JP2009168915A5 - - Google Patents

Download PDF

Info

Publication number
JP2009168915A5
JP2009168915A5 JP2008004412A JP2008004412A JP2009168915A5 JP 2009168915 A5 JP2009168915 A5 JP 2009168915A5 JP 2008004412 A JP2008004412 A JP 2008004412A JP 2008004412 A JP2008004412 A JP 2008004412A JP 2009168915 A5 JP2009168915 A5 JP 2009168915A5
Authority
JP
Japan
Prior art keywords
resin composition
toner
copolymer
mass
molecular weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2008004412A
Other languages
Japanese (ja)
Other versions
JP2009168915A (en
JP5106137B2 (en
Filing date
Publication date
Application filed filed Critical
Priority to JP2008004412A priority Critical patent/JP5106137B2/en
Priority claimed from JP2008004412A external-priority patent/JP5106137B2/en
Publication of JP2009168915A publication Critical patent/JP2009168915A/en
Publication of JP2009168915A5 publication Critical patent/JP2009168915A5/ja
Application granted granted Critical
Publication of JP5106137B2 publication Critical patent/JP5106137B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (14)

少なくとも以下の(a)、(b)、(c)
(a)スチレン系モノマー
(b)アクリレート系モノマー又はメタクリレート系モノマー
(c)活性水素基含有モノマー
を共重合してなる共重合体Aと、ポリエーテル構造又はポリエステル構造を有する両末端にイソシアネート基を有するプレポリマーBとを架橋反応させて得られるトナー用樹脂組成物であり、
該共重合体AのGPCにより算出される重量平均分子量Mwが3000乃至35000であり、該プレポリマーBの該トナー用樹脂組成物に占める構成割合が12乃至49質量%であり、
該トナー用樹脂組成物のGPCにより算出したテトラヒドロフラン可溶分のメインピーク分子量Mpが10000乃至50000であり、テトラヒドロフラン不溶分が3.0質量%未満であることを特徴とするトナー用樹脂組成物。
At least the following (a), (b), (c)
(A) a styrenic monomer ;
(B) an acrylate monomer or a methacrylate monomer ;
(C) an active hydrogen group-containing monomer ;
Is a resin composition for toner obtained by crosslinking reaction of copolymer A obtained by copolymerization with prepolymer B having an isocyanate group at both ends having a polyether structure or a polyester structure,
The weight average molecular weight Mw calculated by GPC of the copolymer A is 3000 to 35000, and the constituent ratio of the prepolymer B in the resin composition for toner is 12 to 49% by mass,
A toner resin composition, wherein a main peak molecular weight Mp of a tetrahydrofuran-soluble component calculated by GPC of the toner resin composition is 10,000 to 50,000, and a tetrahydrofuran-insoluble component is less than 3.0% by mass.
該共重合体Aが有する活性水素基が水酸基であることを特徴とする請求項1に記載のトナー用樹脂組成物。   The resin composition for toner according to claim 1, wherein the active hydrogen group of the copolymer A is a hydroxyl group. 該共重合体Aの活性水素基含量が0.25mmol/g乃至1.20mmol/gであることを特徴とする請求項1又は2に記載のトナー用樹脂組成物。   The resin composition for toner according to claim 1 or 2, wherein the copolymer A has an active hydrogen group content of 0.25 mmol / g to 1.20 mmol / g. 該プレポリマーBは、両末端数(NCO価)より求められる数平均分子量が1000乃至12000であることを特徴とする請求項1乃至3のいずれか一項に記載のトナー用樹脂組成物。 The prepolymer B is at both ends number toner resin composition according to any one of claims 1 to 3 The number average molecular weight determined from (NCO number) is characterized in that it is a 1000 to 12000. 該トナー用樹脂組成物は、GPCにより算出したテトラヒドロフラン可溶分の重量平均分子量Mwが10000乃至100000であることを特徴とする請求項1乃至4のいずれか一項に記載のトナー用樹脂組成物。 The toner resin composition, resin composition for toners according to any one of claims 1 to 4, wherein the weight average molecular weight Mw of tetrahydrofuran-soluble matter was calculated by GPC is 10000 to 100,000 . 