DE976567C - Verfahren zur Behandlung von Primaerelementen - Google Patents
Verfahren zur Behandlung von PrimaerelementenInfo
- Publication number
- DE976567C DE976567C DEC2044A DEC0002044A DE976567C DE 976567 C DE976567 C DE 976567C DE C2044 A DEC2044 A DE C2044A DE C0002044 A DEC0002044 A DE C0002044A DE 976567 C DE976567 C DE 976567C
- Authority
- DE
- Germany
- Prior art keywords
- elements
- primary elements
- treatment
- low
- volts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
In Betracht gezogene Druckschriften:
Deutsche Patentschriften Nr. 97 821, 176064,
Deutsche Patentschriften Nr. 97 821, 176064,
368953, 469 133, 495 800, 601 026, 613 509,
643769; schweizerische Patentschrift Nr. 193 436;
französische Patentschrift Nr. 826688;
USA.-Patentschrift Nr. 2 199 322;
Drotschmann, Trockenbatterien, 3. Auflage,
USA.-Patentschrift Nr. 2 199 322;
Drotschmann, Trockenbatterien, 3. Auflage,
1945, Leipzig, S. 3, 321, 368 bis 373;
Radio-Mentor, 1942, Nr. 9, S. 425.
Radio-Mentor, 1942, Nr. 9, S. 425.
Hierzu 1 Blatt Zeichnungen
© 309 742/3 11.63
Claims (1)
- PATENTANSPRUCH:Verfahren zur Herabsetzung des Innenwiderstandes von solchen Primärelementen mit verfestigtem Salmiakelektrolyten und Zinkelektroden, welche mit einer Gleichstromquelle bzw. einem Gleichrichter im Pufferbetrieb zum Speisen von elektrischen Schwachstromgeräten Verwendung finden, dadurch gekennzeichnet, daß diese Elemente vor ihrer Inbetriebnahme einer einmaligen Formierung unterworfen werden, die mittels eines Ladestromes von geringer Stromstärke in der Größenordnung 40 mA/dm2 und von einer der zwischen 1,65 und 2,0 Volt liegende Klemmenspannung der Elemente entsprechenden Gegenspannung erfolgt.