- ES519365A0 ES519365A0 ES519365A ES519365A ES519365A0 ES 519365 A0 ES519365 A0 ES 519365A0 ES 519365 A ES519365 A ES 519365A ES 519365 A ES519365 A ES 519365A ES 519365 A0 ES519365 A0 ES 519365A0
- Authority
- ES
- Spain
- Prior art keywords
- inhibit
- corrosion
- procedure
- contact
- aqueous systems
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- XEEYBQQBJWHFJM-UHFFFAOYSA-N Iron Chemical compound [Fe] XEEYBQQBJWHFJM-UHFFFAOYSA-N 0.000 title 2
- 238000005260 corrosion Methods 0.000 title 1
- 230000007797 corrosion Effects 0.000 title 1
- 229910052742 iron Inorganic materials 0.000 title 1
- 229910052751 metal Inorganic materials 0.000 title 1
- 239000002184 metal Substances 0.000 title 1
- 150000002739 metals Chemical class 0.000 title 1
- 238000000034 method Methods 0.000 title 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
PCT/US1982/000122 WO1983002628A1 (en) | 1982-01-29 | 1982-01-29 | Method of and composition for inhibiting corrosion of iron base metals |
Publications (2)
Publication Number | Publication Date |
---|---|
ES519365A0 true ES519365A0 (es) | 1984-06-16 |
ES8405851A1 ES8405851A1 (es) | 1984-06-16 |
Family
ID=22167791
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES519365A Expired ES8405851A1 (es) | 1982-01-29 | 1983-01-28 | Procedimiento para inhibir la corrosion de metales a base de hierro en contacto con sistemas acuosos. |
Country Status (9)
Country | Link |
---|---|
US (1) | US4588519A (es) |
EP (1) | EP0100312A4 (es) |
CA (1) | CA1176446A (es) |
DE (1) | DE3249178T1 (es) |
ES (1) | ES8405851A1 (es) |
GB (1) | GB2125393B (es) |
IT (1) | IT1193632B (es) |
SE (1) | SE441369B (es) |
WO (1) | WO1983002628A1 (es) |
Families Citing this family (19)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4936987A (en) * | 1983-03-07 | 1990-06-26 | Calgon Corporation | Synergistic scale and corrosion inhibiting admixtures containing carboxylic acid/sulfonic acid polymers |
US4634532A (en) * | 1984-05-12 | 1987-01-06 | Calgon Corporation | Orthophosphate-containing desalination scale inhibitors |
FR2571745B1 (fr) * | 1984-10-17 | 1988-10-28 | Trest Juzhvodoprovod | Anticorrosif pour proteger la surface interne d'une canalisation contre la corrosion, procede d'obtention de cet anticorrosif et procede de protection de la surface interne d'une canalisation contre la corrosion utilisant cet anticorrosif |
US4575425A (en) * | 1984-12-24 | 1986-03-11 | Calgon Corporation | Process for controlling calcium oxalate scale over a wide pH range |
US4752443A (en) * | 1986-05-09 | 1988-06-21 | Nalco Chemical Company | Cooling water corrosion inhibition method |
US4717543A (en) * | 1986-08-04 | 1988-01-05 | Calgon Corporation | Method of inhibiting the corrosion of copper and copper alloys |
US4867945A (en) * | 1986-08-04 | 1989-09-19 | Calgon Corporation | Method of inhibiting the corrosion of copper and copper alloys |
US4717542A (en) * | 1987-01-23 | 1988-01-05 | W. R. Grace & Co. | Inhibiting corrosion of iron base metals |
US4973428A (en) * | 1987-04-27 | 1990-11-27 | Nalco Chemical Company | Zinc stabilization with modified acrylamide based polymers and corrosion inhibition derived therefrom |
US5049310A (en) * | 1987-04-27 | 1991-09-17 | Nalco Chemical Company | Zinc stabilization with modified acrylamide based polymers and corrosion inhibition derived therefrom |
US4898686A (en) * | 1987-04-27 | 1990-02-06 | Nalco Chemical Company | Zinc stabilization with modified acrylamide based polymers and corrosion inhibition derived therefrom |
US5428095A (en) * | 1992-06-09 | 1995-06-27 | Cal-West Automotive | Protective coating composition and method of using such composition |
