FR2351922A1 - Procede pour ameliorer la resistance d'un verre de scellement - Google Patents
Procede pour ameliorer la resistance d'un verre de scellementInfo
- Publication number
- FR2351922A1 FR2351922A1 FR7616130A FR7616130A FR2351922A1 FR 2351922 A1 FR2351922 A1 FR 2351922A1 FR 7616130 A FR7616130 A FR 7616130A FR 7616130 A FR7616130 A FR 7616130A FR 2351922 A1 FR2351922 A1 FR 2351922A1
- Authority
- FR
- France
- Prior art keywords
- improving
- resistance
- sealing glass
- sealing
- glass
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000000034 method Methods 0.000 title 1
- 239000005394 sealing glass Substances 0.000 title 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C15/00—Surface treatment of glass, not in the form of fibres or filaments, by etching
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C8/00—Enamels; Glazes; Fusion seal compositions being frit compositions having non-frit additions
- C03C8/24—Fusion seal compositions being frit compositions having non-frit additions, i.e. for use as seals between dissimilar materials, e.g. glass and metal; Glass solders
Landscapes
- Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Geochemistry & Mineralogy (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Glass Compositions (AREA)
- Surface Treatment Of Glass (AREA)
- Joining Of Glass To Other Materials (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US05/590,651 US3975175A (en) | 1975-06-26 | 1975-06-26 | Process for increasing the strength of sealing glass |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| FR2351922A1 true FR2351922A1 (fr) | 1977-12-16 |
| FR2351922B1 FR2351922B1 (enExample) | 1980-10-10 |
Family
ID=24363095
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| FR7616130A Granted FR2351922A1 (fr) | 1975-06-26 | 1976-05-21 | Procede pour ameliorer la resistance d'un verre de scellement |
Country Status (5)
| Country | Link |
|---|---|
| US (1) | US3975175A (enExample) |
| JP (1) | JPS5842139B2 (enExample) |
| DE (1) | DE2622141A1 (enExample) |
| FR (1) | FR2351922A1 (enExample) |
| GB (1) | GB1541704A (enExample) |
Families Citing this family (13)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4078923A (en) * | 1977-03-08 | 1978-03-14 | Xerox Corporation | Migration imaging with surfactant-modified solvent development |
| US4199337A (en) * | 1978-10-06 | 1980-04-22 | International Telephone And Telegraph Corporation | Method of fabricating high strength optical preforms |
| US4898777A (en) * | 1989-01-24 | 1990-02-06 | Infrared Fiber Systems | High-strength fluoride glass fibers and process of making |
| DE4009602A1 (de) * | 1990-03-26 | 1991-10-02 | Ivoclar Ag | Polymerisierbare dentalmasse |
| DE69935070T2 (de) * | 1998-03-31 | 2007-05-31 | Hitachi Ltd. | Anzeigetafel |
| DE102010035251B4 (de) * | 2010-02-15 | 2013-09-26 | Schott Ag | Hochtemperatur-Glaslot und dessen Verwendung |
| TWI612017B (zh) | 2011-11-10 | 2018-01-21 | 康寧公司 | 玻璃的酸強化 |
| US10273048B2 (en) | 2012-06-07 | 2019-04-30 | Corning Incorporated | Delamination resistant glass containers with heat-tolerant coatings |
| RU2674269C2 (ru) | 2012-06-07 | 2018-12-06 | Корнинг Инкорпорейтед | Стойкие к расслаиванию стеклянные контейнеры |
| US9034442B2 (en) | 2012-11-30 | 2015-05-19 | Corning Incorporated | Strengthened borosilicate glass containers with improved damage tolerance |
