Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
GB29402/32A
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
MAX LANGENOHI
Original Assignee
MAX LANGENOHI
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by MAX LANGENOHIfiledCriticalMAX LANGENOHI
Publication of GB401875ApublicationCriticalpatent/GB401875A/en
B22D—CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
B22D13/00—Centrifugal casting; Casting by using centrifugal force
B22D13/02—Centrifugal casting; Casting by using centrifugal force of elongated solid or hollow bodies, e.g. pipes, in moulds rotating around their longitudinal axis
Landscapes
Engineering & Computer Science
(AREA)
Mechanical Engineering
(AREA)
Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces
(AREA)
Abstract
The hardening of centrifugally cast tubes is eliminated by embedding the tube, after extraction from the mould and while still glowing, in a mixture of finely distributed zinc and iron, which materials may be heated to a temperature below their melting points and below that of the cast tube.
GB29402/32A1932-02-221932-10-20Improvements in the production of centrifugally chill-cast tubes that are not hard