ガス(窒素ガス、アルゴンガス)を混ぜることで、0.5〜100μmの発泡セル径を持つ発泡部材を使用し、この発泡プリフォームを成形することによって、遮光性を高めることができる。   Examples of the plastic member 40a include polyethylene, polypropylene, polyethylene terephthalate, polyethylene naphthalate, poly-4-methylpentene-1, polystyrene, AS resin, ABS tree, polyvinyl chloride, polyvinylidene chloride, polyvinyl acetate, Polyvinyl alcohol, polyvinyl acetal, polyvinyl butyral, diallyl phthalate resin, fluororesin, polymethyl methacrylate, polyacrylic acid, polymethyl acrylate, polyacrylonitrile, polyacrylamide, polybutadiene, polybutene-1, polyisoprene, polychloroprene, Ethylene propylene rubber, butyl rubber, nitrile rubber, acrylic rubber, silicone rubber, fluoro rubber, nylon 6, nylon 6,6, nylon MXD6, aromatic poly , Polycarbonate, ethylene polyterephthalate, polybutylene terephthalate, poly ethylene naphthalate, U polymer, liquid crystal polymer, modified polyphenylene ether, polyether ketone, polyether ether ketone, unsaturated polyester, alkyd resin, polyimide, polysulfone, polyphenylene Examples thereof include sulfide, polyethersulfone, silicone resin, polyurethane, phenol resin, urea resin, polyethylene oxide, polypropylene oxide, polyacetal, and epoxy resin. Among these, it is preferable to use thermoplastic inelastic resins such as polyethylene (PE), polypropylene (PP), polyethylene terephthalate (PET), and polyethylene naphthalate (PEN). Moreover, those blend materials, multilayer structures, and partial multilayer structures may be used. Furthermore, various additives other than the main component resin may be added to the material of the plastic member 40a as long as the characteristics are not impaired. Examples of additives include plasticizers, UV stabilizers, anti-coloring agents, matting agents, deodorants, flame retardants, weathering agents, antistatic agents, yarn friction reducing agents, slip agents, mold release agents, An oxidizing agent, an ion exchange agent, a coloring pigment, and the like can be added. Also, by mixing an inert gas (nitrogen gas, argon gas) with a melt of a thermoplastic resin, a foam member having a foam cell diameter of 0.5 to 100 μm is used, and this foam preform is molded. , The light shielding property can be improved.

またプラスチック製部材40aが容器本体10(プリフォーム10a)と同一の材料からなっていても良い。この場合、複合容器10Aのうち、例えば強度を高めたい部分に重点的にプラスチック製部材40を配置し、当該箇所の強度を選択的に高めることができる。例えば、容器本体10の肩部12周辺および底部30周辺にプラスチック製部材40を設け、この部分の強度を高めても良い。このような材料としては、熱可塑性樹脂、特にPE(ポリエチレン)、PP(ポリプロピレン)、PET(ポリエチレンテレフタレート)、PEN(ポリエチレンナフタレート)、PC(ポリカーボネート)を挙げることができる。   The plastic member 40a may be made of the same material as the container body 10 (preform 10a). In this case, in the composite container 10A, for example, the plastic member 40 can be intensively arranged at a portion where the strength is to be increased, and the strength of the portion can be selectively increased. For example, plastic members 40 may be provided around the shoulder 12 and the bottom 30 of the container body 10 to increase the strength of this portion. Examples of such materials include thermoplastic resins, particularly PE (polyethylene), PP (polypropylene), PET (polyethylene terephthalate), PEN (polyethylene naphthalate), and PC (polycarbonate).

またプラスチック製部材40aは、酸素バリア性又は水蒸気バリア性等のガスバリア性を有する材料からなっていても良い。この場合、プリフォーム10aとして多層プリフォームやブレンド材料を含むプリフォーム等を用いることなく、複合容器10Aのガスバリア性を高め、容器内への酸素の侵入を防ぎ、内容液が劣化することを防止し、また、容器内から外部への水蒸気の蒸散を防ぎ、内容量が減少することを防止することができる。例えば、容器本体10のうち、肩部12、首部13、胴部20および底部30の全域にプラスチック製部材40を設け、この部分のガスバリア性を高めても良い。このような材料としては、PE(ポリエチレン)、PP(ポリプロピレン)、MXD−6(ナイロン)、PGA(ポリグリコール酸)、EVOH(エチレンビニルアルコール共重合体)またはこれらの材料に脂肪酸塩などの酸素吸収材を混ぜることも考えられる。   The plastic member 40a may be made of a material having a gas barrier property such as an oxygen barrier property or a water vapor barrier property. In this case, without using a multi-layer preform or a preform containing a blend material as the preform 10a, the gas barrier property of the composite container 10A is improved, oxygen is prevented from entering the container, and the content liquid is prevented from deteriorating. In addition, it is possible to prevent the evaporation of water vapor from the inside of the container to the outside and to prevent the internal volume from decreasing. For example, a plastic member 40 may be provided in the entire region of the shoulder portion 12, the neck portion 13, the trunk portion 20, and the bottom portion 30 of the container body 10, and the gas barrier property of this portion may be improved. Examples of such materials include PE (polyethylene), PP (polypropylene), MXD-6 (nylon), PGA (polyglycolic acid), EVOH (ethylene vinyl alcohol copolymer), and oxygen such as fatty acid salts in these materials. It is also possible to mix an absorbent material.

またプラスチック製部材40aは、紫外線等の光線バリア性を有する材料からなっていても良い。この場合、プリフォーム10aとして多層プリフォームやブレンド材料を含むプリフォーム等を用いることなく、複合容器10Aの光線バリア性を高め、紫外線等により内容液が劣化することを防止することができる。例えば、容器本体10のうち、肩部12、首部13、胴部20および底部30の全域にプラスチック製部材40aを設け、この部分の紫外線バリア性を高めても良い。このような材料としては、ブレンド材料、またはPETやPE、PPに遮光性樹脂を添加した材料が考えられる。また、熱可塑性樹脂の溶融物に不活性ガス(窒素ガス、アルゴンガス)を混ぜることにより作製された、0.5〜100μmの発泡セル径を持つ発泡部材を使用しても良い。   The plastic member 40a may be made of a material having a light barrier property such as ultraviolet rays. In this case, the light barrier property of the composite container 10A can be improved and the content liquid can be prevented from being deteriorated by ultraviolet rays or the like without using a multilayer preform or a preform containing a blend material as the preform 10a. For example, a plastic member 40a may be provided in the entire region of the shoulder portion 12, the neck portion 13, the trunk portion 20, and the bottom portion 30 of the container body 10 to enhance the ultraviolet barrier property of this portion. As such a material, a blend material or a material obtained by adding a light-shielding resin to PET, PE, or PP can be considered. Moreover, you may use the foaming member with the foam cell diameter of 0.5-100 micrometers produced by mixing inert gas (nitrogen gas, argon gas) with the melt of a thermoplastic resin.

