FI60253C - MALNINGSSKIVA - Google Patents

MALNINGSSKIVA Download PDF

Info

Publication number
FI60253C
FI60253C FI751095A FI751095A FI60253C FI 60253 C FI60253 C FI 60253C FI 751095 A FI751095 A FI 751095A FI 751095 A FI751095 A FI 751095A FI 60253 C FI60253 C FI 60253C
Authority
FI
Finland
Prior art keywords
dams
grinding
blade
helical
grinding disc
Prior art date
Application number
FI751095A
Other languages
Finnish (fi)
Other versions
FI60253B (en
FI751095A (en
Inventor
Esa Korri
Original Assignee
Yhtyneet Paperitehtaat Oy
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yhtyneet Paperitehtaat Oy filed Critical Yhtyneet Paperitehtaat Oy
Priority to FI751095A priority Critical patent/FI60253C/en
Publication of FI751095A publication Critical patent/FI751095A/fi
Application granted granted Critical
Publication of FI60253B publication Critical patent/FI60253B/en
Publication of FI60253C publication Critical patent/FI60253C/en

Description

Γβΐ m>KUULUTUSJULKAISU s n 0 c τ lBJ (11) UTLAGGNINGSSKMFT 602 5 3 C «*> ^ v ^ (51) K*.ik.3/iBta3 D 21 D 1/30 SUOM I —FI N LAN D (21) P*t*nttH>»k*mu* —P*t*nt»n»eiii>»nj 751095 (22) HakembpUvl —An*öknbipd»j ll.OU.75 ' ' (23) Aikupilvt—Glltl|hM*dag ll.OU.75 (41) Tullut JulkiMlul — Bllvtt affamlig 12.10 76 II**""***" r®^i»terihmllitul NIht*v*k»Jp«non μ kiiuL|ulk*l«in pvm. — ·,. 0g o-.Γβΐ m> AD PUBLICATION sn 0 c τ lBJ (11) UTLAGGNINGSSKMFT 602 5 3 C «*> ^ v ^ (51) K * .ik.3 / iBta3 D 21 D 1/30 ENGLISH I —FI N LAN D (21) P * t * nttH> »k * mu * —P * t * nt» n »eiii>» nj 751095 (22) HakembpUvl —An * öknbipd »j ll.OU.75 '' (23) Aikupilvt — Glltl | hM * dag ll.OU.75 (41) Tullut JulkiMlul - Bllvtt affamlig 12.10 76 II ** "" *** "r® ^ i» terihmllitul NIht * v * k »Jp« non μ kiiuL | ulk * l «in pvm . - ·, .0g o-.

Patent- och regirtarityralMn ' 7 AmHim uthfd odt utUkrifUn publkarad 31.0Ö.Ö1 (32)(33)(31) Pyydetty «uoMmii*—Begird priori»·» (71) Yhtyneet Paperitehtaat Oy, Jylhävaara, 37620 Valkeakoski, Suomi-Finland(FI) (72) Esa Korri, Valkeakoski, Suomi-Finland(Fl) (7U) Oy Heinänen Ah (5U) Jauhinkiekko - Malningsskiva Tämän keksinnön kohteena on jauhinkiekko selluloosa-, paperi- tai sentapaista massasuspensiota varten, jonka jauhinkiekon jauhinpinnassa on säteettäisiä teräuria ja näiden välissä teräharjoja, jotka teräurai on ryhmitelty säteen suunnassa peräkkäisiksi vyöhykkeiksi, jotka on erotettu toisistaan kaarimaisilla padoilla, joiden korkeus on yhtä suuri kuin teräharjojen korkeus ja jotka sijaitsevat poikittain sädettä vastaan.Patent- och regirtarityralMn '7 AmHim uthfd odt utUkrifUn publkarad 31.0Ö.Ö1 (32) (33) (31) Requested «uoMmii * —Begird priori» · »(71) Yhtyneet Paperitehtaat Oy, Jylhävaara, 37620 Valkeakoski, Finland-Finland ( FI: (72) Esa Korri, Valkeakoski, Suomi-Finland (Fl) (7U) Oy Heinänen Ah (5U) Grinding disc - Malningsskiva The present invention relates to a grinding disc for a pulp suspension of cellulose, paper or the like having radial blade grooves in the grinding surface of the grinding disc and between them, the blade ridges, the blade groove being grouped in radially successive zones separated by arcuate dams having a height equal to the height of the blade ridges and located transversely to the radius.

