DE600759C - Photosensitive material containing diazo compounds and azo components - Google Patents

Photosensitive material containing diazo compounds and azo components

Info

Publication number
DE600759C
DE600759C DE1930600759D DE600759DA DE600759C DE 600759 C DE600759 C DE 600759C DE 1930600759 D DE1930600759 D DE 1930600759D DE 600759D A DE600759D A DE 600759DA DE 600759 C DE600759 C DE 600759C
Authority
DE
Germany
Prior art keywords
diazo compounds
photosensitive material
material containing
azo components
containing diazo
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DE1930600759D
Other languages
German (de)
Inventor
Dr Ulrich Ostwald
Waldemar Schwalbe
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kalle GmbH and Co KG
Original Assignee
Kalle GmbH and Co KG
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kalle GmbH and Co KG filed Critical Kalle GmbH and Co KG
Application granted granted Critical
Publication of DE600759C publication Critical patent/DE600759C/en
Expired legal-status Critical Current

Description

DEUTSCHES REICHGERMAN EMPIRE

AUSGEGEBEN AM 31.JULI1934ISSUED JULY 31, 1934

REICHSPATENTAMTREICH PATENT OFFICE

PATENTSCHRIFTPATENT LETTERING

KLASSE 57b GRUPPE 12 osCLASS 57b GROUP 12 os

Patentiert im Deutschen Reiche vom 5. April 1930 abPatented in the German Empire on April 5, 1930

Lichtempfindliche, auf Papier, Leinenpapier, Cellulosehydratfolien oder anderen Unterlagen aufgetragene bzw. eingebettete Präparationen, die Azokomponenten im Gemisch mit am Licht unter Zersetzung ausbleichenden Diazoverbindungen enthalten (wie sie beispielsweise in der deutschen Patentschrift 386 433 beschrieben sind), sind gegen Beschmutzung und Verletzung, wie Striche oder Einrisse, äußerst empfindlich; vor allem gilt dies für die rauhen Papierpräparationen. Ein Abwaschen derartig beschmutzter Papiere ist nicht empfehlenswert, da hierdurch sowohl die lichtempfindlichen Schichten als auch die Unterlage leiden.Photosensitive on paper, linen paper, cellulose hydrate films or other substrates applied or embedded preparations, the azo components in a mixture with light bleaching with decomposition Contain diazo compounds (as for example in the German patent 386 433), are against soiling and injury, such as strokes or Tears, extremely sensitive; This is especially true for the rough paper finishes. A Washing off such soiled papers is not recommended, as this will cause both the light-sensitive layers as well as the base suffer.

Es ist nun gefunden worden, daß man derartige lichtempfindliche Materialien weitgehend gegen äußere mechanische Einflüsse in der Weise schützen kann, daß man die Schichtseite oder auch beide Seiten mit einem transparenten Überzug versieht. Zur Herstellung dieses transparenten Überzuges kann man beispielsweise Folien aus Cellulosederivaten, wie z. B. Celluloseäthern oder -estern, benutzen, ferner Cellulosehydratfolien, die gegebenenfalls noch 'ein- oder beiderseitig mit einem dünnen Lacküberzug versehen sein können. Diese Überzüge werden nach dem üblichen Kaschierverfahren auf die lichtempfindlichen Materialien aufgebracht. Lichtempfindliches Material, das mit diesen neuartigen Überzügen versehen ist, weist eine große Beständigkeit gegenüber' mechanischen Einflüssen auf, ohne daß weder die Lichtempfindlichkeit gelitten hat, noch, was besonders überraschend war, die Möglichkeit, solche lichtempfindlichen Schichten mit gasförmigen Mitteln zu entwickeln. Die Belichtung und Entwicklung dieses neuartigen Materials kann vielmehr in der übliehen Weise erfolgen. Es ist selbstverständlich möglich, derartige lichtempfindliche Materialien, die vorzugsweise nach dem Trockenverfahren entwickelt werden, auch, mittels aller anderen in der Diazotypie üblichen Methoden zu entwickeln, beispielsweise nach dem Naß- oder Halbnaß entwicklungsverfahren. Doch ist es bei Anwendung dieser letzteren Methoden zweckmäßig, die Entwicklungsflüssigkeit auf die nicht mit einem Überzug versehene Seite des Materials einwirken zu lassen.·It has now been found that such photosensitive materials can be used extensively can protect against external mechanical influences in such a way that the layer side or both sides with one transparent coating. To produce this transparent coating can for example, films made from cellulose derivatives, such as. B. cellulose ethers or -esters, use, furthermore cellulose hydrate films, which optionally still 'one or can be provided with a thin lacquer coating on both sides. These coatings are applied to the photosensitive materials using the usual laminating process. Photosensitive material that is provided with these novel coatings has a high resistance to ' mechanical influences, without neither the photosensitivity has suffered nor, what was particularly surprising was the possibility of such photosensitive layers to develop with gaseous means. The exposure and development of this novel Rather, material can be done in the usual way. It goes without saying possible such photosensitive materials, preferably by the dry process can be developed, also, by means of all other methods customary in diazotype to develop, for example by the wet or semi-wet development process. But it is with the application of the latter Methods expedient to apply the developing liquid to the not with a coating to allow the provided side of the material to act.