またプラスチック製部材40aは、容器本体10(プリフォーム10a)を構成するプラスチック材料よりも保冷性の高い材料(熱伝導性の低い材料)からなっていても良い。この場合、容器本体10そのものの厚みを厚くすることなく、内容液の温度が複合容器10Aの表面まで伝達しにくくすることが可能となる。これにより、複合容器10Aの保冷性が高められる。例えば、容器本体10のうち胴部20の全部又は一部にプラスチック製部材40を設け、胴部20の保冷性を高めても良い。また、使用者が複合容器10Aを把持した際、冷たすぎることにより複合容器10Aを持ちにくくなることが防止される。このような材料としては、発泡化したポリウレタン、ポリスチレン、PE(ポリエチレン)、PP(ポリプロピレン)、フェノール樹脂、ポリ塩化ビニル、ユリア樹脂、シリコーン、ポリイミド、メラミン樹脂などが考えられる。これら樹脂を含んでなる樹脂材料に、中空粒子を混合することが好ましい。中空粒子の平均粒子径は、1〜200μmであることが好ましく、5〜80μmであることがより好ましい。なお、「平均粒子径」とは、体積平均粒子径を意味し、粒度分布・粒径分布測定装置(例えば、ナノトラック粒度分布測定装置、日機装株式会社製など)を用いて公知の方法により測定することができる。また、中空粒子としては、樹脂などから構成される有機系中空粒子であってもよく、ガラスなどから構成される無機系中空粒子であってもよいが、分散性が優れるという理由から、有機系中空粒子が好ましい。有機系中空粒子を構成する樹脂としては、例えば、架橋スチレン−アクリル樹脂などのスチレン系樹脂、アクリロニトリル−アクリル樹脂などの(メタ)アクリル系樹脂、フェノール系樹脂、フッ素系樹脂、ポリアミド系樹脂、ポリイミド系樹脂、ポリカーボネート系樹脂、ポリエーテル系樹脂などを挙げることができる。また、ローペイクHP−1055、ローペイクHP−91、ローペイクOP−84J、ローペイクウルトラ、ローペイクSE、ローペイクST(ロームアンドハース(株)製)、ニポールMH−5055(日本ゼオン(株)製)、SX8782、SX866(JSR(株)製)などの市販される中空粒子を用いることも出来る。中空粒子の含有量としては、プラスチック製部材40aに含有される樹脂材料100質量部に対して、0.01〜50質量部であることが好ましく、1〜20質量部であることがより好ましい。   Further, the plastic member 40a may be made of a material having a higher cold insulation property (a material having a low thermal conductivity) than the plastic material constituting the container body 10 (preform 10a). In this case, it is possible to make it difficult for the temperature of the content liquid to be transmitted to the surface of the composite container 10A without increasing the thickness of the container body 10 itself. Thereby, the cool property of 10 A of composite containers is improved. For example, the plastic member 40 may be provided on the whole or a part of the body 20 in the container body 10 to improve the cold insulation of the body 20. Further, when the user grips the composite container 10A, it is prevented that the composite container 10A becomes difficult to hold due to being too cold. Examples of such materials include foamed polyurethane, polystyrene, PE (polyethylene), PP (polypropylene), phenol resin, polyvinyl chloride, urea resin, silicone, polyimide, melamine resin, and the like. It is preferable to mix hollow particles with a resin material containing these resins. The average particle diameter of the hollow particles is preferably 1 to 200 μm, and more preferably 5 to 80 μm. The “average particle size” means the volume average particle size and is measured by a known method using a particle size distribution / particle size distribution measuring device (for example, Nanotrack particle size distribution measuring device, manufactured by Nikkiso Co., Ltd.). can do. The hollow particles may be organic hollow particles composed of a resin or the like, or may be inorganic hollow particles composed of glass or the like. Hollow particles are preferred. Examples of the resin constituting the organic hollow particles include styrene resins such as cross-linked styrene-acrylic resins, (meth) acrylic resins such as acrylonitrile-acrylic resins, phenolic resins, fluorine resins, polyamide resins, and polyimides. Resin, polycarbonate resin, polyether resin and the like. In addition, Ropeke HP-1055, Ropeke HP-91, Ropeke OP-84J, Ropeke Ultra, Ropeke SE, Ropeke ST (made by Rohm and Haas Co.), Nipol MH-5055 (made by Nippon Zeon Co., Ltd.), SX8782 Commercially available hollow particles such as SX866 (manufactured by JSR Corporation) can also be used. As content of a hollow particle, it is preferable that it is 0.01-50 mass parts with respect to 100 mass parts of resin materials contained in the plastic members 40a, and it is more preferable that it is 1-20 mass parts.

またプラスチック製部材40aは、容器本体10(プリフォーム10a)を構成するプラスチック材料よりも滑りにくい材料からなっていても良い。この場合、容器本体10の材料を変更することなく、使用者が複合容器10Aを把持しやすくすることができる。例えば、容器本体10のうち胴部20の全部又は一部にプラスチック製部材40を設け、胴部20を持ちやすくしても良い。   The plastic member 40a may be made of a material that is less slippery than the plastic material that constitutes the container body 10 (preform 10a). In this case, the user can easily hold the composite container 10 </ b> A without changing the material of the container body 10. For example, a plastic member 40 may be provided on all or part of the body 20 of the container body 10 so that the body 20 can be easily held.

このプラスチック製部材40aには、予めデザイン又は印字等の印刷が施されていても良い。この場合、印刷は例えばインクジェット法やグラビア印刷法等の印刷法により、無地のプラスチック製部材40aにデザイン又は印字が施されて形成されても良い。この印刷は、プリフォーム10aに取り付けられる前のプラスチック製部材40aに対して施されても良く、プリフォーム10aの外側にプラスチック製部材40aを設けた状態で施されても良い。また、プラスチック製部材40aは、赤色、青色、黄色、緑色、茶色、黒色、白色等の色に着色されていても良く、また透明であっても不透明であっても良い。   The plastic member 40a may be preliminarily printed with design or printing. In this case, the printing may be formed by designing or printing the plain plastic member 40a by a printing method such as an inkjet method or a gravure printing method. This printing may be performed on the plastic member 40a before being attached to the preform 10a, or may be performed in a state where the plastic member 40a is provided outside the preform 10a. The plastic member 40a may be colored in colors such as red, blue, yellow, green, brown, black, and white, and may be transparent or opaque.

次に、図4(a)〜(b)により、収容凹部49の変形例について説明する。   Next, a modified example of the housing recess 49 will be described with reference to FIGS.

図4(a)において、収容凹部49は、プラスチック製部材40aの底部42を厚み方向に貫通するザグリ形状の貫通孔からなっている。すなわち、収容凹部49は、プラスチック製部材40aの内面側に開口する大径部49aと、プラスチック製部材40aの外面側に開口する小径部49bとからなっている。このうち大径部49a内には、プリフォーム10aのゲート跡突起34aが収容されている。大径部49aの幅(径)は、例えば3mm〜12mmであり、小径部49bの幅(径)は、例えば0.01mm〜5mmとすることが好ましい。また、プラスチック製部材40aの外面のうち収容凹部49に対応する領域が、外方に向けて突出することにより、外面突起49cが形成されている。上述した小径部49bは、外面突起49cの略中央部に開口している。このようなプラスチック製部材40aは、例えばダイレクトブロー成形法によって作製されたダイレクトブロー成形品(ダイレクトブロー成形チューブ)、シート成形法によって作製されたシート成形品(シート成形チューブ)又は射出成形法によって作製された射出成形品(射出成形チューブ)であっても良い。   In FIG. 4A, the housing recess 49 is a counterbore-shaped through-hole that penetrates the bottom 42 of the plastic member 40a in the thickness direction. In other words, the housing recess 49 includes a large-diameter portion 49a that opens to the inner surface side of the plastic member 40a and a small-diameter portion 49b that opens to the outer surface side of the plastic member 40a. Among these, in the large diameter part 49a, the gate trace protrusion 34a of the preform 10a is accommodated. The width (diameter) of the large diameter portion 49a is, for example, 3 mm to 12 mm, and the width (diameter) of the small diameter portion 49b is preferably, for example, 0.01 mm to 5 mm. Further, an outer surface protrusion 49c is formed by projecting an area corresponding to the housing recess 49 in the outer surface of the plastic member 40a outward. The small-diameter portion 49b described above opens at a substantially central portion of the outer protrusion 49c. Such a plastic member 40a is produced by, for example, a direct blow molded product (direct blow molded tube) produced by a direct blow molding method, a sheet molded product (sheet molded tube) produced by a sheet molding method, or an injection molding method. It may be an injection molded product (injection molded tube).