| US10117806B2 (en) | 2012-11-30 | 2018-11-06 | Corning Incorporated | Strengthened glass containers resistant to delamination and damage |
| CN107074628B (zh) | 2014-09-05 | 2020-05-19 | 康宁股份有限公司 | 玻璃制品和用于改善玻璃制品的可靠性的方法 |
| US10065884B2 (en) * | 2014-11-26 | 2018-09-04 | Corning Incorporated | Methods for producing strengthened and durable glass containers |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| NL111359C (enExample) * | 1956-05-29 | 1900-01-01 | ||
| US3023139A (en) * | 1957-03-16 | 1962-02-27 | Floris Van Tetterode And Jan D | Method of strengthening sheet glass in agitated liquid fluoride bath |
| US3281294A (en) * | 1965-06-08 | 1966-10-25 | Corning Glass Works | Method for etching glass |
| NL6817661A (enExample) * | 1968-12-10 | 1970-06-12 | ||
| BE790476A (fr) * | 1971-10-29 | 1973-04-24 | Champion Spark Plug Co | Procede de preparation d'emaux au plomb |
| JPS5130564B2 (enExample) * | 1972-10-09 | 1976-09-01 |
-
1975
- 1975-06-26 US US05/590,651 patent/US3975175A/en not_active Expired - Lifetime
-
1976
- 1976-05-19 DE DE19762622141 patent/DE2622141A1/de not_active Withdrawn
- 1976-05-21 FR FR7616130A patent/FR2351922A1/fr active Granted
- 1976-06-11 JP JP51067874A patent/JPS5842139B2/ja not_active Expired
- 1976-06-22 GB GB25778/76A patent/GB1541704A/en not_active Expired
Also Published As
| Publication number | Publication date |
|---|---|
| DE2622141A1 (de) | 1977-01-20 |
| FR2351922B1 (enExample) | 1980-10-10 |
| US3975175A (en) | 1976-08-17 |
| JPS5842139B2 (ja) | 1983-09-17 |
| GB1541704A (en) | 1979-03-07 |
| JPS525815A (en) | 1977-01-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| FR2326549A1 (fr) | Materiau de vitrage reflechissant l'infrarouge | |
| FR2320275A1 (fr) | Procede perfectionne pour l'attaque chimique du verre | |
| FR2296798A1 (fr) | Procede de realisation d'un joint d'etancheite | |
| FR2310862A1 (fr) | Procede de realisation d'un joint d'etancheite | |
| FR2299895A1 (fr) | Procede pour la | |
| FR2309484A1 (fr) | Composition de verre de scellement et procede de scellement | |
| FR2300964A1 (fr) | Procede d'ali | |
| FR2297978A1 (fr) | Procede d'installation d' | |
| FR2353502A1 (fr) | Procede de soudage d'elements de saphir sur du verre | |
| BE839483A (fr) | Procede d'ammonoxydation | |
| FR2302983A1 (fr) | Procede pour l'obtention de n-acyl-l-methionine | |
| FR2351922A1 (fr) | Procede pour ameliorer la resistance d'un verre de scellement | |
| FR2306176A1 (fr) | Procede et appareil pour le revetement metallique d'une feuille de verre | |
| BE862106A (fr) | Procede de preparation d'electro-corindon fondu | |
| RO71280A (ro) | Procedeu pentru prepararea etilenglicolului | |
| FR2309535A1 (fr) | Procede pour l'obtention de 3-methylpyridine | |
| FR2296933A1 (fr) | Procede de scellement d'une tubulure comportant un verre de scellement preforme | |
| FR2310520A1 (fr) | Procede d'execution de raccords | |
| FR2317760A1 (fr) | Procede pour la production d'ampoules a vide | |
| BE839503A (fr) | Procede d'enduction de bouteilles de verre | |
| FR2309481A1 (fr) | Procede de preparation de verre de scellement a l'oxyde de cuivre | |
| FR2326399A1 (fr) | Procede de production d'un alcane-polyol | |
| FR2300398A1 (fr) | Procede d'aplatissement de la courbe d | |
| BE848796A (fr) | Procede d'inspection de joints, | |
| BE826924A (fr) | Procede de separation d'hydrocarbures |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| ST | Notification of lapse |