ES8303534A1 - Un metodo de impedir el dano a una tobera sumergida - Google Patents
Un metodo de impedir el dano a una tobera sumergidaInfo
- Publication number
- ES8303534A1 ES8303534A1 ES505740A ES505740A ES8303534A1 ES 8303534 A1 ES8303534 A1 ES 8303534A1 ES 505740 A ES505740 A ES 505740A ES 505740 A ES505740 A ES 505740A ES 8303534 A1 ES8303534 A1 ES 8303534A1
- Authority
- ES
- Spain
- Prior art keywords
- tuyere
- blown
- gas
- steel making
- particulate material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
METODO PARA EVITAR EL DAÑADO DE UNA TOBERA SUMERGIDA USADA EN UN HORNO DE FABRICACION DE ACERO CON OXIGENO, EN UN PROCESO DE AFINO POR DESCARBURACION. COMPRENDE LAS SIGUIENTES ETAPAS: PRIMERA, SE FORMA UNA MEZCLA DE GAS-POLVO COMPUESTA POR UN MATERIAL EN PARTICULAS QUE EMITE GAS EN UNA CANTIDAD SUFICIENTE Y POR UN GAS PORTADOR DISTINTO DEL OXIGENO; SEGUNDA, SE INSUFLA LA MEZCLA DE GAS-POLVO EN UN BAÑO DE METAL FUNDIDO A TRAVES DE LA TOBERA SUMERGIDA, AL OBJETO DE FORMAR UNA CAPA DE DICHA MEZCLA SOBRE EL BORDE PERIFERICO INTERNO DE LA MENCIONADA TOBERA; Y POR ULTIMO, SE ENFRIA EL METAL FUNDIDO EN TORNO AL EXTREMO DE DICHA TOBERA SUMERGIDA MEDIANTE LA ABSORCION DE CALOR, OCASIONADO POR LA REACCION ENDOTERMICA DE DESCOMPOSICION DEL MATERIAL EN PARTICULAS, AL TIEMPO QUE ES AGITADO EL BAÑO DE METAL FUNDIDO POR EL CHORRO DE GAS DESPRENDIDO.
Applications Claiming Priority (4)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13396780A JPS6050844B2 (ja) | 1980-09-26 | 1980-09-26 | 溶融鉄中への酸素吹込み羽口の保護方法 |
JP13396880A JPS6027723B2 (ja) | 1980-09-26 | 1980-09-26 | 溶融鉄中への酸素吹込み羽口の保護方法 |
JP55133966A JPS6027722B2 (ja) | 1980-09-26 | 1980-09-26 | 溶融鉄へのガス吹き込み法 |
JP2516181A JPS57140810A (en) | 1981-02-23 | 1981-02-23 | Refining method for steel |
Publications (2)
Publication Number | Publication Date |
---|---|
ES505740A0 ES505740A0 (es) | 1983-02-01 |
ES8303534A1 true ES8303534A1 (es) | 1983-02-01 |
Family
ID=27458262
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES505740A Expired ES8303534A1 (es) | 1980-09-26 | 1981-09-24 | Un metodo de impedir el dano a una tobera sumergida |
Country Status (7)
Country | Link |
---|---|
US (1) | US4388113A (es) |
EP (1) | EP0049148B1 (es) |
AU (1) | AU531023B2 (es) |
BR (1) | BR8106166A (es) |
CA (1) | CA1170460A (es) |
DE (1) | DE3176581D1 (es) |
ES (1) | ES8303534A1 (es) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
ZA966811B (en) * | 1995-08-18 | 1998-02-12 | Colgate Palmolive Co | Cosmetic gel composition having reduced skin irritation. |
Family Cites Families (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2979395A (en) * | 1957-01-22 | 1961-04-11 | Kosmider Johannes | Method of preparing preliminary metal or steel pig iron containing phosphorus |
US2950186A (en) * | 1957-03-02 | 1960-08-23 | Siderurgie Fse Inst Rech | Method for top blowing pulverulent burnt lime and oxygen into cast iron for refining same |
US2991173A (en) * | 1959-02-27 | 1961-07-04 | Siderurgie Fse Inst Rech | Metal refining method and apparatus |
FR1243414A (fr) * | 1959-02-27 | 1960-10-14 | Air Liquide | Procédé d'affinage des fontes phosphoreuses par l'oxygène concentré |
