ES374956A3 - Procedure for the desulfuration of a fertile ferrous metal. (Machine-translation by Google Translate, not legally binding) - Google Patents
Procedure for the desulfuration of a fertile ferrous metal. (Machine-translation by Google Translate, not legally binding)Info
- Publication number
- ES374956A3 ES374956A3 ES374956A ES374956A ES374956A3 ES 374956 A3 ES374956 A3 ES 374956A3 ES 374956 A ES374956 A ES 374956A ES 374956 A ES374956 A ES 374956A ES 374956 A3 ES374956 A3 ES 374956A3
- Authority
- ES
- Spain
- Prior art keywords
- ferrous metal
- weight
- translation
- machine
- legally binding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
Process for the desulfurization of a molten ferrous metal, in the ladle itself or in an ingot mold, characterized in that it comprises adding to said molten ferrous metal, the following ingredients, in the proportions indicated: lime (cao), 40 to 80 parts by weight, iron oxide, 5 to 30 parts by weight; oxidizable material, 5 to 20 parts by weight, the weight of the lime in the mixture being at least double that of the iron oxide, and the weight of iron oxide in the mixture being stoichiometrically insufficient to oxidize all of the oxidizable material present . (Machine-translation by Google Translate, not legally binding)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
ES374956A ES374956A3 (en) | 1969-12-27 | 1969-12-27 | Procedure for the desulfuration of a fertile ferrous metal. (Machine-translation by Google Translate, not legally binding) |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
ES374956A ES374956A3 (en) | 1969-12-27 | 1969-12-27 | Procedure for the desulfuration of a fertile ferrous metal. (Machine-translation by Google Translate, not legally binding) |
Publications (1)
Publication Number | Publication Date |
---|---|
ES374956A3 true ES374956A3 (en) | 1972-02-16 |
Family
ID=8454657
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES374956A Expired ES374956A3 (en) | 1969-12-27 | 1969-12-27 | Procedure for the desulfuration of a fertile ferrous metal. (Machine-translation by Google Translate, not legally binding) |
Country Status (1)
Country | Link |
---|---|
ES (1) | ES374956A3 (en) |
-
1969
- 1969-12-27 ES ES374956A patent/ES374956A3/en not_active Expired
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES331415A1 (en) | Procedure for the continuous steel foundry. (Machine-translation by Google Translate, not legally binding) | |
FR2335300A1 (en) | BASIC AGGLOMERATE FLOW FOR WELDING ORDINARY OR LOW ALLOY STEELS WITH HIGH CAD CONTENT | |
ES277679A1 (en) | Manufacturing procedure for refractory parts (Machine-translation by Google Translate, not legally binding) | |
ES374956A3 (en) | Procedure for the desulfuration of a fertile ferrous metal. (Machine-translation by Google Translate, not legally binding) | |
JPS51115218A (en) | Dephosphorization of molten iron | |
JPS5343019A (en) | Refining method for steel with reduced slag formation | |
ES320750A1 (en) | Procedure for the production of iron to silicon with a low oxygen content. (Machine-translation by Google Translate, not legally binding) | |
GB848567A (en) | Improvements in a method of treating iron and steel to remove dissolved oxygen | |
JPS51151204A (en) | A cupola for melting metal with auxiliary fuel and refining with coke | |
ES405638A1 (en) | Procedure to perform the second stage of refinement of the manufacture of steel in electric oven. (Machine-translation by Google Translate, not legally binding) | |
JPS5270918A (en) | Preparation of clean steel of lonon-metallic inclusion | |
JPS5258012A (en) | Process for producing low phosphorus steel | |
JPS52126601A (en) | Preliminary treatment of molten metal | |
JPS5230713A (en) | Cohesion agent for slag in steel making | |
JPS5278707A (en) | Preparation of low aluminum ferro-silicon | |
JPS5271323A (en) | Reforming of molten pig iron | |
ES402020A3 (en) | Improvements in the procedures for the elimination of sulfur in the iron colado. (Machine-translation by Google Translate, not legally binding) | |
JPS5258011A (en) | Dephosphorizing agent for iron refining | |
JPS5246317A (en) | Process for sintering chromium ore | |
FR2259908A1 (en) | Slag conditioner - for facilitating dissolution of lime content in basic steel refining slag | |
JPS5280212A (en) | Addition of linear additives | |
ES398353A1 (en) | Process for production of plumbiferous steels | |
JPS5242415A (en) | Equipment for refining molten iron alloy | |
ES409924A1 (en) | Procedure for the manufacture of iron or steel. (Machine-translation by Google Translate, not legally binding) | |
JPS51147421A (en) | Method of adding al and ti to molten steel |