このように、プラスチック製部材40aの底部42を貫通する収容凹部49を設けたことにより、有底のプラスチック製部材40aをプリフォーム10aに嵌め込む際(図5(b)参照)、収容凹部49が空気の逃げ道となるため、プラスチック製部材40aをプリフォーム10aに対してスムーズに取り付けることができる。また、収容凹部49は大径部49aと小径部49bとからなっているので、大径部49aの大きさをゲート跡突起34aを収容できる程度の大きさに設定した場合でも、小径部49bを必要以上に大きくする必要がない。このため、収容凹部49が存在することによって、容器本体10の底部30に対するガスバリア性や光線バリア性等の機能が損なわれるおそれは少ない。なお、収容凹部49は、ブロー成形によってプラスチック製部材40aが延伸されて膨張された際に塞がっても良い。   Thus, by providing the accommodating recess 49 that penetrates the bottom 42 of the plastic member 40a, when the bottomed plastic member 40a is fitted into the preform 10a (see FIG. 5B), the accommodating recess 49 is provided. Therefore, the plastic member 40a can be smoothly attached to the preform 10a. Further, since the housing recess 49 is composed of a large diameter portion 49a and a small diameter portion 49b, even when the large diameter portion 49a is set to a size that can accommodate the gate trace protrusion 34a, the small diameter portion 49b is formed. There is no need to make it larger than necessary. For this reason, there exists little possibility that functions, such as gas barrier property with respect to the bottom part 30 of the container main body 10, and light beam barrier property, will be impaired by the accommodation recessed part 49 existing. The housing recess 49 may be closed when the plastic member 40a is expanded and expanded by blow molding.

また、図4(b)において、収容凹部49は、プラスチック製部材40aの底部42を厚み方向に貫通する略均一な幅(径)をもつ貫通孔からなっている。この収容凹部49は、例えば略円柱状であり、ゲート跡突起34aを収容可能な程度の大きさに形成されている。収容凹部49の幅(径)は、例えば3mm〜12mmとすることが好ましい。このようなプラスチック製部材40aは、例えば射出成形法によって作製された射出成形品(射出成形チューブ)のほか、ダイレクトブロー成形法によって作製されたダイレクトブロー成形品(ダイレクトブロー成形チューブ)又はシート成形法によって作製されたシート成形品(シート成形チューブ)であっても良い。   In FIG. 4B, the accommodating recess 49 is a through hole having a substantially uniform width (diameter) that penetrates the bottom 42 of the plastic member 40a in the thickness direction. The accommodating recess 49 is, for example, substantially cylindrical, and is formed to a size that can accommodate the gate trace protrusion 34a. The width (diameter) of the housing recess 49 is preferably 3 mm to 12 mm, for example. Such a plastic member 40a includes, for example, an injection molded product (injection molded tube) manufactured by an injection molding method, a direct blow molded product (direct blow molded tube) or a sheet molding method manufactured by a direct blow molding method. It may be a sheet molded product (sheet molded tube) produced by the above.

このように、プラスチック製部材40aの底部42を貫通する収容凹部49を設けたことにより、有底のプラスチック製部材40aをプリフォーム10aに嵌め込む際(図5(b)参照)、収容凹部49が空気の逃げ道となるため、プラスチック製部材40aをプリフォーム10aに対してスムーズに取り付けることができる。また、収容凹部49は略均一な幅(径)をもつ貫通孔からなっているので、収容凹部49をもつプラスチック製部材40aを容易に作製することができる。なお、収容凹部49は、ブロー成形によってプラスチック製部材40aが延伸されて膨張された際に塞がっても良い。   Thus, by providing the accommodating recess 49 that penetrates the bottom 42 of the plastic member 40a, when the bottomed plastic member 40a is fitted into the preform 10a (see FIG. 5B), the accommodating recess 49 is provided. Therefore, the plastic member 40a can be smoothly attached to the preform 10a. In addition, since the housing recess 49 is a through-hole having a substantially uniform width (diameter), the plastic member 40a having the housing recess 49 can be easily manufactured. The housing recess 49 may be closed when the plastic member 40a is expanded and expanded by blow molding.

次に図5(a)〜(f)により、本実施の形態による複合容器10Aの製造方法(ブロー成形方法)について説明する。   Next, a manufacturing method (blow molding method) of the composite container 10A according to the present embodiment will be described with reference to FIGS.

まず、プラスチック材料製のプリフォーム10aを準備する(図5(a)参照)。この場合、例えば図示しない射出成形機を用いて、射出成形法によりプリフォーム10aを作製しても良い。また、プリフォーム10aとして、従来一般に用いられるプリフォームを用いても良い。   First, a preform 10a made of a plastic material is prepared (see FIG. 5A). In this case, for example, the preform 10a may be manufactured by an injection molding method using an unillustrated injection molding machine. Moreover, you may use the preform generally used conventionally as the preform 10a.

次に、プラスチック製部材40aを準備する。プラスチック製部材40aは、全体として有底円筒形状からなり、円筒状の胴部41と、胴部41に連結された底部42とを有している。底部42には、ゲート跡突起34aを収容する収容凹部49が設けられている(図3参照)。   Next, the plastic member 40a is prepared. The plastic member 40 a has a bottomed cylindrical shape as a whole, and includes a cylindrical body portion 41 and a bottom portion 42 connected to the body portion 41. The bottom portion 42 is provided with a housing recess 49 for housing the gate trace protrusion 34a (see FIG. 3).

次に、プリフォーム10aの外側にプラスチック製部材40aを設けることにより、プリフォーム10aと、プリフォーム10aの外側に密着されたプラスチック製部材40aとを有する複合プリフォーム70を作製する(図5(b)参照)。このとき、プリフォーム10aのゲート跡突起34aが収容凹部49に収容されるので、プラスチック製部材40aの底部42とプリフォーム10aの底部30aとの間に隙間が生じない(図3参照)。   Next, by providing a plastic member 40a on the outside of the preform 10a, a composite preform 70 having the preform 10a and the plastic member 40a in close contact with the outside of the preform 10a is manufactured (FIG. 5 ( b)). At this time, since the gate trace protrusion 34a of the preform 10a is accommodated in the accommodating recess 49, there is no gap between the bottom 42 of the plastic member 40a and the bottom 30a of the preform 10a (see FIG. 3).

本実施の形態において、プリフォーム10aの外径と同一又はわずかに小さい内径をもつプラスチック製部材40aを、プリフォーム10aに対して押し込むことにより、プリフォーム10aの外面に密着させる。   In the present embodiment, a plastic member 40a having an inner diameter that is the same as or slightly smaller than the outer diameter of the preform 10a is pressed into the preform 10a to be brought into close contact with the outer surface of the preform 10a.