Die neuen lichtempfindlichen Präparationen zeigen — dies gilt ebenso für die hieraus erhaltenen fertigen Bilder — bedeutende Vorteile gegenüber den bisher bekannten. Die Überzugsschichten sind wegen ihrer glatten Oberfläche kaum beschmutzbar wie das Papier, andererseits sind sie ohne jede Gefährdung der Grundlage und der lichtempfindliehen Schicht abwaschbar. Sie befestigen und versteifen das Hchtempfindliche Material,The new light-sensitive preparations show - this also applies to those obtained from them finished pictures - significant advantages over the previously known. The coating layers are because of their smoothness The surface can hardly be stained like the paper, on the other hand they are harmless The base and the light-sensitive layer are washable. They fasten and stiffen the highly sensitive material,

*) Von dem Patentsucher sind als die Erfinder angegeben worden:*) The patent seeker indicated the following as the inventors:

Dr. Ulrich Ostwald und Waldemar Schwalbe in Wiesbaden-Biebrich.Dr. Ulrich Ostwald and Waldemar Schwalbe in Wiesbaden-Biebrich.

machen es also widerstandsfähiger gegen Knicken und Einreißen und bewirken vor allem eine bedeutende Erhöhung der Falzfestigkeit. Andererseits liefern sie dank der transparenten Überzugsschicht nach Belichtung und Entwicklung sofort ein für künstlerische und Reklamezwecke wertvolles hochglänzendes Material. Bisher waren die Lichtpausanstalten,, wenn sie ihre Lichtpausen vorso make it more resistant to kinking and tearing and have an effect above all a significant increase in the folding strength. On the other hand, they deliver thanks to the transparent coating layer immediately after exposure and development for artistic and promotional purposes valuable high-gloss material. So far the blueprints were, when they show their blueprints

ίο Beschmutzung schützen und mit einem glänzenden Überzug versehen wollten, gezwungen, die fertigen Pausen einer Kaschieranstalt zur Bearbeitung zu übergeben, da hierzu umfangreiche Maßnahmen notwendig sind, die sich in den Fabrikationsgang einer Lichtpausanstalt nur schlecht einpassen.ίο Protect pollution and with a shiny Wanted to provide a coating, forced to use the finished breaks in a laminating facility Processing to be handed over, as extensive measures are necessary for this, which are in the production aisle of a blueprint institute just bad to fit in.

Es ist zwar schon bekannt, photographische Füme oder Papiere, deren Lichtempfindlichkeit auf der Anwesenheit von Halogensilbersalzen beruht, mit Deckschichten der genannten Art zu überziehen. Doch handelt es sich hierbei nur um Material, das ausschließlich feucht entwickelt werden konnte, wobei sich die Überzüge als wenig zweckmäßig erwiesen haben. Es war aus diesen bekannten Methoden aber nicht vorauszusehen, daß derartige Überzugsschichten auch für solches lichtempfindliches Material geeignet sein würden, dessen Entwicklung hauptsächlich nach dem Trockenverfahren erfolgt. Man mußte vielmehr annehmen, daß solche Überzugsschichten den gasförmigen Entwicklungsmitteln gegenüber gänzlich oder zum größten Teil undurchlässig sein würden und daher überhaupt keine oder nur unvollkommene BiI-der erzeugt werden würden.It is already known that photographic fumes or papers are sensitive to light based on the presence of halogen silver salts, with top layers of the aforementioned Kind of cover. But this is only about material that is exclusive Could be developed wet, the coatings proved to be unsuitable to have. From these known methods, however, it could not be foreseen that such Coating layers would also be suitable for such photosensitive material the development of which is mainly based on the dry process. On the contrary, one had to assume that such coating layers were entirely or to a large extent opposed to the gaseous developing agents Would be partially impermeable and therefore no or only imperfect images would be generated.

Beispielexample

Eine lichtempfindliche Präparation, wie sie beispielsweise nach Patent 386 433 auf Papier hergestellt wird, wird mit einer V200mrn starken Cellulosehydratfolie, die beiderseitig mit einer V1000mm starken Lackschicht versehen ist, unter Verwendung eines Harzleimes überzogen. Dann wird in einer normalen Kopiermaschine belichtet und nach den üblichen Entwicklungsverfahren entwickelt.A light-sensitive preparation, as it is produced on paper according to Patent 386 433, for example, is coated with a V200 mm thick cellulose hydrate film, which is provided on both sides with a V1000 mm thick lacquer layer, using a resin glue. Then it is exposed in a normal copying machine and developed according to the usual development process.

Wählt man die Feuchtentwicklung, so läßt man die Entwicklungsflüssigkeit zweckmäßig auf die nicht kaschierte Rückseite einwirken.If one chooses the wet development, then it is expedient to leave the developing liquid act on the non-laminated back.

Claims (1)

Patentanspruch :Claim: Lichtempfindliches, . Diazoverbindungen und Azokomponenten enthaltendes, trocken, z. B. mit Ammoniakdampf entwickelbares Material, gekennzeichnet durch .einen auf der Schichtseite aufgebrachten transparenten Überzug aus Folien aus Cellulosederivaten oder evtl. lackierten Cellulosehydratfolien. Photosensitive,. Dry containing diazo compounds and azo components z. B. with ammonia vapor developable material, characterized by .eine on the layer side applied transparent coating made of foils made of cellulose derivatives or possibly lacquered cellulose hydrate films.
DE1930600759D 1930-04-05 1930-04-05 Photosensitive material containing diazo compounds and azo components Expired DE600759C (en)