On todettu, että tällaisten jauhinkiakkojen teräharjoissa tapahtuu kuluminen nopeimmin massasuspension virtaussuuntaan katsottuna juuri ennen patoja. Koska padot ovat kehän suuntaisia eli kohtisuorassa sädettä vastaan, muodostuu patojen eteen samoin kehän suuntainen kulunut vyöhyke. Kuluminen tapahtuu samalla tavoin molemmissa toistensa kanssa yhteistoiminnassa olevissa terissä. Näin ollen tässä kuluneessa vyöhykkeessä voi massasuspensio siirtyä teräurasta toiseen ilman, että jauhettavat partikkelit joutuisivat teräharjojen jauhatusvaikutuksen alaiseksi.It has been found that the blade brushes of such grinding hooks wear out most rapidly in the direction of flow of the pulp suspension just before the dams. Since the dams are circumferential, i.e. perpendicular to the radius, a circumferentially worn zone is also formed in front of the dams. Wear occurs in the same way on both co-operating blades. Thus, in this worn zone, the pulp suspension can move from one blade groove to another without the particles to be ground being subjected to the grinding effect of the blade brushes.

Tämän keksinnön tarkoituksena on pienentää edellä mainittua epäkohtaa.The object of the present invention is to reduce the above-mentioned drawback.

2 602532 60253

Keksinnölle on tunnusomaista se, että padot sijaitsevat kierukkamai-sesti niin, että niiden toinen pää on lähempänä jauhinkiekon akselia kuin vastakkainen pää.The invention is characterized in that the dams are helically arranged so that one end is closer to the axis of the grinding wheel than the opposite end.

Keksinnön mukaisessa jauhinkiekossa kuluvat teräharjat myös eniten juuri ennen patoja. Mutta koska padot sijaitsevat kierukkamaisesti, ei kulunut vyöhyke ole kehän suuntainen, vaan vinossa asennossa siihen nähden. Nain ollen teräharjojen kuluneet vyöhykkeet eivät sijaitse kohdakkain, minkä takia jauhettavien partikkeleiden on vaikeampi siirtyä teräurasta toiseen joutumatta teräharjojen jauhatusvaikutuksen alaiseksi, Molemmat jauhinpinnat muodostetaan sopivimmin samanlaisiksi.In the grinding disc according to the invention, the blade brushes also wear the most just before the dams. But because the dams are helically located, the worn zone is not circumferential, but in an oblique position relative to it. Thus, the worn zones of the blade brushes are not aligned, which makes it more difficult for the particles to be ground to move from one blade groove to another without being subjected to the grinding effect of the blade brushes. Both refining surfaces are preferably formed to be similar.

Keksinnön erään edullisen sovellutusmuodon mukaan kierukkamaisten patojen nousukulma on noin 15-30°. Kierukkamaiset padot voivat alkaa jauhinpinnan sisäkehästä ja ulottua yhtenäisinä jauhinpinnan ulkokehään saakka.According to a preferred embodiment of the invention, the pitch angle of the helical dams is about 15-30 °. The helical dams can start from the inner circumference of the refining surface and extend uniformly to the outer circumference of the refining surface.

Keksintöä selostetaan seuraavassa esimerkin avulla viittaamalla oheiseen piirustukseen, jossaThe invention will now be described by way of example with reference to the accompanying drawing, in which

Kuv. 1 esittää jauhinkiekon yhtä sektoria jauhinpinnan puolelta katsottuna.Fig. 1 shows one sector of the refining disc seen from the side of the refining surface.

Kuv. 2 esittää kuviosta 1 pitkin viivaa II-II otettua leikkausta.Fig. 2 shows a section taken along the line II-II in Fig. 1.

Kuv. 3 esittää kuviosta 1 pitkin viivaa III-III otettua leikkausta.Fig. 3 shows a section taken along the line III-III in Fig. 1.

Massanjauhin muodostuu kahdesta jauhinkiekosta, joiden jauhinpintojen väliin muodostuu jauhinrako. Jauhinkiekoista ainakin toinen pyörii. Jauhettava massasuspensio virtaa jauhinpintojen välissä säteen suunnassa akselilta kehälle päin.The pulp refiner consists of two refining discs with a refining gap formed between the refining surfaces. At least one of the grinding wheels rotates. The pulp suspension to be ground flows radially between the grinding surfaces from the axis to the circumference.