このように、予めプリフォーム10aの外側にプラスチック製部材40aを密着させ、複合プリフォーム70を作製しておくことにより、複合プリフォーム70を作製する一連の工程(図5(a)〜(b))と、複合容器10Aをブロー成形により作製する一連の工程(図5(c)〜(f))とを別々の場所(工場等)で実施することが可能になる。   In this way, a series of steps for producing the composite preform 70 (FIGS. 5A to 5B) are performed by previously bringing the plastic member 40a into close contact with the outside of the preform 10a and producing the composite preform 70. )) And a series of steps (FIGS. 5 (c) to 5 (f)) for producing the composite container 10A by blow molding can be performed at different places (factories, etc.).

次に、複合プリフォーム70は、加熱装置51によって加熱される(図5(c)参照)。このとき、複合プリフォーム70は、口部11aを下に向けた状態で回転しながら、加熱装置51によって周方向に均等に加熱される。この加熱工程におけるプリフォーム10aおよびプラスチック製部材40aの加熱温度は、例えば90℃乃至130℃としても良い。   Next, the composite preform 70 is heated by the heating device 51 (see FIG. 5C). At this time, the composite preform 70 is evenly heated in the circumferential direction by the heating device 51 while rotating with the mouth portion 11a facing downward. The heating temperature of the preform 10a and the plastic member 40a in this heating step may be, for example, 90 ° C. to 130 ° C.

続いて、加熱装置51によって加熱された複合プリフォーム70は、ブロー成形金型50に送られる(図5(d)参照)。   Subsequently, the composite preform 70 heated by the heating device 51 is sent to the blow molding die 50 (see FIG. 5D).

複合容器10Aは、このブロー成形金型50を用いて成形される。この場合、ブロー成形金型50は互いに分割された一対の胴部金型50a、50bと、底部金型50cとからなる(図5(d)参照)。図5(d)において、一対の胴部金型50a、50b間は互いに開いており、底部金型50cは上方に上がっている。この状態で一対の胴部金型50a、50b間に、複合プリフォーム70が挿入される。   The composite container 10 </ b> A is molded using this blow molding die 50. In this case, the blow mold 50 is composed of a pair of body molds 50a and 50b and a bottom mold 50c which are divided from each other (see FIG. 5D). In FIG. 5D, the pair of body molds 50a and 50b are open to each other, and the bottom mold 50c is raised upward. In this state, the composite preform 70 is inserted between the pair of body molds 50a and 50b.

次に図5(e)に示すように、底部金型50cが下がったのちに一対の胴部金型50a、50bが閉鎖され、一対の胴部金型50a、50bおよび底部金型50cにより密閉されたブロー成形金型50が構成される。次にプリフォーム10a内に空気が圧入され、複合プリフォーム70に対して2軸延伸ブロー成形が施される。   Next, as shown in FIG. 5E, after the bottom mold 50c is lowered, the pair of body molds 50a, 50b is closed, and sealed by the pair of body molds 50a, 50b and the bottom mold 50c. A blow mold 50 is formed. Next, air is press-fitted into the preform 10 a and biaxial stretch blow molding is performed on the composite preform 70.

このことにより、ブロー成形金型50内でプリフォーム10aから容器本体10が得られる。この間、胴部金型50a、50bは30℃乃至80℃まで加熱され、底部金型50cは5℃乃至25℃まで冷却される。この際、ブロー成形金型50内では、複合プリフォーム70のプリフォーム10aおよびプラスチック製部材40aが一体として膨張される。これにより、プリフォーム10aおよびプラスチック製部材40aは、一体となってブロー成形金型50の内面に対応する形状に賦形される。   As a result, the container body 10 is obtained from the preform 10 a in the blow molding die 50. During this time, the body molds 50a and 50b are heated to 30 ° C. to 80 ° C., and the bottom mold 50c is cooled to 5 ° C. to 25 ° C. At this time, in the blow mold 50, the preform 10a of the composite preform 70 and the plastic member 40a are expanded as a unit. Thereby, the preform 10a and the plastic member 40a are integrally formed into a shape corresponding to the inner surface of the blow mold 50.

このようにして、容器本体10と、容器本体10の外面に設けられたプラスチック製部材40とを備えた複合容器10Aが得られる。   In this manner, a composite container 10A including the container body 10 and the plastic member 40 provided on the outer surface of the container body 10 is obtained.

次に図5(f)に示すように、一対の胴部金型50a、50bおよび底部金型50cが互いに離れ、ブロー成形金型50内から複合容器10Aが取出される。   Next, as shown in FIG. 5 (f), the pair of body molds 50 a and 50 b and the bottom mold 50 c are separated from each other, and the composite container 10 </ b> A is taken out from the blow molding mold 50.

このように、本実施の形態によれば、プラスチック製部材40aの底部42に収容凹部49を設けたことにより、プラスチック製部材40aをプリフォーム10aに嵌め込む際、プラスチック製部材40aの底部42とプリフォーム10aの底部30aとの間に隙間が生じない。これにより、ブロー成形後に容器本体10とプラスチック製部材40との間に空気が残存することによってガスバリア性等の機能が損なわれる不具合を防止することができる。この結果、品質の高い複合容器10Aを得ることができる。   Thus, according to the present embodiment, the housing recess 49 is provided in the bottom 42 of the plastic member 40a, so that when the plastic member 40a is fitted into the preform 10a, the bottom 42 of the plastic member 40a There is no gap between the bottom portion 30a of the preform 10a. Thereby, the malfunction which functions, such as gas barrier property, are impaired by air remaining between the container main body 10 and the plastic members 40 after blow molding can be prevented. As a result, a high-quality composite container 10A can be obtained.

また、本実施の形態によれば、ブロー成形金型50内で複合プリフォーム70に対してブロー成形を施すことにより、複合プリフォーム70のプリフォーム10aおよびプラスチック製部材40aを一体として膨張させ、容器本体10とプラスチック製部材40とを備えた複合容器10Aを作製する。これにより、プリフォーム10a(容器本体10)とプラスチック製部材40a(プラスチック製部材40)とを別部材から構成することができる。したがって、プラスチック製部材40の種類や形状を適宜選択することにより、複合容器10Aに様々な機能や特性を自在に付与することができる。   Further, according to the present embodiment, by performing blow molding on the composite preform 70 in the blow molding die 50, the preform 10a of the composite preform 70 and the plastic member 40a are expanded as a unit, A composite container 10A including the container body 10 and the plastic member 40 is produced. Thereby, preform 10a (container main part 10) and plastic member 40a (plastic member 40) can be constituted from another member. Therefore, various functions and characteristics can be freely imparted to the composite container 10A by appropriately selecting the type and shape of the plastic member 40.

さらに、本実施の形態によれば、複合容器10Aを作製する際、一般的なブロー成形装置をそのまま用いることができるので、複合容器10Aを作製するための新たな成形設備を準備する必要が生じない。また、プリフォーム10aの外側にプラスチック製部材40aを設けているので、プリフォーム10aを成形するための新たな成形設備を準備する必要も生じない。   Furthermore, according to the present embodiment, when producing the composite container 10A, a general blow molding apparatus can be used as it is, so that it is necessary to prepare a new molding facility for producing the composite container 10A. Absent. Moreover, since the plastic member 40a is provided outside the preform 10a, it is not necessary to prepare a new molding facility for molding the preform 10a.

第2の実施の形態
次に、図6乃至図10を参照して本発明の第2の実施の形態について説明する。図6乃至図10は本発明の第2の実施の形態を示す図である。図6乃至図10において、第1の実施の形態と同一部分には同一の符号を付して詳細な説明は省略する。
Second Embodiment Next, a second embodiment of the present invention will be described with reference to FIGS. 6 to 10 are views showing a second embodiment of the present invention. 6 to 10, the same parts as those of the first embodiment are denoted by the same reference numerals, and detailed description thereof is omitted.