LU57833A1 (es) * | 1969-01-23 | 1970-07-29 | ||
LU58309A1 (es) * | 1969-02-27 | 1969-07-15 | ||
BE748041A (fr) * | 1970-03-26 | 1970-09-28 | Centre Rech Metallurgique | Perfectionnements aux procedes d'affinage, |
SE395911B (sv) * | 1974-04-16 | 1977-08-29 | Uddeholms Ab | Behandling av metallsmelta i keramiskt infordrat reaktionskerl |
DE2740842A1 (de) * | 1977-09-10 | 1979-03-22 | Ernst Peter Prof Dipl I Franke | Frischmittel bei bodenblasenden stahlerzeugungsverfahren |
BE880526A (fr) * | 1979-12-10 | 1980-06-10 | Bristol Myers Company Ct De Re | Sels d'argent d'acide phosphanilique, leur procede de production et composition antibacterienne les contenant. |
-
1981
- 1981-09-24 ES ES505740A patent/ES8303534A1/es not_active Expired
- 1981-09-24 US US06/305,259 patent/US4388113A/en not_active Expired - Lifetime
- 1981-09-25 CA CA000386735A patent/CA1170460A/en not_active Expired
- 1981-09-25 BR BR8106166A patent/BR8106166A/pt not_active IP Right Cessation
- 1981-09-25 AU AU75681/81A patent/AU531023B2/en not_active Expired
- 1981-09-28 EP EP81304470A patent/EP0049148B1/en not_active Expired
- 1981-09-28 DE DE8181304470T patent/DE3176581D1/de not_active Expired
Also Published As
Publication number | Publication date |
---|---|
DE3176581D1 (en) | 1988-02-04 |
US4388113A (en) | 1983-06-14 |
ES505740A0 (es) | 1983-02-01 |
CA1170460A (en) | 1984-07-10 |
BR8106166A (pt) | 1982-06-15 |
AU7568181A (en) | 1982-04-01 |
EP0049148B1 (en) | 1987-12-23 |
AU531023B2 (en) | 1983-08-04 |
EP0049148A1 (en) | 1982-04-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0056644B1 (en) | Supersonic injection of oxygen in cupolas | |
JPS62263906A (ja) | 高炉羽口からの微粉炭吹込み方法 | |
TWI743762B (zh) | 製鋼礦渣的改質方法以及噴槍 | |
ES8303534A1 (es) | Un metodo de impedir el dano a una tobera sumergida | |
US2580614A (en) | Manufacture of open-hearth steel | |
GB1532204A (en) | Cupola furnace and a method for the melting and refining of cement copper | |
CN101693931A (zh) | 一种高炉风口部位的冷却装置 | |
EP0040440B2 (en) | A shaft furnace, particularly the refractory construction of the bottom thereof | |
US2970829A (en) | Method of operation of a top-fired open hearth furnace | |
US2829879A (en) | Bottoms for metallurgical furnaces of the bessemer converter type | |
US1948697A (en) | Manufacture of metals | |
US2788964A (en) | Metallurgical furnace | |
US4462825A (en) | Method for increasing the scrap melting capability of metal refining processes | |
KR930004473B1 (ko) | 용광로 내에서 철을 제조하기 위한 방법 | |
US3232595A (en) | Shaft type furnace for smelting scrap and producing steel | |
US3819164A (en) | Operation of a blast furnace | |
US4418893A (en) | Water-cooled refractory lined furnaces | |
US3088821A (en) | Open hearth steelmaking process | |
US1283500A (en) | Process of smelting ore. | |
EP0009104A1 (en) | Method for increasing the scrap melting capability of bottom blown processes | |
SU1074907A1 (ru) | Конвертер | |
US3537841A (en) | Method of reducing iron ores to pig iron | |
US1934081A (en) | Shaft furnace | |
SU933705A1 (ru) | Способ задувки доменной печи | |
US3099551A (en) | Snuffing blast furnaces |