Jauhinkiekko on yleensä koottu sektoreista, joista yksi on esitetty kuviossa 1. Jauhinkiekon jauhinpinnassa on säteettäisiä teräuria 1 ja näiden välissä teräharjoja 2. Teräurat on ryhmitelty säteen suunnassa peräkkäisiksi vyöhykkeiksi 3-6, jotka on erotettu toisistaan kaarimai-silla padoilla 7. Teräurien 1 leveys ja syvyys on erilainen eri vyöhykkeissä 3-6 pienentyen massasuspension virtaussuunnassa eli kehää kohti mentäessä. Patojen 7 korkeus on yhtä suuri kuin teräharjojen 2 korkeus.The grinding disc is generally assembled from sectors, one of which is shown in Figure 1. The grinding surface of the grinding disc has radial blade grooves 1 and between them blade brushes 2. The blade grooves are grouped in radially successive zones 3-6 separated by arcuate dams 7. the depth is different in different zones 3-6, decreasing in the direction of flow of the pulp suspension, i.e. towards the circumference. The height of the dams 7 is equal to the height of the blade brushes 2.

3 602533 60253

Keksinnön mukaan padot 7 sijaitsevat kierukkamaisesti niin, että niiden toinen pää on lähempänä jauhinkiekon akselia kuin vastakkainen pää. Tällä saadaan aikaan se, että teräharjojen 2 kuluneimmat kohdat, jotka sijaitsevat juuri ennen patoa 7, ovat vierekkäsissä teräharjoissa eri etäisyyksillä toisistaan. Täten pienennetään sitä mahdollisuutta, että jauhettavat partikkelit pääsisivät siirtymään teräurasta 1 toiseen joutumatta teräharjojen jauhatusvaikutuksen alaiseksi.According to the invention, the dams 7 are helically arranged so that their one end is closer to the axis of the grinding wheel than the opposite end. This ensures that the most worn points of the blade brushes 2, which are located just before the dam 7, are in adjacent blade brushes at different distances from each other. This reduces the possibility that the particles to be ground could move from one blade groove 1 to another without being subjected to the grinding effect of the blade brushes.

Piirustuksen mukaan on patojen 7 nousukulma noin 20°, mutta tämä kulma voi luonnollisesti keksinnön puitteissa vaihdella laajoissa rajoissa.According to the drawing, the angle of inclination of the dams 7 is about 20 °, but this angle can, of course, vary within wide limits within the scope of the invention.

Piirustuksen mukaan teholliseen jauhinpintaan kuuluvat lähinnä jauha-tusvyöhykkeet 4, 5 ja 6. Kierukkamaiset padot 7 alkavat tehollisen jauhinpinnan sisäkehästä ja ulottuvat yhtenäisinä jauhinpinnan ulkokehään saakka. Tämä ei kuitenkaan ole välttämätöntä, vaan padot 7 voidaan jakaa kahdeksi tai useammaksi osaksi.According to the drawing, the effective grinding surface mainly comprises grinding zones 4, 5 and 6. The helical dams 7 start from the inner circumference of the effective grinding surface and extend uniformly to the outer circumference of the grinding surface. However, this is not necessary, but the dams 7 can be divided into two or more parts.

Piirustuksessa on esitetty ainoastaan yksi jauhinkiekon sektori. Tähän liitetään viereiset sektorit niin, että padot 7 jatkuvat yhtenäisenä sektorista toiseen.Only one sector of the grinding wheel is shown in the drawing. Adjacent sectors are connected to this so that the dams 7 continue as one unit from one sector to another.

Keksinnön mukaan on sopivinta, joskaan ei välttämätöntä, että molempien jauhinkiekkojen jauhinpinnat ovat keskenään samanlaiset. Tällöin voivat kierukkamaiset padot 7 nousta samaan suuntaan tai eri suuntiin riippuen siitä, kuinka voimakas pumppaava vaikutus jauhinpinnnöilla halutaan saada aikaan.According to the invention, it is most suitable, although not necessary, that the grinding surfaces of the two grinding wheels be identical. In this case, the helical dams 7 can rise in the same direction or in different directions, depending on how strong the pumping effect with the grinding surfaces is to be obtained.