まず、図6および図7により、本実施の形態による複合容器の概要について説明する。   First, the outline | summary of the composite container by this Embodiment is demonstrated with FIG. 6 and FIG.

図6および図7に示す複合容器10Aは、後述するように、ブロー成形金型50を用いてプリフォーム10a、内側ラベル部材60aおよびプラスチック製部材40aを含む複合プリフォーム70(図8参照)に対して2軸延伸ブロー成形を施すことにより、複合プリフォーム70のプリフォーム10a、内側ラベル部材60aおよびプラスチック製部材40aを一体として膨張させて得られたものである。   The composite container 10A shown in FIGS. 6 and 7 is formed into a composite preform 70 (see FIG. 8) including a preform 10a, an inner label member 60a, and a plastic member 40a using a blow molding die 50, as will be described later. On the other hand, by performing biaxial stretch blow molding, the preform 10a, the inner label member 60a, and the plastic member 40a of the composite preform 70 are integrally expanded.

このような複合容器10Aは、内側に位置するプラスチック材料製の容器本体10と、容器本体10の外側に密着して設けられた内側ラベル部材60と、内側ラベル部材60の外側に密着して設けられたプラスチック製部材40とを備えている。   Such a composite container 10 </ b> A is provided in close contact with the outer side of the inner label member 60 and the inner label member 60 provided in close contact with the outer side of the container main body 10. The plastic member 40 is provided.

このうち内側ラベル部材60は、容器本体10の外面に薄く延ばされた状態で密着されており、容器本体10に対して容易に移動又は回転しないほどに密着されている。   Among these, the inner label member 60 is in close contact with the outer surface of the container body 10 in a thinly extended state, and is in close contact with the container body 10 so as not to easily move or rotate.

また、プラスチック製部材40は、容器本体10の外面かつ内側ラベル部材60の外面に薄く延ばされた状態で密着されており、容器本体10に対して容易に移動又は回転しないほどに密着されている。   The plastic member 40 is in close contact with the outer surface of the container body 10 and the outer surface of the inner label member 60 in a thinly extended state, and is in close contact with the container body 10 so as not to easily move or rotate. Yes.

プラスチック製部材40は、その少なくとも一部が半透明又は透明であることが考えられ、この場合、この半透明又は透明な部分を介して、内側ラベル部材60を外方から視認できる。なお、プラスチック製部材40は、その全体が半透明又は透明であっても良く、あるいは不透明な部分と半透明又は透明な部分(例えば窓部)とを有していても良い。   It is conceivable that at least a part of the plastic member 40 is translucent or transparent. In this case, the inner label member 60 can be visually recognized from the outside through the translucent or transparent portion. The plastic member 40 may be entirely translucent or transparent, or may have an opaque portion and a translucent or transparent portion (for example, a window portion).

次に内側ラベル部材60について説明する。内側ラベル部材60(60a)は後述するようにプリフォーム10aの外側を取り囲むように設けられ、このプリフォーム10aおよびプラスチック製部材40aと一体となって2軸延伸ブロー成形されることにより得られたものである。   Next, the inner label member 60 will be described. As will be described later, the inner label member 60 (60a) is provided so as to surround the outer side of the preform 10a, and is obtained by performing biaxial stretch blow molding integrally with the preform 10a and the plastic member 40a. Is.

内側ラベル部材60は容器本体10の外面に接着されることなく取付けられており、容器本体10に対して移動又は回転しないほどに密着されている。この内側ラベル部材60は、容器本体10の外面において薄く引き延ばされて容器本体10を覆っている。図7に示すように、内側ラベル部材60は、容器本体10を取り囲むようにその周方向全域にわたって設けられており、略円形状の水平断面を有している。   The inner label member 60 is attached to the outer surface of the container body 10 without being bonded, and is in close contact with the container body 10 so as not to move or rotate. The inner label member 60 is thinly stretched on the outer surface of the container body 10 to cover the container body 10. As shown in FIG. 7, the inner label member 60 is provided over the entire circumferential direction so as to surround the container body 10, and has a substantially circular horizontal cross section.

この場合、内側ラベル部材60は、容器本体10のうち、口部11および首部13を除く、肩部12、胴部20および底部30を覆うように設けられている。これにより、容器本体10の肩部12、胴部20および底部30に所望の文字、画像等を付与し、複合容器10Aに対して装飾性をもたせたり、情報を表示させたりすることができる。   In this case, the inner label member 60 is provided so as to cover the shoulder portion 12, the trunk portion 20, and the bottom portion 30 of the container body 10 except for the mouth portion 11 and the neck portion 13. Thereby, desired characters, images, and the like can be imparted to the shoulder portion 12, the body portion 20, and the bottom portion 30 of the container main body 10, and the composite container 10A can be decorated and information can be displayed.

なお、内側ラベル部材60は、容器本体10のうち口部11以外の全域又は一部領域に設けられていても良い。例えば、内側ラベル部材60は、容器本体10のうち、口部11を除く、首部13、肩部12、胴部20および底部30の全体を覆うように設けられていても良い。さらに、内側ラベル部材60は1つに限らず、複数設けても良い。なお、内側ラベル部材60は、プラスチック製部材40と同一の領域に設けられていても良く、プラスチック製部材40よりも狭い領域に設けられていても良い。後者の場合、内側ラベル部材60はプラスチック製部材40によって完全に覆われることが好ましい。   The inner label member 60 may be provided in the entire region or a partial region other than the mouth portion 11 of the container main body 10. For example, the inner label member 60 may be provided so as to cover the neck portion 13, the shoulder portion 12, the trunk portion 20, and the bottom portion 30 of the container body 10 except the mouth portion 11. Furthermore, the inner label member 60 is not limited to one, and a plurality of inner label members 60 may be provided. The inner label member 60 may be provided in the same region as the plastic member 40, or may be provided in a region narrower than the plastic member 40. In the latter case, the inner label member 60 is preferably completely covered by the plastic member 40.

また内側ラベル部材60の厚みは、これに限定されるものではないが、容器本体10に取り付けられた状態で例えば1μm〜100μm程度とすることができる。   Further, the thickness of the inner label member 60 is not limited to this, but can be set to, for example, about 1 μm to 100 μm in a state of being attached to the container body 10.

このほか、容器本体10およびプラスチック製部材40の構成は、上述した第1の実施の形態の場合と略同様であるので、ここでは詳細な説明を省略する。   In addition, since the configurations of the container body 10 and the plastic member 40 are substantially the same as those in the first embodiment described above, detailed description thereof is omitted here.

次に図8により、本実施の形態による複合プリフォームの構成について説明する。   Next, the structure of the composite preform according to this embodiment will be described with reference to FIG.

図8に示すように、複合プリフォーム70は、プラスチック材料製のプリフォーム10aと、プリフォーム10aの外側に密着して設けられた有底円筒状の内側ラベル部材60aと、内側ラベル部材60aの外側に密着して設けられた有底円筒状のプラスチック製部材40aとを備えている。   As shown in FIG. 8, the composite preform 70 includes a plastic material preform 10a, a bottomed cylindrical inner label member 60a provided in close contact with the outer side of the preform 10a, and an inner label member 60a. And a bottomed cylindrical plastic member 40a provided in close contact with the outside.

