DE676525C - Device for double-point or seam welding using two adjacent electrodes without counter electrodes - Google Patents
Device for double-point or seam welding using two adjacent electrodes without counter electrodesInfo
- Publication number
- DE676525C DE676525C DEB180907D DEB0180907D DE676525C DE 676525 C DE676525 C DE 676525C DE B180907 D DEB180907 D DE B180907D DE B0180907 D DEB0180907 D DE B0180907D DE 676525 C DE676525 C DE 676525C
- Authority
- DE
- Germany
- Prior art keywords
- electrodes
- double
- seam welding
- iron
- point
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Das Hauptpatent 670741 betrifft ein Verfahren zum Doppclpunkt-oder Nahtschweißen unter Verwendung zweier auf einem Werkstückteil nebeneinanderliegender Elektroden 5 ohne Gegenelektroden, bei dem der durch das Oberblech fließende Strom im Verhältnis zu dem das Ünterblech durchfließenden Strom durch elektromagnetisch induktiv wirkende Stromverdrängungsmittel verringert wird, indem beispielsweise massives oder unterteiltes Eisen zwischen die Elektroden eingeschoben wird, wodurch eine Verbesserung des Verhältnisses von Schweißstrom zu Verluststrom sowie eine einwandfreie Schweißung ohne Verletzung der Blechoberfläche erreicht wird.The main patent 670741 relates to a method for double-point or seam welding using two electrodes lying next to one another on a workpiece part 5 without counter electrodes, in which the current flowing through the top plate is in relation to the current flowing through the cover plate by electromagnetically inductive Current displacement means is reduced by, for example, massive or subdivided Iron is inserted between the electrodes, thereby improving the ratio of welding current to leakage current as well as a perfect weld without damaging the sheet metal surface will.
Die vorliegende Erfindung besteht nun in einer Vorrichtung zur Ausübung des im Hauptpatent beschriebenen Verfahrens, welche sich dadurch auszeichnet, daß das Transformatoreisen des Schweißtransformators gleichzeitig das zwischen die Elektroden eingeschobene Eisen bildet. Diese Ausbildung bietet außer der einfacheren Konstruktion den großen Vorteil, daß der Sekundärleiter bedeutend kürzer gehalten werden kann, wodurch die Verluste verringert werden. Es ist also bei dieser Anordnung kein besonderes Eisen mehr erforderlich.The present invention consists in an apparatus for practicing the im Main patent described method, which is characterized in that the transformer iron of the welding transformer at the same time that it is inserted between the electrodes Forms iron. In addition to the simpler construction, this training offers the great advantage that the secondary conductor can be kept significantly shorter, whereby the losses are reduced. So there is nothing special about this arrangement Iron more required.
In der Zeichnung ist die Erfindung an zwei Ausführungsbeispielen näher erläutert, 'und zwar zeigt dieIn the drawing, the invention is explained in more detail using two exemplary embodiments, 'and although it shows
Abb. ι einen Schnitt durch eine Vorrichtung zum Doppelpunkt- oder Nahtschweißen, Abb.. 2 eine Seitenansicht der Vorrichtung nach Abb. 1 und dieFig. Ι a section through a device for colon or seam welding, Fig. 2 is a side view of the device according to Fig. 1 and the
Abb. 3 eine andere Vorrichtung zum Doppelpunkt- oder Nahtschweißen, bei der Rollenelektroden verwendet werden..Fig. 3 another device for double-spot or seam welding, with roller electrodes be used..
In den Abb. 1 'und 2 ist 1 die Primärwicklung, 2 die Sekundärwicklung, die vorzugsweise eine Sekundärbrücke bildet mit den Elektroden 3 und 4. 5 und 6 sind Isolationen, 7 der Eisenkern, der auf der dem Schweißgut benachbarten Seite vorzugsweise stärker ausgebildet ist, damit dem vom Schweißstrom herrührenden magnetischen Fluß im Eisen ein geringer Widerstand geboten wird. Die Elektroden stehen um Bruchteile eines Millimeters über das Eisen vor. Durch das einseitig ausgebildete Magnetfeld . des Schweiß stromes verdrängt sich dieser selbst, und zwar vom Eisen fort. 8 und 9 sind die beiden Schweißpunkte, die die Bleche 10 und 11 verbinden,In Figs. 1 'and 2, 1 is the primary winding, 2 the secondary winding, which preferably forms a secondary bridge with the Electrodes 3 and 4. 5 and 6 are insulation, 7 the iron core, which is on the dem Weld adjacent side is preferably formed stronger, so that from The magnetic flux in the iron caused by welding current offered a low resistance will. The electrodes protrude from the iron by a fraction of a millimeter. Due to the one-sided magnetic field. the welding current displaces it himself, away from the iron. 8 and 9 are the two welding points that the metal sheets Connect 10 and 11,
Die Vorrichtung nach Abb. 3 unterscheidet sich von der Vorrichtung nach Abb. 1 und 2 lediglich dadurch, daß Schweißrollen 12 und 13 für die Nahtschweißung angeordnet sind.The device according to Fig. 3 differs from the device according to Figs. 1 and 2 only in that welding rollers 12 and 13 are arranged for the seam welding.
Claims (1)