US5281436A (en) * | 1992-06-09 | 1994-01-25 | Cal-West Automotive Products | Protective coating composition and method of using such composition |
US5380782A (en) * | 1993-10-04 | 1995-01-10 | Rohm And Haas Company | Polymeric dispersants for ceramic materials |
US5531934A (en) * | 1994-09-12 | 1996-07-02 | Rohm & Haas Company | Method of inhibiting corrosion in aqueous systems using poly(amino acids) |
DE19706410C2 (de) * | 1997-02-19 | 2001-04-05 | Metakorin Wasser Chemie Gmbh | Verfahren und Mittel zur Korrosionsschutzbehandlung wasserführender Metallsysteme |
CA2253679A1 (fr) * | 1998-01-26 | 1999-07-26 | Elf Atochem S.A. | Passivation des aciers inoxydables en milieu acide organosulfonique |
JP4089648B2 (ja) * | 2004-03-31 | 2008-05-28 | 栗田工業株式会社 | 腐食防止方法 |
US20140261567A1 (en) * | 2013-03-15 | 2014-09-18 | Ecolab Usa Inc. | Inhibiting corrosion of aluminum on alkaline media by phosphinosuccinate oligomers and mixtures thereof |
Family Cites Families (23)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
BE611853A (es) * | 1960-12-23 | |||
US3116248A (en) * | 1960-12-23 | 1963-12-31 | Shell Oil Co | Lubricating oil composition |
US3578589A (en) * | 1969-03-17 | 1971-05-11 | Grace W R & Co | Method for treating cooling water |
US3666404A (en) * | 1969-11-05 | 1972-05-30 | Chemed Corp | Method of inhibiting corrosion in aqueous systems with high molecular weight alkylene oxide polymers |
US3709815A (en) * | 1971-07-01 | 1973-01-09 | Calgon Corp | Boiler water treatment |
US3709816A (en) * | 1971-07-01 | 1973-01-09 | Calgon Corp | Control of alluvial and other deposits in aqueous systems |
US3806367A (en) * | 1972-06-01 | 1974-04-23 | Bitz Lab Inc | Acrylamido-sulfonic acid polymers and their use as rust and tubercle removing agents |
US3898037A (en) * | 1972-06-01 | 1975-08-05 | Betz Laboratories | Acrylamido-sulfonic acid polymers and their use |
US4126549A (en) * | 1973-02-14 | 1978-11-21 | Ciba-Geigy (Uk) Limited | Treatment of water |
US3941562A (en) * | 1973-06-04 | 1976-03-02 | Calgon Corporation | Corrosion inhibition |
US3928196A (en) * | 1973-12-05 | 1975-12-23 | Calgon Corp | Inhibition of scale deposition |
US3959167A (en) * | 1973-12-10 | 1976-05-25 | Chemed Corporation | Method and composition of inhibiting scale |
DE2513735A1 (de) * | 1974-04-01 | 1975-10-02 | Calgon Corp | Korrosionsschutzmittel |
SE435456B (sv) * | 1976-01-07 | 1984-10-01 | Calgon Corp | Komposition och forfarande for att kontrollera uppbyggnaden av pannsten i gastvettare |
US4118318A (en) * | 1976-10-26 | 1978-10-03 | Calgon Corporation | Gas scrubber scale and deposit control |
US4048066A (en) * | 1976-11-17 | 1977-09-13 | Chemed Corporation | Method of inhibiting scale |
US4105581A (en) * | 1977-02-18 | 1978-08-08 | Drew Chemical Corporation | Corrosion inhibitor |
US4242242A (en) * | 1977-06-10 | 1980-12-30 | Akzona Incorporated | Highly absorbent fibers of rayon with sulfonic acid polymer incorporated |
US4255259A (en) * | 1979-09-18 | 1981-03-10 | Chemed Corporation | Scale inhibition |
CA1151498A (en) * | 1979-10-23 | 1983-08-09 | Dearborn Chemicals Ltd. | Treatment of aqueous systems |
US4303568A (en) * | 1979-12-10 | 1981-12-01 | Betz Laboratories, Inc. | Corrosion inhibition treatments and method |
US4297237A (en) * | 1980-03-06 | 1981-10-27 | Calgon Corporation | Polyphosphate and polymaleic anhydride combination for treating corrosion |
DE3027236C2 (de) * | 1980-07-18 | 1985-08-01 | Chemische Fabrik Stockhausen GmbH, 4150 Krefeld | Terpolymere aus 2-Acrylamido-2-methyl-propansulfonsäure, Acrylamid und Acrylsäure in Form ihrer Salze, Verfahren zur Herstellung dieser Terpolymeren und Verwendung zur Verhinderung von Inkrustationen in wäßrigen Systemen |
