GB8822837D0 - Coating system - Google Patents
Coating systemInfo
- Publication number
- GB8822837D0 GB8822837D0 GB888822837A GB8822837A GB8822837D0 GB 8822837 D0 GB8822837 D0 GB 8822837D0 GB 888822837 A GB888822837 A GB 888822837A GB 8822837 A GB8822837 A GB 8822837A GB 8822837 D0 GB8822837 D0 GB 8822837D0
- Authority
- GB
- United Kingdom
- Prior art keywords
- coating system
- coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C4/00—Coating by spraying the coating material in the molten state, e.g. by flame, plasma or electric discharge
- C23C4/02—Pretreatment of the material to be coated, e.g. for coating on selected surface areas
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C14/00—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material
- C23C14/02—Pretreatment of the material to be coated
- C23C14/021—Cleaning or etching treatments
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02T—CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y02T50/00—Aeronautics or air transport
- Y02T50/60—Efficient propulsion technologies, e.g. for aircraft
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US10386287A | 1987-10-01 | 1987-10-01 |
Publications (3)
Publication Number | Publication Date |
---|---|
GB8822837D0 true GB8822837D0 (en) | 1989-11-08 |
GB2222179A GB2222179A (en) | 1990-02-28 |
GB2222179B GB2222179B (en) | 1992-04-08 |
Family
ID=22297411
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB8822837A Expired - Fee Related GB2222179B (en) | 1987-10-01 | 1988-09-29 | Protective coatings for metallic articles |
Country Status (2)
Country | Link |
---|---|
FR (1) | FR2638156B1 (en) |
GB (1) | GB2222179B (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN113173694A (en) * | 2021-03-26 | 2021-07-27 | 曲面超精密光电(深圳)有限公司 | Manufacturing method of vehicle-mounted curved glass cover plate thermal forming die |
Families Citing this family (15)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
IT1251168B (en) * | 1991-08-09 | 1995-05-04 | Sviluppo Materiali Spa | THERMAL BARRIER IN CERAMIC MATERIAL FOR BRAKING DEVICES |
US5236745A (en) * | 1991-09-13 | 1993-08-17 | General Electric Company | Method for increasing the cyclic spallation life of a thermal barrier coating |
DE4238369C2 (en) * | 1992-11-13 | 1996-09-26 | Mtu Muenchen Gmbh | Component made of a metallic base substrate with a ceramic coating |
GB9617267D0 (en) * | 1996-08-16 | 1996-09-25 | Rolls Royce Plc | A metallic article having a thermal barrier coating and a method of application thereof |
US6012830A (en) * | 1998-06-23 | 2000-01-11 | Valeo Sylvania L.L.C. | Light shield for a vehicle headlamp |
DE102006004769B4 (en) * | 2006-02-02 | 2022-05-25 | Mercedes-Benz Group AG | Surface conditioning for thermal spray coatings |
GB2475064B (en) * | 2009-11-04 | 2011-12-14 | Rolls Royce Plc | A method of producing an oxide coated nickel-base superalloy and a method of producing an oxide dispersion strengthened nickel-base superalloy |
WO2015130526A2 (en) | 2014-02-25 | 2015-09-03 | Siemens Aktiengesellschaft | Turbine component thermal barrier coating with crack isolating engineered groove features |
US8939706B1 (en) | 2014-02-25 | 2015-01-27 | Siemens Energy, Inc. | Turbine abradable layer with progressive wear zone having a frangible or pixelated nib surface |
US9151175B2 (en) | 2014-02-25 | 2015-10-06 | Siemens Aktiengesellschaft | Turbine abradable layer with progressive wear zone multi level ridge arrays |
US9243511B2 (en) | 2014-02-25 | 2016-01-26 | Siemens Aktiengesellschaft | Turbine abradable layer with zig zag groove pattern |
EP3259452A2 (en) | 2015-02-18 | 2017-12-27 | Siemens Aktiengesellschaft | Forming cooling passages in combustion turbine superalloy castings |