Alan ammattimiehelle on selvää, että keksinnön erilaiset sovellutus-muodot voivat vaihdella jäljempänä esitettävien patenttivaatimusten puitteissa. Edellä on keksintöä selostettu kiekkojauhimeen sovellettuna. Mutta aivan ilmeisesti keksinnön perusajatus on sovellettavissa myös kartiojauhimeen.It will be apparent to those skilled in the art that various embodiments of the invention may vary within the scope of the claims set forth below. The invention has been described above as applied to a disc mill. But quite obviously the basic idea of the invention is also applicable to a conical refiner.

Piirustuksessa on esitetty neljä jauhatusvyöhykettä 3-6, mutta näiden lukumäärä voi luonnollisesti vaihdella.Four grinding zones 3-6 are shown in the drawing, but the number of these may, of course, vary.

Claims (3)

4 60253 Jauhinkiekko selluloosa-, paperi- tai sen tapaista massasuspensiota varten, jonka jauhinkiekon jauhinpinnassa on säteettäisiä teräuria (1) ja näiden välissä teräharjoja (2), jotka teräurat on ryhmitelty säteen suunnassa peräkkäisiksi vyöhykkeiksi (3-6), jotka on erotettu toisistaan kaarimaisilla padoilla (7), joiden korkeus on yhtä suuri kuin teräharjojen korkeus ja jotka sijaitsevat poikittain sädettä vastaan, tunnettu siitä, että padot (7) sijaitsevat kierukkamaisesti niin, että niiden toinen pää on lähempänä jauhinkiekon akselia kuin vastakkainen pää, jolloin vastaavasti porrastuneet teräharjat (2) jauhavat paremmin.4 60253 Grinding disc for pulp suspension of cellulose, paper or the like, having radial blade grooves (1) on the grinding surface of the grinding disc and blade brushes (2) between them, the blade grooves being grouped in radially successive zones (3-6) separated by curves with dams (7) having a height equal to the height of the blade brushes and located transversely to the beam, characterized in that the dams (7) are helically arranged so that one end is closer to the axis of the grinding wheel than the opposite end, the stepped blade brushes (2) ) grind better. 1. Mainingsskiva för cellulosa-, pappers- el. dyl. massasuspension, vilken malningsskiva uppvisar i malningsytan radiella bettspär (1) och mellan dessa bettäsar (2), vilka bettspär är grupperade i radiell riktning efter varandra följande zoner (3-6), vilka är iso-lerade frän varandra medelst bägformiga vallar (7), vilkas höjd är lika med bettäsarnas höjd och som är tvärställda mot radien, kännetecknad därav, att vallarna (7) befinner sig spi-ralformigt sä att deras ena ände är belägen närmare malningsskivans axel än motsatta änden, varvid pä motsvarande sätt de avtrappade bettäsarna (2) malar bättre.1. Mainingsskiva för cellulosa-, pappers- el. Dyl. mass suspension, one-size-fits-all in the upper part of the area (1) and one side of the area (2), one-size-fits-all in the upper part of the area (3-6), one-size-fits-all (7) , vilkas höjd är lika med bettäsarnas höjd och som är tvärställda mot radien, kännetecknad därav, att vallarna (7) 2) malar bättre. 2. Malningsskiva enligt patentkravet 1, kännetecknad därav, att de spiralformiga vallarnas (7) stigningsvinkel är ungefär 15-30°.2. A cutting device according to claim 1, having a helical shape (7) with a helical shape of 15-30 °. 2. Patenttivaatimuksen 1 mukainen jauhinkiekko, tunnettu siitä, että kierukkamaisten patojen (7) nousukulma on noin 15-30°.Grinding disc according to Claim 1, characterized in that the angle of inclination of the helical dams (7) is approximately 15-30 °. 3. Patenttivaatimuksen 1 tai 2 mukainen jauhinkiekko, tunnet-t u siitä, että kierukkamaiset padot (7) alkavat jauhinpinnan sisä-kehästä ja ulottuvat yhtenäisinä jauhinpinnan ulkokehään saakka.Grinding disc according to Claim 1 or 2, characterized in that the helical dams (7) start from the inner circumference of the grinding surface and extend integrally to the outer circumference of the grinding surface. 3. Malningsskiva enligt patentkravet 1 eller 2, kännetecknad därav, att de spiraltormiga vallarna (7) börjar frän mal-ningsytans inre omkrets och sträcker sig enhetliga ända tili malningsytans ^ttre omkrets.3. A method according to claims 1 or 2, which comprises a spiral storm (7) according to the invention, and in this case it is possible to account for the effect.
FI751095A 1975-04-11 1975-04-11 MALNINGSSKIVA FI60253C (en)