内側ラベル部材60aは、プリフォーム10aの外面に密着されており、プリフォーム10aに対して容易に移動又は回転しないほどに密着されているか、又は自重で落下しない程度に密着されている。内側ラベル部材60aは、プリフォーム10aを取り囲むようにその周方向全域にわたって設けられており、略円形状の水平断面を有している。   The inner label member 60a is in close contact with the outer surface of the preform 10a and is in close contact with the preform 10a so that it does not easily move or rotate, or is in close contact with the preform 10a so that it does not fall off due to its own weight. The inner label member 60a is provided over the entire circumferential direction so as to surround the preform 10a, and has a substantially circular horizontal cross section.

内側ラベル部材60aには、予めデザイン又は印字が施されていても良い。例えば、図柄や商品名等のほか、内容液の名称、製造者、原材料名等の文字情報が記載されていても良い。この場合、ブロー成形後に容器本体10に対して別途ラベル等を付与することなく、複合容器10Aに画像や文字を表示することが可能となる。例えば、プリフォーム10aのうち胴部20aの全部又は一部に内側ラベル部材60aを設け、成形後に容器本体10の胴部20に画像や文字が表示されるようにしても良い。これにより、容器を密栓した後、ラベラーを用いてラベルを付与する工程が不要となるので、製造コストを抑制することができるとともに、歩留まりが低下することを防止することができる。   The inner label member 60a may be previously designed or printed. For example, in addition to the design and product name, character information such as the name of the content liquid, the manufacturer, and the name of the raw material may be described. In this case, it is possible to display images and characters on the composite container 10A without separately providing a label or the like to the container body 10 after blow molding. For example, the inner label member 60a may be provided on all or part of the trunk portion 20a of the preform 10a, and images and characters may be displayed on the trunk portion 20 of the container body 10 after molding. This eliminates the need for a labeling process using a labeler after the container is tightly sealed, so that the manufacturing cost can be suppressed and the yield can be prevented from decreasing.

このような内側ラベル部材60aとしては、ポリエステル系樹脂、ポリアミド系樹脂、ポリアラミド系樹脂、ポリプロピレン系樹脂、ポリカーボネート系樹脂、ポリアセタール系樹脂、フッ素系樹脂などの未延伸フィルムを用いることができる。内側ラベル部材60aは、容器本体10(プリフォーム10a)および/またはプラスチック製部材40aと同一の材料からなっていても良く、異なる材料からなっていても良い。   As such an inner label member 60a, an unstretched film such as polyester resin, polyamide resin, polyaramid resin, polypropylene resin, polycarbonate resin, polyacetal resin, or fluorine resin can be used. The inner label member 60a may be made of the same material as the container body 10 (preform 10a) and / or the plastic member 40a, or may be made of a different material.

図8において、内側ラベル部材60aは、全体として有底円筒形状からなり、円筒状の胴部61と、胴部61に連結された半球状の底部62とを有している。底部62には収容凹部66が設けられている。収容凹部66は、プリフォーム10aのゲート跡突起34aを収容するものであり、内側ラベル部材60aをプリフォーム10aに装着した際、ゲート跡突起34aに対応する位置に設けられている。また、内側ラベル部材60aの外面のうち収容凹部66に対応する領域が外方に向けて突出することにより、外面突起66cが形成されている。本実施の形態において、収容凹部66は、底部62の中央1箇所に設けられているが、その位置や個数はこれに限定されるものではない。   In FIG. 8, the inner label member 60 a has a bottomed cylindrical shape as a whole, and includes a cylindrical body portion 61 and a hemispherical bottom portion 62 connected to the body portion 61. An accommodation recess 66 is provided in the bottom 62. The accommodating recess 66 accommodates the gate trace protrusion 34a of the preform 10a, and is provided at a position corresponding to the gate trace protrusion 34a when the inner label member 60a is attached to the preform 10a. Further, an outer surface projection 66c is formed by projecting an area corresponding to the housing recess 66 out of the outer surface of the inner label member 60a. In the present embodiment, the accommodation recess 66 is provided at one central portion of the bottom 62, but the position and number thereof are not limited to this.

また、収容凹部66の深さおよび幅(径)を、それぞれゲート跡突起34aの突出高さおよび幅(径)よりも大きくすることにより、ゲート跡突起34aの全体を収容凹部66に収容できるようにすることが好ましい。具体的には、収容凹部66の深さは、例えば0.5mm〜5mmであり、収容凹部66の幅(径)は、例えば3mm〜12mmである。   Further, by making the depth and width (diameter) of the accommodating recess 66 larger than the protruding height and width (diameter) of the gate trace protrusion 34a, the entire gate trace protrusion 34a can be accommodated in the accommodation recess 66. It is preferable to make it. Specifically, the depth of the housing recess 66 is, for example, 0.5 mm to 5 mm, and the width (diameter) of the housing recess 66 is, for example, 3 mm to 12 mm.

図8において、収容凹部66は非貫通孔からなっている。すなわち、収容凹部66は、内側ラベル部材60aの内面側に開口する一方、内側ラベル部材60aの外面側には開口されていない。   In FIG. 8, the housing recess 66 is a non-through hole. In other words, the housing recess 66 opens to the inner surface side of the inner label member 60a, but does not open to the outer surface side of the inner label member 60a.

一方、プラスチック製部材40aは、内側ラベル部材60aの外面に接着されることなく取付けられており、プリフォーム10aに対して移動又は回転しないほどに密着されているか、又は自重で落下しない程度に密着されている。   On the other hand, the plastic member 40a is attached to the outer surface of the inner label member 60a without being bonded, and is in close contact with the preform 10a so that it does not move or rotate, or close enough not to fall by its own weight. Has been.

なお、内側ラベル部材60aおよびプラスチック製部材40aは、口部11a以外の全域又は一部領域に設けられていても良い。例えば、内側ラベル部材60aおよびプラスチック製部材40aは、口部11aを除く、胴部20aおよび底部30aの全体を覆うように設けられていても良い。さらに、内側ラベル部材60aおよびプラスチック製部材40aはそれぞれ1つに限らず、複数設けても良い。例えば、2つの内側ラベル部材60aおよびプラスチック製部材40aを胴部20aの外側2箇所にそれぞれ設けても良い。   The inner label member 60a and the plastic member 40a may be provided in the entire region or a partial region other than the mouth portion 11a. For example, the inner label member 60a and the plastic member 40a may be provided so as to cover the entire body portion 20a and the bottom portion 30a except for the mouth portion 11a. Furthermore, the inner label member 60a and the plastic member 40a are not limited to one, and a plurality of inner label members 60a and plastic members 40a may be provided. For example, the two inner label members 60a and the plastic member 40a may be provided at two locations on the outer side of the body portion 20a.

このほか、プリフォーム10aおよびプラスチック製部材40aの構成は、上述した第1の実施の形態の場合と略同様であるので、ここでは詳細な説明を省略する。   In addition, since the configurations of the preform 10a and the plastic member 40a are substantially the same as those in the first embodiment described above, detailed description thereof is omitted here.

次に、図9(a)〜(b)により、収容凹部66の変形例について説明する。   Next, a modified example of the housing recess 66 will be described with reference to FIGS.