-
1982
- 1982-01-29 EP EP19820900854 patent/EP0100312A4/en not_active Withdrawn
- 1982-01-29 WO PCT/US1982/000122 patent/WO1983002628A1/en not_active Application Discontinuation
- 1982-01-29 US US06/473,157 patent/US4588519A/en not_active Expired - Fee Related
- 1982-01-29 DE DE19823249178 patent/DE3249178T1/de not_active Ceased
- 1982-01-29 GB GB08325800A patent/GB2125393B/en not_active Expired
- 1982-12-24 CA CA000418602A patent/CA1176446A/en not_active Expired
-
1983
- 1983-01-28 IT IT19313/83A patent/IT1193632B/it active
- 1983-01-28 ES ES519365A patent/ES8405851A1/es not_active Expired
- 1983-03-01 SE SE8301134A patent/SE441369B/sv not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
WO1983002628A1 (en) | 1983-08-04 |
EP0100312A4 (en) | 1984-07-11 |
SE441369B (sv) | 1985-09-30 |
US4588519A (en) | 1986-05-13 |
IT1193632B (it) | 1988-07-21 |
CA1176446A (en) | 1984-10-23 |
IT8319313A0 (it) | 1983-01-28 |
GB2125393A (en) | 1984-03-07 |
SE8301134D0 (sv) | 1983-03-01 |
DE3249178T1 (de) | 1984-09-06 |
SE8301134L (sv) | 1983-07-30 |
GB2125393B (en) | 1985-04-17 |
GB8325800D0 (en) | 1983-10-26 |
EP0100312A1 (en) | 1984-02-15 |
ES8405851A1 (es) | 1984-06-16 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES519365A0 (es) | Procedimiento para inhibir la corrosion de metales a base de hierro en contacto con sistemas acuosos. | |
DE3671950D1 (de) | Metalldichtung. | |
BR8406851A (pt) | Inibidor de corrosao metalica,sistema aquoso com inibidor de corrosao e metodo para inibir corrosao metalica | |
FR2346465A1 (fr) | Agent anticorrosion pour surfaces metalliques | |
BR8503082A (pt) | Inibidor de corrosao para combustivel liquidos | |
ES521761A0 (es) | Procedimiento de tratamiento para mejorar la resistencia a la corrosion de piezas de metal ferreo. | |
DE3576559D1 (de) | Einsetzbarer kontaktkoerper. | |
ES511595A0 (es) | Procedimiento para proporcionar un revestimiento aislante directamente sobre acero electrico. | |
GB2084128B (en) | Inhibiting corrosion in aqueous systems | |
DE3587403D1 (de) | Korrosionsverhuetung von metallen in waessrigen systemen. | |
GB8410589D0 (en) | Inhibiting corrosion in aqueous systems | |
GB2231565B (en) | The inhibition of corrosion in aqueous systems | |
IT1115546B (it) | Inibitore per impedire la corrosione di metalli in sistemi idrici | |
MX157371A (es) | Mejoras en una composicion acidica acuosa a base de fosfato de zinc para tratar superficies metalicas | |
ES515820A0 (es) | Procedimiento para controlar la corrosion de superficies metalicas en sistemas acuosos. | |
ES523167A0 (es) | Procedimiento para inhibir la corrosion de componentes metalicos de sistemas de refrigeracion. | |
BR8303394A (pt) | Composicao para proteger superficies de metal contral corrosao | |
ES524623A0 (es) | Procedimiento para la solucion rapida de polimeros hidrosolubles en agua. | |
NO870292L (no) | Jernmetallkorrosjonshemmende arkmateriale. | |
ES510043A0 (es) | Aparato para utilizarse en el vertido sumergido de metales fundidos. | |
ES516314A0 (es) | Procedimiento para beneficiar minerales de sulfuros metalicos. | |
NO821267L (no) | Ankerlegeme. | |
ES520921A0 (es) | Procedimiento para la produccion de un acero de baja aleacion. | |
JPS5658978A (en) | Corrosion inhibitor stable against hard water | |
ES547690A0 (es) | Procedimiento para la reduccion de iones metalicos en solu- ciones acuosas |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
FD1A | Patent lapsed |
Effective date: 20020506 |