DE503730C - Current discharge for galvanic elements - Google Patents
Current discharge for galvanic elementsInfo
- Publication number
- DE503730C DE503730C DESCH91609D DESC091609D DE503730C DE 503730 C DE503730 C DE 503730C DE SCH91609 D DESCH91609 D DE SCH91609D DE SC091609 D DESC091609 D DE SC091609D DE 503730 C DE503730 C DE 503730C
- Authority
- DE
- Germany
- Prior art keywords
- current discharge
- galvanic elements
- galvanic
- elements
- tin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Stromableitung für galvanische Elemente Zusatz zum Patent 502 i8= Versuche haben gezeigt, daß sich die Korrosionsfestigkeit von Stromableitungen nach dem Hauptpatent noch weiter steigern läßt, wenn die Plattierung statt mit Zink mit einem elektronegativen Metall erfolgt. Als besonders widerstandsfähig hat sich Zinn erwiesen, das auch noch den Vorteil bietet, sich sehr gut weichlöten zu lassen. Die Zusatzerfindung besteht somit darin, daß die Plattierung statt mit Zink mit einem lötfähigen, möglichst elektronegativen Metall erfolgt.Current dissipation for galvanic elements Addendum to patent 502 i8 = Tests have shown that the corrosion resistance of current leads according to the main patent can be increased even further if the plating is carried out with an electronegative metal instead of zinc. Tin has proven to be particularly resistant, and it also offers the advantage of being very easy to soft-solder. The additional invention thus consists in the plating being carried out with a solderable, preferably electronegative metal instead of zinc.
Claims (1)