図9(a)において、収容凹部66は、内側ラベル部材60aの底部62を厚み方向に貫通する略ザグリ形状の貫通孔からなっている。すなわち、収容凹部66は、内側ラベル部材60aの内面側に開口する大径部66aと、内側ラベル部材60aの外面側に開口する小径部66bとからなっている。このうち大径部66a内には、プリフォーム10aのゲート跡突起34aが収容されている。   In FIG. 9A, the housing recess 66 is formed of a substantially counterbore-shaped through hole that penetrates the bottom 62 of the inner label member 60a in the thickness direction. That is, the housing recess 66 includes a large-diameter portion 66a that opens to the inner surface side of the inner label member 60a and a small-diameter portion 66b that opens to the outer surface side of the inner label member 60a. Among these, the gate trace protrusion 34a of the preform 10a is accommodated in the large diameter portion 66a.

図9(b)において、収容凹部66は、内側ラベル部材60aの底部62を厚み方向に貫通する略均一な幅(径)をもつ貫通孔からなっている。この収容凹部66は、例えば円柱状であり、ゲート跡突起34aを収容可能な程度の大きさに形成されている。   In FIG.9 (b), the accommodation recessed part 66 consists of a through-hole with the substantially uniform width | variety (diameter) which penetrates the bottom part 62 of the inner side label member 60a in the thickness direction. The accommodation recess 66 has, for example, a cylindrical shape, and is formed to a size that can accommodate the gate trace protrusion 34a.

図9(a)〜(b)において、内側ラベル部材60aの底部62を貫通する収容凹部66を設けたことにより、有底の内側ラベル部材60aをプリフォーム10aに嵌め込む際(図10(b)参照)、収容凹部66が空気の逃げ道となるため、内側ラベル部材60aをプリフォーム10aに対してスムーズに取り付けることができる。   9 (a) to 9 (b), when the receiving concave portion 66 that penetrates the bottom portion 62 of the inner label member 60a is provided, the bottomed inner label member 60a is fitted into the preform 10a (FIG. 10 (b). )), The accommodation recess 66 serves as an air escape path, so that the inner label member 60a can be smoothly attached to the preform 10a.

なお、図9(a)〜(b)において、プラスチック製部材40aの底部42には、底部42を厚み方向に貫通する開口44が設けられている。これにより、プラスチック製部材40aを内側ラベル部材60aに対してスムーズに嵌め込むことができる。しかしながら、これに限らず、プラスチック製部材40aには開口44が設けられていなくても良い(図8参照)。   9A and 9B, the bottom portion 42 of the plastic member 40a is provided with an opening 44 that penetrates the bottom portion 42 in the thickness direction. Thereby, the plastic member 40a can be smoothly fitted into the inner label member 60a. However, the present invention is not limited to this, and the opening 44 may not be provided in the plastic member 40a (see FIG. 8).

次に図10(a)〜(f)により、本実施の形態による複合容器10Aの製造方法(ブロー成形方法)について説明する。   Next, a manufacturing method (blow molding method) of the composite container 10A according to the present embodiment will be described with reference to FIGS.

まず、プラスチック材料製のプリフォーム10aを準備する(図10(a)参照)。   First, a preform 10a made of a plastic material is prepared (see FIG. 10A).

次に、プリフォーム10aの外側に内側ラベル部材60aを設けるとともに、内側ラベル部材60aの外側にプラスチック製部材40aを設ける。これにより、プリフォーム10aと、プリフォーム10aの外側に密着された内側ラベル部材60aと、内側ラベル部材60aの外側に密着されたプラスチック製部材40aとを有する複合プリフォーム70を作製する(図10(b)参照)。この場合、内側ラベル部材60aは、全体として有底円筒形状からなり、円筒状の胴部61と、胴部61に連結された底部62とを有している。底部62には、ゲート跡突起34aを収容する収容凹部66が設けられている(図8参照)。   Next, an inner label member 60a is provided outside the preform 10a, and a plastic member 40a is provided outside the inner label member 60a. Thus, a composite preform 70 having the preform 10a, the inner label member 60a in close contact with the outer side of the preform 10a, and the plastic member 40a in close contact with the outer side of the inner label member 60a is produced (FIG. 10). (See (b)). In this case, the inner label member 60 a has a bottomed cylindrical shape as a whole, and includes a cylindrical body portion 61 and a bottom portion 62 connected to the body portion 61. The bottom 62 is provided with an accommodation recess 66 for accommodating the gate trace protrusion 34a (see FIG. 8).

この際、プリフォーム10aの外径と同一又はわずかに小さい内径をもつ内側ラベル部材60aおよびプラスチック製部材40aを、それぞれプリフォーム10aに対して押し込むことにより、プリフォーム10aの外面に密着させる。この場合、プリフォーム10aのゲート跡突起34aが収容凹部66に収容されるので、内側ラベル部材60aの底部62とプリフォーム10aの底部30aとの間に隙間が生じない(図8参照)。   At this time, the inner label member 60a and the plastic member 40a having an inner diameter that is the same as or slightly smaller than the outer diameter of the preform 10a are pressed into the preform 10a to be brought into close contact with the outer surface of the preform 10a. In this case, since the gate trace protrusion 34a of the preform 10a is accommodated in the accommodating recess 66, there is no gap between the bottom 62 of the inner label member 60a and the bottom 30a of the preform 10a (see FIG. 8).

また、予め内側ラベル部材60aの周囲にプラスチック製部材40aを設けておき、これら内側ラベル部材60aおよびプラスチック製部材40aを一体としてプリフォーム10aの外側に装着しても良い。あるいは、プリフォーム10aの外側に内側ラベル部材60aを設け、その後、内側ラベル部材60aの外側にプラスチック製部材40aを設けてもよい。   Alternatively, a plastic member 40a may be provided around the inner label member 60a in advance, and the inner label member 60a and the plastic member 40a may be integrally attached to the outside of the preform 10a. Alternatively, the inner label member 60a may be provided outside the preform 10a, and then the plastic member 40a may be provided outside the inner label member 60a.

このように、予めプリフォーム10aおよび内側ラベル部材60aの外側にプラスチック製部材40aを密着させ、複合プリフォーム70を作製しておくことにより、複合プリフォーム70を作製する一連の工程(図10(a)〜(b))と、複合容器10Aをブロー成形により作製する一連の工程(図10(c)〜(f))とを別々の場所(工場等)で実施することが可能になる。   In this way, a series of steps for producing the composite preform 70 (FIG. 10 (FIG. 10 (FIG. 10 (A))) is performed by previously bringing the plastic member 40 a into close contact with the outside of the preform 10 a and the inner label member 60 a and producing the composite preform 70. a) to (b)) and a series of steps (FIGS. 10 (c) to (f)) for producing the composite container 10A by blow molding can be carried out at different places (factories, etc.).

次に、複合プリフォーム70は、加熱装置51によって加熱される(図10(c)参照)。   Next, the composite preform 70 is heated by the heating device 51 (see FIG. 10C).

続いて、加熱装置51によって加熱された複合プリフォーム70は、ブロー成形金型50に送られる。複合容器10Aは、このブロー成形金型50を用いて成形され、上述した第1の実施の形態の場合と略同様にして、容器本体10と、容器本体10の外面に設けられた内側ラベル部材60と、内側ラベル部材60の外側に設けられたプラスチック製部材40とを備えた複合容器10Aが得られる(図10(d)−(f)参照)。   Subsequently, the composite preform 70 heated by the heating device 51 is sent to the blow mold 50. The composite container 10A is molded using this blow molding die 50, and is substantially the same as in the case of the first embodiment described above, and the container body 10 and the inner label member provided on the outer surface of the container body 10. 10 and the composite container 10A provided with the plastic member 40 provided outside the inner label member 60 is obtained (see FIGS. 10D to 10F).

