ES262610A3 - Procedure for simple flat glass decoration and temperature (Machine-translation by Google Translate, not legally binding) - Google Patents

Procedure for simple flat glass decoration and temperature (Machine-translation by Google Translate, not legally binding)

Info

Publication number
ES262610A3
ES262610A3 ES0262610A ES262610A ES262610A3 ES 262610 A3 ES262610 A3 ES 262610A3 ES 0262610 A ES0262610 A ES 0262610A ES 262610 A ES262610 A ES 262610A ES 262610 A3 ES262610 A3 ES 262610A3
Authority
ES
Spain
Prior art keywords
translation
procedure
machine
temperature
legally binding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
ES0262610A
Other languages
Spanish (es)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to ES0262610A priority Critical patent/ES262610A3/en
Publication of ES262610A3 publication Critical patent/ES262610A3/en
Expired legal-status Critical Current

Abstract

Procedure for the simultaneous decoration and tempering of flat glass, characterized in that as a preliminary operation, in a first phase, the glass plate is decorated, either by applying the airbrush or gun system, or by silk screen or silk screen, according to whether the drawing or decoration to be made, or the decoration by hand or brush, always using vitrifiable enamels; and in a second phase the glass plate, after that operation of cold enameling. It is subjected, immediately, to an intensive infrared drying, until it is able to enter an electric oven, which puts the glass plate at a pre-rebinding temperature, which oscillates between 650 and 700 degrees. (Machine-translation by Google Translate, not legally binding)
ES0262610A 1960-11-19 1960-11-19 Procedure for simple flat glass decoration and temperature (Machine-translation by Google Translate, not legally binding) Expired ES262610A3 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
ES0262610A ES262610A3 (en) 1960-11-19 1960-11-19 Procedure for simple flat glass decoration and temperature (Machine-translation by Google Translate, not legally binding)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
ES0262610A ES262610A3 (en) 1960-11-19 1960-11-19 Procedure for simple flat glass decoration and temperature (Machine-translation by Google Translate, not legally binding)

Publications (1)

Publication Number Publication Date
ES262610A3 true ES262610A3 (en) 1961-04-16

Family

ID=34491996

Family Applications (1)

Application Number Title Priority Date Filing Date
ES0262610A Expired ES262610A3 (en) 1960-11-19 1960-11-19 Procedure for simple flat glass decoration and temperature (Machine-translation by Google Translate, not legally binding)

Country Status (1)

Country Link
ES (1) ES262610A3 (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
ES2330599A1 (en) * 2007-10-08 2009-12-11 Bulma Tecnologia S.L. Procedure for drying the surface moisture of enamels, inks and screws in ceramic tiles and glass by infrared radiation. (Machine-translation by Google Translate, not legally binding)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
ES2330599A1 (en) * 2007-10-08 2009-12-11 Bulma Tecnologia S.L. Procedure for drying the surface moisture of enamels, inks and screws in ceramic tiles and glass by infrared radiation. (Machine-translation by Google Translate, not legally binding)

Similar Documents

Publication Publication Date Title
ES262610A3 (en) Procedure for simple flat glass decoration and temperature (Machine-translation by Google Translate, not legally binding)
CA622011A (en) Producing oxide coatings on glass surfaces
CA609447A (en) Process and apparatus for coating glass filaments with metal
AU263520B2 (en) Process. and device for improving the thermal uniformity of molten glass
CA581724A (en) Iron coatings on treated glass fibers
AU1955762A (en) Process. and device for improving the thermal uniformity of molten glass
CA555403A (en) Process for metal coating glass filaments
AU243404B2 (en) Process and furnace for making glass
CA697110A (en) Process for the enameling of articles made of iron with vitreous enamels
CA599739A (en) Heat treating furnace
AU6705360A (en) Process and furnace for making glass
CA507221A (en) Refractory composition, article and process
AU266361B2 (en) Method and composition for decorating glass ceramics
CA522512A (en) Infra-red ray, indirectly heating heat bath
AU242136B2 (en) Composition for coating glass fibers
CA558395A (en) Range oven heating apparatus
CA564737A (en) Refractory glass fibers
CA586696A (en) Glass lehr and method of heating glass ware
CA608629A (en) Yarn coating and wiping process and apparatus
CA514169A (en) Heating furnace
AU1590262A (en) Method and composition for decorating glass ceramics
AU1184961A (en) Furnace for working products such as glass and process for working the said furnace
AU258996B2 (en) Glass fiber forming apparatus utilizing an high output radiant heater
AU5612559A (en) Composition for coating glass fibers
CA600744A (en) Heat treating furnace