US10190435B2 (en) | 2015-02-18 | 2019-01-29 | Siemens Aktiengesellschaft | Turbine shroud with abradable layer having ridges with holes |
DE102015213162A1 (en) | 2015-07-14 | 2017-01-19 | MTU Aero Engines AG | Process for the galvanic coating of TiAl alloys |
CN108342676B (en) * | 2018-02-28 | 2020-03-31 | 江苏大学 | Preparation process of thermal barrier coating of aero-engine blade |
Family Cites Families (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB631362A (en) * | 1940-11-25 | 1949-11-01 | Metallizing Engineering Co Inc | Apparatus for conditioning metal surfaces for spray metal bonding |
FR1431769A (en) * | 1965-02-01 | 1966-03-18 | Comp Generale Electricite | Process for the protection of metals and alloys |
FR1453390A (en) * | 1965-07-27 | 1966-06-03 | Gkn Group Services Ltd | Improvements to processes for continuous galvanizing of elongated metal articles |
DE1282412B (en) * | 1965-12-11 | 1968-11-07 | Siemens Ag | Process for the production of superconducting tapes with inner layers made of a superconducting two-component intermetallic compound |
US4068025A (en) * | 1971-03-22 | 1978-01-10 | Brown, Boveri & Company Limited | Method of applying a protective coating to a body |
JPS58176221A (en) * | 1982-04-09 | 1983-10-15 | Permelec Electrode Ltd | Production of coated electrolytic ion exchange membrane |
JPS6050157A (en) * | 1983-08-30 | 1985-03-19 | Toshiba Eng Co Ltd | Method for spraying thermal metal |
US4818559A (en) * | 1985-08-08 | 1989-04-04 | Sumitomo Chemical Company, Limited | Method for producing endosseous implants |
DE3724626A1 (en) * | 1986-07-31 | 1988-02-04 | Mitsubishi Heavy Ind Ltd | Coated blade for steam turbines and coating method to be used therefor |
JPS63118058A (en) * | 1986-11-05 | 1988-05-23 | Toyota Motor Corp | Member thermally sprayed with ceramic and its production |
-
1988
- 1988-09-29 GB GB8822837A patent/GB2222179B/en not_active Expired - Fee Related
- 1988-10-25 FR FR8813935A patent/FR2638156B1/en not_active Expired - Fee Related
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN113173694A (en) * | 2021-03-26 | 2021-07-27 | 曲面超精密光电(深圳)有限公司 | Manufacturing method of vehicle-mounted curved glass cover plate thermal forming die |
Also Published As
Publication number | Publication date |
---|---|
GB2222179B (en) | 1992-04-08 |
FR2638156B1 (en) | 1992-10-23 |
FR2638156A1 (en) | 1990-04-27 |
GB2222179A (en) | 1990-02-28 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0286755A3 (en) | Coating feeder system | |
GB2204881B (en) | Overlay coating | |
GB8819032D0 (en) | Independent wheel-suspension system | |
GB2206591B (en) | Coatings | |
GB8822837D0 (en) | Coating system | |
GB2239410B (en) | Coating apparatus | |
GB8727938D0 (en) | Carton-packaging systems & processes | |
GB8710318D0 (en) | Turret system | |
GB8708800D0 (en) | Constructional system | |
GB2202480B (en) | Coating for structures | |
GB8703925D0 (en) | Coated fitting | |
GB8910132D0 (en) | Coating system | |
AU103530S (en) | Coat | |
IE871686L (en) | Bath coating system | |
GB8705049D0 (en) | Minehunting systems | |
GB8722170D0 (en) | Tele-management systems | |
GB8722624D0 (en) | Tether-management systems | |
CS623687A1 (en) | Stavebnicovy system podlahove vpusti | |
CS224187A1 (en) | Mazaci system turbodmychadla preplnovaneho plynoveho spalovaciho motoru | |
CS303787A1 (en) | Regeneracni horakovy system | |
CS288387A1 (en) | Kapacitni system hydrostaticke nivelace | |
CS25987A1 (en) | Chladici system vrtaciho vretene | |
GB8716097D0 (en) | Radio-phone system | |
KR890009445Y1 (en) | Robot-arm coating apparatus | |
ZA884352B (en) | Coatings |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PCNP | Patent ceased through non-payment of renewal fee |
Effective date: 19920929 |