DE692589C - Pressed glass shape - Google Patents
Pressed glass shapeInfo
- Publication number
- DE692589C DE692589C DE1939L0096989 DEL0096989D DE692589C DE 692589 C DE692589 C DE 692589C DE 1939L0096989 DE1939L0096989 DE 1939L0096989 DE L0096989 D DEL0096989 D DE L0096989D DE 692589 C DE692589 C DE 692589C
- Authority
- DE
- Germany
- Prior art keywords
- glass shape
- glass
- pressed glass
- pressed
- boron nitride
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Gegenstand der Erfindung ist eine Preßglasform, an der das Glas nicht Hebt. Bisher bereitete das Kleben dies in Formen gepreßten Glases an den Formwandungem Schwierigkeiten, besonders wenn der Glasfluß zur Erzielung großer Leichtfliissiglaeit hoch erhitzt wurde. Es ist zwar in der Glastechnik bekannt, das Kleben des Glases durch Überziehen der mit dem heißen Glas in Berührung kommenden Teile mit einem feuerfesten Mittel, wie Graphit, Speckstein oder Schlämmkreide, nach Möglichkeit zu verhindern, jedoch haben diese Mittel noch nicht voll befriedigt.The invention relates to a pressed glass mold on which the glass does not lift. Until now Prepared gluing this pressed into molds Glass on the mold wall difficulties, especially when the glass flow was heated to a high level to achieve a high level of fluidity. It is in glass engineering, though known, the gluing of the glass by covering the with the hot glass in contact to prevent coming parts with a refractory agent such as graphite, soapstone or whiting chalk, if possible, however, these means have not yet been fully satisfied.
,s Es wurde nun gefunden, daß das Kleben selbst bei den höchsten in Frage kommenden Temperaturen des Glases vollkommen vermieden wird, wenn die Oberfläche der Formen mit Bornitrid (BN) überzogen wird. Das Bornitrid kann auf die Formoberfläche aufgestrichen, aufgebürstet oder nach Verteilung in einer geeigneten Bindeflüssigkeit aufgespritzt werden. Die Verwendung von ganz aus Bornitrid bestehenden Formen ist nicht empfehlenswert wegen der hohen Kosten und Ä5 der leichten Zerbrechlichkeit des Nitrides. ., S We have found that the glue is completely avoided even at the highest temperatures in question of the glass when the surface of the molds with boron nitride (BN) is covered. The boron nitride can be painted, brushed on or sprayed onto the mold surface after distribution in a suitable binding liquid. The use of all forms of boron nitride existing is not recommended because of high costs and ae5 light fragility of the nitride. .
Claims (1)