ES427469A3 - A procedure for preparing hot fusion adhesives of the polyester type. (Machine-translation by Google Translate, not legally binding) - Google Patents

A procedure for preparing hot fusion adhesives of the polyester type. (Machine-translation by Google Translate, not legally binding)

Info

Publication number
ES427469A3
ES427469A3 ES427469A ES427469A ES427469A3 ES 427469 A3 ES427469 A3 ES 427469A3 ES 427469 A ES427469 A ES 427469A ES 427469 A ES427469 A ES 427469A ES 427469 A3 ES427469 A3 ES 427469A3
Authority
ES
Spain
Prior art keywords
translation
machine
legally binding
google translate
polyester type
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
ES427469A
Other languages
Spanish (es)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
VIZKUMNI USTAV KOZEDELNY
Original Assignee
VIZKUMNI USTAV KOZEDELNY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by VIZKUMNI USTAV KOZEDELNY filed Critical VIZKUMNI USTAV KOZEDELNY
Priority to ES427469A priority Critical patent/ES427469A3/en
Publication of ES427469A3 publication Critical patent/ES427469A3/en
Expired legal-status Critical Current

Abstract

Process for preparing hot melt adhesives of the polyester type, characterized in that linear polyesters of terephthalic acid with ethylene glycol are heated to a temperature of 270 to 290º c, until they are hot melted, and then sterolized by addition of ten to forty by mole percent of poly (ethylene isophthalate) whose limiting viscosity index is between 0.2. And 0.5, based on 100 parts of poly (ethylene terephthalate), the low molecular weight products of the sterolysis reaction are then separated from the reaction mixture using reduced pressure, after which the hot melt adhesive the resulting final, which has a limiting viscosity index comprised between 0.2 and 0.5, is introduced into molds in which the adhesive is shaped, by solidification in applicable forms. (Machine-translation by Google Translate, not legally binding)
ES427469A 1974-06-20 1974-06-20 A procedure for preparing hot fusion adhesives of the polyester type. (Machine-translation by Google Translate, not legally binding) Expired ES427469A3 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
ES427469A ES427469A3 (en) 1974-06-20 1974-06-20 A procedure for preparing hot fusion adhesives of the polyester type. (Machine-translation by Google Translate, not legally binding)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
ES427469A ES427469A3 (en) 1974-06-20 1974-06-20 A procedure for preparing hot fusion adhesives of the polyester type. (Machine-translation by Google Translate, not legally binding)

Publications (1)

Publication Number Publication Date
ES427469A3 true ES427469A3 (en) 1976-07-16

Family

ID=8466984

Family Applications (1)

Application Number Title Priority Date Filing Date
ES427469A Expired ES427469A3 (en) 1974-06-20 1974-06-20 A procedure for preparing hot fusion adhesives of the polyester type. (Machine-translation by Google Translate, not legally binding)

Country Status (1)

Country Link
ES (1) ES427469A3 (en)

Similar Documents

Publication Publication Date Title
ES437549A1 (en) Polyesters derived from dihydric phenols which form anisotropic melts
IE42166L (en) Linear polyesters
ES359657A1 (en) Production of a modified diglycol therephthalate polycondensate for injection molding
GB1469186A (en) Partially cross-linked linear aromatic polyesters
GB1447146A (en) Preparation of polyalkylene terephthalates
ES438390A1 (en) Polymerisation process
ES388047A1 (en) Process and apparatus for the continuous production of linear polyesters
GB1556715A (en) Linear copolyesters containing units of terephthalic acid and butane - 1,4 - diol and thermoplastic moulding composition containing them
ES427469A3 (en) A procedure for preparing hot fusion adhesives of the polyester type. (Machine-translation by Google Translate, not legally binding)
ES422143A1 (en) Method for preparing pigmented polyethylene terephthalate
ES431947A1 (en) Linear, thermoplastic polyesters and process for their manufacture
ES400227A1 (en) Thermoplastic elastomeric copolyesters
US3374137A (en) Adhesion of paper materials
ES451776A3 (en) Improved procedure for the preparation of polyesters by direct sterification. (Machine-translation by Google Translate, not legally binding)
ES370219A3 (en) A procedure for the preparation of strengthly polymerized linear polyesters. (Machine-translation by Google Translate, not legally binding)
US3417057A (en) Rapid production of linear polyesters by transesterification
ES444295A1 (en) Process for preparing polyesters
ES292680A1 (en) Procedure for the preparation of linear thermoplastic polyesters (Machine-translation by Google Translate, not legally binding)
JPS54120680A (en) Manufacture of oriented polyester resin
ES370188A3 (en) A procedure for preparing a polyester. (Machine-translation by Google Translate, not legally binding)
ES428183A2 (en) Compositions for colouring thermoplastic polymers
ES451775A3 (en) Procedure for the direct sterification of tereftal acid. (Machine-translation by Google Translate, not legally binding)
GB1402288A (en) Preparation of polyesters
FR2215436A1 (en) High DP polyethylene terephthalate prodn - from prepolymer prepd in a two-stage esterification process, each stage effected at different pressures
ES288173A1 (en) Procedure and device for the continuous obtaining of polyethylene phthalates (Machine-translation by Google Translate, not legally binding)