IT1148302B - Electrolytic capacitor aluminium foil etching method - Google Patents
Electrolytic capacitor aluminium foil etching methodInfo
- Publication number
- IT1148302B IT1148302B IT48269/82A IT4826982A IT1148302B IT 1148302 B IT1148302 B IT 1148302B IT 48269/82 A IT48269/82 A IT 48269/82A IT 4826982 A IT4826982 A IT 4826982A IT 1148302 B IT1148302 B IT 1148302B
- Authority
- IT
- Italy
- Prior art keywords
- etching
- aluminium foil
- soln
- treatment
- high frequency
- Prior art date
Abstract
Method of etching aluminium foil for electrolytic capacitors gives increased effective surface area by preceding conventional AC etching by high frequency etching. The high frequency treatment produces a skin resistant to etching fluid so maintaining surface roughness during etching. In an example, sheets of aluminium foil 0.1 mm thick and 99.99% or more purity were first subjected to 3 minutes etching treatment at 1-100 kHz using a mixed 60 deg.C mixed processing soln. contg. acid added to an aq. soln. of HCl and then to 3 min AC etching at 60 Hz using the same processing soln. at 60 deg. or less. This was followed by water washing and DC voltage forming treatment. Electrostatic capacity achieved was 29.1-60.1 micro F/cm2, with values increasing as the frequency in the first processing stage was higher.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
IT48269/82A IT1148302B (en) | 1982-04-21 | 1982-04-21 | Electrolytic capacitor aluminium foil etching method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
IT48269/82A IT1148302B (en) | 1982-04-21 | 1982-04-21 | Electrolytic capacitor aluminium foil etching method |
Publications (2)
Publication Number | Publication Date |
---|---|
IT8248269A0 IT8248269A0 (en) | 1982-04-21 |
IT1148302B true IT1148302B (en) | 1986-12-03 |
Family
ID=11265602
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
IT48269/82A IT1148302B (en) | 1982-04-21 | 1982-04-21 | Electrolytic capacitor aluminium foil etching method |
Country Status (1)
Country | Link |
---|---|
IT (1) | IT1148302B (en) |
-
1982
- 1982-04-21 IT IT48269/82A patent/IT1148302B/en active
Also Published As
Publication number | Publication date |
---|---|
IT8248269A0 (en) | 1982-04-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3520788A (en) | Process for the extension of the effective surface of aluminium electrodes or foils for electrolytic capacitors | |
MY112930A (en) | Method of surface-roughening treatment of copper foil | |
JPS57208894A (en) | Controlling system for induction motor | |
US4676879A (en) | Method for the production of an aluminum foil for electrolytic _capacitors, and electrolytic capacitors thus produced | |
KR100298834B1 (en) | Etching method of aluminum foil for electrolytic capacitor | |
US4455200A (en) | Method for etching aluminum foil for electrolytic capacitors | |
IT1148302B (en) | Electrolytic capacitor aluminium foil etching method | |
EP0133714B1 (en) | Process for the electrolytic etching of aluminium capacitor foil, and etched foil obtained thereby | |
US4319972A (en) | AC Etching of aluminum capacitor foil | |
US4279715A (en) | Etching of aluminum capacitor foil | |
JP2802730B2 (en) | Etching method of aluminum foil for electrolytic capacitor | |
EP0189595A2 (en) | Method for etching electrode foils for an aluminium electrolytic capacitor | |
JPS6357935B2 (en) | ||
JPH0788476A (en) | Electrolytic liquid clarifying method | |
US6261438B1 (en) | Method and apparatus for roughening a support for radiation-sensitive coatings | |
IT1142706B (en) | Electrolytic etching of aluminium | |
Salvadori | Process for Manufacturing an Aluminium Foil for Electrolytic Capacitors and Electrolytic Capacitors Made of the Foils so Manufactured | |
Feilhauer et al. | Pre-Treatment of Aluminum Anode-Foil for Electrolytic Capacitors | |
JPS5792194A (en) | Formation of opaque white film on aluminum | |
JP2762556B2 (en) | Method for producing electrode foil for aluminum electrolytic capacitor | |
JPH0653084A (en) | Manufacture of electrode foil for aluminum electrolytic capacitor | |
JPS63299309A (en) | Manufacture of electrode foil for aluminum electrolytic capacitor | |
JPH0653085A (en) | Manufacture of electrode foil for aluminum electrolytic capacitor | |
Kawasumi et al. | Method for electrolytic treatment | |
KR920006723B1 (en) | Etching method |