GB1290127A - - Google Patents
Info
- Publication number
- GB1290127A GB1290127A GB1290127DA GB1290127A GB 1290127 A GB1290127 A GB 1290127A GB 1290127D A GB1290127D A GB 1290127DA GB 1290127 A GB1290127 A GB 1290127A
- Authority
- GB
- United Kingdom
- Prior art keywords
- slag
- submerged arc
- flux
- granulated
- starting powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
1290127 Granulated submerged arc flux LINDE AG 29 June 1971 [1 July 1970] 30363/71 Heading C7M A granulated submerged arc flux made by adding an atomized liquid to dry powders and optionally roasting, in which the starting powder contains one or more slags from a submerged arc welding process. The starting powder may contain 100% slag or 20-50% slag with other flux additions. The slag particle size is preferably not more than 0À2 mm.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DE2032794A DE2032794C3 (en) | 1970-07-01 | 1970-07-01 | Process for producing a welding powder for submerged arc welding |
Publications (1)
Publication Number | Publication Date |
---|---|
GB1290127A true GB1290127A (en) | 1972-09-20 |
Family
ID=5775601
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB1290127D Expired GB1290127A (en) | 1970-07-01 | 1971-06-29 |
Country Status (7)
Country | Link |
---|---|
BE (1) | BE767676A (en) |
CH (1) | CH524425A (en) |
DE (1) | DE2032794C3 (en) |
FR (1) | FR2097980A5 (en) |
GB (1) | GB1290127A (en) |
NL (1) | NL169558C (en) |
ZA (1) | ZA713798B (en) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
AU541161B2 (en) * | 1980-10-30 | 1984-12-20 | Lincoln Electric Company, The | Welding flux |
CN118362600B (en) * | 2024-06-17 | 2024-09-06 | 东北大学 | Flux crystallization performance analysis method, device and application |
-
1970
- 1970-07-01 DE DE2032794A patent/DE2032794C3/en not_active Expired
-
1971
- 1971-05-13 CH CH714871A patent/CH524425A/en not_active IP Right Cessation
- 1971-05-26 BE BE767676A patent/BE767676A/en unknown
- 1971-06-11 ZA ZA713798A patent/ZA713798B/en unknown
- 1971-06-18 FR FR7122245A patent/FR2097980A5/fr not_active Expired
- 1971-06-29 GB GB1290127D patent/GB1290127A/en not_active Expired
- 1971-06-30 NL NLAANVRAGE7109034,A patent/NL169558C/en not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
CH524425A (en) | 1972-06-30 |
DE2032794B2 (en) | 1973-03-29 |
FR2097980A5 (en) | 1972-03-03 |
ZA713798B (en) | 1972-02-23 |
DE2032794A1 (en) | 1972-01-05 |
NL7109034A (en) | 1972-01-04 |
NL169558C (en) | 1982-08-02 |
BE767676A (en) | 1971-10-18 |
DE2032794C3 (en) | 1973-10-18 |
NL169558B (en) | 1982-03-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1290127A (en) | ||
GB1075810A (en) | Method of manufacturing small castings of ferroalloy | |
JPS5249915A (en) | Production process of sintered alloy containing titanium | |
JPS5269807A (en) | Recovering of powder of ferromagnetic metal or alloy | |
CA973330A (en) | Production of pure metals, metal oxides and metal chlorides from alloys or scraps | |
CA970998A (en) | Lead-impregnated sintered ferrous alloy | |
JPS5348912A (en) | Water-crushed shot of high carbon ferrochromium and its preparation | |
JPS5228417A (en) | Method of preparing metallic chromium from ferrochromium | |
ES406097A1 (en) | Method of sintering iron, copper tin alloys followed by slow cooling | |
JPS51123712A (en) | A furnace for quick and continuous melting of low-melting metals | |
JPS51117103A (en) | Alloy wire material for addition of rare earth | |
ES156160U (en) | An electrode device for welding the arc electric in the air. (Machine-translation by Google Translate, not legally binding) | |
JPS5253704A (en) | Method of operation of sintering | |
JPS525610A (en) | Process for producing unsintered briquetted ore | |
JPS5269805A (en) | Dipping body formolten metal | |
CA883221A (en) | Metal alloy | |
JPS53132424A (en) | Magnetic iron-cobalt alloy | |
AU436602B2 (en) | Production f iron oxide from non-ferrous metal bearing cinder having high magnette content | |
JPS5220909A (en) | Composition of carbon containing metal oxide and iron-base alloy | |
Leibov et al. | Metallurgical Compensation of Iron in the Secondary AL-9 V Alloy | |
AU6247869A (en) | Production f iron oxide from non-ferrous metal bearing cinder having high magnette content | |
CA678294A (en) | Production of compositions of dispersed refractory metal oxides in metals | |
CA607761A (en) | High temperature powdered metal torch | |
CA591180A (en) | Process for improving parts formed by powder metallurgy by addition of spiegeleisen to metal powders | |
JPS52111811A (en) | Preparation of sintered ore of low zinc content |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PS | Patent sealed | ||
PCNP | Patent ceased through non-payment of renewal fee |