GB632991A - Improvements in electric welding - Google Patents
Improvements in electric weldingInfo
- Publication number
- GB632991A GB632991A GB1302746A GB1302746A GB632991A GB 632991 A GB632991 A GB 632991A GB 1302746 A GB1302746 A GB 1302746A GB 1302746 A GB1302746 A GB 1302746A GB 632991 A GB632991 A GB 632991A
- Authority
- GB
- United Kingdom
- Prior art keywords
- run
- runs
- droplet
- arc
- electric welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
632,991. Uniting by fusion. INTERNATIONAL COMBUSTION, Ltd., POOLE, F., and BAWDEN, E. April 30, 1946, No. 13027. [Class 83 (iv)] In arc welding, particularly circumferential joints for fluid-pressure tubes, the initial runs 1, 2, 3 are deposited in a plurality of circumferentially extending superimposed parallel layers, the arc being broken at regular intervals, for example 40 times per inch of run. Each droplet and run is allowed to cool slightly before the deposition of the next droplet or run respectively, and the sealing run 1 completely fills the gap between the parts. The remainder of the weld is completed in the runs 4-11 in normal manner.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB1302746A GB632991A (en) | 1946-04-30 | 1946-04-30 | Improvements in electric welding |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB1302746A GB632991A (en) | 1946-04-30 | 1946-04-30 | Improvements in electric welding |
Publications (1)
Publication Number | Publication Date |
---|---|
GB632991A true GB632991A (en) | 1949-12-05 |
Family
ID=10015468
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB1302746A Expired GB632991A (en) | 1946-04-30 | 1946-04-30 | Improvements in electric welding |
Country Status (1)
Country | Link |
---|---|
GB (1) | GB632991A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0005945A1 (en) * | 1978-05-30 | 1979-12-12 | Grootcon (U.K.) Limited | Method of welding metal parts |
FR2829049A1 (en) * | 2001-09-04 | 2003-03-07 | Commissariat Energie Atomique | Soldering method with relaxation of residual stresses comprises depositing soldering bead in joint with first deposit pass of junction part and second deposit pass filling joint |
-
1946
- 1946-04-30 GB GB1302746A patent/GB632991A/en not_active Expired
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0005945A1 (en) * | 1978-05-30 | 1979-12-12 | Grootcon (U.K.) Limited | Method of welding metal parts |
US4314132A (en) | 1978-05-30 | 1982-02-02 | Grootcon (U.K.) Limited | Arc welding cupro nickel parts |
FR2829049A1 (en) * | 2001-09-04 | 2003-03-07 | Commissariat Energie Atomique | Soldering method with relaxation of residual stresses comprises depositing soldering bead in joint with first deposit pass of junction part and second deposit pass filling joint |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1347528A (en) | Welding heads | |
GB1052407A (en) | ||
GB632991A (en) | Improvements in electric welding | |
CH259521A (en) | Electrode for welding nickel-chromium alloys. | |
GB972338A (en) | Improvements in and relating to welded rotors of rotary machines | |
SU111056A2 (en) | Method of multi-electrode arc welding | |
GB615986A (en) | Improvements in joints for sheet piles | |
FR2388627A1 (en) | Multipass mig butt welding thick plates - using constant height for nozzle through which consumable electrode wire passes | |
GB166245A (en) | Piston rings | |
GB572043A (en) | Welding ring and method of making same | |
GB589742A (en) | An improved method of and apparatus for cutting metal plates preparatory to welding said plates to metal surfaces | |
GB758368A (en) | Process for protecting the joints of metal pipes coated with multi-layer protecting thermoplastic coverings | |
CA404436A (en) | Direct current generator for arc welding | |
AU122708B2 (en) | Improvements relating to torches for welding, brazing and the like | |
CA188766A (en) | Pipe joint machine | |
DK75788C (en) | Welding torch for arc welding. | |
CA187105A (en) | Gas recovering machine | |
GB527223A (en) | Improvements in or relating to fusion welding | |
CA403198A (en) | Arc welding electrode | |
GB179381A (en) | Improvements in and relating to elastic fluid turbines and methods of manufacturing the same | |
CA424991A (en) | Arc welding method | |
CA402488A (en) | Seam weld | |
CA194258A (en) | Sealing machine | |
CA403465A (en) | Arc welding method | |
AU117513B2 (en) | An improved control for welding torches |