このほか、本実施の形態による複合容器10Aの製造方法(ブロー成形方法)は、上述した第1の実施の形態の場合と略同様であるので、ここでは詳細な説明を省略する。   In addition, the manufacturing method (blow molding method) of the composite container 10A according to the present embodiment is substantially the same as in the case of the above-described first embodiment, and thus detailed description thereof is omitted here.

10 容器本体
10A 複合容器
10a プリフォーム
11、11a 口部
12 肩部
13 首部
14 ねじ部
17 フランジ部
20、20a 胴部
30、30a 底部
34a ゲート跡突起
40、40a プラスチック製部材
41 胴部
42 底部
49、66 収容凹部
50 ブロー成形金型
60、60a 内側ラベル部材
61 胴部
62 底部
70 複合プリフォーム
DESCRIPTION OF SYMBOLS 10 Container main body 10A Composite container 10a Preform 11, 11a Mouth part 12 Shoulder part 13 Neck part 14 Screw part 17 Flange part 20, 20a Body part 30, 30a Bottom part 34a Gate trace protrusion 40, 40a Plastic member 41 Body part 42 Bottom part 49 , 66 Housing recess 50 Blow mold 60, 60a Inner label member 61 Body 62 Bottom 70 Composite preform

Claims (11)

複合プリフォームにおいて、
口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームと、
前記プリフォームの外側を取り囲むように設けられ、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有するプラスチック製部材とを備え、
前記プラスチック製部材は、前記プリフォームの外側に密着されていることを特徴とする複合プリフォーム。
In composite preform,
A preform made of a plastic material having a mouth portion, a trunk portion, and a bottom portion, and a gate mark protrusion formed on the bottom portion;
A plastic member provided so as to surround the outside of the preform, and having a cylindrical body portion and a bottom portion in which an accommodating recess for accommodating the gate trace protrusion of the preform is formed;
The composite preform, wherein the plastic member is in close contact with the outside of the preform.
前記収容凹部は、非貫通孔からなることを特徴とする請求項1記載の複合プリフォーム。   The composite preform according to claim 1, wherein the housing recess is a non-through hole. 前記収容凹部は、前記プラスチック製部材の前記底部を貫通する貫通孔からなることを特徴とする請求項1記載の複合プリフォーム。   The composite preform according to claim 1, wherein the housing recess is a through-hole penetrating the bottom of the plastic member. 複合プリフォームにおいて、
口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームと、
前記プリフォームの外側を取り囲むように密着して設けられ、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有する内側ラベル部材と、
前記内側ラベル部材の外側を取り囲むように設けられたプラスチック製部材とを備え、
前記プラスチック製部材は、前記プリフォームおよび前記内側ラベル部材の外側に密着されていることを特徴とする複合プリフォーム。
In composite preform,
A preform made of a plastic material having a mouth portion, a trunk portion, and a bottom portion, and a gate mark protrusion formed on the bottom portion;
An inner label member provided in close contact so as to surround the outer side of the preform, and having a cylindrical body portion and a bottom portion in which an accommodating recess for accommodating the gate trace protrusion of the preform is formed;
A plastic member provided so as to surround the outside of the inner label member,
The composite preform, wherein the plastic member is in close contact with the outside of the preform and the inner label member.
複合容器の製造方法において、
口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームを準備する工程と、
前記プリフォームの外側に、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有するプラスチック製部材を設ける工程と、
前記プリフォームおよび前記プラスチック製部材に対してブロー成形を施すことにより、前記プリフォームおよび前記プラスチック製部材を一体として膨張させる工程とを備えたことを特徴とする複合容器の製造方法。
In the manufacturing method of the composite container,
A step of preparing a preform made of a plastic material having a mouth portion, a trunk portion, and a bottom portion, and having gate trace protrusions formed on the bottom portion;
A step of providing a plastic member having a cylindrical body portion and a bottom portion in which an accommodating recess for accommodating the gate trace protrusion of the preform is formed on the outside of the preform;
And a step of blowing the preform and the plastic member together to expand the preform and the plastic member as a unit.
前記収容凹部は、非貫通孔からなることを特徴とする請求項5記載の複合容器の製造方法。   The method for manufacturing a composite container according to claim 5, wherein the housing recess is a non-through hole. 前記収容凹部は、前記プラスチック製部材の前記底部を貫通する貫通孔からなることを特徴とする請求項5記載の複合容器の製造方法。   6. The method of manufacturing a composite container according to claim 5, wherein the housing recess is a through-hole penetrating the bottom of the plastic member. 複合容器の製造方法において、
口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームを準備する工程と、
前記プリフォームの外側に、筒状の胴部と、前記プリフォームの前記ゲート跡突起を収容する収容凹部が形成された底部とを有する内側ラベル部材を設ける工程と、
前記内側ラベル部材の外側に、プラスチック製部材を設ける工程と、
前記プリフォーム、前記内側ラベル部材および前記プラスチック製部材に対してブロー成形を施すことにより、前記プリフォーム、前記内側ラベル部材および前記プラスチック製部材を一体として膨張させる工程とを備えたことを特徴とする複合容器の製造方法。
In the manufacturing method of the composite container,
A step of preparing a preform made of a plastic material having a mouth portion, a trunk portion, and a bottom portion, and having gate trace protrusions formed on the bottom portion;
A step of providing an inner label member having a cylindrical body portion and a bottom portion in which an accommodating recess for accommodating the gate mark protrusion of the preform is formed on the outside of the preform;
Providing a plastic member outside the inner label member;
A step of blow-molding the preform, the inner label member, and the plastic member to inflate the preform, the inner label member, and the plastic member together. A method for manufacturing a composite container.
請求項5乃至8のいずれか一項記載の複合容器の製造方法によって作製されたことを特徴とする複合容器。   A composite container manufactured by the method for manufacturing a composite container according to claim 5. 口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームの外側を取り囲むように装着されるプラスチック製部材であって、
前記プリフォームの胴部を覆う筒状の胴部と、
前記プリフォームの底部を覆うとともに、前記プリフォームの前記ゲート跡突起を収容可能な収容凹部が形成された底部とを有することを特徴とするプラスチック製部材。
A plastic member having a mouth portion, a trunk portion, and a bottom portion, and mounted so as to surround the outside of a preform made of a plastic material in which a gate mark protrusion is formed on the bottom portion,
A cylindrical body covering the body of the preform;
A plastic member characterized by having a bottom portion that covers the bottom portion of the preform and has a housing recess that can accommodate the gate trace protrusion of the preform.
口部と胴部と底部とを有し、前記底部にゲート跡突起が形成されたプラスチック材料製のプリフォームの外側を取り囲むように装着されるとともに、プラスチック製部材の内側に装着される内側ラベル部材であって、
前記プリフォームの胴部を覆う筒状の胴部と、
前記プリフォームの底部を覆うとともに、前記プリフォームの前記ゲート跡突起を収容可能な収容凹部が形成された底部とを有することを特徴とする内側ラベル部材。
An inner label that has a mouth portion, a body portion, and a bottom portion, is attached so as to surround the outer side of the preform made of plastic material and has a gate mark projection formed on the bottom portion, and is attached to the inside of the plastic member A member,
A cylindrical body covering the body of the preform;
An inner label member that covers a bottom portion of the preform and has a bottom portion that is formed with an accommodating recess capable of accommodating the gate trace protrusion of the preform.
JP2015008706A 2015-01-20 2015-01-20 Composite preform, method of manufacturing composite container, composite container, plastic member, and inner label member Active JP6516142B2 (en)