JP2000090937A5 - - Google Patents

Download PDF

Info

Publication number
JP2000090937A5
JP2000090937A5 JP1998259898A JP25989898A JP2000090937A5 JP 2000090937 A5 JP2000090937 A5 JP 2000090937A5 JP 1998259898 A JP1998259898 A JP 1998259898A JP 25989898 A JP25989898 A JP 25989898A JP 2000090937 A5 JP2000090937 A5 JP 2000090937A5
Authority
JP
Japan
Prior art keywords
copper foil
batteries
comparative example
thickness
mechanical strength
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP1998259898A
Other languages
English (en)
Japanese (ja)
Other versions
JP2000090937A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP10259898A priority Critical patent/JP2000090937A/ja
Priority claimed from JP10259898A external-priority patent/JP2000090937A/ja
Publication of JP2000090937A publication Critical patent/JP2000090937A/ja
Publication of JP2000090937A5 publication Critical patent/JP2000090937A5/ja
Pending legal-status Critical Current

Links

JP10259898A 1998-09-14 1998-09-14 非水電解質二次電池 Pending JP2000090937A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP10259898A JP2000090937A (ja) 1998-09-14 1998-09-14 非水電解質二次電池

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP10259898A JP2000090937A (ja) 1998-09-14 1998-09-14 非水電解質二次電池

Publications (2)

Publication Number Publication Date
JP2000090937A JP2000090937A (ja) 2000-03-31
JP2000090937A5 true JP2000090937A5 (enExample) 2005-10-13

Family

ID=17340477

Family Applications (1)

Application Number Title Priority Date Filing Date
JP10259898A Pending JP2000090937A (ja) 1998-09-14 1998-09-14 非水電解質二次電池

Country Status (1)

Country Link
JP (1) JP2000090937A (enExample)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
TW201321527A (zh) * 2011-08-05 2013-06-01 Furukawa Electric Co Ltd 二次電池集電體用壓延銅箔及其製造方法
WO2018101048A1 (ja) * 2016-11-29 2018-06-07 三洋電機株式会社 非水電解質二次電池

Similar Documents

Publication Publication Date Title
EP1135818A4 (en) BORNE BATTERIES WITH HIGH ENERGY DENSITY
CA2667299A1 (en) Negative electrode for hybrid energy storage device
JP2000156208A5 (enExample)
CA2249915A1 (en) Lithium secondary battery
TW431013B (en) Nonaqueous electrolyte battery
JP2004022250A5 (enExample)
WO2009019861A1 (ja) 非水電解質二次電池及びその製造方法
EP1463133A3 (en) Negative electrode for rechargeable lithium battery and method for fabrication thereof
WO2003058145A1 (fr) Accumulateur au lithium-ion
WO1986005031A1 (en) Grid for lead storage batteries and a method of producing the same
KR960002935A (ko) 비수전해액 2차전지
JP2000090937A5 (enExample)
JPH11354126A5 (enExample)
JP2003523043A5 (enExample)
EP1115167A4 (en) POSITIVE PANEL STUFFERS FOR STORAGE BATTERY AND HOLDING MEMORY BATTERY THAT CONTAINS HIM
JP2005071680A5 (enExample)
JPH10284060A5 (enExample)
EP0901179A3 (en) Alkaline storage battery
JPH11126604A5 (enExample)
JPH11283871A5 (enExample)
JP2000277160A5 (enExample)
JP2000090981A5 (enExample)
JPS6460959A (en) Inorganic nonaqueous electrolyte battery
JP2001126760A5 (enExample)
JP2000268798A5 (enExample)