該トナー用樹脂組成物のDSCにより算出したガラス転移温度Tgが35℃未満であることを特徴とする請求項1乃至5のいずれか一項に記載のトナー用樹脂組成物。 Toner resin composition according to any one of claims 1 to 5 glass transition temperature Tg calculated by DSC of the toner resin composition and less than 35 ° C.. 請求項1乃至6のいずれか一項に記載のトナー用樹脂組成物を結着樹脂100質量部に対して5.0乃至45.0質量部含有することを特徴とするトナー。 A toner comprising 5.0 to 45.0 parts by mass of the resin composition for toner according to any one of claims 1 to 6 with respect to 100 parts by mass of a binder resin. 少なくとも以下の(d)、(e)、(f)
(d)スチレン系モノマー
(e)アクリレート系モノマー又はメタクリレート系モノマー
(f)活性水素基含有モノマー
を共重合してなる共重合体Cをジイソシアネート化合物で変性したものと、ポリエーテル構造又はポリエステル構造を有する両末端に水酸基を有するプレポリマーDとを架橋反応させて得られるトナー用樹脂組成物であり、
該共重合体CのGPCにより算出される重量平均分子量Mwが3000乃至35000であり、該プレポリマーBの該トナー用樹脂組成物に占める構成割合が12乃至49質量%であり、
該トナー用樹脂組成物のGPCにより算出したテトラヒドロフラン可溶分のメインピーク分子量Mpが10000乃至50000であり、テトラヒドロフラン不溶分が3.0質量%未満であることを特徴とするトナー用樹脂組成物。
At least the following (d), (e), (f)
(D) a styrenic monomer ;
(E) an acrylate monomer or a methacrylate monomer ;
(F) an active hydrogen group-containing monomer ;
A resin composition for a toner obtained by cross-linking a copolymer C obtained by copolymerizing a diisocyanate compound with a prepolymer D having a polyether structure or a polyester structure and having hydroxyl groups at both ends. Yes,
The weight average molecular weight Mw calculated by GPC of the copolymer C is 3000 to 35000, and the constituent ratio of the prepolymer B in the resin composition for toner is 12 to 49% by mass,
A toner resin composition, wherein a main peak molecular weight Mp of a tetrahydrofuran-soluble component calculated by GPC of the toner resin composition is 10,000 to 50,000, and a tetrahydrofuran-insoluble component is less than 3.0% by mass.
該共重合体Cが有する活性水素基が水酸基であることを特徴とする請求項に記載のトナー用樹脂組成物。 The resin composition for toner according to claim 8 , wherein the active hydrogen group of the copolymer C is a hydroxyl group. 該共重合体Cの活性水素基含量が0.25mmol/g乃至1.20mmol/gであることを特徴とする請求項又はに記載のトナー用樹脂組成物。 Toner resin composition according to claim 8 or 9 active hydrogen group content of the copolymer C is characterized by a 0.25 mmol / g to 1.20 mmol / g. 該プレポリマーDは、両末端数(OH価)より求められる数平均分子量が1000乃至12000であることを特徴とする請求項乃至10のいずれか一項に記載のトナー用樹脂組成物。 The prepolymer D is toner resin composition according to any one of claims 8 to 10 number average molecular weight determined from both ends number (OH number) is characterized in that it is a 1000 to 12000. 該トナー用樹脂組成物は、GPCにより算出したテトラヒドロフラン可溶分の重量平均分子量Mwが10000乃至100000であることを特徴とする請求項乃至11のいずれか一項に記載のトナー用樹脂組成物。 The toner resin composition according to any one of claims 8 to 11 , wherein the toner resin composition has a weight average molecular weight Mw calculated from GPC of 10,000 to 100,000. . 該トナー用樹脂組成物のDSCにより算出したガラス転移温度Tgが35℃未満であることを特徴とする請求項乃至12のいずれか一項に記載のトナー用樹脂組成物。 Toner resin composition according to any one of claims 8 to 12 glass transition temperature Tg calculated by DSC of the toner resin composition and less than 35 ° C.. 請求項乃至13のいずれか一項に記載のトナー用樹脂組成物を結着樹脂100質量部に対して5.0乃至45.0質量部含有することを特徴とするトナー。 A toner comprising 5.0 to 45.0 parts by mass of the resin composition for toner according to any one of claims 8 to 13 with respect to 100 parts by mass of the binder resin.
JP2008004412A 2008-01-11 2008-01-11 Resin composition for toner and toner Active JP5106137B2 (en)